Your search resulted in 1197 documents. Displaying 25 entries per page.
Immunogold labelling of size marker proteins in brown rot-degraded pine wood
1990 - IRG/WP 1428
Pine wood degraded by Fomitopsis pinicola was infiltrated with a mixture of ovalbumin (45 kDa) and myoglobin (16.7 kDa). After crosslinking of the proteins with glutaraldehyde and preparation for electron microscopy ultrathin sections were labeled with gold-conjugated antibodies. Simultaneous labeling of both proteins on the same section showed that at 50-70% weight loss ovalbumin did not penetrat...
E Srebotnik, K Messner
A novel lipid-related compound, (Z)-1,7-nonadecadiene-2,3-dicarboxylic acid, produced by white-rot fungus Ceriporiopsis subvermispora
2001 - IRG/WP 01-10411
Lipid peroxidation is a possible oxidative process of lignin-degradation at a site far from the enzymes by selective white rot fungi. Production and peroxidation of saturated and unsaturated fatty acids by Ceriporiopsis subvermispora strongly suggests involvement of lipid peroxidation in its ligninolytic system. In this paper, a new aliphatic lipid-related fungal metabolite was isolated from wood ...
M Enoki, Y Honda, M Kuwahara, K Messner, T Watanabe
Spatial arrangement of lignin peroxidase in pine decayed by Phanerochaete chrysosporium and Fomitopsis pinicola
1988 - IRG/WP 1343
By applying immunoelectronmicroscopic methods, lignin peroxidase of the white rot fungus Phanerochaete chrysosporium has been localized in the cytoplasm of hyphae, close to the plasmalemma and on the plasmalemma. Infiltration of wood specimen with culture filtrates, concentrated 300-fold, gave clear information on the penetration of the enzyme into the wood cell wall. Penetration was restricted to...
E Srebotnik, K Messner
Differential behaviour of wood rotters at water repellent Rubberwood
2000 - IRG/WP 00-10386
Rubberwood samples treated with different concentration of aqueous solution of chromic acid has induced significant increase in water repellency and attains dimensional stability. Though water repellency and dimensional stability was achieved by treatment, the fungal invasion could not be completely controlled. Differential level of decay of brown and white rot in wood treated with water repellent...
H C Nagaveni, S S Chauhan, K S Rao
Removal of heavy metals from treated wood using biological methods
2005 - IRG/WP 05-50226
Heavy metals were removed from wood treated with copper based preservatives using brown-rot fungus Fomitopsis palustris. The amount of effective elements removed by treatment methods was examined. The relationship between oxalic acid concentration and the amount of heavy metals removed from each treated wood was also investigated. The relationship between fungus weight and removal rate was also in...
Dong-won Son, Dong-heub Lee
Development of a method for testing wood preservatives with soft rot fungi
1975 - IRG/WP 250
Although the first publications on experimental soft rot attack date back 20 years ago, so far no test method for evaluating the efficacy of wood preservatives against soft rot attack (Ascomycetes and Fungi Imperfecti) has been generally accepted. The reasons are diverse and the shortcomings and the disadvantages of the methods described are well known and have repeatedly been discussed. The soil ...
M Gersonde, W Kerner-Gang
Preservation of hyphal-forming brown- and white-rot wood-inhabiting basidiomycetes
2001 - IRG/WP 01-10397
Lyophilization is an excellent technique for the long-term preservation of hyphal-forming brown- and white-rot wood-inhabiting basidiomycotina. However, vegetative mycelial isolates are not lyophilizable. In this study, 10 brown-rot and 10 white-rot basidiomycetous non-sporulating, non-chlamydosporulating, and non-bubillerferous basidiomycetes fungi were tested for viability after lyophilization. ...
