Resistance of board materials against fungal decay: A comparative experiment on Kolle flask tests method and direct test method
1985 - IRG/WP 2243
Two sets of plywood (Aucoumea klaineana Pierre) 7 and 11 ply, treated by two preservatives, and untreated, were tested by two methods: 1. Kolle flask test method on malt-agar substrate according to the French standard NF B 51.295; 2. A direct test method in non sterile conditions according to DocNo: IRG/WP/2214. The exposure time far both methods was 12 weeks. After exposure, the degree of attack ...
G R Y Déon, L N Trong


Preservation of basidiomycete hyphae in ancient waterlogged wood materials
1992 - IRG/WP 92-1536
Studies on waterlogged archaeological wood show that basidiomycete hyphae may persist as long as 800 years. In two pine wood samples with Phellinus pini heartrot, one from the foremast of the ship Vasa and the other from a bulwark constructed in the first part of the 12th century, numerous resin covered hyphae were observed. Hyphae with clamp connections that were associated with brown and white r...
T Nilsson, G F Daniel


Preliminary Observations of the Effect of Kerfing on the Surface Checking and Warping of Flat Sawn Southern Pine Decking
2007 - IRG/WP 07-20360
Checking and warping of decking timber are serious defects and methods of reducing their severity are required to ensure that wooden decking can compete with alternative decking materials. Kerfing is effective at reducing the checking and distortion of square cross-section lumber, and the checking of roundwood. In the past it has also been applied to preservative treated decking boards, however, t...
R Ratu, J Weizenegger, P Evans


Control of Moisture Content in Wood Materials for Mold Growth
2007 - IRG/WP 07-10630
Mold growth on wood materials is a major concern for house owners, as it can cause health and aesthetic problems. Mold fungi, present everywhere, usually appear as black or gray patches on wood surfaces in humid environments, and are common in houses. Like any living organism, molds need food, water, oxygen, and a specific temperature range in order to grow. To avoid mold growth on wood materia...
Dian-Qing Yang


Do insects infest wood packing material with bark following heat-treatment?
2007 - IRG/WP 07-10633
As a result of international trade, many bark- and wood-infesting insects are inadvertently transported in wood packing materials (WPM) such as crating, dunnage, and pallets. WPM is suspected as the likely pathway for most of these borers, although the exact mode of entry into the USA is unknown for all 25 borers. The top 10 countries of origin were, in decreasing order, Italy, Germany, China, Spa...
R A Haack, T R Petrice, P Nzokou, D P Kamdem


Difficulties applying Heat Treatment according to ISPM No. 15, when fast growth species are used
2007 - IRG/WP 07-40386
In 2002, the Interim Commission on Phytosanitary Measures (ICPM) adopted the International Standard for Phytosanitary Measures (ISPM) No. 15 (Guidelines for regulating wood packaging material in international trade). Two treatments are recognized: Heat Treatment (HT), in which wood must be heated to a core temperature of 56°C for 30 minutes, and fumigation with methyl bromide. As the last treatme...
O Encinas, J. I Briceño


Brief introduction of a research project on the wood materials from an ancient Byzantine port unearthed during drilling for underground rail tunnel in Istanbul
2008 - IRG/WP 08-10641
A research project has been recently started to evaluate some properties of wooden materials from the biggest port of ancient times called Port of Theodosius I in Istanbul, Turkey. The ruins of the ancient Byzantine port during the excavations were recently uncovered in the Yenikapi site where an underground rail tunnel construction has been in progress in Istanbul. The wooden objects unearthed fr...
A D Dogu, C Köse, S N Kartal, N Erdin


Water Absorption of Various Building Materials and Mold Growth
2008 - IRG/WP 08-10657
Mold growth is a major problem for house owners, as it often occurs on the surface of building materials in damp houses. The principal method to control mold growth on building materials is to prevent water penetration into the materials. A study was recently conducted to determine water absorption rates of different wood species and panel materials used as building materials, when water intrusi...
Dian-Qing Yang


Development of a Weatherometer to Accelerate the Surface Checking of Wood
2008 - IRG/WP 08-20388
There is significant interest in developing preservatives that are better at preventing wood from checking. Currently, however, there is no accepted test methodology for accelerating the development of checks in wood samples so information on the effectiveness of treatments at restricting checking can be obtained more quickly. This paper describes the development of a new type of weatherometer (Ac...
R Ratu, P D Evans


