Window test. Direct testing of wood resistance to decay: A study of its fitness, its reliability and its accelerating factor
1984 - IRG/WP 2219
This is the results of an experiment using the window-test specimens, exposing the specimens to three different types of testing procedure: 1. Natural infestation in the open air; 2. Artificial infestation and exposure in the open air; 3. Artificial infestation in a green-house. The results show good similiraties of the three parallel tests in term of decay, and assess the reliability of the windo...
G R Y Déon, L N Trong


Influence of variable lignin content amongst hardwoods on soft-rot susceptibility and performance of CCA preservative
1982 - IRG/WP 1151
This paper presents the outline of an argument, based on both new and established data, which relates varying lignin content to variation of soft-rot susceptibility between hardwood species and of performance of CCA preservatives in controlling soft-rot. Although more data need to be generated to prove this relationship, sufficient evidence exists for the hypothesis to be given close attention, pa...
J A Butcher, T Nilsson


Electricity pole treatments - Wedding Bells State Forest. Inspection September 1983
1985 - IRG/WP 3334
A survey to study the extent of soft rot in hardwood poles in N.S.W. was commenced in 1975. The results of the survey, published in 1982, indicated that a number of factors contributed towards soft rot attack on poles in service. A detailed rest on pole treatments and maintenance procedures was established in 1976, at a site in Wedding Bells State Forest near Coffs Harbour. The site selected was k...
R S Johnstone, R H Eldridge


Variations in the virulence of test strains of Coniophora puteana (Schum ex Fr) Karst
1982 - IRG/WP 2185
In laboratory experiments using petri-dishes and small wood blocks (30 x 10 x 5 mm³) 6 different isolates of Coniophora puteana strain BAM 15 were compared with strain FPRL 11E for growth rate and decay capability. Only the recently received strain from EMPA was suitably active giving 24% weight loss after 6 weeks compared with 38.1% for 11E. Collation of data from standard test records revealed ...
A F Bravery, J K Carey, W Worley


Use of compression strength loss for measuring decay in the soil block test
1996 - IRG/WP 96-20083
The possibility of using radial direction compression strength of wood, rather than mass loss, was evaluated for both a brown-rot fungus (Gloeophyllum trabeum) and white-rot fungus (Trametes versicolor). With untreated pine wafers (5 x 19 x 19 mm³ - l x r x t) exposed to Gloeophyllum trabeum in a soil block test for five days, the compression strength loss was nearly 50% compared to a 5% mass los...
D D Nicholas, Zhongwei Jin


The potential application of rapid gas-chromatographic assay of microbial respiration to the monitoring of wood decay in field trial situations
1983 - IRG/WP 2196
Gas chromatographic detection of microbial activity (C02 production) within stakes in a field trial situation would appear to provide a sensitive, non-destructive and relatively rapid method for the quantitative assessment of preservative treatments. Most consistent results were obtained when stakes were removed from the soil, washed, saturated with water and incubated in sealed PVC tubes at 25°C...
M A Line


Stake test with ammoniacal copper in combination with different agents started in 1962
1997 - IRG/WP 97-30130
In 1962 a stake test was started with ammoniacal copper in combination with chromium, arsenic, pentachlorophenol, boron, salicylic acid, benzoic acid, sorbic acid, pyridine and tannin. Different concentrations of the copper component were used as well as the added agents. For each concentration and test site, ten stakes of Pinus sylvestris L. sapwood were treated. The stakes were set out at two te...
B Häger, Ö Bergman


Detection of increased metal cations after wood decay using Chromeazurol-S
1997 - IRG/WP 97-20112
Chromeazurol-S (CAS) is a dye used for the spectrophotometric determination of metals, mainly aluminum (Al), berillium (Be) and copper (Cu). CAS has been widely used for determining the penetration of copper containing preservatives like CCA (AWPA A3-96). Additional uses include: i) detection of utility pole decay (Esyln, 1979), ii) a chemical spot test for aluminum in wood (Kukachka and Miller, 1...
F Green III, U Srinivasan, R B Miller


