Your search resulted in 224 documents. Displaying 25 entries per page.
The Effects of Natural Weathering on the Properties of Heat Treated Alder Wood
2010 - IRG/WP 10-40484
Heat treatment is an effective method to improve the dimensional stability and biological durability of wood. The heat treatment technology and the heat treated wood products were recently introduced to Turkey. However, only a few studies have been reported on the effect of natural weathering on the properties of heat treated wood in both Turkey and the world. In this study, heat treated alder (Al...
S Yildiz, Ü C Yildiz, E D Tomak
Study on the thickness swelling of mould-resistant chemical treated bamboo strand woven outdoor flooring
2010 - IRG/WP 10-40489
To prevent bamboo strand woven flooring from mould, several preservatives were chosen to treat bamboo strand before dipping into adhesives and pressing. The thickness swelling and mould resistant effect of the finished board were studied. Results showed that different preservatives had different influences on the thickness swelling of BSWF, and in order to reduce the thickness swelling of the fini...
Fangli Sun, Binfu Bao, Shenyuan Fu, Anliang Chen
Comparison of colour change in wood clear-coating systems including inorganic and organic UV absorbers for exterior use
2010 - IRG/WP 10-40499
The aim of this work is to compare the performance of inorganic and organic UV absorbers used in a wood coating application against weathering. Our study has investigated the colour changes of selected UV absorbers; hombitec 402 RM from the Sachtleben Company as an inorganic UV absorber, tinuvin 477 DW from the Ciba Company as an organic UV absorber. The study was carried out on two wood species; ...
Ö Özgenç, B Forsthuber, A Teischinger, C Hansmann
Performance of selected types of coated and uncoated modified wood in artificial and natural weathering
2010 - IRG/WP 10-40510
The objective of the present work was to investigate the influence of commercial wood modification methods on weathering behaviour and coating performance. It was aimed to compare modification methods and to set up maps of weathering behaviour for these methods with and without a semi-transparent wood stain. Artificial and natural weathering trials were carried out with a selection of different ty...
G Grüll, L Podgorski, M Truskaller, I Spitaler, V Georges, S Bollmus, A Steitz
Study of Microscopy Properties of Modified Wood During Weathering Process
2010 - IRG/WP 10-40517
In this study spruce (Picea excelsa) and Beech (Fagus orientalis) wood acetylated and has been subjected of artificial weathering in difference times (0, 50,150&300 h), then wood surface analyzed using Scanning Electron Microscopy (SEM). The SEM results shown that the surface of wood exposed to weathering undergoes distinct physical changes and the surface degradation appears to be directly propor...
M Akhtari
Impact of wood species on the performance of exterior wood coatings
2010 - IRG/WP 10-40519
To prolong the service life of a wooden construction the protective function of a coating is of utmost importance. The chemical composition as well as the wood-coating interface affects the performance of this protective layer and obviously wood species have an impact too. This paper discusses the influence of wood species on the overall coating performance. Therefore, a range of opaque waterborne...
I De Windt, J Van den Bulcke, J Van Acker
Effect of Coatings on the Durability of Birch and Spruce Plywood. Part 1: Weathering Performance
2010 - IRG/WP 10-40526
Several different coated birch and spruce plywood types were investigated in Finland using outdoor weathering. The weather performance of the tested coated birch plywood was good compared with uncoated birch and spruce plywood. The paint base film coated and painted birch plywood performed well in outdoor testing at VTT's test site. Phenol film coated plywood was sensitive to UV light, but on...
A Nurmi, H Viitanen
Effect of Coatings on the Durability of Birch and Spruce Plywood. Part 2: Biological Durability
2010 - IRG/WP 10-40527
Several different coated birch and spruce plywood types were investigated in Finland using the combination of outdoor weathering and decay test EN 12038. The most important factor to affect on the biological performance of birch plywood, coated and uncoated, was edge sealing. For spruce plywood edge sealing had a smaller effect. However, in spite of positive effect against decay, edge sealing did ...
A Nurmi, H Viitanen
Lignin blocking effects on weathering process of wood plastic composites
2010 - IRG/WP 10-40529
The weathering of wood–plastic composites (WPC) causes discoloration which affects their aesthetic aspects. It has been proved that these discolorations are due to lignin degradation. Effects of blocking the susceptible structure of lignin assessed by chemical treatment such as acetylation and methylation are reported in this study. Surface chemical change of wood plastic composite (WPC) formula...
