Soft rot decay in acetylated wood. Chemical and anatomical changes in decayed wood
2002 - IRG/WP 02-40231
Acetylated Beech (Fagus sylvatica) and Scots Pine (Pinus sylvestris) wood were studied in soil beds under laboratory conditions for longer periods. High mass losses and dynamic MOE losses were measured in non-acetylated wood and at lower weight percent gains (WPG). Rapid losses of lignin, holocellulose and ?-cellulose occurred in non-acetylated beech wood and no losses were detected at the highest...
B Mohebby, H Militz


Penetration of surface applied deltamethrin micro-emulsion formulations in four European timber species
1994 - IRG/WP 94-20030
The Netherland's Government, in line with many other European Governments initiated a programme (KWS2000) aimed at significantly reducing the emission of volatile organic compounds by the year 2000. As part of this programme a research project is currently underway to evaluate the potential for replacing organic solvent based remedial treatments with micro-emulsion formulations of the sam...
P Esser, W L D Suitela, A J Pendlebury


Eucalyptus globulus. Impregnability in relation with plantation and crop
1992 - IRG/WP 92-2402
Eucalyptus globulus Lasill is currently classified in Pr EN 350 on the basis of the characteristics of the first log. In practice, there are usually several following crops of branches developped on each stump in plantations. Up to a diameter of 8 cm, round wood of 2nd crop and further crops present a maximum of sapwood and characteristics which differ significantly from the basic classification a...
D Dirol


The influence of the location of a wood defect on the modulus of elasticity determination in wood durability testing
2004 - IRG/WP 04-20287
This study investigates the influence of the location of a wood failure in stakes upon elastic changes observed in beech specimens with the resonance vibration technique. Natural failures were simulated by artificially created defects at different locations of the test stake. The results indicate that the location of an attack in a stake is important for the measurement outcome. When the attack is...
L Machek, H Militz


Influence of CCA and TnBTO on wood decay, under different oxygen levels and various initial moisture content
2001 - IRG/WP 01-10415
Fagus sylvatica (beech) and Pinus sylvestris (Scots pine) were impregnated by TnBTO (tributyl-tin oxide) and CCA (chromated copper arsenate). In wood blocks two levels of moisture content (50% and 100% of saturation point) were used. Three levels of oxygen concentrations (10, 21, and 50%) were chosen. Treated and untreated wood were exposed to three fungi (C. versicolor a white rot, C. puteana, a ...
S M Kazemi, R J Murphy, D J Dickinson


Evaluation of the european standard ENV 12038 for durability testing of plywood
2001 - IRG/WP 01-20237
The latest improved version of the standard ENV 12038 drafted as document N44 by CEN Technical Committee 38 (WG 7 - WG 23) is used to evaluate the effect of wood composition and structure on plywood durability. The method described is based on the agar-block test of the EN 113 standard used for the determination of the efficacy of wood preservatives and the assessment of the natural durability of ...
J Van Acker, M Stevens, E De Clercq


The WOODCARE project: Development of detection methods for Death watch beetle larvae and fungal decay
1999 - IRG/WP 99-20172
Woodcare was a European project coordinated by English Heritage. The aim of the research was to develop more targeted and more environmentally friendly treatment methods for Death watch beetle infections in Oak constructions of historical buildings. TNO has developed two new methods for fast and reliable detection of Death watch beetle larvae and related fungal decay in Oak. The problem with Death...
P Esser, P Van Staalduinen, A C Tas


Durability of heat-treated wood
1999 - IRG/WP 99-40145
Heat-treated wood from the French process were laboratory tested against decay using agar block test and a modified soil block test. Water absorption, bending strength, lignin content and acid number were also determined to evaluate the effect of heat treatment. Heat treated samples exhibit a higher lignin content and a lower acid number compared to untreated control indicating the degradation of ...
D P Kamdem, A Pizzi, R Guyonnet, A Jermannaud


The treatment of Douglas fir fence posts: specification and compliance using new European standards
1999 - IRG/WP 99-20178
New European standards for the preservative pre-treatment of timber require the results of the treatment process to be specified and subsequently verified by examination of the treated timber for penetration and retention of the preservative. For penetration, the standards are restrictive in that there are only a limited number of options available to the specifier. Thus for ground contact service...
R J Orsler, H Derbyshire


The effectiveness of three tributyltin compounds in beech against soft rot fungi using a soil-bed technique: A preliminary report
1986 - IRG/WP 3390
The effectiveness, towards soft rot fungi, of bis (tributyltin) oxide, tributyltin ethanesulphonate (TBTES) and benzyltributylammonium tributyldichlorostannate in both leached and unleached beech stakes is compared to that of a CCA preservative (Tanalith CT 106), using a soilbed technique. In addition, the effect of test solvent (water or toluene) on the performance of TBTES is evaluated. Total ti...
R Hill, A H Chapman, B Patel, A Samuel, J K Carey


Chemical Remediation of Beech Condensates
2004 - IRG/WP 04-50221
In the present work, The beech wood condensate are subsequently separated from the aqueous phase. Experimental results reveal the electrostatic interaction between the oppositely charged wood extracts after oxidation and Ca(OH)2. The influence of parameters such as pH, oxidation were studied. The increase in aqueous phase pH resulted in enhanced removal of wood extracts from water. The effect of p...
M Irmouli, J P Haluk


Influences of the hydro-thermal treatment on physical properties of beech wood (Fagus orientalis)
2005 - IRG/WP 05-40303
Influences of the hydro-thermal treatment on physical properties of beech wood were studied. Wood specimens (2×2×2cm) were treated in two steps. At first step, samples were treated at 160,180 & 200ºC for 4, 5 & 6 hours. At second step, treated samples were cured based on their first step treatment temperatures (160,180 & 200ºC) for 16 hours. The treated samples were soaked in water...
B Mohebby, I Sanaei


Research on wood protection at the Princes Risborough Laboratory 1975 & 1976
1977 - IRG/WP 3109
This paper is the latest of a 2-yearly series presenting a summarised account of the Laboratory's work in wood preservatives and related fields. The topics dealt with include: environmental studies on the usage of copper-chrome-arsenic and organic solvent preservatives; development of National and International Standards; recent developments in the preservation of external doors and windo...
J M Baker, R A Laidlaw, E R Miller, J G Savory


European standardization for wood preservation
1991 - IRG/WP 2365
Since the last IRG 21 conference in New-Zealand, there one meeting of the plenary committee and several meetings of working groups. The interprative documents prepared by CCE for expliciting the essential requirements of the CCE Directive on the construction products and specially: mechanical resistance and stability / hygiene, health and environment / safety in use are waited to valid the progra...
Anonymous


Effects of heat treatment on modulus of elasticity of beech wood
2002 - IRG/WP 02-40222
Heat treatment is the oldest, simplest and cheapest method for reducing hygroscopicity of wood. The heat treatment protects wood against to biological organisms as well as giving wood dimensional stabilization without damaging environment. The effects of heat treatment on modulus of elasticity (MOE) of beech wood (Fagus orientalis Lipsky) naturally grown and intensively used in forest products in...
S Yildiz, G Çolakoglu, Ü C Yildiz, E D Gezer, A Temiz


Evaluation of the natural durability and ultrasonic method for decay detection of some european hardwood and softwood species
2004 - IRG/WP 04-10537
This paper presents the first part of an investigation on the natural durability of mixed plywood made of durable and non durable plies from the following selected timbers : Cedrus atlantica, Cupressus sempervirens, Castanea sativa, Populus sp. I 214 and Fagus sylvatica. In order to carry out this study, the natural durability of the massive wood used to manufacture the plywood panels was asses...
F Faraji, M-F Thévenon, B Thibaut


