IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 986 documents. Displaying 25 entries per page.


Laboratory Studies on Copper Availability in Wood Treated with Soluble Amine Copper and Micronized Copper Systems
2008 - IRG/WP 08-30489
A laboratory method has been employed to investigate the level of soluble copper in wood treated with various copper-based preservative systems, such as micronized copper (particulate copper) and amine copper solutions. This report describes the methodology and preliminary results on determination of the soluble copper in the treating solutions and the treated wood by these systems, as well as th...
L Jin, P Walcheski, A Preston


Rehabilitación del Portón del templo parroquial de San Juan Vicario de Comanja, Michoacán, México
2008 - IRG/WP 08-40431
The pine gate of the San Juan Vicario parochial temple in the city of Comanja, Michoacan, Mexico was rehabilitated. The gate was damaged by termites, worms, fungi and weathering. Gate metallic bearings were rusted. The lower parts of the gate were the most deteriorated. For rehabilitation, galvanized steel bearings were designed and manufactured and then implemented into the building. Replacement ...
J Reséndiz Sánchez, J Cruz de León


Field Stake Performance of Parallel Strand Lumber Treated with Waterborne Copper Naphthenate
2008 - IRG/WP 08-40435
Wood and wood products have been considered a premium building material for residential and industrial structures for many centuries. More recently, structural composite lumber (SCL) products have played an increasing role in satisfying the needs of the building industry. However, both wood and wood composites are naturally biodegradable materials which require enhanced durability when used in ce...
G P Merrick, M H Freeman, J A Brient


Corrosion of fastener and connector in contact with alkaline copper treated wood – it is a problem
2008 - IRG/WP 08-40437
For many decades, chromated copper arsenate (CCA) was the most common wood preservative used in North America for residential and industrial applications. Since December 31, 2003, the use of CCA for residential application was voluntarily terminated. One of the most widely accepted alternative wood preservatives in Western Canada is Alkaline Copper Quaternary Compound (ACQ). This paper will compar...
J N R Ruddick


Comparison of laboratory and natural exposure leaching of copper from wood treated with three wood preservatives
2008 - IRG/WP 08-50258
Standard and non-standard laboratory and field leaching tests were used to compare copper leaching from wood treated to above ground and ground contact specified retentions for three wood preservative systems, CCA-C, ACQ-D and a micronized copper formulation with quat DDAC as co-biocide. Copper leaching was highest for the ACQ formulation. Percent leaching was lowest for the micronized copper sy...
P A Cooper, Y T Ung


Wood decay fungi from New Zealand ‘leaky’ buildings: PCR identification and laboratory decay tests of wood preservative-treated Pinus radiata (Part 1)
2007 - IRG/WP 07-10620
Fungi colonising Pinus radiata D. Don framing timber of ‘leaky’ New Zealand buildings were isolated to produce pure cultures. Mycelia from these cultures on agar media were collected to extract DNA. To identify the fungi to the species level, polymerase chain reaction (PCR) with primer pairs ITS1-F and ITS4 were performed followed by sequencing of the internal transcribed spacer (ITS) region. ...
D Stahlhut, R L Farrell, R Wakeling, M Hedley


Detecting fungal DNA in treated and non-treated wood
2007 - IRG/WP 07-10621
Isolating fungi from wood has long involved culturing on selective media followed by identification using various keys. This process can be cumbersome, costly, and, most importantly, not always capable of detecting all of the fungi present. The recent development of molecular methods for isolation and identification of fungi has created tremendous opportunities for expanding our knowledge of the...
C Freitag, M Freitag, J Morrell


Comparison of laboratory termite test methods
2007 - IRG/WP 07-20365
Seven standardized laboratory tests with termites were evaluated. The bioassays were made in accordance with EN 117, SAA32 E08, SAA32 E09, Ebw 02, the American Wood-Preservers’ Association (AWPA) Standard E1-97, the Japan Wood Preserving Association (JWPA) Standard 11 (1) and The Protocols for Assessment of Wood Preservatives. Two different wood preservatives each in three concentrations and add...
H-U Kruschinski, W Unger, A F Preston