P Darabi, A Naghi karimi, S Ahmade Mirshokraie, M-F Thévenon
Deterioration of wooden heritage in outdoor exposure in Romania
2010 - IRG/WP 10-40535
The paper contains a study of the deterioration of wooden heritage in Romania, in outdoor exposure.
Romania belongs to the few countries having a rich heritage of this kind. A quantitative image of
this heritage reveals the 1,350 objectives transferred and reconstructed in 16 open-air museums, over
1,500 wooden churches, more than 4,000 buildings and technical facilities, historical monuments
...
L Bucşa, C Bucşa
Performances of Douglas fir in real outdoor use conditions
2011 - IRG/WP 11-20472
The European standard EN 350-2 classifies Douglas fir as moderately resistant to fungal decay on the basis of standardized laboratory and field tests. However, the lifespan expectancy of outdoor structures such as cladding, decking and elements of wood construction carpentry may also vary according to environmental conditions (climate, exposure to weathering), maintenance and design. An investigat...
M Kutnik, S Lepetit, S Le Nevé
Fixed Borates Anyone?
2011 - IRG/WP 11-30563
The quest for a borate based preservative system that resists leaching or is “fixed” has long been a research goal. Boron fixation has been attempted with numerous strategies but there have been problems associated with past methods. This paper discusses new fixation systems based on bio-materials and presents up to five year outdoor exposure testing on full-size decks. Generally, the new f...
C R McIntyre, M A Lake
Standardized Field Trials with Micronized Copper
2011 - IRG/WP 11-30564
In 2008, an extensive review of all available data from standardized tests of micronized copper systems was published and there has been considerable work since then. This paper discusses over 20 field stake trials underway in well-known sites such as Gainesville, FL, Hilo, HI and the Dorman and Saucier sites in MS as well as tests from Australia and New Zealand. In addition, 4 ground proximity ...
C R McIntyre, M H Freeman
Tannin resin-boron for outdoor wood protection and fire retardancy
2011 - IRG/WP 11-30567
Boron in the form of boric acid is well known for its efficacy against wood destroying organisms, as well as for its high leachability from treated wood when in outside exposure. Moreover, due to the European directive 2008/58/EC, boric acid is only authorized at low levels. In order to keep considering boric acid as an interesting active ingredient for wood protection, the issue is now to fix it ...
M-F Thévenon, G Tondi, N Leménager, S Wieland, A Pizzi
The potential of silicone-based formulations to enhance wood properties through industrial treatment for outdoor use
2011 - IRG/WP 11-30578
High hygroscopicity is one of the main weaknesses of wood as far as its susceptibility to biodegradation, and specifically to fungal decay. New wood preservation technologies are constantly entering the wood protection market, competing with traditional, biocide-based preservation. Silicones are commercially used as hydrophobic agents on stones and concrete. They belong to the restricted number of...
F Simon, F Marchal, F Pochon, M Kutnik, I Le Bayon
The Effectiveness of Machined Profiles at Reducing the Checking of Wooden Decking
2011 - IRG/WP 11-40541
This study tests the hypothesis that ‘the ability of surface profiling to reduce checking of deck boards exposed to weathering will vary with wood species and profile type’. Southern pine (Pinus sp.) and Pacific silver fir (Abies amabilis) deck boards were machined to produce three different types of surface profiles: flat (control), ribbed (V-shaped grooves), and rippled (U-shaped grooves). B...
P Evans, I Cullis, P Morris
Moisture protection and performance during 5 years exposure of 19 wood coating systems on a cladding in Vienna
2011 - IRG/WP 11-40561
A cladding with vertical boards of Norway spruce (Picea abies) comprising different coating systems had been exposed to natural weathering oriented south west in Vienna for 5 years. Weathering behaviour of the boards was assessed in intervals and wood moisture content was measured over the first 22 months of exposure. The moisture protective properties of the coating systems were assessed using la...
