Water-based wood preservatives for curative treatement of insect-infested spruce constructions
1998 - IRG/WP 98-30171
On laying down sanitation measures for wooden constructions infested by wood boring insects, we must take into account static risks for the construction - and, thus, for the security of the user - as well as risks for humans and environment due to the chemical preservative compounds of the treated wood. Analyses on many roof constructions made with spruce (Picea abies L.) have revealed that Hylot...
E Graf, P Manser, B Lanz


Treatment of dried sawn spruce and redwood building timbers with water-borne preservatives under a scheme for the quality control of the preservation and preserved wood in the Netherlands
1978 - IRG/WP 3123
Treatment of dried sawn spruce and redwood Building Timbers with water-borne preservatives under a scheme for the quality control of the preservation and preserved wood in the Netherlands. The aim of this article is to give the reader a modest description of the evaluation of fundamental research in wood preservation into a practical application....
H F M Nijman, N Burgers


Improved resistance of Scots pine and Spruce by application of an oil-heat treatment
2000 - IRG/WP 00-40162
Spruce (Picea abies L. Karst.) and Scots pine (Pinus sylvestris L.) were subject to a heat treatment which was carried out in an oil-bath. The aim was to improve the dimensional stability of the treated wood and its resistance against fungi. The bath of vegetable oil provides a uniform heat transfer at temperatures of 180°C, 200°C and 220°C and protects the submersed wood from oxygen. Heat trea...
M Sailer, A O Rapp, H Leithoff


The effects of heat treament on the specific gravity of beech and spruce wood
2003 - IRG/WP 03-40254
The effects of heat treatment on specific gravity of beech (Fagus orientalis) and spruce wood (Picea orientalis) naturally grown and intensively used in forest products industry in Turkey were studied. The wood samples were cut into 2 x 2 x 3 cm. Heat treatment was than applied to the wood samples at four different temperatures (130 °C, 150 °C, 180 °C and 200 °C) and three different durations...
S Yildiz, Ü C Yildiz, G Colakoglu, E D Gezer, A Temiz


Changed susceptibility of the chemically and thermally degraded spruce wood to its attack by the dry rot fungus Serpula lacrymans
1999 - IRG/WP 99-10322
In buildings, some intentional or unintended situations can occur at which some wood products are exposed to aggressive chemicals and also to higher temperatures. Occasional activity of fungi on such pre-attacked wood products can be either higher or lower. This paper deals with changes in the susceptibility of spruce wood (Picea abies L. Karst.) to attack by the dry rot fungus Serpula lacrymans, ...
L Reinprecht


CCA component distribution in the heartwood of treated lodgepole pine and white spruce
1998 - IRG/WP 98-30173
As part of a comprehensive study on the influence of drying on heartwood permeability, the distribution of copper, chromium and arsenic (CCA) in lodgepole pine (Pinus contorta Dougl.) and white spruce (Picea glauca (Moench) Voss.) heartwood was examined with light microscopy. Stained microtomed sections were examined to determine the penetration pathway for the CCA. The microscopic observations re...
Y An, J N R Ruddick, P I Morris


Practical testing of wood preservatives to prevent weathering damage and infection by micro-organisms on spruce and pine
1989 - IRG/WP 3530
Brush application, is generally used to prevent wooden window frames from decay caused by influence of weathering and fungi. Accordingly 10 boards of pine (Pinus sylvestris) and spruce (Picea abies) were treated with 10 commercially used wood preservatives. The efficiency of fungicides by using chiptest and blue stain test (EN 152), the effectiveness against weathering as well as the course of col...
R Gründlinger, O Janotta, H Melzer, K Messner


Factors affecting the sorption of preservative during diffusion treatment of wood
1988 - IRG/WP 3500
The sorption of preservative into wood during soaking in aqueous solution was found to comprise absorption as well as diffusion of solute. Absorption was increased by partially seasoning the wood prior to soaking and was characterised by (a) a very rapid initial rate of uptake and (b) an extended period of slow uptake, the rate of which varied with prior conditioning. It was concluded that some pa...
P Vinden


Performance of treated spruce in Canadian field test sites
1989 - IRG/WP 3506
Spruce material under test in Canadian field test sites is performing better than anticipated. From the comparison of the performance of spruce treated with various preservatives, it appears that penetration may be far more important on durability performance than the preservative itself or the retention of preservatives in the wood. However, there is still insufficient data on the influence of pe...
J P Hösli, E E Doyle


