Your search resulted in 3254 documents. Displaying 25 entries per page.
Copper to quat ratio in alkaline copper quat (ACQ) wood preservative - Effects on fixation and leaching of preservative components in red pine
2009 - IRG/WP 09-30496
This study investigates the effect of the relative proportion of copper oxide (CuO) to didecy dimethyl ammonium carbonate (DDACb) in an alkaline copper quat (ACQ) formulation on the rate of copper fixation or stabilization and the resistance of treated wood to leaching of copper and quat (DDACb). Red pine samples were treated with ACQ, having CuO to DDACb ratios of 2:1 (the normal ratio for ACQ-D...
S Pankras, P A Cooper, T Ung, L Awoyemi
Leaching performance, decay and termite resistance of wood treated with boron compounds incorporated with phenol-formaldehyde resin
2009 - IRG/WP 09-30503
A resol-type phenol-formaldehyde (PF) resin was synthesized and designed to penetrate wood incorporated with boron compounds in order to immobilize boron in wood. The leaching performance, decay and termite resistance of treated wood was investigated. Three kinds of boron compounds, that is, boric acid (BA), borax (BX) and disodium octaborate tetrahydrate (DOT), were selected to mix with PF and tw...
Liping Yu, Jinzhen Cao
Resistance to decay fungi of ammonium borate oleate treated wood
2009 - IRG/WP 09-30505
Ammonium borate oleate molecule (ABO) produced from reaction between boric acid, ammonia and oleic acid was tested as wood preservative treatment against brown and white rot fungi according to European standards. This compound was prepared according to a previous study which has proved existence of synthesis reaction and effectiveness against termites (Lyon et al. 2007b). Four solutions of ABO in ...
F Lyon, M-F Thevenon, A Pizzi, J Gril
Micronized Copper Preservative Systems: Observations on the Release of Cupric ion (Cu2+) from Treated Wood and Performance against Wood Decay Fungi
2009 - IRG/WP 09-30519
In an attempt to address the mechanism of action of micronized copper preservatives, a 20-week continuous water leaching study was conducted. The leaching results indicated that, once impregnated in wood, micronized copper preservatives continuously release cupric ion, and the levels of cupric ion released from micronized copper treated wood are higher than those released from CCA treated wood, a...
J Zhang, R Ziobro
Material properties of furfurylated wood for window production
2009 - IRG/WP 09-40480
Wood modification with furfuryl alcohol is an extensively investigated process and already produced commercially. Furfurylated wood is in the focus of a European project on its use for the production of high performance windows. Different wood species were treated with furfuryl alcohol and tested on water uptake, dimensional changes, leaching in water, resistance to fungal degradation, and ecotoxi...
A Treu, A Pilgård, S Puttmann, A Krause
Mobility of Copper from MCQ in Shell-Treated Wood Exposed Above Ground
2010 - IRG/WP 10-30534
Most Canadian treated decking in service has been given just a thin shell of preservative treatment but it has still performed very well. This is because copper migrated into checks and prevented germination of basidiospores on the freshly exposed untreated wood. Unlike soluble copper systems, MCQ has its copper primarily in the form of small basic copper carbonate particles. For MCQ to be effecti...
R Stirling, P I Morris
Treatment of Scots pine wood with oil in water and water in oil emulsion systems: Effects on boron leaching and water absorption
2010 - IRG/WP 10-30535
The aim of this study was to investigate the water absorption and water repellent efficiency of oils and oil water emulsions [oil-in-water (O/W) and water-in-oil (W/O)] and possibilities of reducing the amount of boron leaching from treated wood. Scots pine wood samples treated with waste or sunflower oil and water formulations contained 3%BA. The level of water absorption and water repellent effi...
E D Tomak, Ü C Yildiz, A Can
Distribution and availability of preservative components in ACQ treated wood - effects of coatings and weathering
2010 - IRG/WP 10-30537
Copper and quaternary ammonium compound (quat) distributions across lumber (gradients) and availability, as measured by amount removed by intensive leaching of wood flour, were measured in ACQ treated southern pine lumber. Samples were evaluated just after treatment and stabilization, or after 3 years of laboratory storage, or after 3 years of natural weathering exposure. The objective was to in...
