MDF manufactured from blends of cypress pine and radiata pine shows enhanced resistance to subterranean termite attack
2001 - IRG/WP 01-40214
Medium density fibreboards consisting of blends of the naturally durable wood species white cypress pine (Callitris glaucophylla) and non-durable wood species were manufactured in a commercial plant and subjected to a bioassay using the subterranean termite species, Coptotermes lacteus. A board composed of 30% cypress pine, 30% slash pine (Pinus elliottii) and 40% of the naturally durable hardwood...
P D Evans, S Dimitriades, C Donnelly, R B Cunningham


Chemical evaluation of borate treated pine sapwood attacked by the subterranean termite Coptotermes acinaciformis
1993 - IRG/WP 93-20003
Sapwood of hoop (Araucaria cunninghamii Ait. ex D. Don) and slash (Pinus elliottii Englem.) pines were treated by Vacuum Pressure Impregnation (VPI) to provide test specimens. The concentration of boron was defined by chemical analyses of the timber, in the zone of primary attack by the termite being bioassayed. A common method of definition of preservative retention, weight uptake of preservative...
A R Moffat, B C Peters


Effects of seed origin and site on both wood density and longitudinal fluid uptake of Sitka spruce (Picea sitchensis (Bong.) Carr.) with height in the tree grown in the United Kingdom
2002 - IRG/WP 02-40226
The variation in density and longitudinal fluid uptake was investigated in short specimens of wood taken from eight seed origins of Sitka spruce trees grown at two sites in the UK. Five trees of each seed origin at each site were sampled at three heights (1, 2 and 3 m above ground level). The density of the samples decreased with increasing height within the stem. This corresponded with increasin...
I Usta, M D C Hale


The critical moisture and temperature conditions for the growth of some mould fungi and the brown rot fungus Coniophora puteana on wood
1988 - IRG/WP 1369
The growth of some mould fungi on pine and spruce sapwood was studied in 40 different constant moisture and temperature conditions. The temperature range was between +10 and +40°C and the relative humidities varied from 76 to 100% relative humidity (RH). The incubation time was 12 weeks. The mixed mould inoculation used included typical fungi growing on wood: Aspergillus versicolor, Cladosporium ...
H Viitanen, L Paajanen


Hygroscopicity of decayed wood - Implications for weight loss determinations
1996 - IRG/WP 96-20085
Hygroscopicity changes were observed in red maple blocks subjected to brown rot, white rot and soft rot. Brown rot reduced hygroscopicity, soft rot increased hygroscopicity, and white rot showed only a very slight increase in hygroscopicity. The effect of these changes on weight loss tests is a slight overestimation of weight loss for brown rot and a slight underestimation for soft rot and white r...
S E Anagnost, W B Smith


Soft rot decay in acetylated wood. Chemical and anatomical changes in decayed wood
2002 - IRG/WP 02-40231
Acetylated Beech (Fagus sylvatica) and Scots Pine (Pinus sylvestris) wood were studied in soil beds under laboratory conditions for longer periods. High mass losses and dynamic MOE losses were measured in non-acetylated wood and at lower weight percent gains (WPG). Rapid losses of lignin, holocellulose and ?-cellulose occurred in non-acetylated beech wood and no losses were detected at the highest...
B Mohebby, H Militz


Effect of cyclic change of temperature on fungal growth and mass loss
1994 - IRG/WP 94-10065
For estimating the effect of cycling change of temparature on fungal growth, four Japanese species, sugi (Cryptomeria japonica), hinoki (Chamaecyparis obtusa), akamatsu (Pinus densiflora) and buna (Fagus crenata), four fungal species, Tyromyces palustris, Gloeophyllum trabeum, Coriolus versicolor, Pycnoporus coccineus, and five temperature conditions, 10, 20, 27, 35°C and cyclic temperature (20°...
K Suzuki, K Okada


The effect of extent and location of decay on strength loss in constructional timber
1994 - IRG/WP 94-30039
Radiata pine heartwood billets, 50 x 100 x 1000 mm³ were end-sealed and treated with copper-chrome-arsenate preservative (NZ Type I) to a range of retentions and penetration patterns. Cross-sections, 10 mm thick, were cut from the centre of each billet and used for determination of preservative distribution, for preservative analysis and for decay tests. The decay test consisted of laying samples...
M E Hedley, H Bier