Performance of treated and untreated sawn fence posts of Scots pine and Norway spruce
2000 - IRG/WP 00-30247
Sawn fence posts are a rather important product and the objective of this trial was to assess their durability. In 1985 a field trial with treated and untreated fence posts of Scots pine (Pinus sylvestris L.) and Norway spruce (Picea abies (L.) Karst.) was set out at the test field in Ultuna, Uppsala, Sweden. The posts had a dimension of 75 x 100 x 1400 mm3. The preservatives applied were a CCA, a...
Ö Bergman


Ammoniacal wood preservative for use in non-pressure treatment of spruce and aspen poplar. Part 1
1984 - IRG/WP 3273
End-matched lumber of Picea glauca (Moench)Voss (white spruce) and Populus tremuloides Michx. (aspen poplar) timbers was treated by a thermal diffusion process in open tank treating vessels using an ammoniacal copper-arsenate wood preservative. The process proved technically feasible with respect to controlling the vapourization of ammonia from open tanks during treatment at high temperatures. Tre...
C D Ralph, J K Shields


The reliability of colouring methods for the determination of biflourides and boron in spruce wood
1994 - IRG/WP 94-20036
From practical reasons, qualitative spraying methods are widely used for the detection of bifluorides and boron in wood. The main aim of this research was to detect whether the concentration of the active ingredient in the coloured area is equal or greater than the toxic value against basidiomycetes. Both colouring methods, Z-A reagent for fluorides and curcuma reagent for boric acid, are a reliab...
R Grell, M G Sanders, W J Homan, H Militz


Moisture requirements and wood degradation of pine and spruce wood by some Basidiomycetes-fungi
1989 - IRG/WP 1406
The minimum moisture requirements for the growth of the brown rot fungi, Coniophora puteana, Gloeophyllum trabeum and Serpula lacrymans were near or above the fibre saturation point of pine and spruce, sap and heartwood, during 160 days incubation according to the standard method EN 113. The moisture of wood for the optimum growth of Coniophora puteana and Serpula lacrymans was about 35-80% and fo...
H Viitanen, A-C Ritschkoff


Effects of seed origin and site on both wood density and longitudinal fluid uptake of Sitka spruce (Picea sitchensis (Bong.) Carr.) with height in the tree grown in the United Kingdom
2002 - IRG/WP 02-40226
The variation in density and longitudinal fluid uptake was investigated in short specimens of wood taken from eight seed origins of Sitka spruce trees grown at two sites in the UK. Five trees of each seed origin at each site were sampled at three heights (1, 2 and 3 m above ground level). The density of the samples decreased with increasing height within the stem. This corresponded with increasin...
I Usta, M D C Hale


Strength properties of preservative treated pine and spruce wood after super-heated steaming
1984 - IRG/WP 3313
Possible changes of strength properties of CCF pressure impregnated pine and spruce with subsequent steaming at 110°C respective 120°C for 30 min were examined. For spruce analysis of variance indicated that none of the processes had a significant effect on bending strength, compression strength and the corresponding modulus of elasticity as well as on impact bending strength and shear strength ...
R-D Peek


Cellular and fractural failure after supercritical fluid impregnation of four wood species
2004 - IRG/WP 04-10503
Supercritical fluids (SCFs) have been investigated for delivering biocides into sawn wood. Pressure differentials during treatment may exceed the compressive or tensile strength perpendicular to grain, creating a potential for transverse deformations that exceed elastic strain limits. Wood treated by SCF processing with CO2, a potential biocide carrier, was inspected macroscopically and microscopi...
M E Anderson, R J Leichti, J J Morrell


The comparative resistance to fungi of the wood munika (Pinus heldreichii Christ.), fir (Abies alba Mill.) and spruce (Picea excelsa Poir.) compared with Pinus sylvestris L. and some physical and mechanical characteristics of munika
1981 - IRG/WP 1129
The munika (Pinus heldreichii Christ.) is situated primarily in the Balkans, and partially in the south of the Apenine peninsula. As an endemic species, with a very little annual increment, it has not been used enough as a timber for mechanical conversion up till now, although the oldest trees can grow to 27 m in height, with a diameter at breast height of about 60 cm. According to data of many Ba...
M Petrovic, M Miric


