IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 91 documents. Displaying 25 entries per page.


Service Life Prediction of Wood Claddings by in-situ Measurement of Wood Moisture Content: Status after 5 years of Outdoor Exposure
2009 - IRG/WP 09-20401
The Danish Technological Institute is in co-operation with industry partners running a project aiming at predicting the service life of different wood protecting systems. The project focuses on examining the moisture reducing effect of different protecting systems for timber claddings and the ability of these to maintain the appearance of the surfaces, when the wood is used in service class 3 (EN ...
E Tang Engelund, B Lindegaard, N Morsing


Effectiveness of a superficial treatment of bifenthrin to protect softwood framing from damage by subterranean and drywood termites in Indonesia
2009 - IRG/WP 09-40443
Various experimental testing procedures were undertaken in Indonesia to determine the effectiveness of a superficial (envelope) treatment of bifenthrin to protect softwood framing from damage by two species of subterranean termite (Macrotermes gilvus and Coptotermes curvignathus) and one species of drywood termite (Cryptotermes cynocephalus). Lengths of framing (Pinus radiata sapwood) were commerc...
P Sukartana, J W Creffield, A Ismanto, N E Lelana


A fast and economic method to produce grey wooden surfaces for decking and cladding: preliminary results
2009 - IRG/WP 09-40474
Uncoated wood is commonly used in France for cladding and decking to minimise maintenance. However wood surfaces progressively turn grey due to exposure to sunlight and water. This grey colour develops after several months depending on the wood species and the exposure: in the northern hemisphere surfaces facing south and west are most exposed and turn grey more rapidly than those facing north and...
L Podgorski, V Georges, I Garmendia, B Sánchez Sarachu


Frequency of fungal decay in softwood windows in Germany
2010 - IRG/WP 10-10725
Knowing how often fungal decay occurs is a fundamental basis for general recommendations of preservative measures. To optimize the German recommendations for chemical wood preservation of windows made out of pine or spruce more than 2000 windows have been inspected. All windows had an opaque coating and were between 2 and 17 years old. The selection of the inspected windows was kept as randomly as...
D Lukowsky, O Moarcas, A Luette


Service life prediction of wooden components – Part 2: Impact of material, exposure and design details
2010 - IRG/WP 10-20440
Dose-response functions permit to estimate the moisture and temperature induced decay potential for any wooden building component and exposure, and thus the service life to be expected. In part 1 of this series dose-response functions were established as a result of double layer field trials carried out at 24 European test sites over up to eight years. Using them makes it no longer necessary to co...
C Brischke, B Lauenstein, M Bilstein, T Bornemann, A O Rapp


Service life prediction for exterior timber cladding
2010 - IRG/WP 10-20460
This discussion paper considers service life prediction for timber and the work within the pan-European WoodExter project. The project aims to develop a model for service life prediction of exterior timber cladding, to enable better end use selection of material suitable for delivering the required service life of cladding and to provide information for professionals wanting to understand and use ...
E Suttie, F Englund


Aesthetic service life of coated and uncoated wooden cladding - influencing factors and modelling
2011 - IRG/WP 11-20470
Mould growth on exterior coated cladding façades is an undesirable element and will often shorten the aesthetical service life. Mould growth on painted surfaces is influenced by type and concentration of film fungicides, the paint formulation and the wood substrate itself, and wooden cladding may experience exponential fungal deterioration caused by variation in the climatic factors, often within...
L Ross Gobakken, O A Høibø


The case for using borates in termite control in tropical Australia
2011 - IRG/WP 11-30573
A brief historical overview of boron based wood preservatives efficacy against subterranean termite management worldwide, and in Australia, is presented. The boron based compounds to be used in H2 hazard conditions, may be applied as a surface treatment by dip, flood coat or spray, and rapidly penetrates to the centre of timber substrates, whether containing sapwood or heartwood. However, section ...
B M Ahmed (Shiday), J R J French


Utilization of thermodesorption coupled to GC-MS to study kinetics of thermodegradation of different wood species
2011 - IRG/WP 11-40559
Thermdesorption coupled to Gas Chromatography coupled to Mass Spectroscopy (TD-GC-MS) has been investigated to identify volatile degradation products generated during wood heat treatment by mild pyrolysis. For this purpose, wood samples of different softwood and hardwood species have been heat treated under nitrogen for different temperatures comprised between 180 and 230°C during 15 min. in the ...
K Candelier, M Chaouch, S Dumarçay, A Pétrissans, M Pétrissans, P Gérardin


Moisture protection and performance during 5 years exposure of 19 wood coating systems on a cladding in Vienna
2011 - IRG/WP 11-40561
A cladding with vertical boards of Norway spruce (Picea abies) comprising different coating systems had been exposed to natural weathering oriented south west in Vienna for 5 years. Weathering behaviour of the boards was assessed in intervals and wood moisture content was measured over the first 22 months of exposure. The moisture protective properties of the coating systems were assessed using la...
G Grüll, I Spitaler, M Truskaller


