IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 348 documents. Displaying 25 entries per page.


The use of the Pilodyn for detecting soft-rot decay in CCA treated eucalypt poles
1986 - IRG/WP 2251
A 6 Joule Pilodyn unit with 2.5 mm diameter pin was used to inspect CCA treated eucalypt poles, suspected of suffering groundline soft-rot decay. Pole plugs were removed at the inspection region and the amount of soft-rot decay present determined microscopically. High correlation (R² = 0.73) was obtained between the amount of soft-rot and Pilodyn pin penetration. The Pilodyn is recommended as a u...
L E Leightley, G A Willoughby


A method to evaluate the effeetiveness of bait application using a transferred nest of Coptotermes formosanus Shiraki (Isoptera: Rhinotermitidae)
1999 - IRG/WP 99-20161
Although a survey of monitoring stations can tell us the decline of termite activity after application of baits, it seems questionable to conclude an eradication of a Whole colony of subterranean termites if the termites move out their foraging territory. Only reliable method to ensure the success of bait application is to determine the absence of living termites in their nest in accordance with a...
K Tsunoda, T Yoshimura, H Matsuoka, Y Hikawa


Ekki heartwood - is “Durable”
2002 - IRG/WP 02-10444
Severe decay damages of bridges made of ekki (Lophira alata Banks) wood which is classified as a durable species in the EN 350:2 as already reported at the 31 IRG annual meeting. This paper deals with results of long-term decay tests of ekki heartwood specimens using 3 isolates (Loweporus tephroporus 2 strains and a fungus of other sp. from damaged ekki bridges) and Trametes versicolor as a refere...
S Doi, R Itoh, S Horisawa


Ultrastructural aspects of bacterial attacks on an archaeological wood
1993 - IRG/WP 93-10007
Transmission electron microscopy of wood from a Chinese ship submerged in the mud for over 900 years showed bacteria to be the main factor for its deterioration. The micromorphology of degraded wood cell walls was similar to that observed during the attacks of wood by erosion bacteria. Other bacterial forms, previously considered lo be scavenging bacteria, were also abundant in degraded areas of t...
Yoon Soo Kim, A P Singh


Resin bleed after light organic solvent preservative treatment - the effect of drying method and process type
1986 - IRG/WP 3378
The effects of drying method and treatment process type on resin bleed were investigated. High-temperature drying of resinous radiata pine (Pinus radiata D. Don) heartwood resulted in improved wood permeability, higher preservative uptake, and greater resin bleed when treated by the Rueping process. Resin bleed was reduced substantially when timber was treated by the Lowry process, and totally eli...
P Vinden


The Relationship of Fiber Cell Wall Ultrastructure to Soft Rot Decay in Kempas (Koompassia malaccensis) Heartwoo
2004 - IRG/WP 04-10541
The ultrastructure of fiber walls in kempas (koompassia malaccensis) heartwood was examined in relation to soft rot cavity formation. The fibers consisted of middle lamella and thick secondary wall. The secondary wall was differentiated in to a S1 layer, and a unique multi-lamellar S2 layer. Two distinct forms of lamellae were recognisable, one type being considerably thicker than the other. They ...
A P Singh, A H H Wong, Yoon Soo Kim, Seung-Gon Wi


The use of plastic meshes in soft rot monoculture testing
1990 - IRG/WP 2353
Plastic meshes were introduced between the wood blocks and agar medium in a miniaturised soft rot monoculture test in order to minimise transfer of the preservative from the wood and mineral salts from the agar. Although several different sizes and types of mesh were used and the blocks were wetted up to an appropriate moisture content for soft rot attack the amount of decay was substantially redu...
S M Gray


A novel defaunation method of the protozoa to investigate cellulose metabolism in Coptotermes formosanus Shiraki (Isoptera: Rhinotermitidae)
1994 - IRG/WP 94-10050
The largest protozoa in the hindgut of workers of Formosan subterranean termite, Coptotermes formosanus Shiraki, was selectively eliminated by forced-feeding on low-molecular weight cellulose (LC) with a mean DP of 17. Although one week's feeding on LC caused perfect disappearance of Pseudotrichonympha grassii Koidzumi, the selective defaunation method itself had no detrimental effect on ...
T Yoshimura, K Tsunoda, M Takahashi


Estimation of effective diffusion path lengths in wood by swelling studies
1989 - IRG/WP 3524
The effective average distance that a solute must diffuse to penetrate the cell wall matrix following pressure treatment is estimated from the rate of swelling of wood, vacuum treated with water. It is assumed that the diffusion paths are similar for water and a solute such as a wood preservative component. Since bound water diffusion coefficients for water in wood have been estimated by others, t...
P A Cooper, R Churma


Testing method for the treatability of wood
1994 - IRG/WP 94-40031
In order to test and classify the treatability of wood species in pressure treatment processes with water-based solutions, a laboratory method was developed which allows the testing of small samples and limited sections of a stem, e.g. sapwood. The penetration of different liquids was determined separately concerning the three anatomical directions of wood. The common parameters for pressure impre...
A O Rapp, R-D Peek


The attack of naturally durable and creosote treated timbers by Limnoria tripunctata Menzies
1995 - IRG/WP 95-10132
Limnoria tripunctata was found tunnelling in creosote treated Douglas fir (Pseudotsuga menziesii) pilings and naturally durable greenheart (Ocotea rodiaei) gate seals at two sites on the south coast of the United Kingdom. Examination of thc creosote-treated wood showed that Limnoria tunnels were concentrated at a depth of 2-3 cm from the timber surface, where creosote loading was lower. Fewer tunn...
A J Pitman, G S Sawyer, G F Daniel


Influence of the peeling on the absorption in the sap displacement method
1990 - IRG/WP 3626
Results of tests on the Eucalyptus and pine fenceposts treated by sap displacement method are presented. Freshly cut post 2 m in length and 8 to 16 cm in diameter were placed for 6 days with their butt ends down in water soluble preservative solution (CCF) to a depth of about 65 cm, and these were inverted and kept in the same way for 3 days more. The treatment began a few hours after felling. The...
M V Baonza Merino


Examination of the Pilodyn as a non-destructive test method for detecting decay in CCA treated eucalypt poles
1982 - IRG/WP 2177
Below groundline condition of 274 CCA treated eucalypt poles comprising 13 different species was examined using 6 and 12 Joule Pilodyn units with 2 and 2.5 mm diameter pins. The data obtained was used to calculate regressions of density on pin penetration. A decrease in density was accompanied by an increase in pin penetration. The best correlation was found using the 6 Joule, 60 x 2.5 mm² diamet...
L E Leightley


Role of cell wall structure in soft rot decay of bamboo
1995 - IRG/WP 95-10133
Models of soft rot hyphal penetration of bamboo cell walls are proposed. Soft rot hyphae show an interesting capability of penetrating the bamboo cell wall in different forms; typical longitudinal penetrating hyphae and tangentially orientated penetrating hyphae. The second form of penetration was found to be different from that normally associated with wood cell walls. The differences can be attr...
O Sulaiman, R J Murphy


Ultrastructure of degraded, CCA-treated Pinus radiata wood from a marine pile
1990 - IRG/WP 1461
During an inspection of marine piles, 12 years after installation, severe degradation was noted on one of them in the vicinity of a corroded eye-bolt. The wood was dark brown in colour and tended to crumble easily. Wood fragments were examined by light microscopy and scanning and transmission electron microscopy and were also analysed for carbohydrates and lignin. Light microscopy showed numerous ...
A P Singh, M E Hedley


The reliability of colouring methods for the determination of biflourides and boron in spruce wood
1994 - IRG/WP 94-20036
From practical reasons, qualitative spraying methods are widely used for the detection of bifluorides and boron in wood. The main aim of this research was to detect whether the concentration of the active ingredient in the coloured area is equal or greater than the toxic value against basidiomycetes. Both colouring methods, Z-A reagent for fluorides and curcuma reagent for boric acid, are a reliab...
R Grell, M G Sanders, W J Homan, H Militz


The shower test method. A leaching test for assessing preservative losses from treated timber under simulated open storage conditions
1993 - IRG/WP 93-50001-04
In the late 1980's against the background of increasing environmental concern a laboratory based accelerated leaching test method for assessing preservative losses-from stored, treated timber was developed by the Dutch organisation for applied Scientific Research (TNO). This test method quantifies the amount of specific preservative components which leach from treated timber under simulat...
J B G A Havermans, W J Homan, M J Boonstra


Degradation of the gelatinous-layer in aspen and rubber wood by the blue stain fungus Lasiodiplodia theobromae
1996 - IRG/WP 96-10168
Studies on the degradative ability of the blue stain fungus Lasiodiplodia theobromae Pat. have shown several strains to cause significant weight losses (i.e. ca 20%) in the temperate and tropical wood species, aspen (Populus tremula) and rubber wood (Hevea brasiliensis). In addition to the consumption of soluble carbohydrates and extractives, major changes in the ultrastructure of fibre cell walls...
O Encinas, G F Daniel


EELS (Electron Energy Loss Spectroscopy) - a technique for quantification of nitrogen and other light elements in the cell wall
1999 - IRG/WP 99-20163
A literature survey was performed to find progress in techniques for monitoring penetration of synthetic resins in wood cell walls. Electron energy loss spectroscopy (EELS) in combination with transmission electron microscopy (TEM) was successfully applied for the high resolution examination of the distribution of a partly methylated hydroxymethyl melamine resin in Norway spruce (Picea abies Karst...
A O Rapp, H Bestgen, W Adam, R-D Peek


A comparison between the effects of ACC & CFK on the durability of beech, hornbeam and cottonwood by using Dipping & Bethel methods in the North of Iran
1997 - IRG/WP 97-40089
From the economical point of view, increasing the lumber durability by the application of preservative treatments is very important. In this study, samples were randomly selected from Fagus orientalis Lipsky., Carpinus betulus L. and Populus deltoides Bartr. in two forms (Board & Squared cross-section) and have been treated with ACC & CFK by using Dipping & Bethel methods. The matched ...
D Parsapajouh, V Etemad, K Pourtahmasebi


Microwave conditioning of Pinus radiata D. Don for preservative treatment
2000 - IRG/WP 00-40182
This paper reviews the effect of pressure steam conditioning on the permeability and treatability of green radiata pine heartwood and the potential for substituting microwave conditioning for steaming. The penetration of liquids into radiata pine occurs mainly in the radial tissue. The permeability of green radiata pine improves following steam conditioning by blowing out the soft radial tissue. T...
P Vinden, G Torgovnikov, J Romero


An in-ground natural durability field test of Australian timbers and exotic reference species. Part 5: Extensive data from a site where both decay and termites are active. Results from a full-replicated set of heartwood specimens from each of ten myrtaceous hardwoods after 18, 19 and 20 years' exposure - A discussion paper
1988 - IRG/WP 2324
Extensive data are presented on the decay situation, the termite situation and the decay-termite associations; all gathered from a fully-replicated set of heartwood specimens of 10 hardwood timbers after 18, 19 and 20 years' exposure in the ground at a single test site, i.e. a semi-arid steppe site. Sixteen tables are presented in addition to the one table providing the rating data; the l...
J D Thornton, G C Johnson, J W Creffield


Comparison between agar-block and soil-block methods for wood-destroying Basidiomycetes
1992 - IRG/WP 92-2401
The object of this work is to compare these methods in order to provide some information to help in the choice between them. The comparison was made by a statistical analysis (factorial completely randomized design) and by a discussion about other aspects of each method. An evaluation of some fungi on attacking wood and a comparison between Picnoporus sanguineus isolated from carpophore and decaye...
M B B Monteiro, S Brazolin, G Catanozi


UV-microspectrophotometry of lignin and accessory compounds in wood cell walls of conifers
1999 - IRG/WP 99-20171
The distribution of lignin in the cell wall of conifer tracheids was determined by UV-VIS microspectro-photometer. Wood sections of one micron thickness were measured between the wavelength 240 and 700 nm. Spectral analyses revealed that the conifer lignin associated with the tracheid secondary wall and middle lamella is composed of guiacylpropane units which exhibit a characteristic UV absorption...
G Kleist, G Koch, J Bauch


Fungus cellar testing as an evaluation method for performance of treated timber in ground contact
2001 - IRG/WP 01-20227
A fungus cellar method for the accelerated evaluation of performance of treated wood in ground contact is described. The test soil comprised of sandy loam, vermiculite and Japanese horticulture soil "Kanumatsuchi" in a ratio of 6:2:2 by volume. The soil was inoculated with the dominant test fungus isolated with selective medium from decayed wood samples. Pairs of treated and untreated wood specime...
Y Nagano


Previous Page | Next Page