Your search resulted in 89 documents. Displaying 25 entries per page.
Microbial decay of an archaeological wood
1994 - IRG/WP 94-10053
A light and transmission electron microscopic investigation of an archaeological wood was undertaken to determine the cause of its deterioration. The wood came from a bulwark constructed in early 1100 in the lake Tingstäde Träsk on the island Gotland in Sweden. The samples of the wood, which was identified as Pinus sylvestris, were taken from a depth of 0.85 m below the bottom level. The wood wa...
A P Singh, T Nilsson, G F Daniel
Microscopic characteristics of microbial attacks of CCA-treated radiata pine wood
1993 - IRG/WP 93-10011
Light and electron microscopic observations were made of CCA-treated radiata timbers, which had been placed in service in a vineyard soil as supporting poles and as part of a house pile, to determine the cause of their deterioration. The house pile had failed in service after between 9 and 13 years and was of particular interest because decay was more severe in deeper regions than at the surface a...
A P Singh, R N Wakeling
IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 21: Report of eighth inspection (7 years) in Australia
1985 - IRG/WP 4119
This report tabulates the seven year (86 month) inspection results, obtained on 28 Fabruary l985, of the IRG/COIPM International Marine Test at Goat Island, Australia. This test was installed in December 1977. The results are given in Tables 1-6. Table 7 lists the number of marine borers identified from blocks (2 cm and 6 cm long respectively) cut from the ends of specimens removed at the previous...
L J Cookson, J E Barnacle
Biological detoxification of wood treated with salt preservatives
1992 - IRG/WP 92-3717
The use of microorganisms that are capable to convert chemically fixed inorganic preservative complexes from impregnated wood waste into watersoluble components is investigated. A number of fungi were isolated from deteriorated and initially well-treated wood. They revealed an exceptionally high production of organic acids (pH 2). The fungi were identified and used together with others of the same...
I Stephan, R-D Peek
Some recent studies on the marine wood-borers of the west coast of India
1982 - IRG/WP 486
Occurrence and distribution of marine wood-borers along the west coast of India from Mangalore to Kandla are presented together with the distribution pattern of all the molluscan and crustacean wood-borers so far reported from India coasts. The survey, conducted for the first time along this coast, revealed the presence of 14 species of Teredinidae, 2 species of Pholadidae, 3 species and one varie...
L N Santhakumaran
Environmental risk assessment of treated wood - A mesocosm study
2005 - IRG/WP 05-50224-8
In order to evaluate the environmental impact of treated poles, we have developed physical models (mesocosms) containing around 250 kg of natural soil and a treated pole.
On the top of each mesocosm, a spraying mechanism, which can distribute ultrapure water through several nozzles, was built.
On the lower part of each mesocosm, a small tank, which can contain some litres of leachate, was placed...
P Marchal, F Poly
New perspectives on the biology of the tropical powderpost beetle, Minthea rugicollis (Walk.)
1994 - IRG/WP 94-10085
Minthea rugicollis (Walk.) is one of the most important pests of seasoned hardwoods in the tropics. The species owes its ubiquity largely to its insidious development within a nutrient-filled environment and also to a strong coevolutionary specialization with its natural habitat, wood. Such an environment provides a buffer to extrinsic fluctuations and accounts for a wider range of tolerance by im...
F Abood, R J Murphy, R W Berry
Microbial fouling of 10-40% naphthalene in creosote treated and untreated wooden pilings in the marine environment - A progress report
1980 - IRG/WP 455
In June 1978, Document No: IRG/WP/442 entitled 'Microbial Biofouling of 10-40% Naphthalene in Creosote Treated and Untreated Wooden Pilings in the Marine Environment" was released to the IRG members as a report on the early results of a long term (about 5 years) study of whether the naphthalene content of creosote was importart in protecting wood pilings in the marine environment from bor...
R R Colwell, A J Emery
Temperature tolerance of Botryodiplodia theobromae causing sapstain on rubber wood
1998 - IRG/WP 98-10259
Botryodiplodia theobromae Pat. is the dominant fungus causing sapstain on tropical timbers. Rubber wood (Hevea brasiliensis) is highly susceptible to sapstain infection. The tropical warm-humid climate also influences the growth of B. theobromae on rubber wood. Additionally, the moisture content of timber provides conducive conditions for the entry and establishment of the fungus. Temperature tole...
