IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 155 documents. Displaying 25 entries per page.


Cleistanthus collinus (Roxb.) Benth. ex Hook. f. and Wrightia tinctoria (Roxb.) R. Br. -- two timbers with promising durability under marine conditions
2005 - IRG/WP 05-10552
During the course of natural durability studies on indigenous timber at Visakhapatnam harbour, two species, namely, Cleistanthus collinus (Karada) and Wrightia tinctoria (Dudhi) were found to resist marine borer attack for reasonably longer periods. The panels of C. collinus completely resisted borer attack for 9 months but became susceptible to teredinid attack thereafter. The teredinids gradua...
M V Rao, M Balaji, V Kuppusamy, K S Rao


Accelerated anti-termite laboratory tests, simulation of field conditions and assessment of results for service life
1994 - IRG/WP 94-20034
Termites are one of the most serious biodegrading agents in the tropics. Though some species of termites occur in the warmer temperate regions, only a few species can withstand the rigours of colder regions. Testing of termite resistance of material is done either by field tests or by accelerated laboratory tests. Field tests, though realistic to assess service life, are elaborate, take a long tim...
P K Sen-Sarma


Biological resistance of wood-based composites under protected, aboveground conditions
2005 - IRG/WP 05-20312
Five kinds of wood-based composites (density fiberboard=MDF, hardwood plywood=HP, softwood plywood =SP, particleboard=PB and aspen oriented strand board=OSB) were tested for their resistance against subterranean termites and decay under protected aboveground conditions. The exposure method was previously developed for evaluating performance of sill plates (dodai) in Japanese homes. Ten replicates ...
K Tsunoda


Deltamethrin effectiveness against subterranean termite attack on wood under natural conditions
1989 - IRG/WP 1407
On fighting subterranean termites on wood, out of ground contact, the synthetic pyrethroid Deltamethrin shows positive aspects such as its efficiency and low mammalian toxicity. To evaluate its performance in conditions very similar to those in service use, specimens of Pinus sp were treated with solutions of Deltamethrin diluted in "white spirits" at 0.005% (w/w) and 0.01% (w/w) and exposed in a ...
P A Zanotto


Changes in some important mechanical and physical properties of untreated and treated mining timber after exposure to the conditions of a colliery
1996 - IRG/WP 96-20082
Each of salt treated and untreated mining timber (wedge) pairs with 5x15 cm² cross-section and 155 cm length prepared from Scots pine, Bornmüller's fir and oriental beech was cut in the small standard test specimens to determine changes in some important mechanical and physical properties, 13 month after exposure to the conditions of Kozlu Hard Coal Mines in the depth of 52 m. Thus, the...
A Bobat


A new process for in situ polymerization of vinyl monomers in wood to delay boron leaching
1998 - IRG/WP 98-40110
Efforts were accelerated on effective use of boron compounds in wood preservation owing to their environmentally safe characteristics and relatively low costs in addition to their well-known high bioactivity and fire resistant properties. Although having these unique favorable properties, they are readily leachable from treated wood at humid conditions. Therefore, they had limited market for exter...
M K Yalinkilic, W Dwianto, Y Imamura, M Takahashi


Experimental variations in the distribution of CCA preservative in lignin and holocellulose as a function of treating conditions (temperature, concentration, pH, species, and time)
1984 - IRG/WP 3277
The exact distributions between lignin and holocellulose and retentions on wood of copper, chromium and arsenic as a function of various sets of conditions in a 3x3x4x2 factorial experiment in which combinations of three temperatures of treatment, three CCA solution concentrations, four pH's of the initial CCA solution and two timber species, namely Pinus radiata and Eucalyptus grandis, a...
A Pizzi, E Orovan, M Singmin, A Jansen, M C Vogel


Information on a project about the conditions of admissibility of wood-protecting agents in connection with environmental protection in Poland
1974 - IRG/WP 57
Wood-protecting agents are compounds acting toxically on fungi and insects. If handled improperly or carelessly, they may exert an action harmful to health and safety of men. This action is concerning: a) workers employed at the production of wood-protecting agents; b) workers employed at the impregnation, or at the transport and handling of impregnated wood; c) inhabitants of buildings with impre...
J Wazny


