Microscopic analysis of southern pine utility pole core segments
1992 - IRG/WP 92-1542
Fifteen macroscopic core descriptive categories were evaluated by microscopic analysis for accuracy in detecting decay and judging decay severity. Five categories were good indicators of decay as decay was detected in 28 of 48 samples. Five categories were possible indicators of early decay as decay was detected in 6 of 40 core segments and an additional 18 contained hyphae. The remaining five cat...
S E Anagnost, C J K Wang, M Wright


Effect of humidity fluctuations on mould growth on pine wood
1989 - IRG/WP 1412
Most studies on mould development on wood material have been made at constant moisture conditions during the experimental period. As a consequence of such studies, a maximum permittable humidity level to avoid mould problems in wood constructions has been recommended. In the practical situation, the constructions are seldom subject to constant humidity or temperature. In the present paper, we repo...
J Bjurman


Colonisation and detection of New Zealand sapstain fungi
2000 - IRG/WP 00-10329
Sapstain is the bluish black discolouration in logs and timber caused in New Zealand by Sphaeropsis sapinea (Diploida pinea) and more than twenty different species of the Ophiostomataceae Family. Laboratory and field trials were conducted by inoculating radiata pine to establish staining colour and extent of colonisation with various New Zealand sapstaining fungal species. Colonisation patterns, c...
J M Thwaites, R L Farrell


Controlled envelope treatments of Pinus sapwood, achieved by modifications to impregnation process and carrier solvents
2003 - IRG/WP 03-40258
Specimens of slash pine or radiata pine were treated to a target retention of 0.02% m/m permethrin with conventional light organic solvent fluids or with oil-modified fluids (Tanalith® T). Best achievable envelopes from LOSP fluids were poorly controlled, penetrating not only the target outer 0-5 mm zone (mean 0.019%, RSD 28%), but also breaking through into the 5-10 mm zone (mean 0.013%, RSD 37%...
M J Kennedy, P R S Cobham


A field test with anti-stain chemicals on sawn pine timber in Brazil
1989 - IRG/WP 3513
Field tests were carried out in São Paulo State - Brazil, to evaluate pre-treatment formulations of O-Phenyl-Phenol (OPP) based products. The Sodium Pentachlorophenate solution was used as a reference formulation. The treated test blocks were stacked in a covered shed, and in an uncovered place for air drying. The evaluation was done by measuring the percentage of stained surface on each test blo...
M B B Monteiro, S Brazolin


Reduction of kiln brown stain in radiata pine lumber after log fumigation with methyl bromide
1997 - IRG/WP 97-30129
Methyl bromide fumigation of freshly felled radiata pine log sections effectively killed living cells in parenchyma to at least 75mm into sapwood. Lumber cut from logs (fumigated and control) stored 1 month outdoors (dry) showed slightly reduced brown stain when kiln dried at conventional temperatures. A more dramatic reduction and elimination of brown stain was noted in lumber cut from fumigated ...
E Schmidt, M E Hedley, D R Page, D Cross


Variable tolerance of Ophiostoma spp. and Diplodia pinea to commercial antisapstain products
1998 - IRG/WP 98-10266
A recent survey of the occurrence of sapstain fungi in New Zealand, conducted at The University of Waikato, provided the opportunity to examine fungicidal tolerance amongst new isolates. It also enabled a comparison of tolerance amongst new isolates with those used in routine antisapstain screening trials at Forest Research. A rapid antisapstain laboratory disc trial was used to determine the ext...
D R Eden, C M Chittenden, B Kreber, J G Van der Waals, R N Wakeling, R L Farrell, T Harrington


Determination of the amine to copper ratio remaining in wood after leaching
2002 - IRG/WP 02-30285
The effectiveness of the protection and the environmental impact of the treated wood are two of the most important aspects that need to be understood for all preservatives. Both are particularly influenced by the loss of biocidal components from treated wood. For amine copper preservatives, copper fixation determines the leaching resistance of the copper and amine compounds formed in wood. Previou...
N Lucas, J N R Ruddick


