Your search resulted in 139 documents. Displaying 25 entries per page.


Bending creep test of plywoods under long term exposure to fungal attack
1981 - IRG/WP 2163
Bending creep test and decay test were coupled in order to evaluate the durability of structural plywoods and preservative efficacy. Experimental blocks, 5.0 x 1.2 cm² section x 35.0 cm length, were impregnated with distilled water and inoculated with mycelial fragments of test fungus. Polyethylene bags stretched with metal frame were used as decay chambers. The chambers containing inoculated blo...
M Takahashi


Rapid analytical methods for wood waste - An overview
1998 - IRG/WP 98-50104
The proper handling of wood after service is a today's problem. Untreated wood could be reused or may be used as fuel. For treated wood special care is demanded to avoid environmental impacts. Thus, analytical methods are requested to detect rapidly whether and to what extend wood is contaminated, covering a wide spectrum of organic and inorganic agents used during the last 50 years. Trad...
A Peylo, R-D Peek


A Preliminary Report on the Properties of Engineered Wood Composite Panels Treated with Copper Naphthenate
2005 - IRG/WP 05-40294
This paper reports on our preliminary investigation of the properties of randomly oriented strandboard which had waterborne or powdered copper naphthenate (CuN) incorporated into the board during manufacture. When compared to zinc borate-treated controls (ZnB), the mechanical properties of strandboard (MOR, MOE, work-to-maximum load, internal bond strength) were not adversely affected by treatmen...
J W Kirkpatrick, H M Barnes


Bending properties of TCMTB-treated Southern pine sapwood using supercritical carbon dioxide impregnation process
1997 - IRG/WP 97-40080
The effects of elevated pressure and treatment with thiocyanomethylthiobenzothiazole (TCMTB) on the bending properties of Southern pine sapwood were evaluated at pressures ranging from 1,800 to 3,600 psi. All bending properties were affected to some extent by supercritical fluid treatment. Modulus of elasticity and work to maximum load were not significantly affected by pressure levels. Modulus of...
Gyu-Hyeok Kim, S Kumar, E S Demessie, K L Levien, J J Morrell


Assessment of dehydrogenase activity, fluoride content and total chromium content of soil profiles exposed to preservative treated wood within a model system
1993 - IRG/WP 93-10015
The development and prospective use of a closed model system to facilitate study of a number of indicators of environmental impact of wood preservatives laboratory conditions has been described (IRG/WP/2395-92). Chemical analysis of leachate samples collected from drained soil profiles containing creosoted pole sections remedially treated with a chromated fluoride preservative indicated small incr...
G M Smith, D C R Sinclair, A Bruce, H J Staines


Life-cycle assessement of treated wood: A view from the roa
1996 - IRG/WP 96-50078
Life Cycle Assessement (LCA) is being used increasingly as a tool to structure information on the environmental characteristics of material and processes. This paper is based on the experience gained from our LCA studies on treated wood products over the last 4 years. The comprehensive and logical examination af the information available on treated timber provided by LCA has allowed identification...
W Hillier, R J Murphy, D J Dickinson, J N B Bell


Initial results and observations of a model system to assess the efficacy and environmetal impact of preservative treated wood
1993 - IRG/WP 93-50001-02
The development of a closed model system for the laboratory assessment of the efficacy and environmental impact of a chromated fluoride remedial treatment for creosoted distribution poles has been described (IRG/WP/2395-92). The model consists of a precipitation apparatus above a treated pole section positioned in a soil profile from which leachate was collected via a series of simulated field dra...
D C R Sinclair, G M Smith, A Bruce, H J Staines


The effect of hemicellulose degradation on the mechanical properties of wood during brown rot decay
2001 - IRG/WP 01-20219
Incipient decay of wood by brown rot fungi causes measurable strength losses in wood before measurable weight loss occurs. Previous studies have shown that the high levels of strength loss that occur during incipient brown rot decay may be related to loss in hemicellulose. This paper investigates the effect of decay on hemicellulose composition and the relationship to the mechanical properties of ...
S F Curling, C A Clausen, J E Winandy


