Treatability of waterstored poles of Norway spruce by sap-displacement and pressure treatment with Boliden K33 and creosote
1973 - IRG/WP 328
Poles of windthrown Norway spruce were stored in bark under water sprinklers for 11-20 months or fully submerged in a lake for 3 years (tab. 1 and 2). Water content after storage is shown in fig. 1 and 8. Treatment with Boliden K33 by sap-displacement (open tank suction) gave a poor result. The Danish requirements of delivery claim a penetration of 20 mm and a net retention of 12 kg/m³ in outer 2...
P Moltesen, E Borsholt, B Bang


Copper storage in the digestive caecae of Limnoria tripunctata and Limnoria quadripunctata (Crustacea: Isopoda) tunnelling in CCA treated and untreated wood in laboratory cultures
1998 - IRG/WP 98-10257
Digestive tract tissues of Limnoria quadripunctata Holthuis and Limnoria tripunctata Menzies, tunnelling untreated and CCA treated Scot's pine sapwood under laboratory conditions were examined using X-ray microanalysis and transmission electron microscopy. Populations of both Limnoria species tunnelling treated and untreated wood stored copper within their digestive caecae in the form of ...
C Wykes, A J Pitman, S M Cragg


A field test with anti-sapstain chemicals on sawn pine timber stored and seasoned under different conditions
1984 - IRG/WP 3245
Newly sawn timber of European redwood (Pinus sylvestris L.) was dip treated in four different anti-sapstain chemicals. The protectife effect against sapstain, mould and decay was examined after 10 weeks' and 10 months' storage in open and closed stacks. The results showed that the performance of individual chemicals was different in open and close stacks, although the wood as wel...
D J Dickinson, B Henningsson


The use of propionic acid to prevent Pinus patula biodeterioration during outside chip storage in Zululand
1989 - IRG/WP 3531
Pinus patula SCHIEDE ET DEPPE IN SCHLD. ET CHAM. is susceptible to biodeterioration during outside chip storage (OCS), reducing pulp quality and tear and burst indices of resulting paper. Accelerated laboratory trials showed that chips treated with 2% (w/v) propionic acid and stored for 17 weeks, produced pulp of quality indistinguishable from fresh untreated chips. Pulp tests during field trials ...
S Ismail, E J Smith, A A W Baecker


Bacterial brown stain on sawn timber cut from water-stored logs
1992 - IRG/WP 92-1532
Brown stains which appear on the surface of sawn radiata pine cut from water-stored logs were identified as tannin-like compounds. They are derived from bacterial breakdown of flavanoid-glucosides. When timber is sawn from infected logs, the free flavanoids migrate to the wood surface as the timber dries. There, they condense and oxidise to form permanent brown discolourations. Stains occurred on ...
M E Hedley, R Meder


Prevention of creosote bleeding from treated Scots pine poles
1970 - IRG/WP III 3B
Creosote, the most widely used preservative for pressure treatment of Electricity Board and GPO transmission poles in the United Kingdom has, when correctly applied, given good performance over a long period of time. Perhaps its only disadvantage as a preservative in the above fields is its tendency to exude or 'bleed' from a proportion of treated poles upon exposure to solar hea...
Anonymous


Kinetics and mechanism of fixation of Cu-Cr-As wood preservatives. Part 5: Effect of wood species and preservative composition on the leaching during storage
1975 - IRG/WP 354
Conversion reactions during storage of CCA treated wood take place even at and below the fiber saturation point as long as ion transport is possible. Increase in drying temperature increases the final pH of the treated wood and the leachability of Cu and decreases slightly the leachability of Cr, while the leachability of As is not affected. This temperature effect is considered to be of no techni...
S-E Dahlgren


Optimun storage period for the boron diffusion treatment of rubber wood
1996 - IRG/WP 96-30121
The study determined the maximum thickness of rubber wood that can be diffusion treated and the effect of diffusion storage period on the distribution of chemicals in treated wood of various thicknesses. Wood of thickness up to 50 mm can be easily diffusion treated with 10% boric acid equivalent (BAE) solution to adequate loading of chemicals. The optimum diffusion storage period to get uniform an...
T K Dhamodaran, R Gnanaharan