Reappraisal of some fungicides by the amended JWPA method
1992 - IRG/WP 92-3689
Organoiodine compounds which have been commercialized these years in Japan poorly performed as fungicides in the amended JWPA decay test (Standard 1, 1989) when applied to superficial treatment of timber. Because some parts of active ingredients seemed to disappear from the treated timber surface mainly due to the severe leaching cycles. This was prominently true for beech (Fagus crenata Blume) sa...
K Tsunoda


Effects of the specimen position on fungal colonisation and wood decay by en 113 test fungi
1998 - IRG/WP 98-20136
For testing wood preservatives according to EN 113 it is common practice to plant the test blocks on neutral supports in order to prevent (1) a diffusion of chemicals into the agar medium and (2) an excessive moistening of the specimens. The procedure was employed in EN 350-1 for testing the natural durability of solid wood. It turned out to be of problematic nature because of the individual requ...
G Kleist, M-T Lenz, R-D Peek


Three years of field tests with "Lignomer" stakes in ground contact
1981 - IRG/WP 3166
The "Lignomer" (Wood Polymer Composite) is a material obtained during the polymerisation of various monomers or its mixtures in wood. As laboratory tests have shown, this material is characterized by a high resistance against biological deteriorating agents. The laboratory investigations on the durability of various materials against biological deterioration are in many instances extended by field...
K Lutomski


A comparative analysis of Coniophora olivacea (Fr. ex Pers.) Karst. and Coniophora puteana (Schum. ex Fr.) Karst. test strains
1993 - IRG/WP 93-20004
Investigations were carried out to compare pure cultures of Coniophora olivacea (Fr. ex Pers.) Karst. used as a test fungus in Australia and other Pacific countries, and Coniophora puteana (Shum. ex Fr.) Karst. which is used in Europe. Comparisons included morphology, growth rate and dry mass of mycelium, decay capacity, influence of temperature, toxic value of CCA and quaternary ammonium compound...
J Wazny, L J Cookson


Decay potential of various New Zealand Phlebiopsis gigantea strains using a soil block method
1999 - IRG/WP 99-10309
The objective of the current study was to determine the decay potential of different strains of Phlebiopsis gigantea using Pinus radiata and European Fagus sylvatica, respectively. A soil block method was used to determine mass weight loss of P. radiata and F. sylvatica following 10 weeks incubation with different strains of P. gigantea. For comparison, Trametes versicolor, Postia placenta, Gloeop...
B Kreber, J G Van der Waals


Limitations of the Pilodyn when assessing decay in graveyard test stakes
1982 - IRG/WP 2168
The following examination was designed to evaluate more precisely the usefulness of the Pilodyn for routine, objective assessments of the condition of field test stakes and to examine its limitations, particularly in respect to: 1.) The importance of variables other than extent of decay which may affect Pilodyn readings; 2.) Practicality of obtaining multiple readings in decayed and non-decayed re...
M E Hedley


The movement of iron into field test stakes
1987 - IRG/WP 2284
Failed and sacrificial stakes recovered from the Westham Island field test site were examined for their iron content. Varying amounts were recorded, which were greatest in the failed stakes. The possible role of the iron taken up by the below ground portion of the stakes, in accelerating the decay process and/or the preservative leaching is under investigation. The reaction of the iron with the ch...
J N R Ruddick, P I Morris


The ground proximity decay test method
2000 - IRG/WP 00-20205
A decay field test method, which has been recently proposed for the standardization by the AWPA, is described for evaluating the relative performance of wood samples in a severe above ground situation exposed to the weather. Data is presented on the relative performance of untreated control samples and standard preservative systems exposed at the same site at different time periods, or at differen...
A F Preston, P J Walcheski, K J Archer, A R Zahora, L Jin


Moisture content and other tested values in. Double layer tests of different size in Lithuania and Germany
2004 - IRG/WP 04-20299
The paper presents measurement results of moisture content and the analysis of durability trial of double layer wood in variants of varying size, conducted in Girionys, Kaunas distr., Lithuania and in Hamburg, Germany. In this trial 3 sample sets of varying size, containing 25, 50 and 100 specimens, are used. The aim of this trial is to ascertain an optimal number of test specimens. The dynamics o...
J Saladis, A O Rapp


