Co-operative research project on L-joint testing. Sampling after 4 years exposure
1987 - IRG/WP 2274
In September 1983, Document No: IRG/WP/2208 was distributed giving guidance on sampling after 8 months exposure and including tables on which to record the test results. Similarly in September 1984, Document No: IRG/WP/2233 was distributed concerning sampling after 18 months exposure. No major problems have been notified to Princes Risborough Laboratory concerning the sampling method. It is theref...
J K Carey, A F Bravery


The resistance of timbers to impregnation with wood preservatives
1979 - IRG/WP 3137
It is anatomical structure which determines liquid flow rate within different timber species. This cannot be deduced from properties such as density or rate of growth, and can only be found by experiment. A standard test has been in use at the Princes Risborough Laboratory for many years, employing a pressure-impregnation treatment, and a large number of timbers have been studied. The test consist...
Anonymous


Permeability measurements on surface layers for detecting wood with abnormally high permeability
1988 - IRG/WP 2298
Wet storage of timber during the warm period of the year may lead to an increased permeability of the wood, an undesirable phenomenon for several wood industries and also for many end-uses. Neither before nor after drying, such wood with "wet storage damage" can be visually distinguished from wood with a normal permeability. A non-destructive method for inspecting the permeability of surface layer...
J B Boutelje, G Hägglund


Mould growth and permeability in relation to wet-storage
1989 - IRG/WP 1414
The positive influences of wet-storage of roundwood to avoid attack by blue stain fungi and insects and to avoid cracking of wood during storage are well documented. Comparatively little information is, however, available on the effects on microbial susceptibility of the material after the storage period. The permeability of the wet-stored and the non-wet-stored material was determined. Wood block...
J Bjurman, E L Holappa


Changes in transverse wood permeability during the drying of rimu and radiata pine
1990 - IRG/WP 3636
When softwoods are dried and subsequently impregnated with waterborne preservatives two problems frequently occur, preservative screening of multi-salt preservatives and difficult re-drying. To study the causes, the permeability of rimu and radiata pine wood has been measured along the three principal directions. The radial and tangential permeabilities of the green sapwood of the two species were...
R E Booker


Comparison of permeability at different levels of moisture content in Bornmullerian fir (Abies bornmulleriana Mattf.) and Eastern spruce (Picea orientalis L.) impregnated under vacuum/pressure through full-cell method by using CCA and CCB of different concentrations
2007 - IRG/WP 07-40366
In this study, a comparison has been made in terms of the combined, longitudinal, tangential, and radial permeability of the species of Bornmullerian fir (Abies bornmulleriana Mattf.) and Eastern spruce (Picea orientalis L.) with moisture contents of 50 % and 15 %, which were impregnated under vacuum/pressure through full-cell method by using water-borne wood preservatives (impregnation materials)...
I Usta


Microwave Surface Modification of Radiata Pine Peeler Cores for Preservative Treatment
2009 - IRG/WP 09-40453
Radiata pine peeler cores are classified as a by-product derived from the cores of logs left over after the veneer peeling process. The core can be potentially developed for value added solid wood products as it is abundantly available and has a constant diameter. However, the core needs to be preservative treated because of low durability in ground contact. An additional problem is that the wood ...
K Sugiyanto, G Torgovnikov, P Vinden


Selection of an appropriate coating system for wooden boats to be used in fresh water
2009 - IRG/WP 09-40472
Properties of several, most commonly used protective low-price coatings, which are used by the pletnja boat owners in Bled, Slovenia, were extensively studied. The aim of this professional, practically oriented study was to compare various coating systems, and to recommend the most suitable one to the boat owners. Regarding specific use conditions, the following properties, including their resista...
M Petrič, B Kričej, A Logar, M Pavlič


Modelling hyphal growth of the bio-incising fungus Physisporinus vitreus
2010 - IRG/WP 10-10710
The white-rot fungus Physisporinus vitreus preferentially degrades the pit membranes of bordered pits in tracheids and subsequently enhances wood permeability. Thus, P. vitreus can be used to improve the uptake of wood preservatives and environmentally-benign wood modification substances. This process can be used to enhance the use and sustainability of native conifer wood species by the wood indu...
M Fuhr, C Stührk, F W M R Schwarze, M Schubert, H J Herrmann