The critical timing of inspections for field testing of natural durability
1994 - IRG/WP 94-20018
An overestimation of performance will almost always result if the condition of a specimen is considered to be attained at the precise time that an inspection is carried out. The time at which the condition is actually attained, referred to in this document as the "Condition time", is best considered to be halfway between two successive inspections. The requirement to obtain data that is relevant t...
J D Thornton


Effects of CCA treatment on settlement and growth of barnacles under field conditions
1998 - IRG/WP 98-50116
As part of a field experiment at seven European marine sites evaluating the effects of CCA treatments on non-target marine organisms, panels treated to nominal loadings of 12, 24 and 48 kg/m3 CCA were exposed at marine sites around the coast of Europe. Within two weeks of exposure, a heavy settlement of barnacles took place on the panels exposed intertidally in France. The intensity of settlement ...
S M Cragg, C Brown, R M Albuquerque, R A Eaton, P Goulletquer


Comparative study on the leaching of wood preservatives between natural exposure and accelerating laboratory conditions
1999 - IRG/WP 99-50134
Impregnated specimens with CCA, ACQ, and BAAC were subjected to leaching tests. Specimens of 2x2x1 cm3 in size were used for the laboratory leaching test for 10 days according to JIS K 1571. Specimens of 25x1 x1 cm3 were used for outdoor leaching test for 6 months. Total leaching amounts of boron per cm3 of specimens treated with BAAC were 325 µg in the laboratory test and 206 µg in the outdoor ...
K Yamamoto, S Motegi, A Inai


Research activities on marine wood biodeterioration in Indian waters
1992 - IRG/WP 92-4182
India has a sea coast of about 8,000 km - taking into account all islands in Arabian sea and Bay of Bengal. Considerable quantity of wood is used for jetties, piles, catamarans, coastal and fishing vessels etc. and expenditure made on all these strutures including losses involved due to damage by marine borers is considerable. Continous and rapid depletion of timber from our forests particulary at...
V V Srinivasan


Molecular characterization of M’jej, decaying agent of cedar forests in Morocco
2006 - IRG/WP 06-10593
Cedar wood is well appreciated since thousand years even though its economical importance is limited because of its world distribution restricted to some Mediterranean countries and Himalaya. The most important species, Cedrus atlantica have its biggest population in Morocco (130 000 ha) where it is submitted to fungal diseases. Among them, the locally named “M’jej” reduced notably saw mile ...
A Zaremski, S Bakkali-Yakhlef, C Chaintreuil, Y Abbas, Y Prin, M Abourouh, M Ducousso


EN 152: Is this Standard Relevant for today’s Wood Preservatives? A Critical Review.
2006 - IRG/WP 06-20331
The paper critically reviews the Blue stain test method described in EN 152 including possible test variables. Whereas EN 152 has been successfully used for solvent borne wood preservatives, it appears that the methodology is not suited for modern water borne products, where the majority fail. The paper will show that there exist different quality claims not concordant with EN 599-1 within diff...
B Jensen, F Imsgard, J Larsen


L-joint based testing for service life prediction of exterior plywood in out of ground contact conditions
2006 - IRG/WP 06-20342
Good biological performance of several plywood types in exterior conditions is most probably related to altered wood moisture behaviour compared to solid wood. Therefore a test set up was developed, using EN 330 L-joint testing methodology, to facilitate differentiation of plywood for exterior applications. The proposed test set up is an adaptation of an accelerated L-joint method introduced by V...
J De Smet, I De Windt, J Van Acker


Leaching of CCA from Paraserianthus falcataria panels exposed to field conditions at Krishnapatnam harbour, Andhra Pradesh
2006 - IRG/WP 06-50241
This study assessed the leaching of copper, chrome and arsenic (CCA) from Paraserianthus falcataria (=Albizia falcataria) panels exposed to marine condition at Krishnapatnam harbour on the east coast of India. Metal loss was assessed in test panels after 6, 12, 24 and 36 months of exposure using Atomic Absorption spectrophotometer (AAS). The metal loss was found slightly higher in panels treated ...
B Tarakanadha, K S Rao


