A comparison of the resistance of pyrethroid-treated wood to damage by Coptotermes acinaciformis in Australia and C. formosanus in China and the USA
2014 - IRG/WP 14-10830
Field trials, using a single aboveground method of exposure, were used to assess a range of retentions of two pyrethroids (bifenthrin and permethrin) in Pinus radiata D. Don sapwood against two species of Coptotermes in three countries to provide directly comparable results. Coptotermes acinaciformis (Froggatt) in Australia, C. formosanus Shiraki in China and C. formosanus in the USA consumed simi...
J Creffield, M Lenz, D Scown, T Evans, Junhong Zhong, B Kard, J Hague, K Brown, E Freytag, J Curole, R Smith, T Shupe


Variability in durability of some selected South-American wood species
2014 - IRG/WP 14-10831
Within the scope of sustainable forest management one wants to encourage the proper use of lesser known wood species. Therefore the market has to shift from a demand-driven towards a supply-driven market without loss of wood quality. It is generally known that the durability from pith to bark varies thus, affecting the overall durability of wood species. Consequently, a detailed analysis is necess...
I De Windt, P ’t Hooft, J Van den Bulcke, J Van Acker


In-ground durability of wood-based products – Comparative assessment of graveyard field tests and terrestrial microcosms
2014 - IRG/WP 14-20538
Traditionally wood durability and the effectiveness of wood preservatives are determined in so-called graveyard tests (according to EN 252 or AWPA E7). For laboratory testing, terrestrial microcosms (TMC) can serve as an alternative. Both tests have been applied for different types of wood-based materials, preservative treated, modified and unmodified wood. However, the usability of laboratory res...
A Soetbeer, L Meyer, C Brischke, P Larsson-Brelid, J Jermer


Field performance of wood-based decking materials in the Western United States
2014 - IRG/WP 14-30645
While wood has long been used for the construction of decks and other outdoor features, a variety of wood-plastic composite (WPC) decking products have emerged over the past decade with claims of exceptional durability and low maintenance. There are relatively few long term comparative tests on these products. The performance of selected WPC decking products was compared with naturally durable we...
S Lipeh, C S Love, J J Morrell


Glutathione transferases and wood extracts
2015 - IRG/WP 15-10845
Wood rotting fungi have developed an efficient detoxification system allowing them to be well adapted to their way of life, these fungi generating and encountering potential toxic compounds during wood degradation. Belonging to this detoxification network, glutathione transferases are particularly extended in these fungi and their presence could reflect the chemical environments encountered by the...
A Deroy, F Saiag, Z Kebbi-Benkeder, N Touahri, M Morel-Rouhier, F Colin, S Dumarcay, P Gérardin,


Introduction of the COST FP 1303 Cooperative Performance Test
2015 - IRG/WP 15-20567
COST Action FP 1303 “Performance of bio-based building materials” successfully started in October 2013 and an ambitious program was set up for the four year programme. COST Actions provide an excellent opportunity for collaborative research, e.g. in the frame of Round Robin tests. The idea of this respective test was to distribute a fairly simple test set up to as many places in Europe as poss...
M Humar, C Brischke, L Meyer, B Lesar, N Thaler, D Jones, S Bardage, C Belloncle, J Van den Bulcke, J M Abascal, G Alfredsen, D Baisch, B Brunnhuber, G Cofta, E Grodås, E Frühwald Hansson, M Irle, H Kallakas, J Kers, M Klamer, P Larsson Brelid, A B Maider, K C Mahnert, E Melcher, R Möller, M Noël, L Nunes, G A Ormondroyd, S Palanti, N Pfabigan, A Pilgård, A O Rapp, P Schumacher, E Suttie, T Teppand, M Touza, J Van Acker


Foundation piles: analysis of beech wood decay in service life conditions
2016 - IRG/WP 16-10858
Wood piles foundation system was largely used over decades. Thus, numerous buildings over the world are based on this constructive system. In the context of reduction of CO2 emissions in the building field of constructions, substitution of concrete by wood as material for foundation piles seems to be a promising alternative. However, fluctuation of the water table level in soil may promote fungal ...
Q Kleindienst, A Besserer, M-L Antoine, C Perrin, J-F Bocquet, L Bléron


Real-Time PCR Assays for the detection of the dry rot fungus Serpula lacrymans and its close relative Serpula himantioides
2016 - IRG/WP 16-10867
Prevention of wood decay by fungi of the phylum Basidiomycota is an important issue of wood protection. The most destructive fungus in buildings in Central Europe is the dry rot fungus Serpula lacrymans, which needs more extensive restauration measures than all other wood decay fungi. Its close relative S. himantioides occurs more frequently in outdoor environment. The assessment and remediation o...
K Jacobs, N Rangno