T Ung, M Nejad, P Cooper
Comparison of laboratory and semi-field tests for the estimation of leaching rates from treated wood
2010 - IRG/WP 10-50274
The authorization of wood preservative formulations in the European Union according to the Biocidal Products Directive (BPD) includes the assessment of environmental risks by the emission of active ingredients. This risk assessment includes scenarios for preserved wood (e.g. house scenario, noise barrier), in which the predicted environmental concentration (PEC) for soil and water is calculated, u...
N Morsing, M Klamer, B Seidel, J Wittenzellner, M Maier, J Habicht
Sample Origin Influencing the Leachability of Wood Preservatives
2011 - IRG/WP 11-20474
The aim of this study is to see if the raw material influences fixation and leachability of wood preservatives. Moving towards more eco-friendly and –concious society, the wood industries must adjust itself to new rules and regulations. Greener solutions in wood protection are being tested and introduced, older systems are being improved, but questions still arise concerning some elements curren...
K Kängsepp. E Larnøy, P Meier
Influence of wood swelling agents on penetration and copper leaching of copper-ethanolamine based wood preservatives
2011 - IRG/WP 11-30556
Copper ethanolamine based preservatives are currently the most important solutions for impregnation of wood in ground contact in Europe. One of the issues related to those and similar water based solutions is insufficient penetration to refractory wood species like Norway spruce. In order to elucidate this issue, commercial copper ethanolamine based solution was supplemented with five different wo...
M Humar, N Thaler, B Lesar
Effect of P/F ratio, PF concentration and treating method on boron leaching from wood treated with PF modified boron compounds
2011 - IRG/WP 11-30559
In order to immobilize boron in wood, three kinds of resol-type phenol-formaldehyde (PF) resin with different P/F ratios were synthesized in laboratory and incorporated with three types of boron compounds to treat wood. The used boron compounds included boric acid (BA), borax (BX) and disodium octaborate tetrahydrate (DOT). The leaching test of boron from wood blocks was performed according to the...
Liping Yu, Jinzhen Cao
Characterizing long term leaching behaviour of copper from preservative treated wood in a practical exposure scenario
2011 - IRG/WP 11-50278
To investigate the prediction of the long term emission of copper from preservative treated wood in a Use Class Class 3 scenario, treated boards were exposed vertically above ground to natural weather conditions. The study included two products; an amine copper ACQ-type formulation, air-dried after treatment to a 22 kg/m3 retention, and the same formulation which was hot oil vacuum dried after tre...
T Mark Venås, M Klamer
Copper Migration from Micronized Copper Preservatives Treated Wood in soil contact:
2011 - IRG/WP 11-50280
Emerging formulations of preservatives made with micronized basic copper carbonates with azoles and/or quat to control copper tolerant fungi have been used to replace formulations containing soluble copper to reduce the leaching of copper and the corrosion of metal in contact with wood. This study proposes to use laboratory soil leaching test AWPA standard (E20-08) to estimate the amount of copper...
Lei Wang, D P Kamdem
Determination of the natural durability of solid wood against wood-destroying fungi - a European round-robin test
2013 - IRG/WP 13-20511
In Europe the durability of wood against wood-destroying basidiomycetes is tested according to CEN/TS 15083-1 (2005). Hitherto existing experience with this standard is quite heterogeneous and results from previous round-robin tests have stayed unreported or have been reported incompletely. In particular the need for natural pre-weathering of the test specimens to allow potential detoxification of...
C Brischke, C R Welzbacher, A Gellerich, S Bollmus, M Humar, K Plaschkies, W Scheiding, G Alfredsen, J Van Acker, I De Windt
Preliminary testing of spiroborate esters as wood preservatives
2013 - IRG/WP 13-30614
Fungicide and insecticide properties of boric acid are known since 30’s of the last century, but high solubility and leachability of inorganic borates limit their use for only applications not directly exposed to liquid water. A number of attempts were made to fixate borate salts into the wood structure but this research topic is still up to date and undiscovered. Water insoluble organoboron est...
