IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 295 documents. Displaying 25 entries per page.


Diffusion of fused borate rods in top ends of poles
1989 - IRG/WP 3518
Diffusion tests of fused borate rods were carried out on extremities of sapwood poles in service. Rods were set in drills under the cone with or without addition of liquid Boracol 40. After one year of weathering, a good diffusion in the slice under the cone and even below the slice and in the cone itself was observed in Scots pine and spruce poles. The rods were still intacts and constitute, in f...
D Dirol, J P Guder


Analysing the characteristic role of moisture content for drying and fluid flow in Sitka spruce. - Part 1: The drying process of sapwood and heartwood of two different thickness of Sitka spruce using a kiln. - Part 2: Effects of moisture content on longitudinal permeability of Sitka spruce in vertical variation of the tree
2000 - IRG/WP 00-40173
The characteristic role of the moisture content in Sitka spruce (Picea sitchensis (Bong.) Carr.) that grown in the United Kingdom was examined by this study on the basis of (1) the reduction of moisture content in two different thickness of sapwood and heartwood by kiln drying process, and (2) the effects of moisture content to the longitudinal void volume filled of tanalith-C by the full-cell pro...
I Usta


Microbial biofouling of 10-40% naphthalene in creosote treated and untreated wooden pilings in the marine environment
1978 - IRG/WP 442
R R Colwell, P L Fish, D A Webb, A J Emery


A standardised procedure for the treatment of timber with test chemicals
1986 - IRG/WP 2257
A procedure is described which allows the standardisation of sample handling and data manipulation during trials invastigating the treatability of timber with test chemicals. The use of computer software allows the data to be handled efficiently....
J Norton, A Zosars, L E Leightley


Effects of pretreatments for the amelioration of preservative impregnability using the Oscillating pressure method (OPM)
1995 - IRG/WP 95-40044
For the purpose of an amelioration of preservative impregnability, three types of pretreatment: the steaming, the explosion and the boiling, were tested. The specimens were prepared by the domestic four species: Itajii, Ryukyumatsu, Sugi and Hinoki, and 1 refractry imported species: Douglas-fir. The dimension of specimens was 20 x 20 x 300 mm³ and were treated with CCA in a laboratory OPM machine...
K Suzuki, I Asaoka, S Tani, K Okada, T Hidaka


Specific gravity and moisture content of particleboards treated with various chemicals
2005 - IRG/WP 05-40310
The aim of the study was to investigated the effects of particleboard treated with various chemical substances on specific gravity and moisture content The wood raw material used in the experiments were the mixture of coniferous wood [70%, Pinus brutia Ten., Pinus nigra Arn (Lamb.), Cedrus libani Ait.] and black poplar (30%, Populus nigra L.). In this mixture, barks have been accepted up to 5 per...
Ü C Yildiz, A A Var, H Kalaycioglu, S Yildiz


The use of C CP/MAS NMR in the chemical identification of decayed and undecayed, tropical timber species
1984 - IRG/WP 1224
13C CP/MAS NMR was found to be an extremely powerful tool for elucidating the chemical composition of Eucalyptus maculata, Pinus elliottii and Alstonia scholaris. The differences in lignin composition were different for each timber and discussed in relation to decay caused by soft-rot and white rot fungi. In particular the presence of syringyl and guaiacyl lignin types are discussed.
L E Leightley


Lignin-copper, a new wood preservative without arsenic and chromium
1992 - IRG/WP 92-3702
A more environmentally sound treatment for wood with preservatives containing no arsenic or chromium, has been developed and studied on a laboratory scale. The method involves a first step impregnation with an aqueous solution containing modified, water-soluble kraft lignin followed by a second step involving impregnation with a copper salt solution to give fixation of the lignin into a water-inso...
B Ohlsson, R Simonson


Addendum to Document No: IRG/WP/428
1977 - IRG/WP 437
A J Emery


Natural resistance of twenty-six Guianese wood species against marine borers
1988 - IRG/WP 4144
This note is a contribution on the study of the natural resistance of some wood species from French Guiana, some of which could be found too in the neighbourhood. Here are presented the results after one year exposure in the marine environment....
L N Trong


An insight into brown rot decay of timber as revealed by 13C CP/MAS NMR
1985 - IRG/WP 1259
L E Leightley


A new approach to the maintenance of wooden railway sleepers. (Second report)
1988 - IRG/WP 3492
The microenvironment and micro-ecology of wooden railway sleepers was investigated to assess their condition to determine the necessary treatment, repair and replacement criteria. In this report the efficacy of the secondary preservative treatment with solid boron rods is discussed and the development of an in-situ, nondestructive test method based on the creation and assessment of structural dyna...
W Beauford, P I Morris, A M Brown, D J Dickinson


The variation in electrical resistance in the CCA-treated wood during the fixation
1989 - IRG/WP 3554
The curve commonly used in Scandinavia for describing the fixation period at different temperatures for CCA-impregnated wood is based on investigation by Dahlgren on the pH-variations in a mixture of sawdust and preservative solution. As far as we know there is no such investigation on solid wood. We have therefore measured the electrical resistance in CCA-treated solid wood to see if this will di...
F G Evans, B Nossen