Accelerated decay tests on DNBP-treated Pinus patula and Eucalyptus grandis
1987 - IRG/WP 3441
Blocks (10 x 10 x 5 mm³) of Pinus patula and Eucalyptus grandis were impregnated to 0, 1.5, 3.0 and 4.5 kg/m³ 2-sec-butyl, 4, 6 dinitrophenol (DNBP). They were monitored microscopically and for weight losses over 16 weeks against monocultures of Coriolus versicolor and Coniophora puteana. Treated ministakes (10 x 10 x 100 mm³) and blocks in soil contact were similarly monitored to determine wei...
L D Abraham, A A W Baecker


Assessment of wood decay in small-scale unsterile soil-bed tests
1997 - IRG/WP 97-20111
This study is concerned with the investigation of wood decay in small-scale unsterile soil-bed tests. Tests were performed with untreated heartwood samples from five hardwood species of different natural durability classes ranging from highly perishable to very resistant. Our results confirmed the critical role of soil moisture content on wood decay. The highest decay rates were observed at moistu...
L Machek, A M Derksen, R Sierra-Alvarez


Steam/hold/APM boron treatment - Treatability trials with green gauged radiata pine
1987 - IRG/WP 3439
Freshly sawn 100 x 50 mm radiata pine was green gauged, steam conditioned and preservative treated with a mixture of borax and boric acid using a modified Alternating Pressure Method (APM) treatment schedule. A 12 hour holding period between steam conditioning and treatment resulted in the necessary moisture loss and moisture re-distribution to facilitate treatment to NZ Timber Preservation Author...
P Vinden


Natural durability, density and extractive contents of 42 wood species of Bangladesh.
2003 - IRG/WP 03-10490
Natural durability, density and major extractive contents of 42 lesser used or unused wood species of Bangladesh have been studied. Correlation analysis between these properties has been performed. It has been shown that natural durability of these species neither explained by water soluble nor by alcohol benzene extractive contents. Density has a weak but significant positive correlation with dur...
S Akhter, K Akhter, S C Das


Natural progression of decay in unrestrained, Southern pine sapwood exposed above ground
1995 - IRG/WP 95-20060
In this study, the natural progression of decay is being monitored in 2.4-m (8-ft) lengths of dimension lumber. The 2.4-m lengths are supported without restraint in a horizontal plane approximately 0.75 m above ground in a partially shaded field plot in southern Mississippi. The lumber is 100% sapwood. Prior to installation in the field, each piece was planed to exactly 38 by 89 mm² (1.5 by 3.5 i...
R C De Groot, R J Ross, W Nelson


Application of a novel strength evaluation technique during screening of wood preservatives
1986 - IRG/WP 2262
The effectiveness of CCA and ACA in treated aspen mini stakes tested using a novel bag procedure, with unsterile soil fortified with Chaetomium globosum and Ceratocystis albida, is reported. Good agreement between toxic limits determined using the standard weight loss procedure, and those determined by the strength technique were found, with some indication that the strength loss method is more se...
J N R Ruddick


Evaluation of wood durability by laboratory test - A new equation to predict wood durability
2001 - IRG/WP 01-20230
To estimate the wood durability in a short term, periodical weight determination was carried out in a laboratory test. This test provided the results comparable to those of the field test and the fungus cellar test, but it required much more jobs in comparison to the usual accelerated laboratory test. To save the time and jobbing for this method, a new equation was devised from simple two assumpti...
I Momohara, K Yamamoto


Eucalyptus globulus. Impregnability in relation with plantation and crop
1992 - IRG/WP 92-2402
Eucalyptus globulus Lasill is currently classified in Pr EN 350 on the basis of the characteristics of the first log. In practice, there are usually several following crops of branches developped on each stump in plantations. Up to a diameter of 8 cm, round wood of 2nd crop and further crops present a maximum of sapwood and characteristics which differ significantly from the basic classification a...
D Dirol


