Leaching of the new boron based biocide from coated wood
2001 - IRG/WP 01-30267
We investigated leachability of the new boron based biocide - a complex of an amine and boric acid - from vacuum impregnated spruce wood samples. It was determined by the standard ENV 1250-2 procedure that the new biocide is susceptible to leaching so from the water borne as well as from the ethanol borne boron containing preservative treated wood. Leaching may be retarded by application of surfac...
M Petric, M Pavlic, F Cadez


Performance results of wood treated with CCA-PEG
1986 - IRG/WP 3363
The addition of polyethylene glycol (PEG) to the CCA system has been shown to reduce the surface hardness of poles and ease spur penetration during climbing. This paper addresses the results of tests dealing with preservative retention and penetration, permanence of CCA and PEG, strength, drying rate, and checking characteristics....
W P Trumble, E E Messina


Effects in vivo of various tensides (surface-active agents) on Reticulitermes santonensis De Feyteaud
2001 - IRG/WP 01-10417
The results of studies of surface active agents (tensides, surfactants) on the feeding behavior and mortality of Reticulitermes santonensis De Feyteaud are described. The effects of these agents on the nature and relative populations of eight gut-inhabiting symbionts are also examined. Among the various tensides tested, bee's poison was the most effective in causing rapid termite death. A...
W Unger


Factors affecting leaching of preservatives in practice
1978 - IRG/WP 3113
At the 7th Meeting of the IRG in Poland in May 1975, the findings of collaborative laboratory leaching techniques were discussed, and the dangers inherent in using such results to predict the behaviour of preservative-treated components in service were emphasised. In order to improve our understanding of the factors governing leaching of preservatives in practice, and to identify areas where furth...
R Cockcroft, R A Laidlaw


Performance of surface-treated hardwoods and softwoods out of ground contact
1990 - IRG/WP 3592
A number of fungicides were tested as brush treatments for protection of southern pine, Douglas-fir, maple, and red oak against decay above ground. Cross-brace and L-joint test units were treated just before assembly and exposed from 3-10 years. Untreated Douglas-fir cross-brace units were not decayed at either the Mississippi or Madison, WI, site. Untreated red oak cross-brace units were not deca...
T L Highley


Protecting wooden structures
1980 - IRG/WP 392
Chromium-containing chemicals that effectively retard weathering of wood improve performance of subsequently applied finishes. Current work is focusing on the performance of wood-derived products (plywood, hardboard, fiberboard, particle board) after surface treatment with inorganic chemicals. The overall objective of the continuing research is to investigate new environmentally safe procedures to...
W C Feist


The influence of formulation on the behaviour of LOSP's during industrial impregnation of spruce
1986 - IRG/WP 3387
Evidence is presented that the comparative behaviour of two LOSP formulations during impregnation treatment of spruce cannot be predicted purely on the basis of their physical characteristics (viscosity, surface tension and contact angle) nor on the extent of their 'passive' penetration into pine sapwood....
L D A Saunders, D M Zuvencko


Effects of the addition of polyethylene glycol to the CCA-C preservative treatment
1985 - IRG/WP 3337
A modification of the CCA-C wood preservative system for utility poles has been investigated to see if spur penetration into the poles is assisted during climbing. Addition of polyethylene glycol to the CCA system has been shown to accomplish this purpose. This paper addresses the effects of the addition of polyethylene glycol to other physical properties germane to utility poles....
W P Trumble, E E Messina


Effects of timber surface properties and dipping conditions on uptake of antisapstain actives from two aqueous suspensions, and ultimate effects on efficacy against mould and staining organisms
1995 - IRG/WP 95-30073
Green-off-saw rough sawn Pinus elliottii (slash pine) boards were dipped in aqueous suspensions of two antisapstain formulations, and the resultant surface retentions of active ingredients MTC (methylene bisthiocyanate), CTL (chlorothalonil) or TCMTB (2(thiocyanomethylthio)benzothiazole) were monitored by chemical analysis. Surface retentions increased with suspension concentration and surface rou...
M J Kennedy, T L Woods


Evaluation of the leach resistance and preservative efficacy of novel biocides as surface treatments applied by brush to spruce (Picea abies)
1998 - IRG/WP 98-30170
The comparative leach resistance and preservative efficacy of a number of alternative organic preservatives (available from Zeneca Specialties) and selected commercially available biocides as surface coatings to wood in Hazard Class 3 have been assessed. Two concentrations of test preservatives were applied by brush to Spruce (Picea abies), including formulation and untreated controls. A leaching ...
I M Tierney, A Bruce, D C R Sinclair, T Yeates


Practical testing of wood preservatives to prevent weathering damage and infection by micro-organisms on spruce and pine
1989 - IRG/WP 3530
Brush application, is generally used to prevent wooden window frames from decay caused by influence of weathering and fungi. Accordingly 10 boards of pine (Pinus sylvestris) and spruce (Picea abies) were treated with 10 commercially used wood preservatives. The efficiency of fungicides by using chiptest and blue stain test (EN 152), the effectiveness against weathering as well as the course of col...
R Gründlinger, O Janotta, H Melzer, K Messner


The resistance of wood coated with different solvent-borne paints against colonisation by decay fungi
2009 - IRG/WP 09-40468
This paper examines different solvent-borne paints characteristics and their decay resistance when applied on pine wood surface. It was determined by the standard ENV 839 procedure. The part of samples were subjected to accelerated ageing according to the EN 84 standard. The discussed commercial paint systems were typical stains or penetrating oil-based products, with or without biocides....
B Mazela, P Hochmańska


Exploring the potential for plasma-assisted coating at atmospheric pressure for wood protection
2023 - IRG/WP 23-40982
J Profili, G Laroche


