Your search resulted in 3425 documents. Displaying 25 entries per page.


Do insects infest wood packing material with bark following heat-treatment?
2007 - IRG/WP 07-10633
As a result of international trade, many bark- and wood-infesting insects are inadvertently transported in wood packing materials (WPM) such as crating, dunnage, and pallets. WPM is suspected as the likely pathway for most of these borers, although the exact mode of entry into the USA is unknown for all 25 borers. The top 10 countries of origin were, in decreasing order, Italy, Germany, China, Spa...
R A Haack, T R Petrice, P Nzokou, D P Kamdem


Evaluating the Process of ACQ-Treated Woods with TGAand CEM Analysis
2007 - IRG/WP 07-20374
To provide an understanding of the fundamental thermal behaviour and the disposal-end products of ACQ-treated woods, this study is comprised of two categories of examination. The first is related to the use of TGA under different thermal decomposition conditions (nitrogen or air, and 5 or 40 oC/min), and the use of EDX to examine certain residual elements of the char. The second applies the CEM ...
Han Chien Lin, Tsang-Chyi Shiah, Jung Ting Tsai


Fire Safety of Wood Floor Assembly: Model and Full-scale Test
2007 - IRG/WP 07-20375
The present paper describes the model for the prediction of fire safety of wood floor assemblies. The model includes heat transfer model for the calculation of the flow of heat in floor assembly and structural model for the analysis of the mechanical performance of wood joists. The floor assemblies considered in this paper are constructed with nominal 2x10 (38x241mm) wood joists lined by Type X ...
H Takeda


Durability of some alternatives to preservative-treated wood. Progress report 2: Results from field tests after 5 years’exposure
2007 - IRG/WP 07-30442
A number of alternatives to preservative-treated wood have been tested according to EN 252 (stake test) and a specially designed ground-proximity field test, the latter in Sweden as well as in Hawaii, USA. Seven untreated wood species and four alternative wood treatments labelled as environmentally friendly (acetylation, linseed oil, heat treatment, vinyl polymer) were included in the study. Four ...
M-L Edlund, J Jermer


Detection of Anti-Fungal Sapwood Extractives in Non-Durable Scots Pine (Pinus sylvestris), Rubberwood (Hevea brasiliensis) and Jelutong (Dyera costulata)
2007 - IRG/WP 07-10634
A general laboratory bioassay method of Woodward and Pearce (1985) was adopted to detect anti-fungal activity of sapwood or heartwood extractives of 5 Malaysian hardwoods [dark red meranti heartwood (Shorea spp.), red balau heartwood (Shorea spp.), kulim heartwood (Scorodocarpus borneensis), jelutong sapwood (Dyera costulata) and rubberwood sapwood (Hevea brasiliensis), including the temperate Pin...
A H H Wong, R B Pearce


Evaluatiang the potency of cinnamaldehyde as a natural wood preservatives
2007 - IRG/WP 07-30444
Since cinnamaldehyde, the major constituent of leaf essential oil from Cinnamomum osmophloeum, has significant antifungal and antitermitic activities, it is worthy of understanding whether cinnamaldehyde has potential to be used as a natural preservative for improving the durability of wood. In this study, the fungi and termite resistance of cinnamaldehyde-treated wood (CTW) were evaluated accordi...
Chun-Ya Lin, Chi-Lin Wu, Shang-Tzen Chang


Effect of cinnamon oil and clove oil against major fungi identified from surface of rubberwood (Hevea brasiliensis)
2007 - IRG/WP 07-30446
Antifungal activities of cinnamon oil and clove oil at ratio 1:1 and pure against major fungi found on surface of rubberwood (Aspergillus niger, Penicillium chrysogenum, and Penicillium sp.) were investigated using the broth dilution method. The minimum inhibitory concentration (MIC) of the combined cinnamon and clove oils for these test moulds was determined to be 80 µL/mL which were less than o...
Narumol Matan, Nirundorn Matan


Potential of some insecticides as wood protectants in South Indian condition
2007 - IRG/WP 07-30447
Wood continues to be one of the most widely used raw materials in spite of the introduction of many modern materials. This naturally renewable resource being an organic matter is amenable to the attack of biodeteriorating organisms. Though some wood species are known for their natural resistance to agents of biodeterioration, their availability is constantly decreasing, besides being too expensive...
R Sundararaj, O K Remadevi, R Muthukrishnan