Immunogold labelling of size marker proteins in brown rot-degraded pine wood
1990 - IRG/WP 1428
Pine wood degraded by Fomitopsis pinicola was infiltrated with a mixture of ovalbumin (45 kDa) and myoglobin (16.7 kDa). After crosslinking of the proteins with glutaraldehyde and preparation for electron microscopy ultrathin sections were labeled with gold-conjugated antibodies. Simultaneous labeling of both proteins on the same section showed that at 50-70% weight loss ovalbumin did not penetrat...
E Srebotnik, K Messner


A novel lipid-related compound, (Z)-1,7-nonadecadiene-2,3-dicarboxylic acid, produced by white-rot fungus Ceriporiopsis subvermispora
2001 - IRG/WP 01-10411
Lipid peroxidation is a possible oxidative process of lignin-degradation at a site far from the enzymes by selective white rot fungi. Production and peroxidation of saturated and unsaturated fatty acids by Ceriporiopsis subvermispora strongly suggests involvement of lipid peroxidation in its ligninolytic system. In this paper, a new aliphatic lipid-related fungal metabolite was isolated from wood ...
M Enoki, Y Honda, M Kuwahara, K Messner, T Watanabe


Spatial arrangement of lignin peroxidase in pine decayed by Phanerochaete chrysosporium and Fomitopsis pinicola
1988 - IRG/WP 1343
By applying immunoelectronmicroscopic methods, lignin peroxidase of the white rot fungus Phanerochaete chrysosporium has been localized in the cytoplasm of hyphae, close to the plasmalemma and on the plasmalemma. Infiltration of wood specimen with culture filtrates, concentrated 300-fold, gave clear information on the penetration of the enzyme into the wood cell wall. Penetration was restricted to...
E Srebotnik, K Messner


The effect of service life and preservative treatment on the hardness of wooden poles
1989 - IRG/WP 3537
The surface hardness of utility poles is an important parameter which effects the acceptability of the pole as being safe to climb during line maintenance. The current investigation was designed to evaluate how the surface hardness of preservative treated utility poles is effected by the type of preservative, and the age of the poles. Chromated-copper-arsenate (CCA) treated red pine and jack pine ...
E B Jonsson, E M A Nilsson, J N R Ruddick


Collaborative soft rot test: Amended test method
1972 - IRG/WP 208
The initial draft of a standard test method (Document IRG/WP/201) was discussed at the meeting in Brussels in 1971. It was agreed that a revised draft should be prepared and that the Princes Risborough Laboratory (formerly FPRL) should conduct a trial test using the method as a preliminary to the main collaborative test....
J G Savory


A summary of tests and practical experiences with the Pilodyn wood testing instrument
1980 - IRG/WP 282
This paper presents a summary of the reports, tests and practical experiences with the Pilodyn wood tester not only, however, concerning poles but also in other fields such as standing trees, sawn timber etc. The principle of the Pilodyn is a spring-loaded pin which is fired into the object and the depth to which the pin penetrates is correlated to physical and mechanical properties of the object....
H Friis-Hansen


Emission of trimethyl borate and methanol from radiata pine (Pinus radiata D. Don)
1995 - IRG/WP 95-30088
Sawn and kiln dried radiata pine conditioned to 3, 6, and 12% moisture content was treated with trimethyl borate (TMB). The treated wood samples were placed in mini-desiccators maintained at 20 or 40°C. The air space within the mini-desiccator was analysed for TMB and methanol. An initial period of emission of TMB and methanol was observed. This was followed by a period of gradual dissipation of ...
F J Romero, P Vinden, J A Drysdale


Some observations on miniaturised soil/block tests
1988 - IRG/WP 2317
Results are presented for miniaturised soil/block tests carried out in 120 ml capacity glass jars. The four test fungi (Coniophora puteana, Coriolus versicolor, Gloeophyllum trabeum and Poria placenta) reacted differently to different moisture regimes established by varying the soil moisture content. Acceptable levels of decay were achieved by the three brown rot fungi with soil at 110% whc; howev...
J K Carey


Report on questionnaire: Facility for accelerated stake tests in unsterile soil
1983 - IRG/WP 2169
In October 1981 a questionnaire (IRG Doc. No. IRG/WP/2166) on the so-called fungus cellar tests in unsterile soil was prepared and despatched to 56 individuals representing various institutes, organisations, or companies. In addition a further 68 letters describing the purpose of the questionnaire were sent to additional IRG members who could request the full questionnaire if appropriate. This rep...
J A Butcher


Development of a method for testing wood preservatives with soft rot fungi
1975 - IRG/WP 250
Although the first publications on experimental soft rot attack date back 20 years ago, so far no test method for evaluating the efficacy of wood preservatives against soft rot attack (Ascomycetes and Fungi Imperfecti) has been generally accepted. The reasons are diverse and the shortcomings and the disadvantages of the methods described are well known and have repeatedly been discussed. The soil ...
M Gersonde, W Kerner-Gang


Involvement of hydrogen peroxide in wood decay by brown-rot and white-rot fungi
1985 - IRG/WP 1256
To gain further understanding of the role of H2O2 in wood degradation by brown- and white-rot fungi, we studied the following: (a) extracellular H2O2 production, (b) effect of various hydroxyl radical (·OH) and singlet O2 (1O2) quenching agents on wood and cellulose degradation, (c) intracellular H2O2 production and catalase activity, and (d) cytochemical localization of H2O2 with diaminobenzidin...
T L Highley, L L Murmanis


Collaborative soft rot tests: Results of analyses of soil samples
1976 - IRG/WP 263
C R Levy


Previous Page | Next Page