A preliminary report on lignicolous marine fungi in the Java Sea, Indonesia
1982 - IRG/WP 488
This report is part of a study on the natural durability of Indonesian timbers against marine borers conducted in Pari Island waters, Java Sea (Suhirman and Eaton, 1981), and contains preliminary information which has not yet been published....
Suhirman, R A Eaton


Monographic card: Coniophora puteana (Schum. ex Fr.) Karst. (Second draft)
1978 - IRG/WP 171
A Käärik


Effects of some essential oils on wood destroying organisms
1993 - IRG/WP 93-10047
Three wood destroying fungi: Botryodiplodia theobromae Pat. (stain), Gloeophyllum sepiarium (brown rot), and Pycnoporus sanguineus (white rot) were exposed to six plant essential oils: the peppermint, kaffir lime or leech lime, lavender, tarragon, holy basil, and the eucalyptus. The peppermint oil showed most effective to inhibit fungal growth, while eucalypus oil was the least effective. The othe...
K Atisongkroh, C Anantachoke, P Lekuthai, S Pensook, T Kittirattrakarn


Basidiosporogenesis by brown-rot basidiomycetes in vitro
1995 - IRG/WP 95-10126
Basidiospores of wood-rotting basidiomycetes are a primary sourse of infection causing wood biodeterioration, especially in wood above ground. Most studies evaluating wood preservatives have used mycelia or basidiospores obtained from wild mushrooms. The objective of this study was to demonstrate in vitro methods that promote carpogenesis and basidiosporogenesis by the brown-rot fungi Antrodia car...
S C Croan


Detection of incipient brown rot decay in wood by fourier transform infrared spectrometry
1987 - IRG/WP 2275
Fourier transform infrared spectrometry was evaluated as a possible method for detecting different levels of brown-rot decay in pine sapwood. By using first derivative spectra and regression analysis, an equation based on 4 absorption peaks, normalized with an internal standard peak, was developed. The correlation between weight loss and absorption was highly significant indicating that this is a ...
D D Nicholas, T Schultz


Immunogold labelling of size marker proteins in brown rot-degraded pine wood
1990 - IRG/WP 1428
Pine wood degraded by Fomitopsis pinicola was infiltrated with a mixture of ovalbumin (45 kDa) and myoglobin (16.7 kDa). After crosslinking of the proteins with glutaraldehyde and preparation for electron microscopy ultrathin sections were labeled with gold-conjugated antibodies. Simultaneous labeling of both proteins on the same section showed that at 50-70% weight loss ovalbumin did not penetrat...
E Srebotnik, K Messner


A summary of tests and practical experiences with the Pilodyn wood testing instrument
1980 - IRG/WP 282
This paper presents a summary of the reports, tests and practical experiences with the Pilodyn wood tester not only, however, concerning poles but also in other fields such as standing trees, sawn timber etc. The principle of the Pilodyn is a spring-loaded pin which is fired into the object and the depth to which the pin penetrates is correlated to physical and mechanical properties of the object....
H Friis-Hansen


Assessment of the natural durability of four Ghanaian hardwoods against the white-rot fungus Coriolus versicolor and soft-rot using laboratory tests
2003 - IRG/WP 03-10498
The natural durability of two lesser-utilized species (LUS) (Corynanthe pachyceras Welw. (pamprana) and Glyphaea brevis (Sprengel) Monachino) (foto) from three forest districts, and two related primary species (Nauclea diderrichii (de Wild.) Merr. (opepe) and Nesogodornia papaverifera (A. Chev.) R. Capuron.) (danta) from one district in Ghana is assessed against Coriolus versicolor Linnaeus Quelet...
C Antwi-Boasiako, A J Pitman, J R Barnett


Spatial arrangement of lignin peroxidase in pine decayed by Phanerochaete chrysosporium and Fomitopsis pinicola
1988 - IRG/WP 1343
By applying immunoelectronmicroscopic methods, lignin peroxidase of the white rot fungus Phanerochaete chrysosporium has been localized in the cytoplasm of hyphae, close to the plasmalemma and on the plasmalemma. Infiltration of wood specimen with culture filtrates, concentrated 300-fold, gave clear information on the penetration of the enzyme into the wood cell wall. Penetration was restricted to...
E Srebotnik, K Messner


Oxalic acid production of fifteen brown-rot fungi in copper citrate- treated southern yellow pine
2001 - IRG/WP 01-10388
Non-arsenical copper-based wood preservatives have grown in number since the 1980's as a response to environmental concerns posed by arsenicals. Interest in copper tolerant decay fungi has increased accordingly. Oxalic acid (OA) production by brown-rot fungi has been proposed as one mechanism of copper tolerance. Fifteen brown-rot fungi representing the genera Postia, Wolfiporia, Serpula,...
F Green III, C A Clausen


Differential behaviour of wood rotters at water repellent Rubberwood
2000 - IRG/WP 00-10386
Rubberwood samples treated with different concentration of aqueous solution of chromic acid has induced significant increase in water repellency and attains dimensional stability. Though water repellency and dimensional stability was achieved by treatment, the fungal invasion could not be completely controlled. Differential level of decay of brown and white rot in wood treated with water repellent...
H C Nagaveni, S S Chauhan, K S Rao