E J M Florence, J K Sharma, R Gnanaharan
Tolerance of Wood Decay Fungi to Commercial Copper Based Wood Preservatives
2002 - IRG/WP 02-30291
Due to the use of copper based preservatives like CCB or CCA for more than a century, copper tolerant fungi have appeared in some European countries in recent times. It is therefore important to find out whether this phenomenon is specific for only classical copper ingredients, or generally for all copper based formulation. Thus, we tested the tolerance of three commercial copper based
pres...
F Pohleven, M Humar, S A Amartey, J Benedik
Sphaeroma terebrans Bate: A note on distribution and preservative tolerance in Florida coastal waters
1987 - IRG/WP 4135
Treated test panels were installed in January 1984 in a Florida estuary where Sphaeroma terebrans had severely damaged pilings treated with copper chromate arsenate (CCA). Test treatments were CCA at three retentions, coal-tar creosote at three retentions, creosote with chlorpyrifos, dual treatment with CCA and creosote, and three types of chemical modification of the wood test panels. We describe...
B R Johnson, E D Estevez, S A Rice
Susceptibility of painted wood to discolouring fungi - influence of binder, solvent and surfactant
1992 - IRG/WP 92-3714
Previous studies have shown that the basic composition of paints, without fungicide addition, can significantly contribute to the varying microbial susceptibility of painted wood. Previously, non-weathered water-borne acrylic paints applied to wood without a primer were shown to be more susceptible to mould attack than solvent-borne alkyd paints. The present study was initiated to reveal if this d...
J Bjurman, C Herder
Relative tolerance of CCA by larvae and adults of the common shipworm, Bankia gouldi
1992 - IRG/WP 92-4174
Southern pine sapwood "2 x 4´s" were created by bolting together four panels 13 mm thick by 89 mm wide by 457 mm long. The two outer laminates were untreated and the two inner laminates were each treated to different CCA retentions, ranging from 8.0 to 43.2 kg/m³. Test specimens were exposed from May to October in a tributary of the Chesapeake Bay. Larvae were unable to settle on and burrow into...
B R Johnson
Aboveground Microbial Decay Test of Biocide Treated and Untreated Wood Exposed to Danish and Humid Tropical Climates
2004 - IRG/WP 04-20306
A co-operative study was initiated to compare the aboveground field decay test of untreated and preservative-treated timbers under Nordic (Danish) and a representative humid tropical (Malaysian) environment according to CEN standard method. Matched specimens of untreated and both preservative-impregnated and surface-treated wood were simultaneously exposed at The Danish Technological Institute (DT...
A H H Wong, N Morsing, K H Henriksen, S Ujang
Influence of acidification on decay processes of CCB treated wood
2004 - IRG/WP 04-10514
The phenomenon of copper tolerance by brown rot fungal strains has been known for a long period but the complete mechanism of copper tolerance by these fungi is not understood yet. Copper tolerance has previously been linked to oxalic acid excreted by copper tolerant brown rot fungal strains. This acid reacts with copper in the wood to form an insoluble and therefore less toxic copper oxalate. The...
M Humar, S A Amartey, M Šentjurc, F Pohleven
Microbial decay in an extremely durable Malaysian hardwood Belian (Eusideroxylon zwageri) - an overview
1997 - IRG/WP 97-10216
The heartwood of Belian (Eusideroxylon zwageri) is highly regarded among the naturally durable Malaysian hardwoods, and is therefore a choice timber for soilcontact use in the humid tropics such as untreated telecommunication poles, fence posts and railway sleepers. The high microbial resistance of the wood is evidenced by the mere superficial degradation observed in some pole samples after 20 yea...
A H H Wong, A P Singh
The Copper Tolerance of Mycelium vs. Spores for Two Brown Rot Fungi
2002 - IRG/WP 02-10422
The copper tolerance of two brown rot fungi, Gloeophyllum sepiarium and Oligoporus placentus, has been tested using both mycelia and basidiospores as inoculum sources. Mycelial growth of O. placentus on agar medium was shown to be much more tolerant to copper (as copper sulfate) than that of G. sepiarium. However, there was no difference in copper tolerance of basidiospores between the two specie...