Factors affecting the sorption of preservative during diffusion treatment of wood
1988 - IRG/WP 3500
The sorption of preservative into wood during soaking in aqueous solution was found to comprise absorption as well as diffusion of solute. Absorption was increased by partially seasoning the wood prior to soaking and was characterised by (a) a very rapid initial rate of uptake and (b) an extended period of slow uptake, the rate of which varied with prior conditioning. It was concluded that some pa...
P Vinden


The effect of service life and preservative treatment on the hardness of wooden poles
1989 - IRG/WP 3537
The surface hardness of utility poles is an important parameter which effects the acceptability of the pole as being safe to climb during line maintenance. The current investigation was designed to evaluate how the surface hardness of preservative treated utility poles is effected by the type of preservative, and the age of the poles. Chromated-copper-arsenate (CCA) treated red pine and jack pine ...
E B Jonsson, E M A Nilsson, J N R Ruddick


Inspection method of surface checking of Sugi posts
2003 - IRG/WP 03-20272
In order to establish the method for evaluating the checking of Sugi posts, checks on exposed posts were examined. Checks on Sugi posts exposed for 18 months were superficially inspected, that is, the length, width, and depth of the checks were measured from the outside with a ruler and 0.1 mm thick feeler gauge. Then, each post was cut into cross sections of the 30 mm width, and the check depth w...
H Kurisaki, H Nakatani, K Mizumoto


Washboard effect: A surface deformation of spruce resulting from vacuum-pressure impregnation with water-borne preservatives
1987 - IRG/WP 3450
The washboard effect has been observed in sawn spruce after both commercial and laboratory based preservative treatments and is of increasing economic importance. The effect is defined as a specific phenomenon at the wood surface. It is distinct from internal collapse in the wood, but it may occur in association with internal collapse damage. Experimental investigations on the causes of washboardi...
H Willeitner, R J Murphy


The efficacy of polyurethane coatings on wood samples exposed in the marine environment. Final Report -10 Year Assessment
1996 - IRG/WP 96-10170
The results of an IRG collaborative marine trial to investigate the long-term permanence and efficacy of polyurethane coatings against marine borers are reported. PU-coated wood samples were exposed at a range of sites from tropical to cold temperate locations. The marine borer species present at the sites included teredinids, pholads, limnoriids and sphaeromatids so that each site offered its own...
R A Eaton


How to keep coated wood structures sufficiently dry to avoid damage caused by rot
1991 - IRG/WP 2376
During the last ten years, a new type of problems with wood rot has emerged in Scandinavia. Thousands of houses have been damaged by wood rot attaching to the exterior wood panel. This paper provides an overview of finished and ongoing work in order to identify the cause of these problems. In field tests, the moisture conditions were measured in panels coated with different paint systems. The infl...
S Hjort


Influence of a dipping preservative treatment on the performance of wood finished with waterborne coatings
1998 - IRG/WP 98-40121
Within a larger European research project on the performance of joinery finished with waterborne coatings, the influence of a water based dipping preservative treatment was studied in several ways. Six different waterborne coatings were tested with and without a preservative underneath the coating. The performance was tested on pine sapwood and spruce panels in a 2-year outdoor weathering trial on...
M De Meijer, J Creemers, W Cobben, P Ahola


Chromium on the surface of CCA-treated wood
1978 - IRG/WP 386
Chromium in solutions of CCA preservatives is predominantly in the hexavalent state (Cr VI). It is well known that Cr VI is associated with dermatitis and skin ulceration in workers handling chromium containing products and processes. When reduced to the trivalent state, however, chromium is considerably safer. An essential part, therefore, of safety procedures in any chromium - using industry is ...
C R Coggins, P Hiscocks


Relationship between bond strength and surface characteristics of CCA-treated Douglas-fir
1993 - IRG/WP 93-30008
Chromated-copper-arsenate (CCA) treated Douglas-fir was laminated using a commercial phenol-resorcinol resin. CCA treatment enhanced the water repelleney of wood espeeially in the presence of extractives. However, the shear strength of CCA treated wood was 12% lower in dry condition and 38% lower in wet condition after six cycles of vacuum-pressure test than that of untreated wood. Slight removal ...
K Yamamoto, J N R Ruddick


Resistance of painted wood to mould fungi. Part 2. The effect of wood substrate and acrylate paint systems on mould growth
1997 - IRG/WP 97-10234
Resistance of acrylate paint systems on different types of pine and spruce sapwood to mould fungi was studied. Dipping into the preservative prior to painting, a primer with and without a fungicide (propiconazole + IPBC 0.50 + 0.2%) and a topcoat with and without a fungicide (propiconazole + IPBC 0.25 + 0.12%) were combinations of the treatments studied. The efficacy of the treatment systems varie...
H Viitanen, P Ahola


Changed permeability and surface properties of hornbeam wood due to its degradation by erosive strain of Phanerochaete chrysosporium
2004 - IRG/WP 04-40290
Specimens of hornbeam wood were submitted to a medium-term degradations by erosive fungus Phanerochaete chrysosporium. Biodegradations of specimens resulted in their apparent structural alterations, changes in permeability and increased intensity of interactions with polar liquids. Modified physical properties of biodegraded wood may significantly influence its penetration with polar media and che...
R Solár, S Kurjatko, L Reinprecht, M Mamon, V Vacek


Natural weathering of wood in a sunny climate effects on surface chemistry and paint adhesion
1997 - IRG/WP 97-20109
Radiata pine veneers and blocks were exposed to natural weathering under Australian summer conditions over a period of 30 days. Infrared spectroscopy revealed that there was perceptible surface delignification after 4 hours exposure, substantial surface delignification after 3 days exposure and almost complete surface delignification after 6 days. Viscometry determinations on holocellulose samples...
P D Evans, P D Thay, K J Schmalzl