Long term durability of the heartwood of seven common softwood species in above ground conditions
2012 - IRG/WP 12-10771
The natural durability for wood in above ground use has been evaluated based on results after 11 years of exposure in a test site situated at the Danish Technological Institute in Taastrup, Denmark. Selected results for seven common softwood species exposed horizontally are reported. The test results cover samples with direct rain exposure (use class 3 of the European standard EN335-1:2006) and sa...
E Tang Engelund, M Klamer, T Mark Venås, B Lindegaard


Evaluation of fungal infestation and decay in a simulated use class 3 situation (block test) after some years of exposure
2012 - IRG/WP 12-20487
The so named “block test” was designed as part of the assessment methodology for testing the behaviour of natural and modified wood used under use class 3 (EN 335-2) conditions. The test was developed to expose the wood close to the ground to an environment with high humidity and high biological activity, but not in soil contact. The present study describes the evaluation of fungal infestatio...
A Gellerich, K Röhl, S Adamopoulos, H Militz


Effects of microclimate, wood temperature and surface colour on fungal disfigurement on wooden claddings
2012 - IRG/WP 12-20490
Wooden claddings are common in façades in Norway, and Norway spruce (Picea abies) is the most frequently used species. The cladding is a major part of the facade, and it has visual requirements that may define the aesthetic service life. The visual changes that occur during weathering can be colour changes, abrasion or wear, blistering, flaking, and even cracks in the wood or coating, but more of...
L Ross Gobakken, G I Vestøl


Utilization of thermodesorption coupled to GC-MS to characterize volatiles formation kinetics during wood thermodegradation
2012 - IRG/WP 12-40587
Identification of volatile degradation products produced during wood mild pyrolysis is important to have better insight on thermodegradation mechanisms. Previous studies have shown that thermodesorption coupled to GC-MS is an attractive tool to characterize and quantify products formed during wood thermodegradation indicating an higher susceptibility of hardwoods to thermodegradation compare to so...
K Candelier, S Dumarçay, A Pétrissans, M Pétrissans, P Kamdem, P Gérardin


Relationships between heat treatment intensity and some conferred properties of different European softwood and hardwood species
2012 - IRG/WP 12-40593
Effect of treatment intensity on conferred properties like elemental composition, durability, anti swelling efficiency (ASE) and equilibrium moisture content (EMC) of different European softwood and hardwood species subjected to mild pyrolysis at 230°C under nitrogen for different durations has been investigated. Independently of the wood species studied, elemental composition is strongly correl...
M Chaouch, S Dumarçay, A Pétrissans, M Pétrissans, P Gérardin


Field-testing of Norway Spruce Claddings with Monitoring of Moisture Content, Material Temperature and Microclimate
2012 - IRG/WP 12-20502
The physical function of a cladding is to protect the interior construction. Under normal circumstances the performance requirements can be met for a very long time, meaning that the technical service life of a wooden cladding can be very long. Since the cladding is a major part of the facade, it also has visual requirements that may define the aesthetic service life, and often it is much shorter ...
G I Vestøl, L Ross Gobakken


Mould growth on wood-based materials – a simulated in-service study
2012 - IRG/WP 12-20503
Ten different wood-based materials including preservative-treated wood, fire retardant-treated wood, modified wood, WPCs and untreated references of pine sapwood and spruce were placed in three different environments (an attic and two crawl spaces) for a period of 26 months. Mould growth was analysed at five to seven month intervals in an effort to map the growth development. The relative humidit...
G Bok, P Johansson, J Jermer


Cell wall properties of softwood deteriorated by fungi: combined chemical analyses, FT-IR spectroscopy, nanoindentation and micromechanical modelling
2013 - IRG/WP 13-20527
Mechanical properties of wood are determined by its inherent hierarchical microstructure, starting at the nanometer scale, where the elementary components cellulose, hemicelluloses, and lignin build up the wood cell wall material. Fungi cause degradation and decomposition of these components and, thus, alter the mechanical properties of wood. The aim of this study is to gain new insight into these...
L Wagner, T K Bader, K de Borst, T Ters, K Fackler


Three-year field test of preservative-treated Canadian species in Korea
2014 - IRG/WP 14-30646
The purpose of this study was to generate field performance data in Korea on Canadian softwood species preservative-treated to Canadian standards. Two field tests of preservative-treated Canadian softwood species, one in ground contact and one above ground, were installed in Jinju, Korea in November 2010. Western hemlock and white spruce were incised and pressure-treated with alkaline copper quate...
Jieying Wang, