Application of (n-a)-radiography for determination of boron in wood impregnated with boron-containing antispetics
1975 - IRG/WP 351
The method of (n-a)-radiography for quantitative determination of boron is based on creation of defective regions (tracks) in a polymer (the detector), which form during passage of a particles through the detector, these particles being produced in the reaction 10B(n, a)7Li when the test specimen in contact with the detector is irradiated with neutrons. Etching of the detector with an appropriate ...
N A Dubinskaya, M Ya Tsel'millere


The influence of the location of a wood defect on the modulus of elasticity determination in wood durability testing
2004 - IRG/WP 04-20287
This study investigates the influence of the location of a wood failure in stakes upon elastic changes observed in beech specimens with the resonance vibration technique. Natural failures were simulated by artificially created defects at different locations of the test stake. The results indicate that the location of an attack in a stake is important for the measurement outcome. When the attack is...
L Machek, H Militz


A novel guide for the determination of the physical properties of wood including kiln drying and full-cell preservative treatment
2004 - IRG/WP 04-20298
An ideal flow chart for the sequential experimental determination of a range of physical properties relevant to wood drying and subsequent preservation was designed as a novel guide to assist wood scientists. In this manner, data assembly and experimental processing are shown. This was designed according to experience and published literature. Aspects emphasised in this review were the physical p...
I Usta, M D C Hale


A comparison between different accelerated test methods for the determination of the natural durability of wood
1996 - IRG/WP 96-20099
According to the European standard EN 350-1 the natural durability of wood is defined as: "the inherent resistance of wood to attack by wood destroying organisms". This standard also describes how, for certain hazard classes, the durability is determined. The two methods described in this standard are the kolleflask method (EN 113) and the field-stake-test method (EN 252). The EN 113 test gives re...
H Militz, S G L Michon, J E Polman, M Stevens


Determination of chlorine-containing wood preservatives in art objects using Micro-XRF
2003 - IRG/WP 03-20266
The applicability of a mobile energy-dispersive micro X-ray fluorescence (μ-XRF) spectro-meter for the analysis of organochlorine-containing wood preservatives in art objects was tested. Information about the relative degree of contamination and the efficacy of detoxification measures with emulsive solvent systems can be gained using the intensity of the chlorine signals. μ-XRF t...
J Bartoll, A Unger, S Krug, K Püschner, H Bronk


The quantitative determination of quaternary ammonium compounds in treated timber – results of an extended ring test
2002 - IRG/WP 02-20240
The determination of quaternary ammonium compounds (QAC) by means of a 2-phase-titration or photometry is a well established procedure for the quantification of cationic detergents in aqueous solutions. It is known that this analytical principle can also be used for the measurement of QAC extracted from treated timber. However only few information are available concerning the reproducibility or th...
E Melcher, C Bornkessel, J Gunschera, R Hamberg, H Härtner, H-N Marx, U Schoknecht, J Wittenzellner


Collaborative field trial out-of-ground contact
1982 - IRG/WP 2179
At the 12th meeting of the IRG in Sarajevo, Yugoslavia it was decided after considerable discussion that the best way to proceed with the work of the subgroup was to centre it around a co-operative field trial based on the L-joint test detailed in IRG/WP/2157. At the same time it was agreed that interested laboratories would also conduct their own methods, particularly the German planner test and ...
D J Dickinson, A F Bravery, J K Carey


Determination of N-cyclohexyl-diazeniumdioxide (HDO) containing compounds in treated wood using GC-MS
2000 - IRG/WP 00-20201
Beside the biological effectiveness the approval of a chemical wood preservative requires also techniques for the analytical determination of active ingredients in different matrices. Fulfilling of the last requirement is particularly difficult in the case of impregnated timber treated with wood preservatives containing organic compounds. This paper describes a procedure for the determination of t...
P Jüngel, J Wittenzellner, E Melcher


Determination of boron levels in solution and in treated wood
1994 - IRG/WP 94-20041
Four methods of measuring boron levels in solutions were investigated. The methods compared included the azomethine-H method which is commonly used in soils and plant tissues, the methods outlined in the Australian Standard AS 1605 (1974) and in Wilson (1958), and the atomic absorption spectrophotometry method. Defect-free radiata pine (Pinus radiata D. Don) sapwood and wood flakes were treated to...
F J Romero, P Vinden, P Kho