The use of spruce for transmission poles
1973 - IRG/WP 326
A series of preservative treatments with creosote using Lowry and Rueping schedules was undertaken. From these treatments the most suitable impregnation conditions for water stored Sitka spruce (Picea sitchensis) and Norway spruce (Picea abies) transmission poles were determined. Preservative distribution and permeability values for poles of both species were used to decide the optimum season and ...
J A Dunleavy, D J Balfe, J P Prendergast


Water-storage for improving the permeability of sugi (Cryptomeria japonica D. Don)wood
1999 - IRG/WP 99-40129
The viable bacterial counts in sapwood and intermediate wood of sugi bolts increased immediately after floated in a fresh water pond. Bacterial invasion into the heartwood was not detected apparently during water-storage for 36 weeks, although a few bacterial species have inhabited in freshly-cut heartwood samples. The bacterial species isolated from the water-stored bolts were almost Gramnegative...
S Ohta, S Doi


The wood-attacking insects in wooden houses of an old open air museum in southern Finland
1989 - IRG/WP 1409
Harmful insects of wood in a open-air museum were investigated in 1985-1988 by order of the National Board of Antiquities and Historical Monuments of Finland in nine old log houses. Many thousands of insects and altogether 1073 anobiids (Coleoptera, Anobidae) were obtained by window and light traps. The most common Anobiidae-species were Hadrobregmus confusus (Kraatz) 60.3%, Hadrobregmus pertinax ...
H Viitanen, M Pulkkinen


A shower test protocol for measuring antisapstain wash-off from small individual log billets
1996 - IRG/WP 96-50069
According to New Zealand Timber Industry Federation statistics New Zealand exported 4,835,000 m³ of logs in 1994 and it is estimated that c. 20% were anti-sapstain treated. Loss of preservative from logs as a result of rain impact after application is of considerable concern both with respect to potential loss of efficacy and environmental contamination. Whilst Environment Canada have a proposed ...
A J Pendlebury, H Pearson


The effect of water storage on the cell-structure of Sitka spruce (Picea sitchensis) with reference to its permeability and preservation
1970 - IRG/WP III 3A
Commercial treatment trials with full sized transmission poles have shown that water storage considerably improves the permeability of Sitka and Norway spruce. These results were confirmed by laboratory measurements which showed that in the sapwood of ponded Sitka spruce there is a vast improvement in permeability in all three grain directions. Heartwood permeability does not seem to be affected t...
J A Dunleavy, A J McQuire


Preservative treatment of wood by diffusion processes - Simulation of commercial treatment processes
1988 - IRG/WP 3498
Spruce (Picea abies), Scots pine (Pinus sylvestris) and birch (Betula pendula) were preservative treated by diffusion with mixtures of copper sulphate and arsenic pentoxide. The preservative was fixed after a suitable diffusion storage period by soaking in ammonia solution. A high standard of treatment could be achieved in spruce sapwood. This was attributed to its low wood density, and high wood ...
P Vinden


Timber preservatives and corrosion
1983 - IRG/WP 3228
A survey of preservative treated timber commodities has illustrated problems that may be caused by corrosion. After treatment, timber should be compatible with commonly used fasteners. Whilst many corrosion methods have been used in the past, no standardized method is used by workers in timber preservation. The Queensland Department of Forestry is developing laboratory test methods for assessing c...
R I Davis


Ponding of radiata pine (Pinus radiata) - 2. The effect of ponding on coating penetration into wood
1998 - IRG/WP 98-10249
Radiata pine (Pinus radiata) wood panels which had been ponded for periods ranging from 2 to 12 weeks, dried and subsequently coated with a primer and examined by light microscopy after staining sections with Sudan IV to enhance the contrast of the primer material. A correlation between the extent of ponding and the extent of coating penetration into wood was observed. The coating penetration var...
A P Singh, S S Gallagher, U Schmitt, B S Dawson, Yoon Soo Kim


Time limits for holding logs to achieve successful antisapstain treatment
1997 - IRG/WP 97-30126
The purpose of these trials was to determine the maximum time that logs can be left in winter and summer before treatment if sapstain, caused by pre-treatment infection, was to be prevented. Pre-treatment storage conditions representative of average temperature and humidity for the winter months of June, July and August, and of moderately severe summer conditions, for the Bay of Plenty, New Zealan...
D R Eden, R N Wakeling, C M Chittenden, J G Van der Waals, B Carpenter


