Method to determine the depth of penetration of the biologically active components of wood preservatives
1978 - IRG/WP 2108
A time-saving method for determining the depth of penetration of the biologically active components of wood preservatives is described. The test specimens were obtained by cutting thin slices from the wood either parallel or perpendicular to the treated surface. The slices were then exposed to fungal attack. A good correlation was found between the test results obtained by the modified German Stan...
H-P Sutter


Soft rot test of copper/chrome/arsenic treated heartwood of three Malaysian timbers by the vermiculite-burial method. (+ correction document of 25 July 1990)
1990 - IRG/WP 2354
Heartwood of copper-chrome-arsenic (CCA) treated kempas (Koompassia malaccensis), tualang (Koompassia excelsa) and keruing (Dipterocarpus spec.) was found to be susceptible to soft rot in recent pole surveys. Standardized heartwood blocks were impregnated with 0 to 6.3% (w/v) CCA and challenged to decay for twelve weeks by a mixed inocula of Chaetomium globosum, Glenospora graphii, Humicula grisea...
R-D Peek, A H H Wong


The ground proximity decay test method
2000 - IRG/WP 00-20205
A decay field test method, which has been recently proposed for the standardization by the AWPA, is described for evaluating the relative performance of wood samples in a severe above ground situation exposed to the weather. Data is presented on the relative performance of untreated control samples and standard preservative systems exposed at the same site at different time periods, or at differen...
A F Preston, P J Walcheski, K J Archer, A R Zahora, L Jin


A field study on the suitability of the European lap-joint test
2001 - IRG/WP 01-20239
Within the framework of the European SM&T Research Project "Co-normative research on field tests for wood preservatives out of ground contact in conjunction with methods for preconditioning test specimens prior to test" (FACT) one aim was to establish the suitability of the European lap-joint test (as it is described in ENV 12037:1996) to assess wood preservatives in the field in EHC 3. Scots ...
M Grinda, Ö Bergman, H-V Borck, D Dickinson, P Esser, R Gründlinger, H Leithoff, S Molnar, L Paajanen, N Pfabigan, E D Suttie, F Thomassin, T Nilsson, J Van Acker, M Van Der Zee, A Voss


A novel method for evaluating the performance of water repellents
1987 - IRG/WP 2279
Application of water repellent formulations to timber surfaces offers protection from the weather, reducing degrade and movement. A novel test method has been developed to evaluate the comparative efficacy of such formulations when samples are exposed to weather. The method uses sapstain free sapwood of defect free, untreated, seasoned Radiata pine, (Pinus radiata D. Don.) Water Repellency was det...
A R Moffat


Resistance of board materials against fungal decay: A comparative experiment on Kolle flask tests method and direct test method
1985 - IRG/WP 2243
Two sets of plywood (Aucoumea klaineana Pierre) 7 and 11 ply, treated by two preservatives, and untreated, were tested by two methods: 1. Kolle flask test method on malt-agar substrate according to the French standard NF B 51.295; 2. A direct test method in non sterile conditions according to DocNo: IRG/WP/2214. The exposure time far both methods was 12 weeks. After exposure, the degree of attack ...
G R Y Déon, L N Trong


Leaching from field test stakes. Results from two different methods of analysis
1993 - IRG/WP 93-50013
Field test stakes treated with Boliden K33 containing copper, chromium and arsenic exposed at three different fields in Sweden and rejected due to decay, have in two studies been analysed regarding leaching and remaining preservatives. The stakes have been exposed during 20 to 43 years. The density of the stakes and content of copper, chromium and arsenic have been determined in the top part of th...
F G Evans, M-L Edlund


High-energy multiple impact (HEMI)-test – Part 2: A mechanical test for the detection of fungal decay
2006 - IRG/WP 06-20339
The suitability of the high-energy multiple impact (HEMI)-test for detection of early fungal decay was examined. The HEMI – test characterizes the treatment quality of thermally modified wood by stressing the treated material by thousands of impacts of pounding steel balls. This method differentiates between heat treatment intensities, which are expressed by structural changes of the wood. Simil...
C R Welzbacher, C Brischke, A O Rapp