Determination methods of phytotoxic effect of wood preservatives
1990 - IRG/WP 2349
The phytotoxic effect of wood preservatives so widely used plays a considerable role in the protection of natural environment. A review was made of the existing methods with which to assess the phytotoxicity of the above chemicals and some suggestions were given concerning the methods most appropriate for their unification. Two areas of research are proposed: 1) estimating the direct effect on ind...
A Kundzewicz, J Wazny


Microwave digestion of preserved wood for the determination of Cu, Cr, As, B and P in quality control
1991 - IRG/WP 2364
A microwave digestion method for the determination of copper, chromium, arsenic, boron and phosphorus in preserved woods is described. Samples were digested with nitric acid in pressure-relief type teflon PFA vessels by microwave heating in a commercial laboratory microwave oven. Fast, efficient and complete digestion was achieved within 29 min for 12 samples. The digestion time compared favourabl...
N Bernth, L B Sheard


Estimation of mycelial biomass by determination of the ergosterol content of wood decayed by Coniophora puteana and Fomes fomentarius
1989 - IRG/WP 1415
The mycelial biomass of fungi decomposing wood materials may be estimated by the use of an ergosterol assay technique.ln decay tests, essentially according to EN 113, estimates made by HPLC analyses on wood decayed by Coniophora puteana and Fomes fomentarius show the increase in biomass in the wood blocks. The ergosterol contents were correlated with dry weight loss determinations. Degradation of ...
K Nilsson, J Bjurman


Determination of the amine to copper ratio remaining in wood after leaching
2002 - IRG/WP 02-30285
The effectiveness of the protection and the environmental impact of the treated wood are two of the most important aspects that need to be understood for all preservatives. Both are particularly influenced by the loss of biocidal components from treated wood. For amine copper preservatives, copper fixation determines the leaching resistance of the copper and amine compounds formed in wood. Previou...
N Lucas, J N R Ruddick


Computerized axial tomography. A non-destructive method for three-dimensional wood density/moisture content measurement
1987 - IRG/WP 2285
Computerized Axial Tomography (CAT-scanning) - used for medical investigations of the brain - has been evaluated as a nondestructive method of three-dimensional wood density/moisture content measurements. Density can be measured with an accuracy of ±3 kg/m³, and the accuracy in average moisture content is ±1% below and above fibre saturation point. It is theoretically possible that measurements...
L O Lindgren


Optimisation of an analytical method for the determination of total fluoride in preservative-contaminated soils using water steam distillation and an ion-selective electrode
1999 - IRG/WP 99-20153
This paper describes a simple modified procedure for the quantitative fluoride determination of different origin in a soil matrix using a water steam distillation and an ion-selective electrode. Distillation methods generally require a preliminary preparation step like fusing. The modified method presented here is based on the direct distillation of fluoride so that no further sample preparation i...
E Melcher


The quantitative determination of N-cyclohexyl-diazeniumdioxide (HDO) containing compounds in treated wood using TD-GC-MS
2001 - IRG/WP 01-20223
Last year we presented the paper (IRG/WP/00-20201) "Determination of N-cyclohexyl-diazeniumdioxide (HDO) containing compounds in treated wood using GC-MS". Based on the intensive discussion at the meeting, the first experiences made with the calibration of the system for this application will be reported. For the quantitative determination of N-cyclohexyl-diazeniumdioxide in treated wood, milled m...
P Jüngel, J Wittenzellner, E Melcher


The accelerated L-joint test method for determination of the out of ground natural durability
1998 - IRG/WP 98-20146
The accelerated L-joint test incorporates a moistening device and uses a close end water trap in an open joint connection with a laminated tenon member consisting of the perishable reference wood species scots pine sapwood and beech. After one year of exposure it is possible to show a distinct identification of natural durability classes 4 and 5 against the more durable wood species. Both weight ...
J Van Acker, C Brauwers, M Stevens