Dip-diffusion of dressed timber - Effect of drying
1990 - IRG/WP 3603
The effect of drying on BFCA dip-diffused, dressed, freshly sawn timber was determined by the depth of penetration of boron achieved on two test timber species, White Cheesewood (Alstonia scholaris) and Light Hopea (Hopea papuana). The results obtained showed that the light density White cheesewood was completely penetrated even after 3 days drying while Light Hopea, treated immediately achieved 5...
H C Konabe


A technique for the rapid assessment of wood surface degradation during weathering
1987 - IRG/WP 2281
Radiate pine (Pinus radiata D. Don) sapwood samples taken from four trees were converted into thin strips 100 x 10 x 0.085 (85 µm) mm³, (longitudinal x radial x tangential) in size and exposed in preweighed hatches to the weather inclined at 45° facing equatorially for 10, 20, 40, 60, 80 and 100 days. Significant (P < 0.001) weight losses occurred with time over the exposure period. Differen...
P D Evans, D Abbott, S Thein


A novel guide for the determination of the physical properties of wood including kiln drying and full-cell preservative treatment
2004 - IRG/WP 04-20298
An ideal flow chart for the sequential experimental determination of a range of physical properties relevant to wood drying and subsequent preservation was designed as a novel guide to assist wood scientists. In this manner, data assembly and experimental processing are shown. This was designed according to experience and published literature. Aspects emphasised in this review were the physical p...
I Usta, M D C Hale


Variation in natural durability of British grown Douglas fir ((Pseudotsuga menziesii (Mirb.) Franco). Part I. Effect of density and growth rate
2002 - IRG/WP 02-10445
Seed origin trials of Douglas fir (Pseudotsuga menziesii) in Britain have provided important information on growth differences between origins (Lines, 1987), but the variation in wood properties between origins has not been reported. The present paper describes a study of the variation in natural durability against two brown rot fungi (Coniophora puteana and Postia (Poria) placenta) and in a fung...
S Akhter, M D C Hale


IUFRO rating system compares favourably to weight loss for soil-bed testing
1990 - IRG/WP 2343
The soil-bed/small stake test is commonly used for rapidly evaluating the performance of new, more environmentally acceptable, preservatives. In a 1.5 year experiment with three copper-based waterborne preservatives, visual evaluation and probing using the IUFRO performance rating scale (0-4) gave very similar toxic thresholds to those derived from measurement of weight loss at the end of the expe...
P I Morris


Soluble nutrient influences on toxicity and permanence of CCA preservatives in wood
1980 - IRG/WP 3144
The influence of soluble carbohydrate and nitrogenous components concentrated at evaporative surfaces of wood on the toxicity and permanence of CCA preservatives has been examined using soil-burial techniques. Nutrient concentrations in lime (Tilia vulgaris Hayne) have been shown to be associated with reduction of toxic limits of preservatives to an extent in which a 100% increase in preservative ...
B King, G M Smith, A Bruce


Treatment of poplar plywood with solvent and water-borne preservatives
1989 - IRG/WP 3538
Poplar as a light hardwood is appropriate for plywood production. Owing to its low natural durability it is generally recommended to preserve it in all conditions where risks of fungal attack may be present. A research project has been carried out on preservative treatments of plywood commodities. Parameters studied were various treatment cycles, three types of plywood, and a number of solvent and...
J Van Acker, M Stevens


Laboratory testing of wood natural durability - In soil-bed assays
1998 - IRG/WP 98-20141
Laboratory methods for assessing wood decay resistance are being investigated in the framework of an ongoing European research project. This paper summarizes the main results obtained for soil-bed tests based on the European prestandard ENV 807-Test 2. The data suggest that this testing methodology is suitable for evaluating the natural durability of timber species in soil-contact under conditions...
R Sierra-Alvarez, I Le Bayon, J K Carey, I Stephan, J Van Acker, M Grinda, G Kleist, H Militz, R-D Peek


On the laboratory use of X-rays in timber decay evaluations
1981 - IRG/WP 2144
The paper reports the results of laboratory experiments on the X-raying of some Pinus radiata sapwood blocks infected with Serpula lacrymans to determine the effect of density and moisture content on the absorption of X-rays by wood. It is concluded that with increasing moisture content there is a very marked increase in time required to pass a constant quantity of X-rays through a test block and ...
J D Thornton, J W Creffield, O Collett