Microbial decay of an archaeological wood
1994 - IRG/WP 94-10053
A light and transmission electron microscopic investigation of an archaeological wood was undertaken to determine the cause of its deterioration. The wood came from a bulwark constructed in early 1100 in the lake Tingstäde Träsk on the island Gotland in Sweden. The samples of the wood, which was identified as Pinus sylvestris, were taken from a depth of 0.85 m below the bottom level. The wood wa...
A P Singh, T Nilsson, G F Daniel


An appraisal of methods for environmental testing of leachates from salt-treated wood; part 1
1998 - IRG/WP 98-50115
The magnitude and diversity of leaching tests with salt-treated wood, performed by institutes as well as industry, strongly appeal for harmonisation towards one single method. That procedure should be well-defined, cost- and time-effective and moreover be extended with a clear detection and interpretation scheme. The paper(s) presented here tend to evaluate 2 existing leaching methods, the ENV 12...
G M F Van Eetvelde, M Stevens, F Mahieu, H-W Wegen, A Platen


Composting of waste building up in sawmill dipping basins
1990 - IRG/WP 3570
We have studied composting of waste building up in dipping basins at sawmills although this waste can also be disposed of by incineration. Controlled composting within the sawmill area seems to be a feasible method. Another possibility is to accomplish composting directly at the local dumping site. Waste containing antistain chemicals is generally classed as hazardous. It cannot therefore be place...
I A Linderborg, U Ek


Qualifying ecotoxicity research on tropical hardwood leachates
1997 - IRG/WP 97-50096
Almost as a rule, quantification and identification of various types of environmental contamination is grounded on chemical evaluation principles. Yet for monitoring surface water pollution, aquatic bio-assays may provide a more direct way to assess the potential hazard of environmental samples. A battery of such tests is experienced onto leachates of tropical hardwoods used in ground and water co...
G M F Van Eetvelde, P Marchal, M Stevens


Losses of CCA components and creosote from treated timber to soil
1997 - IRG/WP 97-50098
Components of creosote and CCA preservatives can migrate within the wood and move into surrounding soil. However, at present, the ecological significance of such losses is uncertain. This paper examines the distribution of four target polyaromatic hydrocarbons (PAHs ) and of copper, chromium and arsenic in treated stakes and surrounding soil after long term exposure in field trials. Concentrations...
N J Hudson, R J Murphy


Timber deterioration and its prevention in marine environment
2005 - IRG/WP 05-10559
Wood-borer activity is an established fact in Mumbai harbour that leads to severe deterioration of timber. In order to prevent the deterioration caused by wood borers three resin preservatives containing Zinc borate, Organo-copper polymer (4 wt% Cu) and Organo-Tin polymer Copoly(TBTM-MMA) were used for timber treatment. Test panels were treated using standard method and the...
B S Swami, M Udhayakumar, P Kumar, A B Samui


Fumigation of New Zealand grown western red cedar for export markets
2001 - IRG/WP 01-30262
The objective of this study was to demonstrate that methyl bromide fumigant penetrates into the centre of western red cedar (Thuja plicata L.) timber to meet the standard for export markets. Kiln dried western red cedar was used and a cavity (50x 30 x 13mm3) was prepared into the centre of each sample board (500 x 200 x 26 mm3 thick). An absorbent sachet used in industry for cross checking that th...
B Kreber, G Durbin, D Wilson


Losses of preservatives from treated wood during service. Results from a questionnaire
1994 - IRG/WP 94-50031
From environmental as well as from performance point of view it is of interest to know how much of the preservatives in treated wood that is leached out or evaporated from the wood during service. Many laboratory studies are carried out on leaching from small samples in distilled water or water with different pH. These studies give a good picture of the relative leaching from wood treated with dif...
M-L Edlund


Scandinavian experience – 25 years’ experience in transforming used creosoted wood into bio-fuel
2005 - IRG/WP 05-50224-18
Swedish experiences show that the best and most efficient way to handle the creosoted wood waste is through combustion. The preparation of creosoted waste wood to fuel chips at IQR AB’s plant in Trollhättan is done by splinting the wood according to a special method. Mainly railroad sleepers, but also other wooden commodities, from all over Europe are delivered to the plant. The wood material i...
T Karlström