D Panov, N Terziev
The Effect of Water Repellent on Semi-Field Leaching of Active Substances from Metal Free Wood Preservative Formulation
2013 - IRG/WP 13-30615
The risk assessments for the use of wood preservatives proposed by the OECD and used under the Biocidal Products Directive (BPD) (98/8/EC) require the derivation of leaching rates for active substances. These rates are to be used as input data in to agreed exposure scenarios. A comparison of the leaching of active substances from wood treated with a metal free preservative formulation with and wit...
D G Cantrell
Copper leaching from copper-ethanolamine treated wood during exposure to terrestrial microorganisms
2013 - IRG/WP 13-30621
Copper-ethanolamine based wood preservatives are still the most important solutions for protection of wood in ground applications in Europe. Wood in ground is exposed to variety of organisms, which can act synergistically. In order to simulate these conditions in laboratory, Scots pine (Pinus sylvestris) specimens impregnated with copper-ethanolamine preservative of three different concentrations ...
M Humar, N Thaler, B Lesar
Combined effects of thermal modification and ACQ-D impregnation on properties of southern yellow pine wood
2013 - IRG/WP 13-40637
In this study, samples of southern yellow pine sapwood were first thermally modified and then treated by the alkaline copper quat-type D (ACQ-D) wood preservative. Two heating temperature (180℃ and 220℃) and two concentrations of ACQ-D solution (0.9% and 1.35%) were used in the experiments. The combined effects of thermal modification and ACQ-D on leaching performance, mechanical prope...
Wang Wang, Yuan Zhu, Jinzhen Cao
A screening of factors that might influence the result of laboratory decay tests
2014 - IRG/WP 14-20548
Laboratory fungal decay tests provide important tools for performance testing of wood materials. But they are also hampered with some uncertainties regarding reproducibility. In addition to variation between fungal species and strains the test conditions are also believed to have some influence. The aim of this study was to screen the effect of a selection of test parameters that might influence t...
E Larnøy, G Alfredsen, A Treu, S Kolstad
Fire resistance of wood treated with potassium carbonate and silanes
2014 - IRG/WP 14-30657
This paper reports on the effect that organosilicon compounds and potassium carbonate and urea (PCU) have on wood flammability. The study focus on reducing wood flammability by promoting char formation through manipulation of the condensed phase decomposition chemistry. Potassium carbonate is known as an effective fire retardant, however it is easily leached out from wood and increases its hygrosc...
B Mazela, M Broda, W Perdoch
Copper and chromium leaching from wood impregnated with chromium-copper containing preservatives: Results of different studies
2014 - IRG/WP 14-50300
Copper and chromium based wood preservatives remained one of the most important ingredients for wood protection solutions for protection of wood in demanding applications all-over the world. Leaching of heavy metals from treated wood is important from two different aspects; firstly from performance point of view, and secondly from environmental issues. However, the importance of these studies is i...
M Humar, N Thaler, E Melcher
Influence of Exposure Direction on Leaching of a Biocide from Painted Wood Surfaces
2014 - IRG/WP 14-50303
The objective of this project was to investigate the influence different exposure directions – North, East, South and West on the cumulative quantity of a biocide leached from painted wood surfaces due to rainfall and the consequences for the risk assessment.
The study included a solvent-borne primer without biocides and a topcoat protected with a biocidal active substance. Both products were a...
M Klamer
Development of new wood treatments combining boron impregnation and thermo modification - Effect on decay and termites durability
2014 - IRG/WP 14-40666
Environmental pressures appeared in most European countries during the last decade has lead to the development of more environmentally acceptable preservation methods. In this context, wood heat treatment has been one of the most investigated alternative methods during the last years. Treated at temperatures ranging between 180 and 220°C, wood components undergo more or less important chemical mo...
S Salman, A Pétrissans, M-F Thévenon, S Dumarçay, B Pollier, P Gérardin
Laboratory Study of Relative Leachability of Chromated Copper Arsenate Preservative from Treated Woods among Soil Types of Sarawak
2014 - IRG/WP 14-50307
Wood and soils are important natural resources from the environment and serves mankind well respectively as structural materials and natural platform erecting such materials. With shortfalls of naturally durable timber species for protected in-ground uses under Malaysian environments, Chromated Copper Arsenate (CCA) treated woods are widely used instead, incurring serious potential threats of pres...
A H H Wong, P K F Chong