Studies on the determination of the durability of wooden poles and fence posts
1982 - IRG/WP 3195
This study was carried out by the Forestry Research Institute. 5 Turkish main tree species, Oak (Quercus), pine (Pinus sylvestris), beech (Fagus orientalis) and Fir (Abies bornmülleriana) wooden poles and fence posts, were treated with Tanalith-U and creosote applying pressure process. Tanalith-U was applied by full-cell process and creosote was applied by empty cell process. Treated and untreate...
R Ilhan, O Taskin, A P Erten


An alternative method for the determination of lignocellulolytic enzymatic activities of white rot fungi
1998 - IRG/WP 98-10261
Some lignocellulolytic activities of wood decay fungi can be evaluated in an indirect way through the study of the decolorization that white rot fungi produces in culture media in the presence of dyes. In this assay, ten dyes were selected, which were added in concentrations of 0.00 1% - 0.003% (P/V) to four-day cultures of Trametes versicolor containing 1% of beech sawdust in a basal salt medium...
D Muñoz-Mingarro, F Llinares, F Rubio, M Yuste, C Rodríguez-Borrajo, J Jiménez, M T De Troya


Investigation of CCA fixation in wood by sequential extraction. I Determination of CCA component fixation and preliminary extraction results
2002 - IRG/WP 02-50188
The fixation of CCA-C preservative was investigated in sapwood of red pine (Pinus resinosa Ait.), trembling aspen (Populus tremuloides Michx.) and red maple (Populus tremuloides Michx.) at target retentions of 4.0, 6.4, 9.6 and 30.0 kg/m3. Treated wood sawdust was water extracted at close time intervals during the fixation and analyzed for the contents of unfixed hexavalent chromium, total Cr, Cu ...
S Radivojevic, P A Cooper


Determination of corrosive effect of liquid wood preservatives to metals – First experiences with a National Standard which is in revision
2006 - IRG/WP 06-20321
The development of standards is an essential tool to characterise different kind of materials and products. An important aspect during the development of a new product is to check the corrosion behaviour with other materials. Corrosion can cause several problems like pitting corrosion. Consequently the knowledge concerning the corrosive effect of liquid wood preservatives is important due to the s...
E Melcher


Determination of bis-(N-cyclohexyl-diazeniumdioxy)-copper in different matrices by photometer, thermal energy analyzer and HPLC
1999 - IRG/WP 99-20179
For the quantitative analysis of bis (N-cyclohexyl-diazeniumdioxy)-copper (Cu-HDO) three analytical methods are used. The employment of the different methods depends on the matrices involved. For several years now, the colorimetric determination of Cu-HDO by photometer has been applied to solutions and concentrates of wood preservatives. In principle, the technique consists of a quantitative conve...
J Wittenzellner, W Hettler, M Maier


Determination of fungitoxic value of preservatives in laboratory wood-block tests. Part 2: Statistical estimation
1989 - IRG/WP 2327
Laboratory modified agar-block tests were made to determine the fungitoxic value of the wood preservative CCA against the test fungus Serpula lacrymans using statistical methods. With the aid of statistical computer programmes based on the least square method. the regression equation was found for the dependence between sample mass loss and preservative retention both in terms of percentage and fo...
J Wazny, J D Thornton, K J Krajewski


Determination of fungitoxic value of preservatives in laboratory wood-block tests. Part 1: Standard procedures
1989 - IRG/WP 2326
By applying a modified agar-block method, a comparative analysis was made on the toxic value of the wood preservative CCA against the test fungus Serpula lacrymans. The procedure applied to determine the results accounted for different standards: EN (Toxic limit), ASTM (threshold retention), GOST (threshold retention and protection probability), PN (toxic doses) and JIS (value of efficiency). Desp...
J Wazny, J D Thornton


Inter-laboratory comparison of assessment methods for wood preservatives against subterranean termites: Determination of protection threshold limits for CCA
1999 - IRG/WP 99-10317
In 1996, several institutes conducted laboratory bioassays on the efficacy of unleached Pinus radiata specimens treated with copper-chromium-arsenic (CCA) and copper naphthenate (Cu Naph) at retentions of 0.5, 1.0, 2.0 and 4.0 kg/m3 (total salt for CCA; elemental copper for Cu Naph) against a range of species of subterranean termites (IRG/WP/96-10174). Each participant employed the standard test m...
J W Creffield, M Lenz