IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 154 documents. Displaying 25 entries per page.


Cytoplasmic and extracellular localization of manganese II dependent peroxidase(s) in white rot fungi during degradation of woody materials
1989 - IRG/WP 1416
The manner by which lignin is degraded in-situ in natural substrates by white rot fungi still remains a controversial issue particularly the distribution and role(s) played by lignin degrading enzymes (i.e. manganese II peroxidase and lignin peroxidase). In the present study, use was made of anti-manganese II peroxidase and immunolabelling techniques in conjunction with transmission electron micro...
G F Daniel, B Pettersson, T Nilsson, J Volc


Evaluation of teak sawdayst Tectona grandis L Fil as a potential source to obtain a natural wood preservative in Colombia
2004 - IRG/WP 04-30356
Plantation Teak (Tectona grandis L. Fil) has been tested as a possible source of natural wood preservatives due to the known excellent durability of old-growth teak wood. Field tests (ground proximity termite and above ground simulated decking exposures) were established in Colombia in April 2003 at two different test sites with different climates (Tropical Dry and Rain forest). Teak heartwood ex...
A Castillo, Y Cabrera, A F Preston, R Morris


Protection of buildings, other structures and materials in ground contact from attack by subterranean termites with a physical barrier - a fine mesh of high grade stainless stee
1993 - IRG/WP 93-10014
A new type of physical barrier for the prevention of attack by subterranean termites on buildings, other structures and materials in ground contact - a fine mesh of highalloy (originally 304, now 316) stainless steel - has recently been developed and patented worldwide by industry in Australia. The termite resistance of the material was assessed by CSIRO in laboratory and field trials. In the labo...
M Lenz, S Runko


Environmental consequences of various materials in utility poles - A life cycle analysis
1992 - IRG/WP 92-3726
A model for environmental life cycle analysis, LCA, has been created to compare environmental impact from transmission poles, made alternatively of concrete, steel, aluminium and pine wood treated with CCA type B or creosote. The main pollution sources and energy use are included in the LCA. One pole size, 12 meters long, is presented in the study, a so called "45 kV" pole. Poles of different mate...
M Erlandsson, K Ödeen, M-L Edlund


Colonization of treated and untreated ponderosa pine exposed in Hilo, Hawaii
1995 - IRG/WP 95-20068
The rate of decay in above ground exposures is largely controlled by rainfall and temperature, factors which can be used to construct a climate index of decay hazard in above ground exposures. Developers of new biocide formulations have utilized this knowledge by establishing test sites in sub-tropical regions such as the Gulf Coast of the United States. More recently, field sites have been locate...
C M Freitag, J J Morrell, K J Archer


Deterioration and preservation of Japanese pampas grass as a roofing material
1991 - IRG/WP 1490
The deterioration and preservation of Japanese pampas grass as a roofing material were investigated. The pith of stem and sheath were more rapidly decomposed. The vessels were the most important pathway of microbial prevalence. Hyphae invaded into the cell wall of fiber and parenchyma, and made the cavities with conical ends. The contacting cell wall of parenchyma in pith with hyphae was decompose...
K Fukuda


Principles behind the laboratory assessment of materials with subterranean termites - Recent perspectives and shifts in emphasis
1986 - IRG/WP 1291
Laboratory assessments of materials against termites aim to give an indication of the likely performance of materials in the field. To meet this objective, test procedures have to provide the conditions that promote the most vigorous activity of the insects. Implications of recent findings on inter- and intracolony variability in vigour, the need to monitor termite activity with differing types of...
M Lenz


The effects of preservative treatment and exposure to wood degrading fungi on fiber reinforced polymer (FRP) materials used for structural wood reinforcement
2001 - IRG/WP 01-40204
Glass fiber reinforced phenolic (GFRP) composite materials are becoming increasingly accepted for use in the construction industry because they combine advantages of both wood and advanced polymeric materials. Addition of only 1-3% FRP in the tension zone, for example, can typically improve the strength of the hybrid system by 200%. As more applications are found for wood/FRP hybrids, (e.g. lamina...
C Tascioglu, B Goodell