Potential for using dip/supercritical fluid treatments for wood impregnation
2004 - IRG/WP 04-40276
While supercritical fluid impregnation offers tremendous potential for impregnating wood species that resist conventional liquid preservative treatments, the resulting treatments are often not uniform among samples in a charge or between charges. One factor that influences treatment is the dynamic change in pressure that occurs during introduction of the biocide laden supercritical fluid into the ...
Sung-Mo Kang, J J Morrell


Effect of origin and orientation of Radiata pine substrates on the development of fungal degrade
2000 - IRG/WP 00-30221
The objective of this study was to determine the influence of different radiata pine substrates on colonisation by sapstain fungi. Freshly-cut branch wood, stem wood and sawn lumber were used to prepare test samples with the largest wood surface area showing a transverse, radial or tangential face. Test samples were evaluated against sapstain fungi using a rapid laboratory antisapstain screening m...
B Kreber, D R Eden, C M Chittenden, B Carpenter, J G Van der Waals


Pretreatment decay in air-seasoning Scots and Corsican pine poles in England
1989 - IRG/WP 1390
British grown Scots and Corsican pine poles were sampled for colonization by basidiomycetes after air-seasoning for 6 to 9, or 16 to 20 months. The amount of infection present in these poles was compared with that in poles which were imported from Finland. After 6 to 9 months seasoning, the British grown pine poles were heavily infected with Peniophora gigantea, Cylindrobasidium evolvens, Stereum ...
A R Zahora, D J Dickinson


The efficacy of polymer/preservative treatments in soil-bed exposure
1992 - IRG/WP 92-3729
Southern pine was treated with CCA, CCB, sodium borax/boric acid, or disodiumoctaborate, alone or in combination with an acrylic polymer system containing a water repellent. Treated samples were subjected to an unsterile soil burial test. The addition of polymer reduced the weight loss in borontreated samples at the lower retentions but not at the higher retention. Results with borates indicate th...
R J Murphy, H M Barnes, S M Gray


The effect of of sorbitol on the decay of boric acid treated Scots pine
1991 - IRG/WP 1509
The tetra-hydroxy borate ion is known to undergo complexation with polyols of biological importance and probably protects treated timber by this action. The inhibitory effect of boric acid upon fungal growth and dehydrogenases has been shown to be prevented by the addition of certain polyols. This work was extended, with a study of the effects of a polyol on the performance of boric acid in treate...
J D Lloyd, D J Dickinson, R J Murphy


Sentry®), a new antisapstain formulation for protecting logs and lumber. - Part 1: advances in protection of New Zealand radiata pine logs
1999 - IRG/WP 99-30188
Until recently antisapstain formulations gave approximately 10 weeks protection to radiata pine logs and even within this time frame protection was often not consistent. Industry requires 20 weeks protection. The degree of protection sought by industry is in the order of 90-95%. For example, this equates to a maximum of 5 - 10% surface cover of sapstain in the first whole veneer produced from a pe...
R N Wakeling, D R Eden, C M Chittenden, J G Van der Waals, B Carpenter, I Dorset, R Kuluz, J Wakeman, T Price, B Nairn


Inhibitory effects of leachates from Scots pine wood on germination of some wood rotting fungi
1986 - IRG/WP 1282
Leachates from sapwood of Pinus sylvestris inhibited or reduced the germination of basidiospores of the wood decay fungi tested. The fungi were selected among those preferentially colonizing hardwood or softwood, representatives for brown rot and white rot fungi, early basidiomycete colonizers and late basidiomycete colonizers in above-ground parts of pine as well as fungi found in high frequencie...
J Bjurman


Mould growth at lumber surfaces of pine after kiln and air drying
1994 - IRG/WP 94-40033
Distribution of water soluble substances in green wood and later redistribution during drying is of importance for the colonisation of wood by microorganisms. According to literature the availability of nitrogenous materials is probably a major limiting factor to the microbial colonisation of wood. King et al. (1974) and Oxley et al. (1976) have shown correlation between surface nutrient concentra...
N Terziev, J Bjurman, J B Boutelje


New principles for the protection of wood: Impregnation with waterborne resins
1995 - IRG/WP 95-40047
The environmental impact of classical wood preservatives as well as the use of tropical wood species with high natural durability is regarded increasingly critically in the public. Therefore other partially new principles for the protection of wood, like chemical modification, or treatment with resins were examined especially in USA, Japan and in Europe with promising results predominantly in the ...
A O Rapp, R-D Peek