S C Croan
Fungi associated with groundline soft rot decay in copper/chrome/arsenic treated heartwood utility poles of Malaysian hardwoods
1992 - IRG/WP 92-1567
Copper-chrome-arsenic treated heartwood from Malaysian hardwood utility poles in service for 8-23 y at two localities in the wet tropical Peninsula Malaysia were surveyed for soft rot in the ground-contact region. Soft rot decay was detected in all the poles. Isolation studies indicated the ability of a variety of microfungi and basidiomycetes to colonize treated heartwood. Most isolates exhibited...
A H H Wong, R B Pearce, S C Watkinson
Standardisation of tests of toxicity of preservatives to soft rot fungi
1978 - IRG/WP 2119
J G Savory
Some tests on ES - AS 11, a novel anti-sapstain formulation, and its properties
1987 - IRG/WP 3399
The results of some tests with the formulation ES - AS 11 are given. The formulation is an attempt to improve the performance of an anti-sapstain chemical by: 1) increasing its penetrability 2) uniquely combining its active ingredients. Very short times of treatment (dipping not longer than 5 seconds), low concentrations of active ingredients, and lower toxicological and environmental risks may be...
U Straetmans
Decay resistance of Scots pine (Pinus sylvestris) heartwood against brown rot
2002 - IRG/WP 02-10433
Natural decay resistance of wood is mainly restricted in the heartwood and based on wood microstructure and chemical composition. The genetic variation in the durability of Scots pine (Pinus sylvestris L.) wood against decay and the relationship between resistance and chemical composition was studied. The laboratory tests of 6 and 8 weeks were carried out with a brown rot fungus Coniophora puteana...
H Viitanen, A M Harju, P Kainulainen, M Venäläinen
The preliminary characterization of ß-1,4-xylanase of the brown-rot fungus Gloeophyllum trabeum
1990 - IRG/WP 1447
The extracellular ß-1,4-xylanase of the brown-rot fungus, Gloeophyllum trabeum, was isolated from crude extract by chromatofocusing method (PBE 94 column chromatography). The isoelectric point was estimated to 4.2-4.8 by cromatofocusing and 4.5 by isoelectric focusing (IEF). The molecular weight of the enzyme was estimated to 37,000 dalton by SDS-PAGE. The optimal temperature for the crude extrac...
A-C Ritschkoff, M Rättö, L Viikari
Documentation on Merulius (Serpula) lacrimans (Wulf.) Fr. according to the "Model Questionnaire for preparation of monographic cards for wood-destroying fungi"
1972 - IRG/WP 108
J Segmüller, O Wälchli
The effect of low molecular weight chelators on iron chelation and free radical generation as studied by ESR measurement
2000 - IRG/WP 00-10367
The focus of this work was to improve our current knowledge of the non-enzymatic mechanisms involved in brown-rot decay. Electron Spin Resonance (ESR), also known as Electron Paramagnetic Resonance (EPR), is an attractive technique for the identification and study of chemical species containing unpaired electrons (such as radicals and certain transition metal species). ESR spin-trapping techniques...
Yuhui Qian, B Goodell
Comparison of the effect of different soil sources on the type and rate of decay of CCA-treated pine exposed in a soil-bed
1984 - IRG/WP 2213
The types of decay observed in CCA-treated pine posts in horticultural situations in New Zealand can be reproduced using a soil-bed exposure. Radiata pine stakelets, untreated or treated to 1.4, 2.7, or 5.4 kg/m³ with Tanalith NCA, were exposed to six different soil sources. The local nursery soil used for all standard laboratory tests was found to represent the greatest decay hazard to untreated...
J A Drysdale
Importance of bacteria in the deterioration of archaeological woods
1995 - IRG/WP 95-10122
An electron microscopic study of archaeological woods from different sites and of different ages revealed that the woods had been attacked by erosion bacteria, tunnelling bacteria and soft rot fungi. Bacterial erosion appeared to be most widespread, and was present independently as well as together with tunnelling and soft rot attacks. Thus, in many instances bacterial erosion was the only type of...