A review of Sitka spruce (Picea sitchensis (Bong.) Carr.) as its Importance and Breeding
2010 - IRG/WP 10-10717
Foresters tend to concentrate on those species which are the easiest to handle silviculturally, and which will produce the greatest volume of generally useful wood in the shortest time. Sitka spruce (Picea sitchensis (Bong.) Carr.), which is a softwood species from the western seaboard of North America with a range extending from southern Alaska to northern California, is one of the pioneer specie...
I Usta, R Despot


Trace chemicals used for studying fluid permeability of wood
2010 - IRG/WP 10-20442
Wood is a construction material and in its natural condition vulnerable to biological decay caused by fungi, insects and bacteria. To facilitate its outdoor application, wood protection systems are applied since ages. In the course of restrictions for well established but hazardous wood protection treatments, newer systems get utilized. Its uniform allocation within the wooden matrix is essential ...
K Zimmer, E Larnøy, O Høibø


Chapter 11 - Preservation of talla bamboo
2007 - IRG/WP 07-10635-11
Researches revealed that the talla bamboo (Bambusa tulda Roxb.)) in Bangladesh could be full-cell pressure treated with CCA in green and dry conditions. The dry bamboo gives higher loading absorptions than green one when impregnated at same treating conditions. Also higher absorptions are obtained at nodes rather than internodes. Adequate penetration and retention results for ground and wate...
A K Lahiry


Effects of Heat-Treatment in Hot Water and Steam Mediums on Gas Permeability of Beech Wood
2011 - IRG/WP 11-40557
Heat-treatment, as a major method of wood modification, improving dimensional stability, and natural durability, has been studied greatly from different aspects. The effect of heat-treatment on gas permeability, as an important physical property of wood, in two different mediums of hot water and steam, as well as in two buffers of 7 and 8, is the main topic of the present study. Hydrothermal treat...
H Reza Taghiyari, A Talaei, A Karimi


Treatability variation of scots pine heartwood from Northern Europe
2011 - IRG/WP 11-40563
Scots pine (Pinus sylvestris L.) is one of the most common construction materials for general exterior applications in northern Europe. It has a wide natural geographical distribution, a good availability and it is low-priced compared to other materials. According to EN 350-2 Scots pine heartwood is considered being “untreatable” and having durability class 3. This means that its durability co...
G Behr, E Larnøy, C-T Bues


A Review of Radial Flow of the Refractory Softwoods: An Example of Sitka Spruce
2011 - IRG/WP 11-40564
As one of the refractory softwood species, the major problems in the preservative treatment of spruce based on the radial flow relate to the anatomical structure of the wood material. The most important morphological features influencing this were the amount of the nature and the condition of both ray tracheids and ray parenchyma cells, and the cross-field pits in particular. The conducting pathwa...
Ilker Usta, Radovan Despot


The Significance of Natural Durability of Croatian Mediterranean Wood Species for their Traditional and Present Protection Methods and Use
2012 - IRG/WP 12-10770
The aim of this article is to contribute to the better cognition of the protection and use of some most important Croatian autochthonous Mediterranean wood species. Their traditional use and protection are observed by two aspects. The first one is the presence of these species in the Croatian Mediterranean regions for many centuries, and the long tradition of their use, regardless of their natural...
R Despot, M Hasan


Effects of Nano-Zycosil on Liquid and Gas Permeability of MDF
2012 - IRG/WP 12-40578
Effects were studied of zycosil nanoparticles, with size range from 30 to 90 nm, on liquid and gas permeability of medium density fiberboard. 100 g of nanozycosil was added to each kg of dry fibers. Density was kept constant at 0.67 g/cm3. The obtained results indicated that addition of zycosil to the mat resulted in a significant increase in gas permeability due to the lower fiber-content in the ...
H Reza Taghiyari, K Heidarhaee, P Noori, A Karimi


Microwave Modification of Bamboo Culm to Improve Permeability
2012 - IRG/WP 12-40592
Bamboo is a woody, valuable and strong material that has been used for a long time. In spite of its numerous beneficial properties, bamboo is susceptible to attack by fungus and insect therefore preservative treatment is regarded as necessary. Preservative treatment must provide sufficient uptake and even distribution in the culms for adequate protection. The treatability of dry bamboo, however, i...
K Sugiyanto, P Vinden, G Torgovnikov, S Przewloka