Difficulties applying Heat Treatment according to ISPM No. 15, when fast growth species are used
2007 - IRG/WP 07-40386
In 2002, the Interim Commission on Phytosanitary Measures (ICPM) adopted the International Standard for Phytosanitary Measures (ISPM) No. 15 (Guidelines for regulating wood packaging material in international trade). Two treatments are recognized: Heat Treatment (HT), in which wood must be heated to a core temperature of 56°C for 30 minutes, and fumigation with methyl bromide. As the last treatme...
O Encinas, J. I Briceño


Effect of fiber type and content on the natural durability of wood flour/high density polyethylene composites against rainbow fungus (Coriolus versicolor)
2007 - IRG/WP 07-40387
In order to evaluate the effect of fiber type and content on the natural durability of wood flour/high density polyethylene (HDPE) composites against Coriolus versicolor, samples containing 25% and 50% by weight of various natural fibers and HDPE were selected. Natural fibers included in the study were wood flour, rice hulls, hemp fibers and newsprint. Samples containing 25% and 50% natural fiber ...
A Karimi, M Tajvidi, S Pourabbasi


Effect of Compatibilizer on the Natural Durability of Wood Flour/High Density Polyethylene Composites Against Rainbow Fungus (Coriolus versicolor)
2007 - IRG/WP 07-40388
To evaluate the effect of compatibilizer on the natural durability of wood flour/high density polyethylene composites against Coriolus versicolor, composites containing 25% and 50% by weight maple wood flour and 1% and 2% compatibilizer (Maleic anhydride polyethylene (MAPE)), respectively, were sampled. Identical specimens of the same composites without the compatibilizer were also prepared. ...
Sara Pourabbasi, A Karimi, D Parsapajouh, M Tajvidi, M Soleymani


Run-off quality from sprinkled debarked logs and logs with bark from Picea abies and Pinus contorta
2007 - IRG/WP 07-50248
Storage of roundwood is necessary for efficient industrial production at sawmills and pulpmills. The need for wood storage becomes even more critical when large storm fellings create huge volumes of wood that is at risk for deterioration. In Scandinavia, the technique of sprinkling of water on roundwood is used to protect stored wood from fungal and insect infestation and drying during the summer....
M Jonsson


Development of boron/linseed oil combined treatment as a low-toxic wood protection. Evaluation of boron fixation and resistance to termites according to Japanese and European standards
2007 - IRG/WP 07-30448
Combinations of boric acid as a first step of treatment and linseed oil as a second step have been performed in order to enhance boron retention to leaching and wood resistance to termites. Classic leaching and termites resistance standards are inappropriate to evaluate this combination which can be considered as both a wood core preservation treatment and a coating. Japanese Industrial Standard...
F Lyon, M-F Thevenon, Y Imamura, J Gril, A Pizzi


An Investigation on Use and Durability of Some Industrial and Domestic Woods of Iran against Destructive Factors in Caspian Sea
2008 - IRG/WP 08-10636
In this study the use of domestic and commercial woods of the Caspian Sea forest fringes and evaluation of their durability against marine destructive factors were investigated. The samples of elm (Zelkova carpinifolia), oak (Quercus castanifolia), beech (Fagus orientalis), Maple (Acer insgin), Alder (Alnus subcordata), and horn beech (Carpinus betulus) species were impregnated with CCA (Chrome–...
S M Kazemi


Influence of ring width and wood density on durability of oak heartwood
2008 - IRG/WP 08-10639
Oak (Quercus sp.) is considered as one of the most durable European wood species. The most important factor influencing oak durability was extractive content. In our work, we were interested in if oak-wood durability is affected by ring-width and related density. Therefore, oak heartwood specimens made of boards with different ring widths were exposed to five different fungal species Daedelea quer...
M Humar, P Oven, F Pohleven


A hypothesis on a second non-biocidal property of wood extractives, in addition to toxicity, that affects termite behavior and mortality
2008 - IRG/WP 08-10638
While it is has long been recognized that heartwood extractives affect termite behavior, the exact cause and relationship between total extractives, extractive types, and termite resistance remains unclear. Generally, researchers have proposed that the extractives are toxic and/or repel termites. We propose, based on the well known fact that many extractives have excellent antioxidant properties...
T P Schultz, K Ragon, D D Nicholas