Yoon Soo Kim, A P Singh, T Nilsson
Available iron promotes brown rot of treated wood
1992 - IRG/WP 92-1526
Exposure of treated wood blocks to rusting iron increased the toxic threshold of chromated copper arsenate and ammoniacal copper arsenate to a brown-rot fungus Leucogyrophana sp. This supports the hypothesis that the movement of iron ions into wood contributes to the unexpectedly high decay rate of treated wood at the stake test site at Westham Island BC. To what extent this phenomenon may occur e...
P I Morris
The dry rot and other fungi in houses. Part 4
1995 - IRG/WP 95-10124
J Bech-Andersen
Biological resistance of phenol-resin treated wood
1990 - IRG/WP 3602
Biological resistance of PF (phenol formaldehyde resin) - treated wood has been tested in relation to the resin properties, wood species and biological factors. When tested using water-soluble PF (mol. wt. 170), ca. 10% RI (resin impregnation) was enough to suppress the decay of Japanese cedar (Cryptomeria japonica) and western hemlock (Tsuga heterophylla) blocks exposed to Tyromyces palustris (br...
M Takahashi, Y Imamura
Suppression of aerial hypha formation by spent culture filtrate of a non-degradative strain of Postia placenta
1991 - IRG/WP 1498
ME20, a wild-type monokaryotic strain of the brown-rot fungus Postia placenta, does not cause significant weight losses in standard soil-wood block decay tests and fails to form aerial hyphae in liquid and agar culture. This abnormal morphological feature may be caused by the same aberrant physiology that prevents the strain from degrading wood efficiently. ME20 releases elevated levels of the aut...
J A Micales
Influence of variable lignin content on brown rot decay of wood
1987 - IRG/WP 1320
Compilation of published data and new experiments with brown-rotting fungi on different timber species suggest that their decay activity, in contrast to soft rot and white rot fungi, is not greatly influenced by the type or amount of lignin present....
T Nilsson, G F Daniel
Wood degradation mechanisms by the brown rot fungus Gloeophyllum trabeum
1997 - IRG/WP 97-10229
A mechanism for the degradation of wood by the brown rot fungus Gloeophyllum trabeum is outlined. The mechanism includes the function of redox-cycling, low molecular weight phenolic derivatives which sequester and reduce iron in acidic environments. The role of oxalate for the sequestration of iron (hydr)oxides and the pH dependent transfer of iron to the G. trabeum phenolic chelators, as well as ...
B Goodell, J Jellison
Analysis of degradation observed on ancient wooden objects buried underground
2001 - IRG/WP 01-10403
Ancient wooden objects were sometimes excavated from the moat of mounded tombs in Japan. Such wooden objects were in the shape of a sunshade, bird, shield, pole, yugi(a bag that holds arrows) among others. Archaeologists discussed the usage of such shaped objects, but no one could clearly explain their use. Some objects were observed using an ordinary microscope. Deterioration by bacteria was foun...
H Sakai
Defining fungal decay types - Final proposal
1988 - IRG/WP 1355
The term soft rot is proposed for all forms of decay caused by Ascomycetes and non-basidiomyceteous Fungi imperfecti. The terms brown rot and white rot should be used only for decay caused by Basidiomycetes. Brown rot is characterized by extensive depolymerization of the cellulose and limited lignin degradation. White rot is characterised by significant degradation of the lignin component in wood....
T Nilsson
Decay types observed in small stakes of pine and Alstonia scholaris inserted in different types of unsterile soil
1990 - IRG/WP 1443
The attack of various wood-degrading microorganisms occurring in mini-stakes of pine and Alstonia scholaris buried in various types of unsterile soil was studied. Attacks by white rot, brown rot, soft rot, erosion bacteria, tunnelling bacteria and actinomycetes were found. Soft rot occurred in all soils, whereas attack by white rot and especially brown rot and erosion bacteria was rare. The type o...
T Nilsson, G F Daniel