Immuno-electron microscopic localization of extracellular metabolites in spruce wood decayed by brown-rot fungus Postia placenta
1990 - IRG/WP 1441
Degradation by Postia placenta in spruce and birch wood was shown to occur not only in the wood cell wall but also in the middle lamellae region. Middle lamellae was often found to be degraded along the centerline so that cells could separate along this line. Extracellular membrane structures were found surrounding the hyphae and this matrix labelled positively with antisera produced to Postia pla...
Y S Kim, B Goodell, J Jellison


Durability of heat-treated wood
1999 - IRG/WP 99-40145
Heat-treated wood from the French process were laboratory tested against decay using agar block test and a modified soil block test. Water absorption, bending strength, lignin content and acid number were also determined to evaluate the effect of heat treatment. Heat treated samples exhibit a higher lignin content and a lower acid number compared to untreated control indicating the degradation of ...
D P Kamdem, A Pizzi, R Guyonnet, A Jermannaud


Supercritical fluid treatment: Effects on bending strength of white spruce heartwood
1993 - IRG/WP 93-20008
The effects of supercritical carbon dioxide on wood strength were evaluated using white spruce heartwood, a species known to be especially susceptible to collapse during exposure to higher pressures. The effects of pressures of 2000 or 3600 psig and temperatures of 40 or 80°C were evaluated using 30 or 60 minute exposure periods. No significant differences were noted in modulus of rupture or modu...
S M Smith, J J Morrell, E Sahle-Demessie, K L Levien


Movement of borates in a range of timber species at various moisture contents
1998 - IRG/WP 98-30181
Borate-based wood preservatives are used in industrial pre-treatment as well as remedial treatment of timbers in situ. In both of these areas, understanding the mobile nature of these compounds is important in optimizing the main benefits of borates. Considerable work has been conducted on movement of borates in dip-diffusion treatment of freshly felled wood, as well as focusing on subsequent diff...
M W Schoeman, J D Lloyd, M J Manning


Differences in pH, electrical resistance, cation composition and NIR spectra of red spruce wood during early stages of brown rot degradation
2002 - IRG/WP 02-10449
Red spruce sapwood was exposed to degradation by the brown rot fungi Coniophora puteana, Postia placenta, Gloeophyllum trabeum and Serpula lacrymans for 0, 1, 2 or 3 weeks using a modified soil block assay design. Average weight losses over time ranged from 0-8.9% during this time period. Detectable changes in pH, electrical resistance and cation compostion were observed in the wood as early as 1 ...
J Jellison, S Kelley, B Goodell, D Hui, A Ostrofsky


Färbeverfahren zur Unterscheidung von Holzzonen mit unterschiedlichem Absorptionsvermögen, insbesondere bei Fichtenholz (Picea abies Karst.). [Staining method for distinguishing zones of wood with different absorption behaviour, particularly in spruce (Picea abies Karst.)]
1980 - IRG/WP 3163
A simple regressive staining method for crosscut wood surfaces is described. Phloroglucinol-hydrochloric acid serves as stain; flowing water and a solution of sodium carbonate are used for development and fixation of a picture showing the differences of absorption. Hydrophobic zones and, contrary to this, zones with a high water content can also be shown. Comparing green spruce wood before and dur...
S Cymorek


Sawn timber of fir (Abies alba Mill.) - Treatability and usability for the Hazard Classes 3 and 4
1999 - IRG/WP 99-40147
Within a national research project, tests on the treatability on sawn timber of fir (Abies alba Mill.) in oscillation pressure, vacuum pressure and double-vacuum processes have been worked out with 95 trunks taken from 3 different altitude levels (up to a height of 590 metres, 600 to 990 metres and over 1000 metres) and from 4 different regions of Switzerland. As the treatability of round wood can...
E Graf, T Bör


Influence of surface coating on the leachability of boric acid and bifluorides from spruce wood
1995 - IRG/WP 95-50050
In the Netherlands, window joinery made from non-durable timber species (spruce) are widely protected with preservative rods. These rods contain non-fixing wood preservatives (e.g. bifluorides or boric acid). This reseach was performed to show the possible influence of a coating system to hinder the leaching of the active ingredients. The results of the leaching tests show, that bifluorides and ev...
W J Homan, H Militz