Natural Weathering of Coated Oil Heat Treated Wood
2007 - IRG/WP 07-30440
Oil heat-treated (thermally modified) pine wood was coated with 9 different types of solvent- or water-borne exterior finishes. The systems with modified wood substrate as well as unpainted and painted non-modified controls were exposed to weathering (EN 927-3) on two locations with sub-alpine and alpine climate. The influence of natural ageing on surface systems was evaluated after one year of ex...
M Petric, B Kricej, M Pavlic, A Rapp
Bi-oleothermal treatment of wood at atmospheric pressure: resistance to fungi and insects, resistance to weathering and reaction to fire results
2008 - IRG/WP 08-40418
Bi-oleothermal process is a simple treatment which has been developped by CIRAD in cooperation with FCBA. It allows a deep impregnation of wood with hydrophobic products using cheap facilities. The process includes two steps at atmospheric pressure. The first one is a dipping of wood samples in a hot oil bath (between 110 °C and 200°C) which creates an overpressure inside the wood. The second on...
L Podgorski, I Le Bayon, I Paulmier, J-D Lanvin, V Georges, D Grenier, H Baillères, J-M Méot
Continuous moisture measurement (CMM) to detect failure of moisture resistance
2009 - IRG/WP 09-20422
A wood coating system will fail to perform properly after a certain time of weathering. From that moment, the substrate is especially prone to fungal attack. Moisture plays a key role on weathering performance, wood protection efficacy and decay susceptibility of wood. Therefore, knowledge of the moisture dynamics of the applied wood protection is of significant importance in the prediction of the...
I De Windt, J Van den Bulcke, J Van Acker
Weathering of Wood Modified with the N-Methylol Compound 1,3‑dimethylol-4,5-dihydroxyethyleneurea (DMDHEU)
2009 - IRG/WP 09-40467
Scots pine (Pinus sylvestris L.) sapwood boards were treated with a methylated 1,3‑dimethylol-4,5-dihydroxyethyleneurea (mDMDHEU) causing weight gains of approx. 25% and exposed to weathering for 18 months. Compared to untreated boards, treatment with mDMDHEU reduced surface discoloration mainly caused by staining fungi. Boards treated with mDMDHEU exhibited clearly lower moisture content th...
C Mai, Yanjun Xie, A Krause, K Urban, P D Evans, K Richter, H Militz
A fast and economic method to produce grey wooden surfaces for decking and cladding: preliminary results
2009 - IRG/WP 09-40474
Uncoated wood is commonly used in France for cladding and decking to minimise maintenance. However wood surfaces progressively turn grey due to exposure to sunlight and water. This grey colour develops after several months depending on the wood species and the exposure: in the northern hemisphere surfaces facing south and west are most exposed and turn grey more rapidly than those facing north and...
L Podgorski, V Georges, I Garmendia, B Sánchez Sarachu
Wet and dry adhesion of coatings on modified and unmodified wood: comparison of the pull-off test and the cross-cut test
2010 - IRG/WP 10-40524
The objective of this paper is to study the influence of several types of modification (acetylation, furfurylation, thermal modification) on coatings adhesion and to compare two methods of assessing the adhesion: the cross-cut test and the pull-off test both tested in dry and wet conditions. The study also investigates the effect of other parameters of the wood substrates on adhesion like the ring...
L Podgorski, G Grüll, M Truskaller, J D Lanvin, V Georges, S Bollmus
Silicon compounds as additives improving alkyd-based wood coatings performance
2010 - IRG/WP 10-40531
The reactivity of cellulose with solvent-born alkyd-based wood coatings supplemented with organosilanes was analyzed. Structural analysis of cellulose subjected to the reaction with organosilanes and following extraction with water was performed using Fourier-transform infrared spectroscopy (FTIR). The analyzed IR spectra comprise bands 1250 cm-1 typical for the SiC group and 800 cm-1 typical for ...
B Mazela, I Ratajczak, K Wichłacz-Szentner, P Hochmańska
Aesthetic service life of coated and uncoated wooden cladding - influencing factors and modelling
2011 - IRG/WP 11-20470
Mould growth on exterior coated cladding façades is an undesirable element and will often shorten the aesthetical service life. Mould growth on painted surfaces is influenced by type and concentration of film fungicides, the paint formulation and the wood substrate itself, and wooden cladding may experience exponential fungal deterioration caused by variation in the climatic factors, often within...