Reduction of kiln brown stain in radiata pine lumber after log fumigation with methyl bromide
1997 - IRG/WP 97-30129
Methyl bromide fumigation of freshly felled radiata pine log sections effectively killed living cells in parenchyma to at least 75mm into sapwood. Lumber cut from logs (fumigated and control) stored 1 month outdoors (dry) showed slightly reduced brown stain when kiln dried at conventional temperatures. A more dramatic reduction and elimination of brown stain was noted in lumber cut from fumigated ...
E Schmidt, M E Hedley, D R Page, D Cross


Some practical implications from recent research on the fixation of CCA preservatives
1975 - IRG/WP 358
The mechanism of fixation of CCA preservatives is briefly described. If the temperature is increased during the primary fixation period, the formation of intermediate fixation compounds is less extensive. The length of the primary fixation period is of practical interest. It is determined by preservative composition and concentration, temperature and wood species. Diagrams are given for Pinus sylv...
S-E Dahlgren


The effect of storage and subculturing on in vitro fruit body formation and spore production in Gloeophyllum sepiarium and Oligoporus placentus
2001 - IRG/WP 01-20232
Spores are widely assumed to be the main mode of infection of wood in conditions conducive to decay above ground. In order to supply spores on demand as an experimental material, fruiting body and basidiospore production in vitro by Gloeophyllum sepiarium and Oligoporus placentus have been examined. The optimum medium, time to spore production, and duration of fruiting as well as fruiting body sha...
S Choi, J N R Ruddick, P I Morris


Anti-bluestain treatment developed for log cargoes stacked in subtropical conditions for export on logging ships
1995 - IRG/WP 95-30081
Subtropical environments impose conditions of temperature, humidity and rainfall which are optimal for growth of bluestain fungi. Unprotected softwoods under such conditions become bluestained three days after felling. Furthermore, intervals between harvesting and delivery to export marketplaces exceed the 30-day protection periods attributed to anti-bluestain formulations in such conditions. Thes...
A A W Baecker, M Behr, G D Shelver


Industrial fixation of chromium based wood preservatives
1990 - IRG/WP 3630
Fixation is an abstract and non-defined process. Nevertheless it is a specified requirement in most impregnation standards. The impregnation industry is facing increased pressure to deliver fixed products and to increase the safety of the handling of impregnated products. Industrial fixation of impregnated wood can be obtained by using different methods. The purpose of the process is to transform ...
T Christensen


Log fumigation prevents enzyme-mediated sapwood discolorations in hardwoods
1993 - IRG/WP 93-10003
Non-microbial sapwood discolorations in hardwood lumber can cause economic loss by degrade of quality. Based on the hypothesis that the enzyme-mediated sapstain may develop in part from byproducts of parenchyma cells in wood, reshly felled logs of red oak (Quercus spp.) and sugar hackberry (Celtis laevigata) were fumigated under a plastic tarp with methyl bromide. Log sections were checked after f...
E L Schmidt, T L Amburgey


Migration of chlorothalonil and carbendazim in fruits stored in wood treated with the anti-sapstain formulation Tuff Brite C
1997 - IRG/WP 97-50097
Fruits and vegetables stored in treated wood boxes are in contact with the products used for the treatment. In order to obtain regulatory approval for incidental food contact it is necessary to determine the quantity of residues on these fruits or vegetables. When the active materials are used in agriculture it is required that residues found are below to the MRL fixed for these substances. In the...
J F Cooper, D Riboul, M De Vleeschauwer, T L Woods


Chemical treatment of chips for outdoor storage. Evaluation of sodium N-methyldithiocarbamate + sodium 2,4-dinitrophenol treatment
1980 - IRG/WP 2134
Fresh slash pine chips were treated by spraying them with a dilute aqueous solution of sodium N-methyldithiocarbamate and sodium 2,4-dinitrophenol. The were then formed into an experimental chip file 10 feet high, and the pile was maintained for seven months. The treatment effectively slowed heat release and retarded losses in wood substances, tall oil, pulp yield, and pulp strenght. Under certain...
E L Springer, M Benjamin, W C Feist, L L Zoch, G J Hajny