Fouling assemblage development on copper-chromium-arsenic-treated timber submerged in European waters
2002 - IRG/WP 02-50181
The effect of the anti-marine-borer timber preservative CCA on community development of non-target marine fouling animals was investigated. Panels of Scots pine treated to target retentions of 12, 24 and 48 kg CCA per m3 of wood, plus untreated controls were submerged at seven coastal sites (Portsmouth, UK; La Tremblade (2 sites), France; Ria Formosa, Portugal; Sagres, Portugal; Kristineberg, Swed...
C Brown, R J Eaton, S M Cragg, P Goulletquer, A Nicolaidou, M J Bebianno, J Icely, G F Daniel, T Nilsson, A J Pitman, G Sawyer


Work Programme of CEN/TC 38 (April 2001) and European Publications
2001 - IRG/WP 01-20234
New scope of the CEN/TC 38: " Standardization of the natural or conferred durability of wood and wood-based products against biological agents and their characteristics associated with exposure ". " Normalisation de la durabilité naturelle ou conférée du bois et de ses produits dérivés visà-vis des agents biologiques et leurs caractéristiques associées à leur exposition ". " Normung der n...
R Hüe


Effect of test site location on in-ground preservative performance after 6 years
2001 - IRG/WP 01-20231
Pinus radiata test stakes were treated with 4.1 kg/m3 of CCA and Fagus sylvatica with 6.1 kg/m3 of CCA. Both wood species were also treated with a copper plus triazole preservative (3 kg/m3 of copper) and chlorothalonil plus chlorpyriphos in oil (4.8 kg/m3 chlorothalonil). Furthermore, P. radiata was treated with ammoniacal copper plus a quaternary ammonium compound (2.6 kg/m3 copper) and a 60/40 ...
R N Wakeling


European standardization for wood preservation. Progress report 91-92
1992 - IRG/WP 92-2398
Since the IRG 22 conference in Kyoto, CEN/TC 38 Plenary met twice in relation with several working group meetings. 5 upon 6 of the interpretative documents have been prepared by adhoc groups of the Standing Committee for Construction within the scope of the 89/106/EEC directive on Construction Products. The expected requirements attached to wood preservation are both requirements 1) and 3): 1) mec...
R Hüe


The development of blue stain in service in sapwood of European softwood species
1997 - IRG/WP 97-10236
The utilisation of softwood species for window joinery applications is gaining importance in countries frequently using tropical hardwood species up to now. Since wood preservation is not always part of the total concept of window frames manufactured from sapwood containing wood elements it is essential to know the impact of durability on the performance. Moisture content control is a major tool i...
J Van Acker, R Klaassen, H Militz, M Stevens


Fungal decay of acrylate treated wood
2004 - IRG/WP 04-30357
Natural durability of wood species is variable. Chemical wood preservatives, such as biocides are necessary for extension of their service life. Many methods have been developed to increase the resistance of wood and wood products against wood-destroying organisms during the last years. The most frequently used methods are chemical and thermal modification of wood. In wood modification the basic c...
Z Tiralova, L Reinprecht


Physiological properties of fungal test strains according to the European Standard EN 113
1986 - IRG/WP 2258
For the discussion of the European standard EN 113 the EMPA's procedure of culturing the test fungi and the corresponding virulence of the test fungi as well as the wood moisture content at the end of the test are shown. It is mainly shown that within the standard the choice of the solvent may not be left at the test lab if reproducible results shall be obtained. The different solvents in...
E Graf, B Zgraggen, P Manser


Specifying preservative-treated resistant timber: Conforming to European Standards
2001 - IRG/WP 01-20235
The most common construction timbers used in the UK are of low natural durability and, generally, resistant to preservative treatment. These include species of spruce, hemlock and fir. However, their characteristically limited and non-uniform uptake of preservatives may still confer sufficient protection to give satisfactory durability performance in terms of biological resistance. This paper desc...
E D Suttie, A F Bravery, T B Dearling


Fumigation of red beech in New Zealand for prevention of graystain
2000 - IRG/WP 00-10343
The discoloration of sapwood of red beech (Nothofagus fusca) after drying has been an ongoing problem which may lower value of material for certain applications (such as flooring) by as much as 50%. The dark gray stain noted after the drying and planing of lumber is not prevented by fungicide dips, and is most likely similar to the enzyme-mediated stain noted in a variety of commercial hardwoods. ...
E L Schmidt, B Kreber