Paper for discussion - Incising of spruce to improve preservative penetration
1973 - IRG/WP 318
Large quantities of whitewood or Norway spruce (Picea abies) are regularly imported into the United Kingdom from continental Europe. In addition, increasing amounts of Sitka spruce (Picea sitchensis) are likely to become available over the next decade from the Forestry Commission. In many ways spruce is a good structural timber, eg it is relatively cheap and easily available, it has adequate stren...
W B Banks


Délavabilité de bois ronds traités avec un sel CCA dans des conditions réelles de stockage. Incidence pratique de la fixation accélérée par étuvage. Impact effectif sur l'environnement
1993 - IRG/WP 93-50001-23
Un essai de terrain a été organisé pour mesurer concrètement, dans des conditions aussi proches que possibles des conditions réelles de terrain, les pertes effectives en produit de traitement lorsque le bois traité est soumis à des intempéries. L'essai a été conduit sur des bois ronds (poteaux), traités en autoclave par procédé Bethell avec un sel CCA de type C, avec comme fi...
M Rayzal, F Larroze


Bending & tensile properties of vapor boron-treated composites
2002 - IRG/WP 02-40228
North American composites including laminated veneer lumber, oriented strandboard, and medium density fiberboard were treated by vapor boron technology and subsequently tested in static bending. Tensile properties were also determined for the two composite boards. The study was designed as 3 x 2 factorial with three treatment levels and two mill locations for each composite type. In general, mil...
H M Barnes, R J Murphy, B K Via


Strength properties of preservative treated pine and spruce wood after super-heated steaming
1984 - IRG/WP 3313
Possible changes of strength properties of CCF pressure impregnated pine and spruce with subsequent steaming at 110°C respective 120°C for 30 min were examined. For spruce analysis of variance indicated that none of the processes had a significant effect on bending strength, compression strength and the corresponding modulus of elasticity as well as on impact bending strength and shear strength ...
R-D Peek


An initial evaluation of the environmental impact of potential marine biocides
1978 - IRG/WP 441
Pilings and other structures in the marine environment are protected primarily by impregnation with creosote alone, or in combination with coal tar or waterborne preservatives such as copper-chrome-arsenate. Some of these materials are considered as possible ecological hazards and face an uncertain future; perhaps newly developed treatments to replace these conventional ones will pose different pr...
J D Bultman, P J Hannan


Assessment of wood decay in small-scale unsterile soil-bed tests
1997 - IRG/WP 97-20111
This study is concerned with the investigation of wood decay in small-scale unsterile soil-bed tests. Tests were performed with untreated heartwood samples from five hardwood species of different natural durability classes ranging from highly perishable to very resistant. Our results confirmed the critical role of soil moisture content on wood decay. The highest decay rates were observed at moistu...
L Machek, A M Derksen, R Sierra-Alvarez


Statistical evaluation of 'micro-bending' samples for classification of wood attacking fungi
1992 - IRG/WP 92-1544
Micro-specimens from both hardwood and softwood were exposed to selected species of field isolated fungi. The strength reduction and weight loss caused by these fungi were determined. A statistical procedure was then developed to classify the fungi into brown-, white-rot, or non-decay fungal categories based on these data. The procedure reveals the extent of hazard a fungus poses to wood members. ...
B Goodell, Jing Liu, A Homola, J Jellison, J Shottafer


Isolation of soil borne bacteria and fungi from treated timber
2001 - IRG/WP 01-50174
Most research in the last few decades has focused on the development of new strategies to control biological attack and the means to quantify this. Comparatively little work has been done to examine the effect that treated timber might have on its surrounding environment. This presentation will describe a methodology that attempts to detect any changes which might occur in the soil microflora foll...
I Stephan, A Stegemann, G Heidrich


A laboratory technique to measure the performance of preservative treated hardwoods in ground contact
1982 - IRG/WP 2172
A laboratory technique to measure the performance of preservative treated timber in ground contact is described. It uses partially sealed blocks of timber which are treated, leached and sawn into small stakelets for soil exposure in a fungal cellar. Performance is monitored by the loss of static bending strength with time, and a simple apparatus for measuring the deflection of a stakelet under a l...
E F Baines