Determination of corrosive effect of liquid wood preservatives to metals – First experiences with a National Standard which is in revision
2006 - IRG/WP 06-20321
The development of standards is an essential tool to characterise different kind of materials and products. An important aspect during the development of a new product is to check the corrosion behaviour with other materials. Corrosion can cause several problems like pitting corrosion. Consequently the knowledge concerning the corrosive effect of liquid wood preservatives is important due to the s...
E Melcher


Some fundamental thoughts on the prediction of field performance from lab-testing based on comparison of lab and field test results of some copper-free materials
2003 - IRG/WP 03-20269
In the paper results from lab testing (ENV 807 and EN 113) are compared with field results (EN 252) of differently treated wood. Depending on the type of the organic biocide containing material and depending on type of soil and type of decay differences were found in suitability of the lab methods to predict field performance. The attempt is made to interpret the found differences. Furthermore it ...
A O Rapp, U Augusta


Wood durability in the light of recent trends and research on the durability of building materials and components
2000 - IRG/WP 00-20195
Building-related research of today demonstrates a clear shift in focus from the design and production phases to usage and to the entire life time. A consequence is that the performance criteria of materials, components and of the entire building must be regarded over the life time rather than at the time of production or delivery. As one example can be mentioned the Building Construction Directive...
K Ödeen


Information from the COIPM Wood Group
1988 - IRG/WP 4146
Abstract from the COIPM minutes: Wood in marine environment: Mrs Gambetta stated that the main item discussed by the Group was the collaborative work to test the durability of heat shrinkable polyolephin sheating materials for the protection of wood against marine organisms. The work began last year when wood samples were sent out to the participants. Three samples of Pinus sylvestris wrapped in ...
A Gambetta


Biodetioration and strength reductions in preservative treated aspen waferboard
1983 - IRG/WP 2195
Experimental aspen waferboards, bonded with liquid or powdered phenol formaldehyde resins and treated by various methods with a wide selection of preservatives, were tested for fungal resistance in accelerated laboratory trials. Mold growth on the surface as well as weight and strength losses due to the actions of decay fungi were determined. Testing of board strength after decay in high and moder...
E L Schmidt, H J Hall, R O Gertjejansen, R C De Groot


Inorganic preservative levels in soil under treated wood decks after 8 years natural exposure in Borås, Sweden
2005 - IRG/WP 05-50233
Inorganic preservative components (Cu, Cr and As) were measured to a depth of 150 mm under deck structures made with Scots pine lumber treated with several different wood preservatives and installed in Borås Sweden 8 years ago. Higher contaminant levels were observed mainly under the drip lines and in the top 50 mm of soil. Under CCA treated decks, soil arsenic concentrations increased from ba...
P A Cooper, Y T Ung, M-L Edlund, J Jermer


A field test on susceptibility of wood-based board materials to moulds
1989 - IRG/WP 3545
A field test on susceptibility of wood-based board materials to mould growth was carried out under practical, but severe, service-conditions. A total of 19 commercially available composite boards were investigated. It was found that all board materials tested were not completely immune to mould attack. Test results revealed that among the three main categories of wood-based boards involved, partic...
Qiao Wang, B Henningsson


Surface checking of CCA-treated radiata pine decking timber exposed to natural weathering
2000 - IRG/WP 00-40165
A field trial was established at four locations in Australia to assess the effect of CCA and CCA-wax treatment on the checking (cracking) of radiata pine decking timber exposed to natural weathering. Untreated decking timber and timber that had been pressure treated with water acted as controls. After 1 year's exposure the number and sizes of checks occurring in treated timber and control...
P D Evans, P J Beutel, C F Donnelly, R B Cunningham


Information from the COIPM wood group. (With Appendix: Préserver les matériaux en milieu marin sauvegarder l'environment marin telles sont la vocation et la mission du C.O.I.P.M.)
1989 - IRG/WP 4156
During the last COIPM Meeting, up to date information on cooperative work to test the resistance of plastic wrapping for pilings were submitted and discussed. In 1986 untreated wood samples wrapped with shrinkable polyolefin sleeves were submerged in 9 stations, situated in temperate and tropical waters. After 1 or 2 years of immersion the samples showed no sign of penetration by marine borers and...
A Gambetta