Resistance of board materials against fungal decay: A comparative experiment on Kolle flask tests method and direct test method
1985 - IRG/WP 2243
Two sets of plywood (Aucoumea klaineana Pierre) 7 and 11 ply, treated by two preservatives, and untreated, were tested by two methods: 1. Kolle flask test method on malt-agar substrate according to the French standard NF B 51.295; 2. A direct test method in non sterile conditions according to DocNo: IRG/WP/2214. The exposure time far both methods was 12 weeks. After exposure, the degree of attack ...
G R Y Déon, L N Trong


Performance of above ground decay test units treated with a substituted isothiazolone
1989 - IRG/WP 3503
RH 287, a substituted isothiazolone, was evaluated for efficacy against decay fungi in an above ground test in Mississippi. After 45 months of exposure, all test units that were pressure treated with this biocide at levels of 0.026 pcf and higher have no deterioration. In addition, the test units that were dip-treated with a solution concentration of 0.5% also have no deterioration. Compared to pe...
D D Nicholas, J A Wilson, D E Greenley


Evaluation of extractives from African Padauk (Pterocarpus soyauxii Taub.) for protection of non decay resistant species
2002 - IRG/WP 02-10419
The development of a wood preservative made up of natural extracts is a potentially attractive prospect for the wood preservation industry. In this study, organic solvents were used to remove extractives from African padauk wood samples. The solvent was removed by rotoevaporation, and the total content of the viscous extracts determined to be 54.4mg/ml. The toxicity of various extracts concentrat...
P Nzokou, D P Kamdem


Laboratory Evaluation of Soft Rot Resistance of Non-Durable Lesser-Known Malaysian Hardwoods
2006 - IRG/WP 06-10582
Resistance of six non-durable lesser-known Malaysian hardwoods, Pulai (Alstonia spp.), Rubberwood (Hevea brasiliensis), Ludai (Sapium spp.), Jelutong (Dyera costulata), Gaham Badak (Blumeodendron tokbrai) and Kayu arang (Diospyros spp.) compared with temperate Scots pine sapwood (Pinus sylvestris), were evaluated using the unsterile soil burial (mixed with Chaetomium globosum) versus vermiculite-b...
A H H Wong


Is Field Test Data from 20 x 20mm Stakes Reliable? Effects of Decay Hazard, Decay Type and Preservative Depletion Hazard
2006 - IRG/WP 06-20327
Effects of decay hazard, decay type and preservative depletion hazard on the performance of variously preservative treated 20 x 20 x 500 mm Radiata pine and Fagus sylvatica test stakes across 13 field test sites in New Zealand and Queensland Australia were determined. Radiata pine treated with an ammoniacal copper quaternary preservative (ACQ) (1.56% m/m a.i.) and copper chrome arsenate (CCA) (...
R Wakeling


Effect of wood decay on the proportional limit of thin wood samples stressed in the bending mode
2006 - IRG/WP 06-20334
When using bending stiffness as a measure of wood decay it is advantageous to repeatedly test individual samples after they are exposed to decay fungi for varying periods of time. In order to obtain reliable results, variation in modulus of elasticity (MOE) values of the test samples that are repeatable bent to a given deflection must be considered. In this study it was shown that sound 3mm thick ...
G Li, D Nicholas, T Schultz


The Use of Modulus of Elasticity and Modulus of Rupture to Assess Wood Decay in Laboratory Soil-Bed Test
2006 - IRG/WP 06-20338
The efficacy of wood preservatives were determined in a soil-bed test. Samples of alder wood sapwood (Alnus glutinosa subsp. barbata) (5x10x100 mm) were treated with Solutions of CCA (1 % and 2 %), ACQ-1900 (2 % and 3 %), ACQ-2200 (1 % and 2 %), Tanalith E 3491 (2 % and 2.8 %), Wolmanit CX-8 (% 1 and 2 %). Modulus of Elasticity, modulus of rupture, mass loss and decay rate according to AWPA E7 wer...
A Temiz, Ü C Yildiz


High-energy multiple impact (HEMI)-test – Part 2: A mechanical test for the detection of fungal decay
2006 - IRG/WP 06-20339
The suitability of the high-energy multiple impact (HEMI)-test for detection of early fungal decay was examined. The HEMI – test characterizes the treatment quality of thermally modified wood by stressing the treated material by thousands of impacts of pounding steel balls. This method differentiates between heat treatment intensities, which are expressed by structural changes of the wood. Simil...