High-energy multiple impact (HEMI)-test – Part 1: A new tool for quality control of thermally modified timber
2006 - IRG/WP 06-20346
Thermal modification processes improve durability and dimensional stability of wood, but the strength properties, especially the dynamic ones, are compromised and need to be considered with respect to industrial quality control. Results from standard dynamic strength testing, such as impact bending tests, suffer from high variability, and therefore require a high number of replicates. To overcome ...
C Brischke, A O Rapp, C R Welzbacher


Laboratory Leaching Tests to Study the Effects of Post-Treatment Storage Periods on CCA Leachability and Fixation in Treated Permeable and Refractory Malaysian Hardwoods
2006 - IRG/WP 06-50240
The biological resistance and environmental safety of CCA-treated wood relies on the extent of post-treatment storage fixation of CCA in wood prior to being utilized. A study on the comparative leachability (fixation) of CCA-treated refractory and permeable heartwoods of 3 Malaysian hardwoods subjected to different post-treatment storage (fixation) periods of up to 4 weeks, at 2 laboratory leachin...
A H H Wong, H C Lai, N P T Lim


Accelerated Above-ground Testing of Wood Preservatives
2007 - IRG/WP 07-20358
The Canadian wood preservation industry is interested the introduction of new preservative formulations, some of which are intended only for above ground uses. Canada’s Pest Management Regulatory Agency requires data from field tests under Canadian conditions but these can take many years to generate results. Forintek has therefore developed an accelerated above ground test, under contract to a ...
P I Morris, S McFarling


Comparative Laboratory Leaching Test Methods to Study Post-Treatment Storage Period Impacts on CCA Leachability and Fixation in Treated Kempas (Koompassia malaccensis) Heartwood
2007 - IRG/WP 07-20376
Three laboratory leaching test methods were compared to determine the effects of different post-treatment storage fixation periods on leachability/fixation of CCA components from treated kempas (Koompassia malaccensis) permeable heartwood. End-sealed test wood blocks of permeable were treated with CCA to target retention of 5.6 kg/m3, immediately stored to fix at ambient conditions for 0 and 48 ho...
A H H Wong, H C Lai


Above Ground Field Testing – Influence of test method and location on the relative performance of various preservative systems
2008 - IRG/WP 08-20393
Standardized above ground tests such as the lap-joint or test deck methods can be very slow in producing useful information on the relative performance of wood preservative systems. It often requires many years for decay to develop in wood treated to sub-optimal concentrations of standardized preservatives, making relative comparisons of performance between new systems and established preservativ...
A Zahora


Development of microbiological test methods for the wooden packaging of foodstuffs
2010 - IRG/WP 10-20453
Whereas different sampling methods already exist for analysing contaminated surfaces or packaging made of plastic or paper, there is no methodology that enables the sampling and quantification of microorganisms in packaging made of wood. The objective of this study was to compare the most commonly used microbiological methods and to develop a reliable quality control test adapted to wooden packagi...
I Le Bayon, H Callot, M Kutnik, C Denis, A-M Revol-Junelles, J-B Millière, M Giraud, M Gabillé, N Passédat


Performance of Wood Protection Systems at Multiple Field Test Sites Using the Ground Proximity Test Method
2012 - IRG/WP 12-20499
A series of preservative systems were used to treat southern pine ground proximity test samples which were then exposed at a range of test sites located throughout the world. The sites were chosen on the basis of having vastly different Scheffer Climate decay indices. After almost 14 years exposure, distinct differences are apparent in how different preservative systems perform at the different ...
A Zahora, A Preston, L Jin


Mold Control for Treated Lumber in Block-Stack Storage Conditions
2012 - IRG/WP 12-30588
The mold development and control for freshly treated and block-stacked wood have been evaluated using a green house mold testing method. The results for the mold resistance of several commonly used water boron preservative treatment systems, such as ACQ, Copper Azole, and borates with and without inclusion of mold inhibitors are presented. The data suggest that the different preservative treatme...
L Jin, P Walcheski, A Preston


Method for determining the critical moisture level for mould growth on building materials
2013 - IRG/WP 13-20530
The natural conditions of relative humidity (RH) and temperature (T) in different parts of a building is rarely constant over time. Instead, RH and T often vary cyclically and may pose a risk of mould growth as these conditions are the two key environmental parameters that controls mould growth. Consideration to both humidity and temperature conditions and the susceptibility to mould in a material...
A Ekstrand-Tobin, P Johansson, G Bok