Fungal decay of archaeological waterlogged oak timber: role of the mineral content
2016 - IRG/WP 16-10873
In service, wood foundation poles are subjected to water level fluctuation in soil. While wood is saturated by water only bacterial decay occurs. When oxygen content increases and moisture content decreases, severe fungal attack may occur. To evaluate the long term fungal durability of wood foundation pole in the context of service, 300 years waterlogged archaeological wood poles were used. The oa...
A Besserer, M Letellier, E Fredon, Q Kleindienst, M-L Antoine, C Perrin, J Lallemand, C Rose, M-C Trouy


Weather degradation of thin wood samples
2016 - IRG/WP 16-20578
Untreated wooden surfaces degrade when exposed to varying doses of natural weathering. In this study, thin wood samples were studied for weathering effects with the aim of modeling the degradation utilizing Near-infrared hyperspectral imaging. Several sets of samples were exposed outdoors for time intervals from 0 to 21 days, and one set of samples was exposed to UV-radiation in a laboratory chamb...
I Burud, K A Smeland, K Hovde Liland, T K Thiis, J Sandak, A Sandak, L Ross Gobakken


Engineering for Rural and Civil Development. Uni Performance of wood exterior structures above ground contact in Spain built with softwood species. The situation of cases in northern Spain
2016 - IRG/WP 16-20597
Across Europe is very common to find exterior structures build in sawn and glue-laminated wood. Most of these exterior structures used softwood wood species such as fir, spruce, larch and pine. In Spain wood exterior structures, as for example bridges, became more and more popular since eighties, when sawn and glue-laminated wood were utilized for building exterior wooden structures in overall Spa...
D Lorenzo, J Fernández-Golfín, M Touza


Bacterial Degradation of Pentachlorophenol Indicated in Groundwater Undergoing Long Term In-Situ Remediation
2016 - IRG/WP 16-50318
Pentachlorophenol (PCP, Penta) is a worldwide soil and water contaminant. The pervasive use of PCP as a fungicide, herbicide, pesticide, and as preservative for wood products has led to its global distribution. It is a highly effective preventative measure for most invasive insects, bacteria, fungi, and molds, as well as an excellent wood protection treatment. This study examined a known PCP conta...
C E Stokes, H Borazjani, L Prewitt


Estimation of wood degradation determined by visual inspection, mechanical testing and DNA characterisation – report after 3 years of exposure
2016 - IRG/WP 16-30700
The influence of two separate treatments, thermal modification and alkaline copper quaternary (ACQ, Silvanolin©) treatment, on fungal decay, visual disfigurement, deterioration in mechanical properties and fungal community structure was assessed on Norway spruce (Picea abies) and compared with the performance of two naturally more resistant tree species native to North America: Douglas fir (Pseud...
N Thaler, T Martinović, M Bajc, D Finžgar, H Kraigher, A Sinha, J J Morrell, M Humar


Prevention of fungal damage of oil and date palm wood by organic acids
2017 - IRG/WP 17-10877
Felled palm trunks are susceptible to fungi as long as their moisture content is above fibre saturation. During this period, palm wood has to be protected against mould and rot fungi. Environmental-friendly organic acids are suitable. Small samples of oil palm (Elaeis guineensis) and date palm (Phoenix dactylifera) wood were treated with 1 to 10% solutions of acetic acid and propionic acid, respec...
M Bahmani, O Schmidt


Effects of wollastonite nanofibers on biological resistance of historical paper against Aspergillus niger
2017 - IRG/WP 17-10878
Effect of wollastonite nanofibers on biological resistance of historical paper against Aspergillus niger was studied. Specimens from A4 papers were also prepared for comparison purposes. Paper specimens were dipped in aqueous nanowollastonite (NW) with 10, 20, 30, and 40% concentrations and compared with control specimens. In order the nanofibers be fixed on paper specimens, 5% of polyvinyl acetat...
H R Taghiyari, A Kalantari, A Ershad-Langroudi, A Kalantari


The First Description of Soft-rot Cavity in Waterlogged Archaeological Woods by a Japanese Wood Anatomist Prof. F. Onaka in 1935
2017 - IRG/WP 17-10885
The term soft rot, which was caused by Ascomycetes and Deuteromycetes, was first used by J G Savory in 1954. Soft rot decay can be characterized by cavities within secondary cell walls align along the cellulose microfibrils. Our recent literature search revealed, however, that Prof. F. Onaka in Kyoto University described the soft rot cavities in the waterlogged archaeological woods in detail from ...
Yoon Soo Kim, K Yamamoto


Quality of the impregnated wood in the Slovenian hardware stores
2017 - IRG/WP 17-20606
Ten different samples from Slovenian hardware stores were analysed. Samples were treated with copper based wood preservatives and designed and advertised to be used in heavy duty applications in use classes 3.2 or 4. In order to determine the quality of the treatment penetration, retention and fungicidal properties were determined. Retention was determined with XRF analysis, while modified EN 113 ...
M Humar, B Lesar, N Thaler, D Kržišnik, N Kregar, S Drnovšek


COST FP 1303 Cooperative Performance Test – Results after two years outdoor exposure
2017 - IRG/WP 17-20620
COST Action FP 1303 ‘Performance of Bio-Based Building Materials’ started in October 2013 and an ambitious program was set up for four years. Among this a collaborative field test was planned. The idea of the cooperative performance test was to distribute a fairly simple test set up to as many places in Europe as possible in order to collect performance data reflecting the full range of climat...
B Lesar, M Humar, C Brischke, L Meyer-Veltrup, D Jones, N Thaler, J M Abascal, G Alfredsen, B Brunnhuber, E Grodås, M Irle, J Kers, M Klamer, K-C Mahnert, E Melcher, S Palanti, M Noël, E Suttie, N Pfabigan, M Touza


The Protective Effect of Different Tree Bark Extractives against Decay Fungi
2017 - IRG/WP 17-30707
There are various modification methods which increase the resistance of wooden materials. Due to recent environmental regulations, there is a need for new and environmentally-friendly wood preservatives. In this study, six different tree bark extractives were evaluated for their wood resistance against fungal degradation. For this purpose, the white rot fungi (Tramates versicolour) and brown rot f...
Ö Özgenç, S Durmaz


Thermal stability of a wood protective biofinish and the influence of flame retardants on Aureobasidium cells
2017 - IRG/WP 17-30716
In general there is an increasing need for sustainable resources, including sustainable building materials. Wood is one of these sustainable resources and is more used as an outdoor building material. Since unprotected wood will usually be degraded during outdoor exposure, many different protection systems are available on the market. Protection systems containing biocides however might create obs...
S Rensink, E A M Klein Rot, M F Sailer


Agar block durability test of plywood made of neem (Azadiracta indica) leaves treated veneer using two white rot fungi
2017 - IRG/WP 17-40782
This study has been undertaken to investigate the durability of plywood made from non-durable wood (simul, Bombax ceiba) veneer treated by neem (Azadiracta indica, A. Juss.) leaves. The veneers were treated with cold and hot water solution of neem leaves of different concentrations (10%, 5%, 2.5%) and treatment durations (1, 2, 3 days) for cold water and 20, 40 and 60 minutes for hot water. The pl...
K Akhter, M A Hashem, S Akhter


Performance of Norway spruce bridge in North-West Spain after 12 years exposure
2017 - IRG/WP 17-40796
Across Europe is very common to find bridges build in sawn and glue-laminated wood. Most of these bridges used softwood wood species such as: fir, spruce, larch and pine. In Spain wooden bridges, became more and more popular since nineties, when sawn and glue-laminated wood were utilized for building exterior wooden structures in overall Spain. This material, sawn and glue-laminated wood, are ma...
D Lorenzo, J Fernández-Golfín, M Touza, M Guaita, A Lozano, J Benito


Biodegradation of creosote by white rot fungus Phanerochaete chrysosporium and a strains of Pseudomonas
2017 - IRG/WP 17-50329
The aim of this study was to determine degradation effectiveness of polycyclic aromatic hydrocarbons (PAH) contained in creosote by white rot fungus and bacteria. The following two species of bacteria Pseudomonas putida and Pseudomonas sp. as well as Phanerochaete chrysosporium fungus characterised by the ability to decompose aromatic compounds were selected for experiments. Bacterial strains were...
J Zabielska-Matejuk, A Stangierska, A Kropacz, E Kaczorek


Effects of exposure time on detection of the behavior of white-rot fungi on Oriental beech wood properties
2017 - IRG/WP 17-10902
The comparison of fungal degradation of Orientalis beechwood by two white-rot fungi was evaluated in this study. Biological, mechanical, and chemical assessments of beech wood were carried out at 30 day interval for 120 days. The results demonstrated that both fungi have greater effects on beech wood during each exposure time. However, Trametes versicolor degraded beech wood more effectively than ...
E Bari, D D Nicholas, K M Ohno


Interactions between wood polyphenols and detoxification enzymes of the white rot Trametes versicolor
2018 - IRG/WP 18-10906
Wood decay fungi have complex detoxification systems that enable them to cope with secondary metabolites produced by plants. Although the number of genes encoding for glutathione transferases (GSTs) is especially expanded in lignolytic fungi, little is known about their physiological target molecules. In this study, by combining thermal shift assay and affinity crystallography we highlighted inter...
M Schwartz, T Perrot, E Aubert, S Dumarçay, F Favier, P Gérardin, M Morel-Rouhier, G Mulliert, F Saiag, C Didierjean, E Gelhaye