Brief introduction of a research project on the wood materials from an ancient Byzantine port unearthed during drilling for underground rail tunnel in Istanbul
2008 - IRG/WP 08-10641
A research project has been recently started to evaluate some properties of wooden materials from the biggest port of ancient times called Port of Theodosius I in Istanbul, Turkey. The ruins of the ancient Byzantine port during the excavations were recently uncovered in the Yenikapi site where an underground rail tunnel construction has been in progress in Istanbul. The wooden objects unearthed fr...
A D Dogu, C Köse, S N Kartal, N Erdin


Performance of softwood preservative treated stakes after 4 years exposure in-ground to decay fungi and termites in tropical Australia
2008 - IRG/WP 08-10643
This field study was based on the 1993 IUFRO method and designed as a graveyard (in-ground) test in the tropical region of the Northern Territory to examine the efficacy of novel preservative formulations developed as alternative protection for softwood timber against decay fungi and termites for Hazard Class 3 and 4. This study was supported by the Forest and Wood Products Research and Develop...
B M Ahmed (Shiday), J R J French, S R Przewloka, P Vinden, J A Hann, P Blackwell


Quantitative and qualitative losses in wood of oriental spruce, Picea orientalis (L.) Link., induced by insects from forest to utility
2008 - IRG/WP 08-10647
In this study, some quantitative and qualitative losses in wood of oriental spruce, Picea orientalis (L.) Link., induced by insects from forest to utility were evaluated. In experimental plots, volume of trees damaged by Dendroctonus micans (Kug.) was 34% of the volume of total standing spruce trees in the oriental spruce forests of Turkey. The volume of standing trees that D. micans damaged was ...
H A Akinci, M Eroglu, G E Özcan, Ü C Yildiz


Needs for wood durability research on planted tree species in the tropics
2008 - IRG/WP 08-10651
The area of forest plantation has been expanding especially in tropical Asia since 1990’s. Most of them are developed for pulp and paper industries and planted with fast growing trees. It is expected that wood from those fast growing trees are also used for value added products such as sawn timber. In order to promote the utilization of fast wood as the resource of value added products, natural...
K Yamamoto, T Toma, Ngo Duc Hiep, Nguyen Trong Nhan


A step towards a better understanding of fungal colonization of modified wood - QRT-PCR studies
2008 - IRG/WP 08-10653
The area of wood protection is in a period of change. New wood protection systems have been developed while their mode of action remains insufficiently understood. The development of molecular methods provides potential tools to investigate the interaction between modified wood and decay fungi. One small step to tackle some of the unsolved questions about the mode of action of modified wood is tak...
G Alfredsen, A Pilgård, A Hietala


Characterization of protein patterns from decayed wood of loblolly pine (Pinus taeda L.) by proteomic analysis
2008 - IRG/WP 08-10654
The primary biotic decomposers of wood belong to the basidiomycetes. The members of this group can attack and biodegrade both wood in the forest and in service. By the time wood decay is visible, there has already been a significant loss of strength. The identification of basidiomycetes and other organisms on wood only tell us what is present, not what is actively decaying the wood. When organisms...
Young-Min Kang, L Prewitt, S Diehl


A Review of Wood as Material and Source of Innumerable Products
2008 - IRG/WP 08-10662
As we known that “wood –which is a source of innumerable pruducts (Tsoumis, 1968)– is a fascinating and challenging material (Dinwoodie, 1975)”, and hence, “an understanding of the basic properties of wood and of the factors that affect its serviceability is vital background for the preservation of wood structures (Sherwood, 1986)”. This paper therefore presents an overview of structru...
I Usta, R Despot


Water Absorption of Various Building Materials and Mold Growth
2008 - IRG/WP 08-10657
Mold growth is a major problem for house owners, as it often occurs on the surface of building materials in damp houses. The principal method to control mold growth on building materials is to prevent water penetration into the materials. A study was recently conducted to determine water absorption rates of different wood species and panel materials used as building materials, when water intrusi...
Dian-Qing Yang


Natural durability of fast growth plantation Eucalyptus grandis Hill, ex Maiden
2008 - IRG/WP 08-10660
One of the fast growing species cultivated in Uruguay of mayor economical importance is Eucalyptus grandis. Physical and mechanical properties of juvenile and mature wood from different regions have been deeply studied. However, since no scientific data of natural durability of this specie has been reported, natural durability of E. grandis from two sites (Rivera and Rio Negro) was evaluated. Two ...
S Böthig, A Sánchez, J Doldán