L Ross Gobakken, O A Høibø
Moisture protection and performance during 5 years exposure of 19 wood coating systems on a cladding in Vienna
2011 - IRG/WP 11-40561
A cladding with vertical boards of Norway spruce (Picea abies) comprising different coating systems had been exposed to natural weathering oriented south west in Vienna for 5 years. Weathering behaviour of the boards was assessed in intervals and wood moisture content was measured over the first 22 months of exposure. The moisture protective properties of the coating systems were assessed using la...
G Grüll, I Spitaler, M Truskaller
Wet and dry adhesion of coatings on modified and unmodified wood: influence of 18 months of natural weathering on the pull-off test and cross-cut test results
2011 - IRG/WP 11-40569
The objective of this paper is to study the influence of several types of modification (acetylation, furfurylation, heat treatment) on coatings adhesion after 18 months of natural weathering according to EN 927-3 in Vienna (Austria).
The paper compares two methods for assessing the adhesion: the cross-cut test (EN ISO 2409) which is the conventional method used and recommended in EN 927-3 and th...
L Podgorski, G Grüll, M Truskaller, J D Lanvin, S Bollmus
Water uptake of wood surfaces with and without coating: influence of weathering
2012 - IRG/WP 12-40580
The objective of this study was to compare liquid water absorption of wood surfaces with and without coating, before and after artificial weathering. Samples of spruce, oak and sapelli were exposed to the EN 927-6 cycle for 1500 and 1850 hours and to the weathering produced by the Garner wheel for 1000 hours. Two highly pigmented coatings (solventborne and waterborne) and two semi-transparent stai...
L Podgorski, S Collignan, J D Lanvin
Protective nanoparticle coating reducing water absorption of wood species
2012 - IRG/WP 12-40614
Nanoparticle coatings were deposited onto different tropical wood samples for controlling the surface hydrophobicity. The styrene(maleimide) nanoparticles were synthesized in aqueous dispersions under pure conditions or in combination with 70 wt.-% palm oil. A first evaluation of the non-coated wood surfaces indicates a high dependence between the water contact angles, the average surface roughnes...
P Samyn, A Paredes, G Becker, H Van den Abbeele, L Vonck, D Stanssens
Detection of Aureobasidium as the dominant fungus on coated wood
2013 - IRG/WP 13-10796
Wood is often covered with a coating in order to protect the surface. Unwanted dark mold growth on paint covered surfaces in external conditions is a familiar phenomenon. Simple microbial techniques have commonly been used to determine the dominant fungal species present in the discoloured area, for example morphological analysis of microscopic preparations of fungal pieces sticking to an adhesive...
E J Van Nieuwenhuijzen, M F Sailer, R A Samson, O C G Adan
Copper Coating on Wood: a New Way of Protecting Wood
2013 - IRG/WP 13-30617
Thermal spray metal coating technology was used to apply a thin layer of copper on the surfaces of a number of wood species. The adhesion of metal coating to mahogany, oak, soft maple, spruce, white pine and medium density fibreboard (MDF) was evaluated by pull off adhesion test. The resistance of copper coated wood samples to mildew were assessed in the lab. Also, the decay resitance and water re...
M Nejad, R Shafaghi, L Pershin, J Mostaghimi, P Cooper
Study of UV resistance and natural weathering of coatings on chemically modified wood
2013 - IRG/WP 13-40629
In this study, UV resistance and weathering performance of rubberwood (Hevea brasiliensis) and radiata pine (Pinus radiata) modified with benzoyl chloride and acetic anhydride was studied. Performance of polyurethane based wood coatings on modified wood was also evaluated. Unmodified and chemically modified specimens were exposed to accelerated and natural weathering. Modified and unmodified woo...
K K Pandey, K Srinivas
Influence of coatings on water uptake of wood surfaces before and after natural and artificial weathering
2013 - IRG/WP 13-40641
Liquid water absorption of wood surfaces with and without coating, before and after exposure to artificial and natural weathering has been studied. Spruce, oak and sapele samples have been exposed to the cycle of EN 927-6, to the cycle of the Gardner wheel and to natural weathering. Five coatings were tested including solventborne and waterborne, semi-transparent and opaque products. Exposure to w...
L Podgorski, S Collignan, J-D Lanvin
Using hyperspectral imaging to detect and quantify mould and blue stain on coated and uncoated wood
2014 - IRG/WP 14-10822
Hyperspectral imaging has been applied on the surface of samples of coated and uncoated Norway spruce (Picea abies) as a new technique to detect and quantify growth of mould and blue stain fungi. Principal Component Analysis of the hyperspectral images resulted in a clear visualization of the fungi and the amount of mould coverage could be estimated. This indicates that NIR hyperspectral imaging c...