Serpula lacrymans the dry rot fungus. Revue on previous papers
1989 - IRG/WP 1393
It is found that the Dry rot fungus Serpula lacrymans grows in houses only because of its need for basic materials to neutralize the oxalic acid production or heavy metals which celate the oxalic acid. The average distance from the mycelium to the basic materials is found in average to be 14.2 cm with a variation from 0-100 cm. In contrast to Serpula lacrymans the Coniophora puteana and the Rigido...
J Bech-Andersen


Compatibility of deltamethrin with wood-finishing and construction materials
1993 - IRG/WP 93-30010
Under normal use conditions, treated wood comes to close contact with the structural components of a buiLding, and/or receives finishing, forming a new interface, which can affect the performance of a new product such as deltamethrin. To study this possibility, block-tests of Parana-Pine (Araucaria angustifolia), measuring 12 x 24 x 0.5 cm³ (with the largest dimension parallel to the wood-grain),...
E S Lepage


Impact of leachates from CCA- and copper azole-treated pine decking on soil-dwelling invertebrates
2002 - IRG/WP 02-50183
This study assessed the short-term effects on non-target soil invertebrates of leachates from a naturally durable hardwood and timber treated with two copper-based wood preservatives. Natural rainwater leachates from kwila decking, and radiata pine-decking treated with CCA or copper-azole, were collected and applied on mown lawn soil in Brisbane, Queensland. The soil study consisted of 5 treatment...
N Crumière, A House, M J Kennedy


Aquatic toxicity research of structural materials
1998 - IRG/WP 98-50114
Continuing from preliminary results reported on the aquatic toxicity of some tropical hardwoods under high hazard conditions, a more comprehensive research study is set-up in order to assess the environmental toxicology of various structural materials in water applications. Hazard class 4 preservative treated wood is tested for its toxic response on a battery of aquatic test organisms, next to con...
G M F Van Eetvelde, S De Geyter, P Marchal, M Stevens


Preliminary observations of the effect of growth ring orientation on the surface checking of flat sawn Southern pine decking
2005 - IRG/WP 05-20313
Checking in decking timber is a serious defect and methods of reducing its severity are required to ensure that wood can compete with alternative decking materials. The first aim of this research was to test the hypothesis that flat sawn Southern pine decking boards with growth rings oriented concave to the exposed surface will develop less severe checking when exposed outdoors than similarly expo...
K Urban, P D Evans


Leaching of Copper from ACQ treated wood exposed above ground
2004 - IRG/WP 04-50219
The leaching of chemicals of ACQ Type C treated wood exposed above ground for 16 months was studied. Commercially treated Hem-fir boards (Tsuga heterophylla Raf. and Amabilis fir Forb) of 37.5 mm by 87.5 mm were used. The amounts of chemical leached monthly by the rainfall were determined and the leachate was collected and analyzed. Also, the environmental factors influencing the leaching were ...
P A Chung, J N R Ruddick


Relating CCA fixation to leaching of CCA components from treated products
1995 - IRG/WP 95-50045
The relationship between chromium fixation in CCA-C treated wood, as determined by CrVI analysis of solution expressed from treated wood and the leaching of Cu, Cr, As and CrVI in a simulated rain test are evaluated for dimension lumber (2"x6") and pole sections. Leachate concentrations after 2 hour exposure to a misting spray (about 300 mm cumulative rainfall) decrease rapidly with increased degr...
P A Cooper, R MacVicar, Y T Ung


Resistance of board materials against fungal decay: A comparative experiment on Kolle flask tests method and direct test method
1985 - IRG/WP 2243
Two sets of plywood (Aucoumea klaineana Pierre) 7 and 11 ply, treated by two preservatives, and untreated, were tested by two methods: 1. Kolle flask test method on malt-agar substrate according to the French standard NF B 51.295; 2. A direct test method in non sterile conditions according to DocNo: IRG/WP/2214. The exposure time far both methods was 12 weeks. After exposure, the degree of attack ...
G R Y Déon, L N Trong


Previous Page | Next Page