The impact of global warming on the UK distribution of house longhorn beetle Hylotrupes bajulus (L)
2001 - IRG/WP 01-10414
This paper reviews the effects of global warming on insect populations and distribution. The affects of global warming on the spread of Hylotrupes is predicted through a review of research related to the influence of temperature on its life-cycle and flight. Records of Hylotrupes distribution were obtained from published surveys, entomologists and museum collections and were plotted for the UK. Th...
P Oevering, A J Pitman


In-ground field test of scots pine (Pinus sylvestris L.) sapwood and heartwood
2004 - IRG/WP 04-30336
Scots pine (Pinus sylvestris L.) sapwood and heartwood stakes treated with CCA-C and creosote were tested for one- year in a field plot in Bartın region in Turkey. Scots pine heartwood stakes had lower preservative retention than sapwood stakes. Bending strength of the stakes was decreased after impregnation and one-year field test. While the bending strength of untreated sapwood was 93....
H Sivrikaya, H Hafizoglu


Laboratory testing of wood natural durability - In soil-bed assays
1998 - IRG/WP 98-20141
Laboratory methods for assessing wood decay resistance are being investigated in the framework of an ongoing European research project. This paper summarizes the main results obtained for soil-bed tests based on the European prestandard ENV 807-Test 2. The data suggest that this testing methodology is suitable for evaluating the natural durability of timber species in soil-contact under conditions...
R Sierra-Alvarez, I Le Bayon, J K Carey, I Stephan, J Van Acker, M Grinda, G Kleist, H Militz, R-D Peek


Development of a model system to assess the efficacy and environmental impact of a chromated fluoride remedial treatment for creosoted distribution poles
1992 - IRG/WP 92-2395
A closed model system was designed to facilitate a controlled study of the leachability and environmental fate of a remedial preservative under laboratory conditions. The elements of the model include a precipitation apparatus above a treated pole section which is positioned in a representative soil profile supporting a sward of perennial ryegrass. The model will allow detailed examination of the ...
D C R Sinclair, G M Smith, A Bruce, B King


Durability of heat-treated wood
1999 - IRG/WP 99-40145
Heat-treated wood from the French process were laboratory tested against decay using agar block test and a modified soil block test. Water absorption, bending strength, lignin content and acid number were also determined to evaluate the effect of heat treatment. Heat treated samples exhibit a higher lignin content and a lower acid number compared to untreated control indicating the degradation of ...
D P Kamdem, A Pizzi, R Guyonnet, A Jermannaud


A methodology for the life-cycle assessment of treated timber products
1993 - IRG/WP 93-50001-01
Using case studies of CCA-treated motorway fenceposts and creosote-treated electricity transmission poles, the paper suggests an approach to evaluation of the overall environmental impact of treated timber products, utilising the emerging systems analysis method of life-cycle assessment (LCA). The development and application of LCA methodologies to date is reviewed and the key features identified....
S R Smith, R J Murphy, D J Dickinson


Supercritical fluid treatment: Effects on bending strength of white spruce heartwood
1993 - IRG/WP 93-20008
The effects of supercritical carbon dioxide on wood strength were evaluated using white spruce heartwood, a species known to be especially susceptible to collapse during exposure to higher pressures. The effects of pressures of 2000 or 3600 psig and temperatures of 40 or 80°C were evaluated using 30 or 60 minute exposure periods. No significant differences were noted in modulus of rupture or modu...
S M Smith, J J Morrell, E Sahle-Demessie, K L Levien


Resistance to decay of particle boards: Presentation of a test method
1986 - IRG/WP 2260
The experimentations were undertaken on particle boards 35 and 50 mm thick. The rot resistance tests were carried out on specimens whose dimensions were 600 x 75 x 35 mm³ for particle boards 35 mm thick and 800 x 75 x 50 mm³ for particle boards 50 mm thick according to a method derived from the one described in the documents IRG/WP/2214 and IRG/WP/2243. Two exposure periods were used: 12 and 16 ...
G R Y Déon, N Trong