Corrosion of metal fasteners in contact with copper preservative treated wood
2007 - IRG/WP 07-20370
The corrosion rates of metal fasteners in contact with alkaline copper quat (ACQ) treated wood with or without commercially available water repellent was compared to that of cedar. In this experiment, fasteners were sandwiched between two pieces of treated wood and exposed to a humid environment at a slightly elevated temperature. The use of a “sandwich” design allowed periodic examination of ...
BaekYong Choi, J N R Ruddick


Use of the Digital Refractometer for the On-site Analysis of Copper-based Preservative Systems
2007 - IRG/WP 07-20371
In some counties, there are no on-site chemical analysis methods available for treatment plants to use to determine the key active ingredients in the preservative treatment solutions. The complexity of the sophisticated methodology; cost of analytical instruments and training required for operating these instruments in treating plant level are the reasons for lacking such practice. In this paper...
L Jin, T Cashman, A Preston, J Trompetter, H Trompetter


Some textile auxiliaries as wood protective agents
2007 - IRG/WP 07-30417
This study evaluated some textile auxiliaries applicable for wood protection. Commercial alkoxysilane quarternary ammonium formulation and fluorocarbon based water-oil repellent were tested for their ability to provide hydrophobicity and antifungal effect to solid wood samples. Scots pine (Pinus sylvestris L.) sapwood samples were impregnated with 25, 50 and 100 % concentrations of the above menti...
E Dizman, A Temiz, N Terziev, Ü C Yildiz


Silver – The Next Generation Wood Preservative
2007 - IRG/WP 07-30419
The successful introduction and commercial use of products designed to have controlled release of silver ion over long time periods prompted the Silver Research Consortium and the US Forest Products Laboratory to undertake research to see if silver could also be an effective wood preservative to be used in place of chromated copper arsenate (CCA) now prohibited for use in the United States and els...
J R Ellis, K Jayachandran, D Nicholas


Preservative treatment of Golla cane (Daemonorops jenkinsiana) by pressure process
2007 - IRG/WP 07-40379
The feasibility of preservative treatment of golla cane (Daemonorops jenkinsiana (Griff) Mart). by pressure process has been studied using water borne preservatives CCB (copper-chrome-boron). Cane samples of three different lengths 1m, 2m and 3 m. were treated at different pressure and time period to evaluate the extent of penetration and retention of preservative chemicals. It was observed that t...
K Akhter, M Hoque Chowdhury


Reduction of Environmental Toxicity Through Eco-friendly Wood Biopreservative
2007 - IRG/WP 07-50243
Many chemicals are used today to enhance the durability of wood and wood-derived products that are very important in our life. Such chemicals are copper, chromium, arsenate, zinc, etc. Though these preservatives are useful to protect wood from biodeterioration, but environmental toxicity is also related with them. The present study is to investigate the fungitoxic activities of Dalbergia sissoo le...
A Humayan Kabir, M Firoz Alam


Influence of ethanolamine on lignin depolymerization and copper leaching from treated Norway spruce and beech wood
2007 - IRG/WP 07-30423
Copper-ethanolamine based wood preservatives are replacing several classical copper-chromium based solutions, due to foreseen ban of chromium. Fixation of copper-ethanolamine based wood preservatives is not as good as fixation of copper-chromium ones. The main object of this manuscript was to prove, that ethanolamine is the prime reason for insufficient fixation of copper-ethanolamine formulations...
M Humar, B Bucar, M Zupancic, D Žlindra, F Pohleven


Laboratory test of blue stain control by chemicals
2007 - IRG/WP 07-30430
8 chemicals and some mixtures against Botryodiplodia theobromae Pat., Fusarium verticillioides(Sacc.)Nirenberg, Trichoderma harzianum Rifai, Trichoderma viride Pers., and Penicillium purpurogenum Stoll were conducted in laboratory by inhibition zone in the paper. The results were shown that: CBZ and benomyl as well as copper oxine alone are much high efficacy for inhibiting most of the 5 fungi tha...
Zhijuan Wang, Zehui Jiang, Mingliang Jiang, Chungen Piao


Copper fixation in ACQ-D treated Chinese fir at various temperature and relative humidity conditions
2007 - IRG/WP 07-30436
In this study, the effect of different conditions of temperature, relative humidity, and duration of post-treatments on accelerating copper fixation in ACQ-D treated Chinese fir wood blocks was investigated. The conditions include the combination of three temperatures (21, 50, and 70?) and two relative humidity levels (20% and 80%), also include four temperatures (50, 70, 90, and 110?) without con...
Jinzhen Cao, Lili Yu