Losses of pyrethroids from treated wood due to photodegradation
1998 - IRG/WP 98-30177
The fact that significant photodegradation of pyrethroids can occur in use has been established for over 20 years. It is known, mainly from experience with tsetse fly control, that such degradation leads to marked reductions in efficacy. This realisation has lead to extensive investigation into ways of stabilising this group of important insecticides. Pyrethroids are widely used as the insecticid...
J D Lloyd, M W Schoeman, F Brownsill


The biological effectiveness of wood modified with heptadecenylsuccinic anhydride against two brown rot fungi: Coniophora puteana and Gloeophyllum trabeum
1992 - IRG/WP 92-3705
A modified soil block test was carried out using wood samples reacted with heptadecenylsuccinic anhydride (ASA). This modification gave good resistance to decay brought about by the brown rot fungi Coniophora puteana and Gloeophyllum trabeum during the twelve week exposure period. Results indicated that there was a good correlation between increased loading of modifying reagent and an increase in ...
C Codd, W B Banks, J A Cornfield, G R Williams


An investigation of the factors influencing the rate of deterioration of timber samples due to microfungi in laboratory tests
1997 - IRG/WP 97-20116
An investigation was performed into the comparative performances of test 1 (vermiculite burial) and test 2 (soil burial) as described in ENV 807. Two test preservatives were used - copper naphthenate and propiconazole. Copper chromate was included as a reference preservative. The wood species used was beech (Fagus sylvatica). Test 1 was performed using both a mixed inoculation of the five stipulat...
I J Herring, D J Dickinson, S M Gray, J K Carey


Study of the degradation caused by micro-organisms in Pinus sp. waterlogged wood
1989 - IRG/WP 1411
So far, the different Centers are trying the restoration and the conservation of wood structures, coming from subaquatic archeological deposits, with interest from the historic - artistic point of view. The main objective of this paper has been the determination of the decay level of Pinus sp. wood coming from a roman ship (approximately 2000 years old), where we have analyzed their physical prope...
M T De Troya, M C Escorial, J Garcia, A Cabanas


Some studies on fungal deterioration of rubber wood (Hevea brasiliensis)
1980 - IRG/WP 2140
For the sreening of anti-stain chemicals trials with selected agricultural fungicides and new chemicals were carried out. Botryodiplodia theobromae, Aspergillus sp. and Penicillium sp. were used at test organisms. For testing the durability of rubber wood (Hevea brasiliensis) suitable local rotting fungi (Basidiomycetes), based on high degrading power, which may later be employed in standard tests...
A Sujan, A G Tan, M Stevens


Creosote losses due to ageing methods prior to laboratory efficacy testing
2002 - IRG/WP 02-20256
Laboratory efficacy testing of creosote is affected by the impact of volatile components on the fungal growth. European test methods for assessing efficacy against Basidiomycetes and soft rot fungi is based on two standard methods, EN 113 and ENV 807 respectively. Combined with both fungal tests two pre-treatment methods are commonly used, namely EN 84 (leaching) and EN 73 (evaporation). Within th...
J Van Acker, K Ghekiere, M Stevens


Deterioration of wood viewed from iron nail
1991 - IRG/WP 2368
Deterioration of nail was graded by a five - rank numerical - rating. The rating of nail moisture content and decay of wood were inspected in a mortal-wall of 34-year-old house. The wood was mostly in decay, when the rating of the nail was above about 4, and the moisture content was above about 20%. Nailed wood specimens kept in several humidity room of 20°C for 4 years showed that the rating of ...
H Imamura


