IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 110 documents. Displaying 25 entries per page.


Termite resistance of copper-based preservative supplemented aspen strandboards
2012 - IRG/WP 12-30594
Termite resistance of aspen strandboards treated with various copper-based preservative systems was evaluated in field exposure tests. Five copper-based chemicals or zinc borate were blended into aspen furnish at three retention levels prior to pressing. Tebuconazole or 4,5-dichloro-2-N-octyl-4-isothiazolin-3-one (DCOI) were added as co-biocides to selected copper-based treatments. Sections from...
J J Morrell, C Vidrine, A Preston, L Jin


Service trial of different materials exposed in jetties at Öresund. Progress report No. 5
2022 - IRG/WP 22-30764
This report contains results of the fifth inspection on the performance of different decking materials – preservative-treated wood, modified wood, natural durable wood, re-cycled plastics and wood-plastic composites (WPCs) - available on the market and exposed since 2013 (some since 2014 and 2016) by the City of Malmö in two jetties near the Øresund Bridge, south of central Malmö in Sweden. T...
J Jermer


The decay resistance of chemically modified aspen composites to the white rot fungus Coriolus versicolor (L.) Quelet
1998 - IRG/WP 98-40122
Chemical modification of Aspen wood (Populus tremula L.) in the form of solid wood, veneers and sawdust was undertaken by a two step procedure consisting of esterification with maleic anhydride (MA) and subsequent oligoesterification with MA and glycidyl methacrylate (GMA) or allyl glycidyl ether (AGE). Modified wood was thermoplastic and was thermally formed by hot-pressing to produce veneer or s...
M C Timar, A J Pitman, M D Mihai


Biological Durability of Laminated Veneer Lumber from Durable and Non-Durable Wood Species
2005 - IRG/WP 05-10567
Laminated Veneer Lumber (LVL) was laboratory manufactured using veneers from decay and non decay resistant species in order to evaluate changes in the durability as a result of the LVL manufacturing process, and to test if the mixing of decay resistant species and non decay resistant species can improve durability. Laboratory soil block test and field test were conducted. The durability of solid w...
P Nzokou, J Zyskowski, S Boury, D P Kamdem


Ultrastructure of the attack of a naturally durable timber by tunnelling bacteria
1990 - IRG/WP 1462
The attack of the wood of Eusideroxylon zwageri, a naturally durable species, by tunnelling bacteria (TB) was examined by light microscopy and transmission electron microscopy. Observations were made primarily on fibres. Parenchyma were included in some cases. Both fibres and parenchyma are rich in extractives. In fibres, extractives are primarily present in the lumen. The amber colouration of fib...
A P Singh, T Nilsson, G F Daniel


About the water and biological resistance of some new chemically modified wood composites
1997 - IRG/WP 97-40077
As well known, wood represents a valuable natural composite material with a very large utilisation as solid wood or in wood based composite materials. Its qualities but also its defects as the dimensional instability, the susceptibility to biological attack, the anisotropy, are due to its complex structure. Research has demonstrated that the chemical modification of wood, meaning the involving of ...
M C Timar, M D Mihai, G Baciu


Biocide Treatments for Wood Composites - A Review
2006 - IRG/WP 06-40323
This paper reviews the biocidal treatment of wood composites. Included are in-process and post-process treatments. Various biocides are covered as are methods of application. Novel treatments and technologies are also presented....
J W Kirkpatrick, H M Barnes


Durable fibre for durable MDF – testing Tricoya®
2015 - IRG/WP 15-40704
The chemical modification of wood has been a commercial reality for a decade on release of technologies for the modification of solid wood including Accoya®. A challenge and an opportunity for the modification technologies which typically impart dimensional stability, water stability and enhanced biological durability was the adaptation of the technology to wood based panels. This paper presents ...
E Suttie, J Alexander, M Maes