Micro-Distribution of Metals in Wood Treated with a Nano-Copper Wood Preservative
2007 - IRG/WP 07-40360
The microdistribution of copper in southern pine treated with a newly-developed nano-copper wood preservative was examined to determine if it differed from that reported for wood treated with conventional copper-based wood preservatives. Field Emission Scanning Electron Microscopy (FE-SEM) in combination with x-ray microanalysis (EDX) revealed the presence of nano-sized copper and iron particles i...
H Matsunaga, M Kiguchi, P Evans


Effects of sodium hypochlorite on compression strength and copper retention of spruce wood treated with copper azole and alkaline copper quat
2007 - IRG/WP 07-40362
This work investigates the effects of sodium hypochlorite on compression strength values and copper retention ratios of refractory spruce wood (Picea oriental L.) treated with the waterborne preservative Copper Azole, (CBA-A, Tanalith-E 3492) and alkaline copper quat (ACQ-2200). Before the copper azole and alkaline copper quat treatment, the samples were immersed in 500 ml of sodium hypochlorite s...
S Yildiz, E Dizman, A Temiz, Ü C Yildiz


The influence of different creosote process parameters on penetration, retention and bleeding on glulam
2007 - IRG/WP 07-40368
Different process parameters were used to treat Scots Pine glulam beams with creosote. Parameters like pre-heating, pre-pressure time, pressure and pressure time were changed. Most treatments gave a full or almost full penetration of creosote into the sapwood, but the uptake of creosote in the sapwood varies. All samples, except the one with poor penetration, showed heavily bleeding of creosote ...
F G Evans


Effect of barriers on moisture content of treated and non-treated utility poles
2007 - IRG/WP 07-40369
The potential for non-biocidal barriers to slow moisture sorption was investigated using butt treated western redcedar poles immersed in either water or moist soil over a 2 year period. Moisture sorption was initially slowed by the barriers, but openings at the bottoms of the barriers eventually allowed moisture to migrate upward. Moisture levels in wrapped poles eventually reached those found in...
C S Love, J J Morrell


The Role of Moisture Content in Above-ground Leaching
2007 - IRG/WP 07-50245
This paper reviews previous reports on the moisture content of wood exposed above ground and compares those values to moisture contents obtained using simulated rainfall and immersion methods. Laboratory leaching trials with CCA-treated specimens were also conducted and the results compared to published values for leaching of CCA-treated specimens exposed above ground outdoors. Previous researcher...
S Lebow, P Lebow


The effect of additives on copper losses from alkaline copper treated wood
2007 - IRG/WP 07-50246
The replacement of chromated copper arsenate (CCA) by alkaline copper compounds has heightened awareness of the potential impact of copper losses on aquatic organisms. While there remains a healthy debate concerning the actual risk of copper leaching from wood preservatives into aquatic ecosystems, it is clear that reducing these losses will be necessary to avoid continued regulatory actions aga...
J Mitsuhashi, J J Morrell, L Jin, A F Preston


Durability of timber from exotic species against termite attack in Indian conditions
2007 - IRG/WP 07-10629
Exotic trees species, Acacia mangium Willd. and A. auriculiformis A. Cunn. ex Benth. and their hybrid are widely grown in India for multiple uses including use as timber. It is essential to know the natural durability of timbers against termites for predicting the service life of the timber and deciding on the application of preservatives to enhance the durability. Studies were conducted to test t...
O K Remadevi, R Muthukrishnan


Evaluating the Process of ACQ-Treated Woods with TGAand CEM Analysis
2007 - IRG/WP 07-20374
To provide an understanding of the fundamental thermal behaviour and the disposal-end products of ACQ-treated woods, this study is comprised of two categories of examination. The first is related to the use of TGA under different thermal decomposition conditions (nitrogen or air, and 5 or 40 oC/min), and the use of EDX to examine certain residual elements of the char. The second applies the CEM ...
Han Chien Lin, Tsang-Chyi Shiah, Jung Ting Tsai


Previous Page | Next Page