IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 113 documents. Displaying 25 entries per page.


Paintability and gluability of wood treated with arsenic-free and chromium free preservative treatments
2006 - IRG/WP 06-40342
The objective of this project was to study, in comparison with traditional CCA treatment, the paintability and gluability of wood treated with arsenic-free and chromium-free preservative treatments. Four formulations, all certified CTB P+, were selected in accordance with their representativeness of the preservative product market: one CCA reference formulation and three chromium and arsenic free...
L Podgorski, G Legrand


Micro- and hydro-sandblasting for wood and wood coatings
2007 - IRG/WP 07-40380
Exterior wood coatings are getting increasingly durable and often more film forming. As a result they become difficult to renovate. Conventional renovation techniques (chemical or thermal stripping, sanding) are demanding techniques which take a long time to implement. Therefore renovation techniques are requested which are easier to use and which ensure that the wood surface is suitable for a re-...
L Podgorski, V Georges, P Svane


End Coating Masson Pine Grown in South China to Prevent the Development of Blue Stain
2007 - IRG/WP 07-30428
One end (randomly selected) of logs of mason pine (Pinus massoniana) were coated with a wax-type end coating called ANCHORSEAL® immediately after tree cutting. The logs were then stored in summer weather in Guangxi, China. During the storage, at week 1, 2, 3, 4, 6, 8 and 12, five logs of mason pine were sawn into lumber or veneer for the visual observation and measurement of blue stain at the coa...
Zhao Youke, Qin Li, Huang Rongfeng, Lu Jianxiong


Natural Weathering of Coated Oil Heat Treated Wood
2007 - IRG/WP 07-30440
Oil heat-treated (thermally modified) pine wood was coated with 9 different types of solvent- or water-borne exterior finishes. The systems with modified wood substrate as well as unpainted and painted non-modified controls were exposed to weathering (EN 927-3) on two locations with sub-alpine and alpine climate. The influence of natural ageing on surface systems was evaluated after one year of ex...
M Petric, B Kricej, M Pavlic, A Rapp


Relationship between coating properties and their performance on treated wooden decks
2008 - IRG/WP 08-30454
Preservative treated wood benefits from the application of a surface coating to protect it from weathering (UV and rain). Different preservative formulations may affect surface properties of treated wood differently; therefore compatibility of coatings with different preservative treated wood types should be considered. This paper examines coatings characteristics and their weathering performance ...
M Ahmadinejad, P A Cooper


Effect of CCA and Tanalith E on the performance of surface finishing
2008 - IRG/WP 08-40405
Effect of CCA and Tanalith E treatment on the performance of surface finishing properties was the objectives of this study. Sapwood of scots pine, (Pinus sylvestris L.) and oriental beech (Fagus orientalis Lipsk.) specimens (300 x 100 x 15 mm along the grain) were impregnated with aqueous solution of CCA 2% and Tanalith E 2%. Surface roughness, dry film thickness, adhesion strength, gloss measur...
T Ozdemir, A Temiz, I Aydin


Bi-oleothermal treatment of wood at atmospheric pressure: resistance to fungi and insects, resistance to weathering and reaction to fire results
2008 - IRG/WP 08-40418
Bi-oleothermal process is a simple treatment which has been developped by CIRAD in cooperation with FCBA. It allows a deep impregnation of wood with hydrophobic products using cheap facilities. The process includes two steps at atmospheric pressure. The first one is a dipping of wood samples in a hot oil bath (between 110 °C and 200°C) which creates an overpressure inside the wood. The second on...
L Podgorski, I Le Bayon, I Paulmier, J-D Lanvin, V Georges, D Grenier, H Baillères, J-M Méot


Control de calidad eficiente de proteccion superficial sobre madera
2008 - IRG/WP 08-20397
Quality control is important to assure efficient protection of wood surfaces. When wood is exposed to the environment, it degrades due to weathering or environmental factors alone. Aging tests are utilized to test coating products. Quality control techniques are performed on exposed products according to standardized methods (NCh, ASTM, ISO, DIN, EN, FTMS, NTF, NBINT, or equivalents). Certified l...
A M Fernández S