Permethrin: A Critical Review of an Effective Wood Preservative Insecticide
2007 - IRG/WP 07-30413
Permethrin is a synthetic pyrethroid used in the wood preservation industry. The generally favorable environmental profile of pyrethroids coupled with their high efficacy led to their wide substitution of the chemically resistant organochlorines dieldrin, lindane, and chlordane formerly used for protection of buildings against wood destroying organisms. Much of the research on performance of perm...
M H Freeman, D N Obanda, T F Shupe


Copper fixation in ACQ-D treated Chinese fir at various temperature and relative humidity conditions
2007 - IRG/WP 07-30436
In this study, the effect of different conditions of temperature, relative humidity, and duration of post-treatments on accelerating copper fixation in ACQ-D treated Chinese fir wood blocks was investigated. The conditions include the combination of three temperatures (21, 50, and 70?) and two relative humidity levels (20% and 80%), also include four temperatures (50, 70, 90, and 110?) without con...
Jinzhen Cao, Lili Yu


Durability of timber from exotic species against termite attack in Indian conditions
2007 - IRG/WP 07-10629
Exotic trees species, Acacia mangium Willd. and A. auriculiformis A. Cunn. ex Benth. and their hybrid are widely grown in India for multiple uses including use as timber. It is essential to know the natural durability of timbers against termites for predicting the service life of the timber and deciding on the application of preservatives to enhance the durability. Studies were conducted to test t...
O K Remadevi, R Muthukrishnan


Development of preservative treatment method using sub and super critical carbon dioxide
2007 - IRG/WP 07-40385
Significant efforts have been devoted for developing biocide impregnation method into wood materials using supercritical fluid. Developing better understandings of fluid phase and its effect on treatment results would facilitate a more rational development of supercritical fluid (SCF) impregnation. In this project, the preservative treatabilities under super- and sub-critical fluid conditions we...
Myeung-Won Cho, Sung-Mo Kang, Gyu-Hyeok Kim


Service Life Prediction of Wood Claddings by in-situ Measurement of Wood Moisture Content: Status after 5 years of Outdoor Exposure
2009 - IRG/WP 09-20401
The Danish Technological Institute is in co-operation with industry partners running a project aiming at predicting the service life of different wood protecting systems. The project focuses on examining the moisture reducing effect of different protecting systems for timber claddings and the ability of these to maintain the appearance of the surfaces, when the wood is used in service class 3 (EN ...
E Tang Engelund, B Lindegaard, N Morsing


Evaluation of exposure conditions for wooden facades and decking
2009 - IRG/WP 09-20408
During their functional life, building components are exposed to moisture and other environment stress conditions in numerous ways. This is a fact that should be taken into account during manufacture, product development, designing and work execution of building components. For wood material, moisture stress and biological factors like mould and decay fungi are often critical in cladding and decki...
H Viitanen, T Toratti, R Peuhkuri, T Ojanen, L Makkonen


Modelling of onset of mould growth for wood exposed to varying climate conditions
2009 - IRG/WP 09-20414
A performance-based service life design format based on climatic exposure on one hand and “resistance” of wood against mould growth on the other hand, is presented in this paper. A limit state for onset of mould growth is defined as the occurrence of traces of mould observed by microscopy. A dose-response model is proposed by which onset of mould growth can be predicted for an arbitrary climat...
S Thelandersson, T Isaksson, A Ekstrand-Tobin, P Johansson


The Relative Performance of an Organic Preservative System under UC3A and UC3B Conditions using Two Test Methods
2010 - IRG/WP 10-20429
Coated L-joints have been used for decades to evaluate the performance of wood preservatives in protected environments. This study was conducted using matched coated and uncoated L-joints to simulate above ground protected and unprotect exposures. When exposed to constant moisture in a greenhouse environment, coated and uncoated L-joints give very similar performance results. In contrast, exposi...
C F Schauwecker, A Zahora, A F Preston


A Review on Conditions for Decay Initiation and Progression
2010 - IRG/WP 10-20444
This paper reviews the key publications available on service life prediction of exterior wood applications, critical conditions for decay initiation and progression, and the impact of decay on wood strength. While it is helpful to use climatic data to predict general trend of decay potential, more precise decay initiation and progression information is required by hygrothermal modeling for its dam...
Jieying Wang, P I Morris


Previous Page | Next Page