G Grüll, I Spitaler, M Truskaller
Wet and dry adhesion of coatings on modified and unmodified wood: influence of 18 months of natural weathering on the pull-off test and cross-cut test results
2011 - IRG/WP 11-40569
The objective of this paper is to study the influence of several types of modification (acetylation, furfurylation, heat treatment) on coatings adhesion after 18 months of natural weathering according to EN 927-3 in Vienna (Austria).
The paper compares two methods for assessing the adhesion: the cross-cut test (EN ISO 2409) which is the conventional method used and recommended in EN 927-3 and th...
L Podgorski, G Grüll, M Truskaller, J D Lanvin, S Bollmus
Use of Variable Pressure Scanning Electron Microscopy for in situ Observation of Degradation of Wood Surfaces during Artificial Weathering
2012 - IRG/WP 12-20489
Variable pressure scanning electron microscopy (VPSEM) is capable of observing electrically non-conductive materials like wood without the need to render the surface conductive by applying a coating of gold, platinum or carbon. Hence, there is the possibility that VPSEM could be used to non-destructively follow the structural changes occurring at wood surfaces during weathering, because specimens ...
F Hatae, Y Kataoka, M Kiguchi, H Matsunaga, J Matsumura
Water uptake of wood surfaces with and without coating: influence of weathering
2012 - IRG/WP 12-40580
The objective of this study was to compare liquid water absorption of wood surfaces with and without coating, before and after artificial weathering. Samples of spruce, oak and sapelli were exposed to the EN 927-6 cycle for 1500 and 1850 hours and to the weathering produced by the Garner wheel for 1000 hours. Two highly pigmented coatings (solventborne and waterborne) and two semi-transparent stai...
L Podgorski, S Collignan, J D Lanvin
Comparison of exterior performance of two coating systems based polyurethane applied Pinus sylvestris L. and Picea orientalis L. wood
2012 - IRG/WP 12-40588
Some surface changes in sapwood and heartwood of two species before applying clear-coating were characterized after accelerated weathering time. Wood specimens covered with two types polyurethane (PU) films were also observed in accelerated weathering exposure. In this study, changes on the wood surface were compared of between wood specimens covered with two types polyurethane (PU) films after ir...
Ö Özgenç, Û Cafer Yıldız
Determination of the natural durability of solid wood against wood-destroying fungi - a European round-robin test
2013 - IRG/WP 13-20511
In Europe the durability of wood against wood-destroying basidiomycetes is tested according to CEN/TS 15083-1 (2005). Hitherto existing experience with this standard is quite heterogeneous and results from previous round-robin tests have stayed unreported or have been reported incompletely. In particular the need for natural pre-weathering of the test specimens to allow potential detoxification of...
C Brischke, C R Welzbacher, A Gellerich, S Bollmus, M Humar, K Plaschkies, W Scheiding, G Alfredsen, J Van Acker, I De Windt
Changes of fungicidal, mechanical and sorption properties of wood during above ground outdoor exposure
2013 - IRG/WP 13-20513
The aim of this preliminary study was to investigate differences in mechanical, fungicidal, and sorption properties of four different wood species (sweet chestnut (Castanea sativa), common beach (Fagus sylvatica), Norway spruce (Picea abies), and copper-ethanolamine (CuE) impregnated Norway spruce (Picea abies)) that were exposed in the 3rd use class (CEN, 1992) for periods between 4 and 30 months...
N Thaler, M Humar
Climatic impacts on the moisture performance of wooden decking and facades
2013 - IRG/WP 13-20518
In outdoor usage wood is exposed to a variety of influences, which reduce its durability against biological deterioration and wetting. Besides many other factors the service life of wooden facades and cladding is dominated by occurring moisture loads on the one hand and their capability to withstand moisture on the other hand. Hence, climatic factors have a direct impact on the material climate an...
T Bornemann, C Brischke, G Alfredsen
Moisture distribution in glulam beams with natural cracks observed with CT Scanning before and after rain
2013 - IRG/WP 13-20534
The way cracks in outdoor wooden constructions affect durability is an interesting topic, since a certain amount of cracks can always be found naturally in wood and glued laminated wood. The question in this was, can cracks lead water into the wood and thereby increase the risk for decay and reduce strength and service life. Moisture balance, i.e., water absorption and water distribution were stud...
K Sandberg