L Ross Gobakken, I Burud, A Flø, K Kvaal, T K Thiis
Modern Instrumental Methods to Investigate the Mechanism of Biological Decay in Wood Plastic Composites
2014 - IRG/WP 14-40674
Various instrumental techniques were used to study the fungal decay process in wood plastic composite (WPC) boards. Commercial boards exposed near Hilo, Hawaii (HI) for eight years in both sun and shadow locations were inspected and tested periodically. After eight years of exposure, both boards were evaluated using magnetic resonance imaging (MRI), while a selected area of the board exposed in sh...
G Sun, R Ibach, M Gnatowski, J Glaeser, M Leung, J Haight
Lignin Modification to Produce Sustainable Polyurethane Resin for Wood Coatings
2014 - IRG/WP 14-40682
The use of lignin as the most abundant aromatic natural polymer has been evaluated for use in the production of lignin-based polyurethane resin for coating applications. Coatings are made of resins (ca. 50%), which today are mainly derived from petroleum-based polymers. This study is focused on the development of an environmentally friendly method of modifying lignin to be used as source of natura...
M Nejad, M Arefmanesh, S Chandra, J Mostaghimi, E Master
Acceptance levels of surface disfigurement - tolerance to defects of coated wood
2015 - IRG/WP 15-20564
Service life planning (PSL) has become an important issue in performance based building and substantial progress has been made in recent years. The role of predicting the aesthetical service life of wooden building components has been underestimated for quite long time but is recently attracting more and more notice. It is influenced by numerous factors such as discoloration, fading, flaking, crac...
C Brischke, P Kaudewitz
Application of nanoparticles of silver and nanoparticles of titanium dioxide in reinforcement of wood and coating for wood in Costa Rica
2015 - IRG/WP 15-40698
Wood is one of the most widely used materials in last 20 years by society in many applications, with a considerable proportion of this material coming from forest plantations. Plantations usually produce timber with reduced strength properties and low natural durability. On the other hand, nanotechnology applications have the potential to increase wood properties. Likewise, nanotechnology cannot o...
A Berrocal Jiménez, R Moya Roque, A Lucrecia Rodríguez, J R Vega Baudrit
Investigation of Dimensional Stability and Coating Performance of Different Heat-Treated Poplar Wood Before and After Accelerated Aging
2015 - IRG/WP 15-40702
In this investigation, coating performance of heat-treated poplar wood (Populus tremuloioes) in different environments, before and after accelerated aging was studied. Specimens with 150×100×20 mm and 20×20×20 mm in dimensions were prepared. Heat treatments were performed in air, steam and linseed oil media. Specimens were coated by alkyd based stain. Adhesion strength before and after aging, ...
A Talaei, D Ansari Movahed, G Rassam
Engineering for Rural and Civil Development. Uni Performance of wood exterior structures above ground contact in Spain built with softwood species. The situation of cases in northern Spain
2016 - IRG/WP 16-20597
Across Europe is very common to find exterior structures build in sawn and glue-laminated wood. Most of these exterior structures used softwood wood species such as fir, spruce, larch and pine. In Spain wood exterior structures, as for example bridges, became more and more popular since eighties, when sawn and glue-laminated wood were utilized for building exterior wooden structures in overall Spa...
D Lorenzo, J Fernández-Golfín, M Touza
Accelerated Weathering Performance of Impregnated Wood Samples Coated with Zinc by Means of Plasma-Assisted Particle Deposition
2016 - IRG/WP 16-30682
Many different methods are currently applied for wood protection against outdoor conditions. The most important of these is the process of impregnation with liquid substances. However, this kind of wood preservatives cannot provide a long-term protection of wooden surfaces. Weathering-resistant surfaces can be obtained by applying UV absorbing agents. In this study, the influence of zinc particles...
A Can, H Sivrikaya
Variation in coating hardness during the EN 927-6 weathering test: influence of pigmentation
2016 - IRG/WP 16-40739
The objective of the SERVOWOOD project is to develop and establish European Standards that will facilitate the prediction of service life for exterior wood coatings. Within this project an extensive round robin exercise has been carried out by five partners to establish the repeatability and reproducibility of the EN 927-6 artificial weathering test. This round robin included the exposure of the I...
L Podgorski, L Malassenet, C Reynaud