S Choi, J N R Ruddick, P I Morris
Variable tolerance of Ophiostoma spp. and Diplodia pinea to commercial antisapstain products
1998 - IRG/WP 98-10266
A recent survey of the occurrence of sapstain fungi in New Zealand, conducted at The University of Waikato, provided the opportunity to examine fungicidal tolerance amongst new isolates. It also enabled a comparison of tolerance amongst new isolates with those used in routine antisapstain screening trials at Forest Research.
A rapid antisapstain laboratory disc trial was used to determine the ext...
D R Eden, C M Chittenden, B Kreber, J G Van der Waals, R N Wakeling, R L Farrell, T Harrington
Growth of the copper tolerant brown rot fungus Antrodia vaillantii on different substrates
1995 - IRG/WP 95-10121
In recent years the copper tolerant brown rot fungus Antrodia vaillantii caused severe damages on impregnated wood in ground contact. The pattern of decay gave the impression that impregnated wood was even more severely attacked than unimpregnated. To investigate this question more closely laboratory tests were carried out. In a "choice test" Antrodia vaillantii grew preferably towards CC-impregna...
H Leithoff, I Stephan, M-T Lenz, R-D Peek
Characterization of Poria indoor brown-rot fungi
1995 - IRG/WP 95-10094
The heterogeneous group of "Poria" fungi causing brown rot in buildings and also of wood in ground contact comprises Antrodia vaillantii, Antrodia serialis, Antrodia sinuosa, Antrodia xantha and Tyromyces placenta. These fungi have similar morphological appearance and biology. Their nomenclature has a confusing history and is still not uniform. As a consequence, misinterpretations may occur. SDS p...
O Schmidt
Isolation and identification of non-decay fungi affecting the performance of alkylammonium compounds
1993 - IRG/WP 93-10020
The isolation of DDAC tolerant fungi was carried out on lumber treated with a range of antisapstain chemicals containing DDAC as one of their active ingredients. The tolerant fungi were selected by using malt media spiked with DDAC (100 and 2500 ppm). Isolations were tentatively identified into a range of fungi commonly found associated with wood deterioration (i.e. Penicillium sp. and Trichoderma...
A K Doyle, J N R Ruddick
The potential application of rapid gas-chromatographic assay of microbial respiration to the monitoring of wood decay in field trial situations
1983 - IRG/WP 2196
Gas chromatographic detection of microbial activity (C02 production) within stakes in a field trial situation would appear to provide a sensitive, non-destructive and relatively rapid method for the quantitative assessment of preservative treatments. Most consistent results were obtained when stakes were removed from the soil, washed, saturated with water and incubated in sealed PVC tubes at 25°C...
M A Line
Log fumigation prevents enzyme-mediated sapwood discolorations in hardwoods
1993 - IRG/WP 93-10003
Non-microbial sapwood discolorations in hardwood lumber can cause economic loss by degrade of quality. Based on the hypothesis that the enzyme-mediated sapstain may develop in part from byproducts of parenchyma cells in wood, reshly felled logs of red oak (Quercus spp.) and sugar hackberry (Celtis laevigata) were fumigated under a plastic tarp with methyl bromide. Log sections were checked after f...
E L Schmidt, T L Amburgey
Prevention of non-microbial sapwood discolorations in hardwood lumber: chemical and mechanical treatments
1997 - IRG/WP 97-30137
Sapwood discolorations in hardwood lumber that are non-microbial in origin result from the formation of pigmented starch-like granules in ray parenchyma cells. These discolorations can be prevented by treating unseasoned lumber with an antioxidant (sodium bisulfite). Exposing unseasoned lumber to microwaves or treating logs with fumigants also will prevent these discolorations. Subjecting unseason...
T L Amburgey, S Kitchens
Working plan: Second international collaborative field trial
1995 - IRG/WP 95-20056
This paper describes the scope, objectives, and approaches to be used in the second international collaborative field trial approved by the Scientific Programme Committee for partial funding in 1994. The trial is designed to develop a broad data base on causal mechanisms, interactions, and factor affecting the performance of treated wood in ground contact. The trial encompasses 12 different field ...
H M Barnes, T L Amburgey