Effect of growth rate and radial position on the natural durability of Douglas-fir
2012 - IRG/WP 12-10791
In terms of natural durability, Douglas-fir (Pseudotsuga menziesii (Mirb.) Franco) fame owns to the favourable characteristics of centuries-old trees harvested in old-growth North American forests. The properties of wood coming from plantations harvested between 50 and 100 years-old are likely to be different. In such stands, plantation density and thinning intensity may have a large impact on the...
C Pollet, J-M Henin, B Jourez, J Hébert


Influence of coatings on water uptake of wood surfaces before and after natural and artificial weathering
2013 - IRG/WP 13-40641
Liquid water absorption of wood surfaces with and without coating, before and after exposure to artificial and natural weathering has been studied. Spruce, oak and sapele samples have been exposed to the cycle of EN 927-6, to the cycle of the Gardner wheel and to natural weathering. Five coatings were tested including solventborne and waterborne, semi-transparent and opaque products. Exposure to w...
L Podgorski, S Collignan, J-D Lanvin


Effect of electron beam irradiation on the fire retardant penetration into wood
2013 - IRG/WP 13-40642
Electron beam processing which can fast and easy change the nature of the material has received considerable attention recently. Studies using electron beam has been conducted in various fields and it has been applied in many industrial sectors. Electron beam has higher energy than other electromagnetic waves. It has excellent object permeability. It affects degradation of intermolecular cross-lin...
Dong won Son, Jong Sin Lee, Mee Ran Kang, Sang Bum Park


Nano-Zycosil in MDF. Part I: Gas and Liquid Permeability
2014 - IRG/WP 14-40652
Effects were studied of zycosil nanoparticles, with size range from 20 to 80 nm, on liquid and gas permeability of medium density fiberboard. Nanozycosil was used at four consumption levels of 0, 50, 100, and 150 g/kg dry wood fibers. Density of all treatments was kept constant at 0.67 g/cm3. The obtained results indicated that the addition of zycosil to the mat resulted in a significant increase...
H Reza Taghiyari, A Karimi, P M D Tahir, O Schmidt, E Bari, P Nouri , A Jahangiri


Leachability and Dimensional Stability of Nanosilver-Steamed Densified Poplar
2014 - IRG/WP 14-40684
This study was aimed to investigate leachability and dimensional stability of nanosilver impregnated poplar (Popolus alba), steamed before hot compression. Wood samples were impregnated with nanosilver suspension (200 and 400 ppm) under pressure of 4 bar for 20 minutes. Steam treatment was carried out at 150°C for 2 hours. Then samples were compressed (33%) radially in a hot press at 170°C for 3...
G Rassam, A Talaei, A Ahmadi


Effects of fungal exposure on air and liquid permeability of nanosilver- and nanozincoxide-impregnated Paulownia wood
2016 - IRG/WP 16-30680
Effects of aqueous dispersion of silver and zinc-oxide nano-particles on air and liquid permeability of Paulownia wood exposed to T. versicolor were studied in the present research project. Specimens were also heat-treated at 100 and 150°C and compared with the control specimens. Permeability values were measured when the moisture content of the specimens was 12%. Results showed significant incre...
H R Taghiyari, A Kalantari, M Ghorbani Kookandeh, F Bavaneghi, M Akhtari


Effect of Nano-Silane on Permeability in MDF as a Result of Susceptibility to Moulds and Fungi
2016 - IRG/WP 16-40716
Effects were studied of vapor chamber on specific gas permeability of nanosilane-treated medium-density fiberboards (MDF). Size range of nanoparticles was 20 – 80 nm. Nano-silane (NS) was used at four consumption levels of 0, 50, 100, and 150 g/kg dry wood fibers. Density of all treatments was kept constant at 0.67 g/cm3. Specimens were kept for 18 weeks in vaporized chamber; their specific gas ...
H R Taghiyari, J Norton, A Moradiyan, M Sadegh Taher Tolou Del, H Siahposht, B Moradi-Malek, M Noferesti