Collaborative soft rot tests: Results of analyses of soil samples
1976 - IRG/WP 263
C R Levy


Results from soft rot tests in vermiculite jars
1976 - IRG/WP 272
T Vihavainen


Monographic information on Serpula (Merulius) lacrymans (Schum. ex Fr.) S. F. Gray, according to the 'Model Questionnaire for preparation of monographic cards for wood-destroying fungi'
1978 - IRG/WP 170
J Segmüller, O Wälchli


Results of collaborative work on laboratory soft rot testing
1989 - IRG/WP 2341
S M Gray, D J Dickinson


Removal of heavy metals from treated wood using biological methods
2005 - IRG/WP 05-50226
Heavy metals were removed from wood treated with copper based preservatives using brown-rot fungus Fomitopsis palustris. The amount of effective elements removed by treatment methods was examined. The relationship between oxalic acid concentration and the amount of heavy metals removed from each treated wood was also investigated. The relationship between fungus weight and removal rate was also in...
Dong-won Son, Dong-heub Lee


Development of a method for testing wood preservatives with soft rot fungi
1975 - IRG/WP 250
Although the first publications on experimental soft rot attack date back 20 years ago, so far no test method for evaluating the efficacy of wood preservatives against soft rot attack (Ascomycetes and Fungi Imperfecti) has been generally accepted. The reasons are diverse and the shortcomings and the disadvantages of the methods described are well known and have repeatedly been discussed. The soil ...
M Gersonde, W Kerner-Gang


Collaborative soft rot tests: Proposed amendments to Document No: IRG/WP/208
1973 - IRG/WP 224
J K Carey, J G Savory


Involvement of hydrogen peroxide in wood decay by brown-rot and white-rot fungi
1985 - IRG/WP 1256
To gain further understanding of the role of H2O2 in wood degradation by brown- and white-rot fungi, we studied the following: (a) extracellular H2O2 production, (b) effect of various hydroxyl radical (·OH) and singlet O2 (1O2) quenching agents on wood and cellulose degradation, (c) intracellular H2O2 production and catalase activity, and (d) cytochemical localization of H2O2 with diaminobenzidin...
T L Highley, L L Murmanis


Preservation of hyphal-forming brown- and white-rot wood-inhabiting basidiomycetes
2001 - IRG/WP 01-10397
Lyophilization is an excellent technique for the long-term preservation of hyphal-forming brown- and white-rot wood-inhabiting basidiomycotina. However, vegetative mycelial isolates are not lyophilizable. In this study, 10 brown-rot and 10 white-rot basidiomycetous non-sporulating, non-chlamydosporulating, and non-bubillerferous basidiomycetes fungi were tested for viability after lyophilization. ...
S C Croan


Decay resistance of Scots pine (Pinus sylvestris) heartwood against brown rot
2002 - IRG/WP 02-10433
Natural decay resistance of wood is mainly restricted in the heartwood and based on wood microstructure and chemical composition. The genetic variation in the durability of Scots pine (Pinus sylvestris L.) wood against decay and the relationship between resistance and chemical composition was studied. The laboratory tests of 6 and 8 weeks were carried out with a brown rot fungus Coniophora puteana...
H Viitanen, A M Harju, P Kainulainen, M Venäläinen


Standardisation of tests of toxicity of preservatives to soft rot fungi
1978 - IRG/WP 2119
J G Savory


The preliminary characterization of ß-1,4-xylanase of the brown-rot fungus Gloeophyllum trabeum
1990 - IRG/WP 1447
The extracellular ß-1,4-xylanase of the brown-rot fungus, Gloeophyllum trabeum, was isolated from crude extract by chromatofocusing method (PBE 94 column chromatography). The isoelectric point was estimated to 4.2-4.8 by cromatofocusing and 4.5 by isoelectric focusing (IEF). The molecular weight of the enzyme was estimated to 37,000 dalton by SDS-PAGE. The optimal temperature for the crude extrac...
A-C Ritschkoff, M Rättö, L Viikari


Characterization of glycopeptide from white-, brown- and soft rot fungi
2002 - IRG/WP 02-10424
Extracellular low-molecular-weight substances that catalyze a redox reaction between O2 and electron donors to produce hydroxyl radicals have been isolated from wood degrading cultures of white-rot, brown-rot, and soft-rot fungi. They contained protein, neutral carbohydrate, and Fe(II). These substances were glycosylated (glycated) peptides and suggested to form Amadori product (ketoamine). The...
H Tanaka, S Itakura, A Enoki


Some tests on ES - AS 11, a novel anti-sapstain formulation, and its properties
1987 - IRG/WP 3399
The results of some tests with the formulation ES - AS 11 are given. The formulation is an attempt to improve the performance of an anti-sapstain chemical by: 1) increasing its penetrability 2) uniquely combining its active ingredients. Very short times of treatment (dipping not longer than 5 seconds), low concentrations of active ingredients, and lower toxicological and environmental risks may be...
U Straetmans