Improving the Dimensional Stability and Fire Resistance of OSB by Roller-Coating Panels with UV-Curable Finishes
2008 - IRG/WP 08-40434
Oriented strandboard was sanded and roller-coated with UV-cured finishes. The effects of these treatments on the surface roughness, dimensional stability and fire resistance of OSB were assessed. Sanding reduced the average roughness of OSB, but it had a smaller effect on maximum roughness because sanded boards still contained surface voids between some strands. Sanded boards absorbed less than ha...
P D Evans, I Cullis


Continuous moisture measurement (CMM) to detect failure of moisture resistance
2009 - IRG/WP 09-20422
A wood coating system will fail to perform properly after a certain time of weathering. From that moment, the substrate is especially prone to fungal attack. Moisture plays a key role on weathering performance, wood protection efficacy and decay susceptibility of wood. Therefore, knowledge of the moisture dynamics of the applied wood protection is of significant importance in the prediction of the...
I De Windt, J Van den Bulcke, J Van Acker


Weathering of Wood Modified with the N-Methylol Compound 1,3‑dimethylol-4,5-dihydroxyethyleneurea (DMDHEU)
2009 - IRG/WP 09-40467
Scots pine (Pinus sylvestris L.) sapwood boards were treated with a methylated 1,3‑dimethylol-4,5-dihydroxyethyleneurea (mDMDHEU) causing weight gains of approx. 25% and exposed to weathering for 18 months. Compared to untreated boards, treatment with mDMDHEU reduced surface discoloration mainly caused by staining fungi. Boards treated with mDMDHEU exhibited clearly lower moisture content th...
C Mai, Yanjun Xie, A Krause, K Urban, P D Evans, K Richter, H Militz


Selection of an appropriate coating system for wooden boats to be used in fresh water
2009 - IRG/WP 09-40472
Properties of several, most commonly used protective low-price coatings, which are used by the pletnja boat owners in Bled, Slovenia, were extensively studied. The aim of this professional, practically oriented study was to compare various coating systems, and to recommend the most suitable one to the boat owners. Regarding specific use conditions, the following properties, including their resista...
M Petrič, B Kričej, A Logar, M Pavlič


A fast and economic method to produce grey wooden surfaces for decking and cladding: preliminary results
2009 - IRG/WP 09-40474
Uncoated wood is commonly used in France for cladding and decking to minimise maintenance. However wood surfaces progressively turn grey due to exposure to sunlight and water. This grey colour develops after several months depending on the wood species and the exposure: in the northern hemisphere surfaces facing south and west are most exposed and turn grey more rapidly than those facing north and...
L Podgorski, V Georges, I Garmendia, B Sánchez Sarachu


Impact of wood species on the performance of exterior wood coatings
2010 - IRG/WP 10-40519
To prolong the service life of a wooden construction the protective function of a coating is of utmost importance. The chemical composition as well as the wood-coating interface affects the performance of this protective layer and obviously wood species have an impact too. This paper discusses the influence of wood species on the overall coating performance. Therefore, a range of opaque waterborne...
I De Windt, J Van den Bulcke, J Van Acker


Wet and dry adhesion of coatings on modified and unmodified wood: comparison of the pull-off test and the cross-cut test
2010 - IRG/WP 10-40524
The objective of this paper is to study the influence of several types of modification (acetylation, furfurylation, thermal modification) on coatings adhesion and to compare two methods of assessing the adhesion: the cross-cut test and the pull-off test both tested in dry and wet conditions. The study also investigates the effect of other parameters of the wood substrates on adhesion like the ring...
L Podgorski, G Grüll, M Truskaller, J D Lanvin, V Georges, S Bollmus


Silicon compounds as additives improving alkyd-based wood coatings performance
2010 - IRG/WP 10-40531
The reactivity of cellulose with solvent-born alkyd-based wood coatings supplemented with organosilanes was analyzed. Structural analysis of cellulose subjected to the reaction with organosilanes and following extraction with water was performed using Fourier-transform infrared spectroscopy (FTIR). The analyzed IR spectra comprise bands 1250 cm-1 typical for the SiC group and 800 cm-1 typical for ...
B Mazela, I Ratajczak, K Wichłacz-Szentner, P Hochmańska


Aesthetic service life of coated and uncoated wooden cladding - influencing factors and modelling
2011 - IRG/WP 11-20470
Mould growth on exterior coated cladding façades is an undesirable element and will often shorten the aesthetical service life. Mould growth on painted surfaces is influenced by type and concentration of film fungicides, the paint formulation and the wood substrate itself, and wooden cladding may experience exponential fungal deterioration caused by variation in the climatic factors, often within...
L Ross Gobakken, O A Høibø