Natural durability of larch heartwood against decay
1997 - IRG/WP 97-10201
Larch heartwood has been promoted in Sweden and in other European countries as an alternative to preservative treated timber. It has even beeen stated that larch heartwood is more durable than preservative treated timber. This paper presents a compilation of facts from scientific reports on the durability of larch heartwood. Some recent data from this department are also reported. All data suggest...
T Nilsson


Solid state NMR study on pine wood degraded by brown rot fungus Gloeophyllum trabeum
1994 - IRG/WP 94-10067
Blocks of Pinus koraiensis wood were degraded by Gloeophyllum trabeum and examined by solid-state 13C NMR spectroscopy. Chemical compositions were estimated from relative signal aras. There was no evidence for preferential degradation of the noncrystalline cellulose which accounted for about 4% by weight of the wood. Loss of partly ordered cellulose on crystal surfaces exceeded the loss of crystal...
Yoon Soo Kim, R Newman


Sediment toxicity study of marine piles treated with CCA-C
1995 - IRG/WP 95-50040-35
A study was undertaken to demonstrate the effects of 10-day exposure to sediments mixed with leachate from chromated copper arsenate Type-C (CCA-C) southern pine marine piles treated to a retention of 40 kg/m³ (2.5 pcf) and untreated southern pine piles on the benthic amphipod, Ampelisca abdita. The biological endpoint used to establish effects was organism survival. Leachate obtained during a 28...
W J Baldwin, E A Pasek, P D Osborne


Field studies investigating the efficacy of biological treatments in preventing decay of freshly-felled pine
1993 - IRG/WP 93-10022
Four species of fungi (Trichoderma viride, Ascocoryne sarcoides, Potebniamyces conifererum and Cryptosporiopsis terraconensis) and sterile distilled water were applied separately to unpeeled, freshly-felled pine billets. The fungi were all in the form of concentrated aqueous spore suspensions, and were spread onto the end-grains of the logs by brush. Destructive sampling of the billets was carried...
M W Schoeman, D J Dickinson


Oxidation of wood components during CCA-C fixation
1993 - IRG/WP 93-30024
Pre-extracted radial sections of southern yellow pine sapwood were treated with CCA-C and analyzed by X-ray photoelectron spectroscopy (XPS). The ratio of C1 (carbon bonded to carbon and/or hydrogen) to C2 (carbon bonded to one oxygen) in XPS Cls spectra was taken as a measure of the progress of oxidation of wood components during CCA fixation. This ratio was 0.82 before CCA treatment and increase...
M Kaldas, P A Cooper


Molecular phylogeny of Ophiostoma spp. related to blue-stain in pine
2002 - IRG/WP 02-10432
Blue-stain in coniferous woods is an economically important disease in many temperate countries, caused specially by genus Ophiostoma. Classical taxonomy of genus Ophiostoma is limited for the correct identification of many species, because of the similar macroscopic and microscopic characters, as well as the existence of some species complex. Molecular identification is a good complement to eluci...
M Villarreal, F Arenal, J Sánchez-Ballesteros, M T De Troya, F Llinares, V Rubio, A Navarrete


Protection of rubberwood timber. Part 1: Impregnation with boron preservatives
1989 - IRG/WP 3551
Rubberwood (Hevea brasiliensis) were treated with a 3% proprietary mixture of borax/boric acid using three different treatment schedules i.e. full-cell, full-cell to refusal and full-cell with 12 cycles of vacuum/pressure. Freshly cut samples had mean preservative retentions of 187 kg/m³, 214 kg/m³ and 178 kg/m³ respectively. Pre-air dried samples for one week had retentions of 252 kg/m³, 308 ...
L T Hong, C C K Liew


Impregnation of timber and regulations applied to preservation practice in Greece
1998 - IRG/WP 98-50101-04
The practice of wood preservation in Greece was started about 80 years ago and refer to creosote-treated timber used in ground contact (i.e. railway sleepers, poles). At present, three creosote impregnation plants and thirteen CCA or CCB units exist in Greece treating about 90.000 m3 of wood per year. Most of the research on wood preservation has been carried out in the last 15-20 years and refer ...
S Adamopoulos, E Voulgaridis