Alkaline copper treated wood for use in residential decking
2008 - IRG/WP 08-30490
Alkaline copper quaternary ammonium compound (ACQ) treated decking was exposed in a field experiment and the mobile copper assessed based on that collected in the leachate. The amount of copper which leached was modeled after 4 years. The results showed that boards which leached most chemical initially provided the greatest loss over four years. The reduction in the mobility of copper with time wa...
J N R Ruddick


Evaluation of exposure conditions for wooden facades and decking
2009 - IRG/WP 09-20408
During their functional life, building components are exposed to moisture and other environment stress conditions in numerous ways. This is a fact that should be taken into account during manufacture, product development, designing and work execution of building components. For wood material, moisture stress and biological factors like mould and decay fungi are often critical in cladding and decki...
H Viitanen, T Toratti, R Peuhkuri, T Ojanen, L Makkonen


Leaching of the copper component from full scale decking boards during one summer season
2009 - IRG/WP 09-50260
The leaching of copper has been tested in laboratory and in outside exposure for freshly treated pine sapwood samples with three different copper preservatives, Cu HDO, copper quat and copper triazoles. We found in the laboratory leaching test that a fixation with warming to 60 °C (140 °F) for 48 hours without drying and then drying in the laboratory in room temperature gave the lowest leaching of copper. We also found that surface treatments with wood oils reduced the leaching, and that washing of the surface before testing had no effect. Full scale decking board samples (0.25 m2) were then exposed outdoors for rain. The rain water was collected and analysed for copper. After one summer season (about 600 mm rain) we found that the leaching differ for the three preservatives. All samples with a water borne surface treatment had the lowest leaching, about half the amount of untreated.
F G Evans


Barefoot-heat-impact of oil-heat-treated wood: An important thermal property of decking boards
2009 - IRG/WP 09-40458
In this study the phenomenon of sensual heat impression was examined, when walking with bare feet on sun exposed wood based decking boards. A suitable method for measuring the heat flux from decking boards into an artificial foot was developed. The method and measuring device is described as well as results from measuring three different decking board materials: Oil-heat-treated spruce (OHT), untr...
A O Rapp, C R Welzbacher, C Brischke


Eco-Friendly Composites from Bagasse and Soy-based Resin
2009 - IRG/WP 09-40462
In this study, bagasse and soy-based resin were used for producing composite materials. The objective of this study was evaluation of some physical and mechanical properties of boards made of various ratios (100:0, 60:40, 40:60 and 0:100) of bagasse to wood fiber mixtures (wt: wt) with addition of Soy/PF resin at three levels (4, 8 and 10%) and 1.5% wax. All properties were tested according to AST...
G Rassam, B Jamnani


A fast and economic method to produce grey wooden surfaces for decking and cladding: preliminary results
2009 - IRG/WP 09-40474
Uncoated wood is commonly used in France for cladding and decking to minimise maintenance. However wood surfaces progressively turn grey due to exposure to sunlight and water. This grey colour develops after several months depending on the wood species and the exposure: in the northern hemisphere surfaces facing south and west are most exposed and turn grey more rapidly than those facing north and...
L Podgorski, V Georges, I Garmendia, B Sánchez Sarachu


Service life prediction of wooden components – Part 2: Impact of material, exposure and design details
2010 - IRG/WP 10-20440
Dose-response functions permit to estimate the moisture and temperature induced decay potential for any wooden building component and exposure, and thus the service life to be expected. In part 1 of this series dose-response functions were established as a result of double layer field trials carried out at 24 European test sites over up to eight years. Using them makes it no longer necessary to co...
C Brischke, B Lauenstein, M Bilstein, T Bornemann, A O Rapp


Drying Rates and Mold Growth on Various Building Materials under Different Environmental Conditions
2010 - IRG/WP 10-20454
Mold growth on building materials is a major problem for homeowners. The most suitable method to control mold growth on building materials is to utilize design features, construction tools and practices that prevent moisture accumulation, and keep the wood as dry as possible. In order to achieve this, engineers and homebuilders have to know the effects of various temperature and moisture conditi...
Dian-Qing Yang