Effects of air-seasoning on fungal colonization and wood strength of Douglas fir poles
1987 - IRG/WP 1315
Air seasoning economically reduces the moisture content of Douglas fir poles before pressure treatment with preservatives. Advanced decay in poles in service has resulted when decay fungi (Basidiomycetes) colonized poles during air-seasoning and survived the treatment process. These problems have led to recommendations to severely limit this practice. To determine the role of these fungi in peeled...
J J Morrell, M E Corden, R D Graham, B L Kropp, P Przybylowicz, S M Smith, C A Sexton


Isolation and identification of non-decay fungi affecting the performance of alkylammonium compounds
1993 - IRG/WP 93-10020
The isolation of DDAC tolerant fungi was carried out on lumber treated with a range of antisapstain chemicals containing DDAC as one of their active ingredients. The tolerant fungi were selected by using malt media spiked with DDAC (100 and 2500 ppm). Isolations were tentatively identified into a range of fungi commonly found associated with wood deterioration (i.e. Penicillium sp. and Trichoderma...
A K Doyle, J N R Ruddick


Deterioration and preservation of Japanese pampas grass as a roofing material
1991 - IRG/WP 1490
The deterioration and preservation of Japanese pampas grass as a roofing material were investigated. The pith of stem and sheath were more rapidly decomposed. The vessels were the most important pathway of microbial prevalence. Hyphae invaded into the cell wall of fiber and parenchyma, and made the cavities with conical ends. The contacting cell wall of parenchyma in pith with hyphae was decompose...
K Fukuda


Electrochemical deterioration of wood in sea-water
1981 - IRG/WP 464
In the specialistic literature only few items can be found dealing with the specific kind of wood deterioration called electrochemical corrosion of wood. This deterioration occurs predominantly on marine vessels, yachts, and other marine craft where wood is jointed by means of various metal connectors. Up to date information demonstrates that in wood surrounding copper connectors, when in proximit...
J Raczkowski


Imaging fungal deterioration of wood using x-ray microtomography
1997 - IRG/WP 97-10240
Nondestructive tomographic images of solid Southern yellow pine (SYP) wood and SYP during deterioration by wood decay fungi were obtained by using a new class of synchrotron X-ray computed microtomography (CMT). The CMT images will provide information about spatial relationship between degrading fungi and wood structures. Wood samples were scanned with synchrotron-generated X-rays at high resoluti...
B Illman, B A Dowd


The effect of acid rain on CCA treated timber
1990 - IRG/WP 3579
The effect of acid precipitation on the leaching of copper, chromium and arsenic from timber treated with different CCA preservatives was studied in the presence of three types of soil under simulated field conditions. Pine sapwood, embedded in soil, was subjected to simulated rainfall at three different levels of acidity. The CCA preservative formulations tested were:- American Wood Preservers&am...
R J Murphy, D J Dickinson


Method to determine the depth of penetration of the biologically active components of wood preservatives
1978 - IRG/WP 2108
A time-saving method for determining the depth of penetration of the biologically active components of wood preservatives is described. The test specimens were obtained by cutting thin slices from the wood either parallel or perpendicular to the treated surface. The slices were then exposed to fungal attack. A good correlation was found between the test results obtained by the modified German Stan...
H-P Sutter


A technique for measuring preservative loss or redistribution during leaching
1983 - IRG/WP 2199
Radiata pine sapwood stakes were treated with benzalkonium chloride (AAC) or copper-chrome-arsenate (CCA). After fixation and drying the outer 2 mm and 2-4 mm layers were removed from one radial longitudinal face. The planed face was coated with a waterproof coating and AAC-treated stakes were leached for 6, 12 or 18 weeks; 12 weeks for the CCA-treated stakes. After airdrying three 2 mm layers (0-...
J A Drysdale


Micromorphological and chemical changes of archaeological woods from wrecked ship's timbers
1987 - IRG/WP 4136
Micromorphological and chemical alterations of sea-waterlogged woods obtained from the ship-wrecked materials which had been submerged in Yellow Sea for over 700 years were investigated. The woods were deteriorated in varying degrees by marine organisms depending on species and parts of the woods. Under the light and scanning electron microscope the morphological characteristics of deteriorated wo...
Y S Kim