Moisture protection and performance during 5 years exposure of 19 wood coating systems on a cladding in Vienna
2011 - IRG/WP 11-40561
A cladding with vertical boards of Norway spruce (Picea abies) comprising different coating systems had been exposed to natural weathering oriented south west in Vienna for 5 years. Weathering behaviour of the boards was assessed in intervals and wood moisture content was measured over the first 22 months of exposure. The moisture protective properties of the coating systems were assessed using la...
G Grüll, I Spitaler, M Truskaller


Wet and dry adhesion of coatings on modified and unmodified wood: influence of 18 months of natural weathering on the pull-off test and cross-cut test results
2011 - IRG/WP 11-40569
The objective of this paper is to study the influence of several types of modification (acetylation, furfurylation, heat treatment) on coatings adhesion after 18 months of natural weathering according to EN 927-3 in Vienna (Austria). The paper compares two methods for assessing the adhesion: the cross-cut test (EN ISO 2409) which is the conventional method used and recommended in EN 927-3 and th...
L Podgorski, G Grüll, M Truskaller, J D Lanvin, S Bollmus


Water uptake of wood surfaces with and without coating: influence of weathering
2012 - IRG/WP 12-40580
The objective of this study was to compare liquid water absorption of wood surfaces with and without coating, before and after artificial weathering. Samples of spruce, oak and sapelli were exposed to the EN 927-6 cycle for 1500 and 1850 hours and to the weathering produced by the Garner wheel for 1000 hours. Two highly pigmented coatings (solventborne and waterborne) and two semi-transparent stai...
L Podgorski, S Collignan, J D Lanvin


Comparison of exterior performance of two coating systems based polyurethane applied Pinus sylvestris L. and Picea orientalis L. wood
2012 - IRG/WP 12-40588
Some surface changes in sapwood and heartwood of two species before applying clear-coating were characterized after accelerated weathering time. Wood specimens covered with two types polyurethane (PU) films were also observed in accelerated weathering exposure. In this study, changes on the wood surface were compared of between wood specimens covered with two types polyurethane (PU) films after ir...
Ö Özgenç, Û Cafer Yıldız


Field-testing of Norway Spruce Claddings with Monitoring of Moisture Content, Material Temperature and Microclimate
2012 - IRG/WP 12-20502
The physical function of a cladding is to protect the interior construction. Under normal circumstances the performance requirements can be met for a very long time, meaning that the technical service life of a wooden cladding can be very long. Since the cladding is a major part of the facade, it also has visual requirements that may define the aesthetic service life, and often it is much shorter ...
G I Vestøl, L Ross Gobakken


Protective nanoparticle coating reducing water absorption of wood species
2012 - IRG/WP 12-40614
Nanoparticle coatings were deposited onto different tropical wood samples for controlling the surface hydrophobicity. The styrene(maleimide) nanoparticles were synthesized in aqueous dispersions under pure conditions or in combination with 70 wt.-% palm oil. A first evaluation of the non-coated wood surfaces indicates a high dependence between the water contact angles, the average surface roughnes...
P Samyn, A Paredes, G Becker, H Van den Abbeele, L Vonck, D Stanssens


Detection of Aureobasidium as the dominant fungus on coated wood
2013 - IRG/WP 13-10796
Wood is often covered with a coating in order to protect the surface. Unwanted dark mold growth on paint covered surfaces in external conditions is a familiar phenomenon. Simple microbial techniques have commonly been used to determine the dominant fungal species present in the discoloured area, for example morphological analysis of microscopic preparations of fungal pieces sticking to an adhesive...
E J Van Nieuwenhuijzen, M F Sailer, R A Samson, O C G Adan


Inhibitory extractives or nutrients? Mould growth on coated heartwood and sapwood of Pinus sylvestris and Gleditsia triacanthos
2013 - IRG/WP 13-10806
Sometimes mould fungi grow over weathered coated sapwood, whereas the coated heartwood is not colonised. Two factors may be responsible for these differences: Either the larger content of nutrients in the sapwood, or the content of biocidal extractives in the heartwood. In this study the factors for the difference in mould growth on coated heartwood and sapwood of Pinus sylvestris (Scots Pine) and...
D Lukowsky, N Buddruhs


Previous Page | Next Page