Estimation of service life of durable timber species by accelerated decay test and fungal cellar test
2002 - IRG/WP 02-20249
Many kinds of durable wood species for outdoor uses has been imported from all over the world to Japan. However information on the natural durability of these species is not sufficient to estimate the service life of them in the climate of Japan. Highly durable species such as Jarrh, Teak, Ipe, Ekki, Selangan batu, Red wood, Western red cedar showed no significant percent mass losses by accelerate...
K Yamamoto, I Momohara


Leaching of chromium and other cca components from wood-cement composites made with spent CCA treated wood
2000 - IRG/WP 00-50153
Wood cement composites are an attractive option for recycling spent treated wood, since the CCA treatment enhances the physical, mechanical and biological resistance properties of the composite. However, we have noted a higher than normal leaching of chromium from these products and this appears to result from conversion of some of the trivalent chromium to the more leachable and toxic hexavalent ...
D Qi, P A Cooper


Ancillary properties of vapor boron-treated composites
2001 - IRG/WP 01-40210
This paper discusses the water absorption, thickness swelling, and internal bond strength of North American composites treated using a vapor boron treatment process. For oriented strandboard, high boron loadings led to lower internal bond strength and lower thickness swelling. Water absorption results were variable but no deleterious effect of treatment was noted. For medium density fiberboard, th...
W A Jones, H M Barnes, R J Murphy


Ekki heartwood - is “Durable”
2002 - IRG/WP 02-10444
Severe decay damages of bridges made of ekki (Lophira alata Banks) wood which is classified as a durable species in the EN 350:2 as already reported at the 31 IRG annual meeting. This paper deals with results of long-term decay tests of ekki heartwood specimens using 3 isolates (Loweporus tephroporus 2 strains and a fungus of other sp. from damaged ekki bridges) and Trametes versicolor as a refere...
S Doi, R Itoh, S Horisawa


Leachability of borate-modified oriented strandboard: A comparison of zinc and calcium borate
2002 - IRG/WP 02-40232
The leachability of boron in zinc and calcium borate-modified oriented strandboard (OSB) was investigated in this study. The leaching experiments were conducted by exposing edge-sealed OSB samples under running water for 8, 24, 72, and 216 hours. The results were compared with those from the unleached controls. Boron leaching of the modified OSB occurred upon the initial water exposure, and the le...
S Lee, Q Wu


Sustainability Through New Technologies for Enhanced Wood Durability. COST Action E37 – A New Action in the Forestry Domain
2004 - IRG/WP 04-40293
The main overall objective of the action is to concentrate on the contribution of wood durability on the sustainability through the development of systems for quality assurance and perfoamance of modified wood and wood products as alternatives to wood treated with traditional preservatives. By this means it seeks to improve and consequently increase the cost-effective use of sustainably produced E...
R-D Peek


The attack of naturally durable and creosote treated timbers by Limnoria tripunctata Menzies
1995 - IRG/WP 95-10132
Limnoria tripunctata was found tunnelling in creosote treated Douglas fir (Pseudotsuga menziesii) pilings and naturally durable greenheart (Ocotea rodiaei) gate seals at two sites on the south coast of the United Kingdom. Examination of thc creosote-treated wood showed that Limnoria tunnels were concentrated at a depth of 2-3 cm from the timber surface, where creosote loading was lower. Fewer tunn...
A J Pitman, G S Sawyer, G F Daniel


Termite Response to Agricultural Fiber Composites: Hemp
2005 - IRG/WP 05-10548
Industrial hemp, Cannabis sativa, is a fiber usable in manufacture of nutritional products, rope, textiles, paper and building products. Due to the illicit recreational uses of Cannabis sativa varieties with high tetrahydrocannabinol content (marijuana), hemp is not grown commercially in the United States. However, it is grown in many other nations, and has been proposed as a replacement for sugar...
J K Grace


The colonization of selected naturally durable timbers by marine fungi and borers
1977 - IRG/WP 439
In recent years, concrete and metal have been widely substituted for wood in contact with sea water, but wood products have not lost their usefulness under such conditions. In many cases, wood if sound and durable, may prove to be the most practical and economical of materials used in sea water exposure. Timber when immersed in the sea may be attacked by micro-organisms (bacteria and fungi) and ma...
S E J Furtado, E B G Jones


