Comparison of the agar-block and soil-block methods used for evaluation of fungitoxic value of QAC and CCA wood preservatives
1994 - IRG/WP 94-20039
The modyfied agar-block and soil-block methods were used for comparing the fungitoxic value of QAC and CCA type preservatives against Coniophora puteana and Coniophora olivacea The mass loss and moisture contents of wood were analysed....
J Wazny, L J Cookson


Collaborative soft rot tests: Programme and test method
1973 - IRG/WP 229
J G Savory, J K Carey


Influence of moisture content of rubber wood on the growth of Botryodiplodia theobromae
1993 - IRG/WP 93-10029
Botryodiplodia theobromae is the main fungus causing sapstain on rubber wood (Hevea brasiliensis). The entry and establishment of the stain fungus is nighly influenced by the moisture content of the wood. To determine the optimum moisture content of wood required for maximum growth of Botryodiplodia theobromae wood blocks at different moisture contents were inoculated with the test fungus and incu...
E J M Florence, R Gnanaharan, J K Sharma


Quantitative determination of Chromium: A comparison of three instruments
1995 - IRG/WP 95-50053
A comparison is made between three instruments for measuring levels of chromium in the leachate of copper-chrome-arsenic (CCA) treated timber. These include an atomic absorption spectrophotometer, an inductively coupled plasma spectrometer and the RQflexâ. The RQflexâ is a new hand-held instrument which measures chromium by dipping a ReflectoquantÒ strip into the leachate and inserting the stri...
S Walley, P R S Cobham, P Vinden


Observations on the failure of anti-sapstain treated timber under non-drying conditions
1990 - IRG/WP 1437
A range of bacteria and yeasts were isolated from antisapstain treated timber and fresh sawdust. Solution samples containing 100 ppm of TCMTB in a nutrient medium were inoculated with these organisms and incubated at 25°C for 5 days. The levels of TCMTB remaining in solution were determined by HPLC analysis after this time. Results indicated high losses of active ingredient for a range of organis...
G R Williams


Co-operative research project on L-joint testing. Progress report to March 1988
1988 - IRG/WP 2315
Further sets of data received from CTFT (France), BAM (Germany) and PRL (UK) after 46-48 months exposure and STU (Sweden) after 22 months exposure are presented and discussed in conjunction with data reported previously. Colonisation and attack of the L-joints has progressed with increasing exposure period. The new data are generally in agreement with those presented previously and the major diffe...
J K Carey, A F Bravery


Exposure monitoring of creosote vapors
1989 - IRG/WP 3511
Creosote oils contain hundreds of compounds. During impregnation and handling of treated wood the main component in the vapors released in air is naphthalene. Other main components are alkyl naphthalenes, indene, phenol and its methyl derivatives, benzothiophene, diphenyl, acenaphthalene and fluorene. In the measurement of creosote vapors, naphthalene can be used as an indicator agent. One of the ...
P Heikkilä, M Loutamo, V Riihimäki, M Romo


Collaborative soft rot tests: Interim report on PRL tests of Cu/Cr/As preservative using method of Document No: IRG/WP/208
1972 - IRG/WP 211
Preservative: Tanalith CT.106 - Results obtained with beech are given in the table and indicate a toxic limit of 16.7-19.2 kg/m³ - The initial soil moisture content was adjusted to 27.8% (the water holding capacity). Noticeable drying out has occurred in some of the test bottles....
J G Savory


A simple leaching procedure for in-plant monitoring of CCA fixation
1993 - IRG/WP 93-30023
A simple leaching test is described to quantitatively estimate the extent of fixation of chromated copper arsenate (CCA) preservative treated wood products. It is based on the reaction between diphenylcarbazide and unreacted hexavalent chromium leached from borings taken from treated wood during the fixation process. The test requires about 20 minutes to complete and can be set up in a treating pl...
P A Cooper, Y T Ung


Forest products laboratory methodology for monitoring decay in wood exposed above ground
1995 - IRG/WP 95-20074
Research at the Forest Products Laboratory on the durability of wood in service has included a full complement of laboratory and field tests. In this report, we present a review of past and current methods used to evaluate the condition of preservative-treated wood exposed above ground. Current protocols are described for tests on wood packaging, roofing, and dimension lumber....
R C De Groot, T L Highley


Diffusion of fused borate rods in top ends of poles
1989 - IRG/WP 3518
Diffusion tests of fused borate rods were carried out on extremities of sapwood poles in service. Rods were set in drills under the cone with or without addition of liquid Boracol 40. After one year of weathering, a good diffusion in the slice under the cone and even below the slice and in the cone itself was observed in Scots pine and spruce poles. The rods were still intacts and constitute, in f...
D Dirol, J P Guder


Analysing the characteristic role of moisture content for drying and fluid flow in Sitka spruce. - Part 1: The drying process of sapwood and heartwood of two different thickness of Sitka spruce using a kiln. - Part 2: Effects of moisture content on longitudinal permeability of Sitka spruce in vertical variation of the tree
2000 - IRG/WP 00-40173
The characteristic role of the moisture content in Sitka spruce (Picea sitchensis (Bong.) Carr.) that grown in the United Kingdom was examined by this study on the basis of (1) the reduction of moisture content in two different thickness of sapwood and heartwood by kiln drying process, and (2) the effects of moisture content to the longitudinal void volume filled of tanalith-C by the full-cell pro...
I Usta