Mould growth on wood-based materials – a comparative study
2010 - IRG/WP 10-20455
Ten different wood-based materials - preservative-treated wood, fire retardant-treated wood, modified wood, WPCs and untreated references of pine sapwood and spruce - were tested for mould growth according to SP method 2899 during 42 days at 90% RH and 22°C. Even though the results must be interpreted carefully, they indicate significant differences in mould resistance between the materials tes...
P Johansson, J Jermer


Extruded wood plastic composites based on ACQ and MCQ-treated wood materials
2010 - IRG/WP 10-40495
This paper deals with wood plastic composites manufactured using ACQ and MCQ-treated wood fibers recovered from a wood treatment plant. The goal was to investigate the effect of coupling treatments on the properties of manufactured wood plastic composites (WPCs) through injection molding and to manufacture co-extruded WPC with treated wood fibers. The result demonstrated sound mechanical propertie...
Qinglin Wu, Fei Yao, K Ragon, J Curole, M Voitier, T Shupe


Copper distribution in soil leached from full scale decking boards during one year
2010 - IRG/WP 10-50265
The distribution of copper in the soil under exposed decking boards after one year has been analysed. The decking boards were impregnated with copper HDO, copper quat and copper triazoles. The decking boards were pine sapwood and pressure treated in a full cell process, fixed by heating and then dried. The samples were not surface treated. Each decking sample of five boards (0.25 m2) was placed on...
F G Evans


Determination of Equilibrium Moisture Content (EMC) of wood in the neighboring Countries of Iran
2011 - IRG/WP 10-40540
The mean value of annual temperature and relative humidity of 33 cities in Azerbaijan, Armenia, Turkmenistan, Afghanistan, Pakistan, Oman, United Arab Emirates, Bahrain, Qatar, Kuwait, Iraq and Turkey were determined using climatic data of the past 11 years. The EMC values were calculated using the Hailwood-Horrobin sorption model and its annual fluctuation, together with Temperature and relati...
A A Enayati, H Z Hosseinabadi


Classification of wood materials using Fourier Transform Near Infrared Spectroscopy and multivariate analysis
2011 - IRG/WP 11-20471
A distinction between preservative-treated wood and non-treated wood can be demonstrated by the combination of Fourier Transform-Near Infrared Spectroscopy (FT-NIRS) and Multivariate Analysis (MVA). This technique is non-destructive, quick, easy to use and can be portable. The calibration models for different heavy metals are set up using principal component analysis (PCA) to classify species of t...
M A Bouslamti, M A Irle, C Belloncle, V Salvador, S Hulot, B Caron, E M Qannan


Comparison of rates of wood decay from four different field test protocols following 4-5 years exposure at a site in New Zealand
2011 - IRG/WP 11-30565
The rate of decay of Pinus radiata was evaluated using four different field test protocols at a site near New Plymouth, New Zealand. The average Scheffer index was 86 over the five year period of testing. The field tests were an in-ground stake test (AWPA Std E7-01) and three above ground tests – lap-joint (AWPA Std E16-98), decking (AWPC protocol) and ground proximity tests (AWPA Std E18-06) T...
P Lobb, K Day, A Siraa


The Effectiveness of Machined Profiles at Reducing the Checking of Wooden Decking
2011 - IRG/WP 11-40541
This study tests the hypothesis that ‘the ability of surface profiling to reduce checking of deck boards exposed to weathering will vary with wood species and profile type’. Southern pine (Pinus sp.) and Pacific silver fir (Abies amabilis) deck boards were machined to produce three different types of surface profiles: flat (control), ribbed (V-shaped grooves), and rippled (U-shaped grooves). B...
P Evans, I Cullis, P Morris


Thermally modified timber (TMT) for decking applications – determination of relevant surface properties
2011 - IRG/WP 11-40544
In recent years thermally modified timber (TMT) entered various market segments. It is used for facades, horticultural equipment, garden furniture, and also for kitchen and bathroom cabinets. However, flooring turned out to be the most important application for TMT, either as interior parquet or as exterior decking. Besides durability and dimensional stability, which had been the initial target pr...
L Meyer, C Brischke, C R Welzbacher