Termite response to Agricultural Fiber Composites: Bagasse
2005 - IRG/WP 05-10549
Bagasse, or sugarcane rind, is a fibrous by-product of sugar extraction from sugarcane, Saccharum officinarum L. Bagasse fiber performs similarly to hardwood fiber in composite board products. In laboratory studies, Formosan subterranean termites survived as well on a diet of Bagasse as on Douglas-fir wood. Field tests with a compressed Bagasse panel (produced by heat extrusion) indicated that ter...
J K Grace


Durability of Wood Plastic Composites Relative to Natural Weathering and Preservative Treatment With Zinc Borate
2005 - IRG/WP 05-40316
Wood-Plastic Composites (WPCs) used for decking have experienced dramatic increases in North America, averaging 25% growth per annum since 1998. A key factor contributing to this growth has been the successfully communicated message that they are "virtually maintenance free". The common perception being that the wood fiber is completely encapsulated by the thermoplastic resin, minimizing the pot...
M E Mankowski, F M Ascherl, M J Manning


Wood-based composites exposed to fungal degradation: Laboratory results
2001 - IRG/WP 01-40215
Oriented strandboard (OSB) and laminated veneer lumber (LVL) are widely used as residential construction materials. The durability of OSB and LVL against biological degradation has not been studied comprehensively. The objective of this research was to investigate the durability of OSB and LVL when exposed to wood decay fungi. Fourteen brown-rot and eight white-rot wood decay fungi were screened f...
V W Yang, B Illman, L A Ferge, R J Ross


Thermal modification of non-durable wood species 1. The PLATO technology: thermal modification of wood
1998 - IRG/WP 98-40123
The PLATO technology is an innovative upgrading technology with low environmental impact, which can be applied to fast grown and non-durable wood species. This technology is based on a thermal modification of solid wood without the addition of chemicals (e.g. preservatives), consisting of a hydrothermal treatment, followed by drying and curing. The PLATO technology results in a substantial improve...
M J Boonstra, B F Tjeerdsma, H A C Groeneveld


Bending & tensile properties of vapor boron-treated composites
2002 - IRG/WP 02-40228
North American composites including laminated veneer lumber, oriented strandboard, and medium density fiberboard were treated by vapor boron technology and subsequently tested in static bending. Tensile properties were also determined for the two composite boards. The study was designed as 3 x 2 factorial with three treatment levels and two mill locations for each composite type. In general, mil...
H M Barnes, R J Murphy, B K Via


Comparison of three methods for assessing the in-ground termite resistance of treated timber, durable timber and plastics at sites in Australia, USA and Thailand - First results
1998 - IRG/WP 98-20132
The in-ground resistance of materials to attack by subterranean termites is most commonly assessed with one form or another of the conventional graveyard method, despite the significant shortcomings of this method. In Australia, an alternative method, in which all samples of test materials are placed below-ground, has been in use for more than 10 years. The method provides reliable exposure of sam...
M Lenz, A F Preston, J W Creffield, K J Archer, B M Kard, C Vongkaluang, Y Sornnuwat


The practice of using concrete on wood piling for marine use in Thailand
1982 - IRG/WP 492
The practice of using concrete on wooden poles has been carried on in Thailand for a long time in pile-houses and pier constructions which have been situated in, or partly in the sea. In such instances, the hewed round and/or square-sawn heartwood poles of naturally durable timber species have been coated with concrete of about 5 to 10 cm or more in thickness, and to about 100 cm above the highest...
B Anuwongse


Evaluation of chlorpyrifos and fungicides alone and in combination for control of insects and fungi in wood and wood composites
1998 - IRG/WP 98-30187
Wood composites are rapidly being adapted for use in exterior applications. The incorporation of a preservative system to prevent fungus and insect attack is necessary with most exterior composites. Research studies were reviewed pertaining to organic preservative systems based on Lentrek* insecticide wood treatment which contains the active ingredient chlorpyrifos alone and in combination with te...
M P Tolley, P E Laks, R Fears