Effects of pretreatments for the amelioration of preservative impregnability using the Oscillating pressure method (OPM)
1995 - IRG/WP 95-40044
For the purpose of an amelioration of preservative impregnability, three types of pretreatment: the steaming, the explosion and the boiling, were tested. The specimens were prepared by the domestic four species: Itajii, Ryukyumatsu, Sugi and Hinoki, and 1 refractry imported species: Douglas-fir. The dimension of specimens was 20 x 20 x 300 mm³ and were treated with CCA in a laboratory OPM machine...
K Suzuki, I Asaoka, S Tani, K Okada, T Hidaka


A standardised procedure for the treatment of timber with test chemicals
1986 - IRG/WP 2257
A procedure is described which allows the standardisation of sample handling and data manipulation during trials invastigating the treatability of timber with test chemicals. The use of computer software allows the data to be handled efficiently....
J Norton, A Zosars, L E Leightley


A new approach to the maintenance of wooden railway sleepers. (Second report)
1988 - IRG/WP 3492
The microenvironment and micro-ecology of wooden railway sleepers was investigated to assess their condition to determine the necessary treatment, repair and replacement criteria. In this report the efficacy of the secondary preservative treatment with solid boron rods is discussed and the development of an in-situ, nondestructive test method based on the creation and assessment of structural dyna...
W Beauford, P I Morris, A M Brown, D J Dickinson


Collaborative soft rot test: Amended test method
1972 - IRG/WP 208
The initial draft of a standard test method (Document IRG/WP/201) was discussed at the meeting in Brussels in 1971. It was agreed that a revised draft should be prepared and that the Princes Risborough Laboratory (formerly FPRL) should conduct a trial test using the method as a preliminary to the main collaborative test....
J G Savory


A summary of tests and practical experiences with the Pilodyn wood testing instrument
1980 - IRG/WP 282
This paper presents a summary of the reports, tests and practical experiences with the Pilodyn wood tester not only, however, concerning poles but also in other fields such as standing trees, sawn timber etc. The principle of the Pilodyn is a spring-loaded pin which is fired into the object and the depth to which the pin penetrates is correlated to physical and mechanical properties of the object....
H Friis-Hansen


Specific gravity and moisture content of particleboards treated with various chemicals
2005 - IRG/WP 05-40310
The aim of the study was to investigated the effects of particleboard treated with various chemical substances on specific gravity and moisture content The wood raw material used in the experiments were the mixture of coniferous wood [70%, Pinus brutia Ten., Pinus nigra Arn (Lamb.), Cedrus libani Ait.] and black poplar (30%, Populus nigra L.). In this mixture, barks have been accepted up to 5 per...
Ü C Yildiz, A A Var, H Kalaycioglu, S Yildiz


Wood preservatives ecotoxicology on Gammarus pulex (L.) - toward an environmental monitoring method and a getting rid of pollution process
2005 - IRG/WP 05-50224-9
Wood preservatives can have a strong impact on freshwater invertebrates when used close to aquatic ecosystems. It has been reported in Jura that different arthropod taxa, specially crustaceans, have disappeared along several kilometers downstream from factories using insecticides and fungicides as wood preservatives. The crustacean Gammarus pulex (L.) is a relevant bioindicator to characterize th...
O Adam, F Degiorgi, G Crini, P-M Badot


Technique for monitoring absorption during a vacuum pressure process
1992 - IRG/WP 92-3696
A laboratory technique was developed and an apparatus constructed which allowed for the direct and continuous measurement and observation of volumetric uptake of water-borne preservative into wood samples throughout a controlled vacuum-pressure treatment process. Fractional filling of void space was calculated. Graphing (fractional saturation) against time allows prediction of optimum cycle length...
A J Pendlebury, J A Petty


The variation in electrical resistance in the CCA-treated wood during the fixation
1989 - IRG/WP 3554
The curve commonly used in Scandinavia for describing the fixation period at different temperatures for CCA-impregnated wood is based on investigation by Dahlgren on the pH-variations in a mixture of sawdust and preservative solution. As far as we know there is no such investigation on solid wood. We have therefore measured the electrical resistance in CCA-treated solid wood to see if this will di...
F G Evans, B Nossen


Collaborative soft rot tests: Results of analyses of soil samples
1976 - IRG/WP 263
C R Levy


Maintaining the adoption of the equilibrium moisture content in timber by bifluorides under outdoor circumstance
1989 - IRG/WP 3541
A description is given of the practical application of bifluorides, f. ex. Diffusec in maintaining the adaption of the equilibrium moisture content in timber, as a result of a many years observation of treated timber under outdoor circumstances....
H F M Nijman


Soil-bed studies
1982 - IRG/WP 2181
This paper discusses factors affecting the design and use of a soil-bed....
P Vinden, J G Savory, D J Dickinson, J F Levy


A deflection test for monitoring decay in miniature beams
1986 - IRG/WP 2269
A laboratory apparatus for assessing decay in small stakes is described. It involves the measurement of deflection in a static bending apparatus using a displacement transducer linked to a microcomputer. Measurements are non-destructive, rapid, accurate and automatic and decay can be assessed repeatedly over long time periods....