Development of a rapid method to assess the rate of fungal colonization of wood
2013 - IRG/WP 13-20531
Testing of wood durability is today done mainly with accelerated exposure tests under rather realistic conditions (in ground, outdoors with moisture traps etc). Although such tests are accelerated with respect to the conditions that outdoor exposed wood structures are exposed to, they tend to take rather long time. The present paper presents the development of a rapid method intended to assess at ...
L Wadsö


Screening method to test efficacy of fumigants against fungi and preliminary data on the efficacy of sulfuryl fluoride
2014 - IRG/WP 14-20551
Methyl bromide is being phased out and there is an urgent need to find a suitable replacement that is effective in reducing exotic pest establishments via trade in wood products. Efficacy data for established phytosanitary fumigants were mostly developed for arthropods and nematodes, and limited information exists for plant pathogens. Increased interest in developing a fast screening process for f...
A Uzunovic, A Mukherjee, R Mack, P Elder, S Myers


Testing the durability of timber products above ground using the block-test method – A critical review
2018 - IRG/WP 18-20637
The block-test method for testing the durability of wood and wood products above ground is reviewed critically with respect to practical aspects, moisture loads, corresponding decay development, and the possibilities of assessing test specimens by determining the dynamic modulus of elasticity (MOEdyn) of wood. In total, 36 blocks representing different modifications of the original set-up and a wi...
C Brischke, A Gellerich, H Militz


Improvement of analytical methods of wood preservatives and its validation with collaborative testing
2019 - IRG/WP 19-20655
This discussion paper presents on-going collaborative test of analytical methods of wood preservatives according to the standardization process of Japan Agricultural Standard (JAS) by the Ministry of Agriculture, Forestry and Fisheries (MAFF). Food and Agricultural Materials Inspection Center (FAMIC) in close cooperated organization with the MAFF, has wide range of tasks about inspections and anal...
T Miyauchi, K Yamamoto, N Shota, Y Akabori, M Ikeda, J Eisawa, K Kambara, T Osawa, C Igarashi, Y Baba, W Ohmura, M Shimizu, M Samejima


Mini-stakes – an alternative test method for EN 252?
2023 - IRG/WP 23-20691
Market approval of wood treatment products requires knowledge and prove of long-term durability. Efficiency of wood treatment with a specific product is evaluated based on variety of tests, including penetration evaluation, leaching studies as well as decay tests. EN 252 standard test is a core method for wood durability evaluation in a ground contact, both for commercial product approval and scie...
R Digaitis, P Larsson Brelid, N Terziev, M Klamer, A W Christof, J Stenaek, N Morsing


Field durability testing of wood above ground - Part 1: 15 years’ experience with the Bundle method
2023 - IRG/WP 23-20695
A ‘jack of all trades’ method for above-ground wood durability testing has been sought for decades, but until now no method has found its way into standardization. The method of choice shall be applicable for untreated and treated wood – ideally also for wood composites. It shall be reproducible, objective, fast, easy, and inexpensive. Finally, it shall provide high predictive power. This s...
C Brischke, G Alfredsen, L Emmerich, M Humar, L Meyer-Veltrup


Field durability testing of wood above ground - Part 2: The full guideline of the Bundle method
2023 - IRG/WP 23-20696
To determine the biological durability of wood above ground, numerous approaches for test methods have been pursued and tried out in the field in the past. So far, no method has managed to find its way into a European standard. During the last 15 years, experience with the Bundle method has been gained. As described in Part 1 of this paper, the method is recommended as a suitable tool for determin...
C Brischke, G Alfredsen, L Emmerich, M Humar, L Meyer-Veltrup


Field test method for wood in above ground situation - The full CEN/TC 38 guideline for the Sandwich method. Part 1 - Determining the relative protective effectiveness of a wood preservative
2024 - IRG/WP 24-41013
The attached draft CEN Technical Specification (i.e. pre-EN standard) has been drafted in order to become an alternative to the Lap-Joint test method (EN 12037:23) for testing of wood in above ground situation and the draft CEN/TS Part 1 is specifically intended for determining the relative protective effectiveness of a wood preservative. The new draft CEN/TS is based on a test method developed by...
M Westin, R Ringman, A Christof, F Friese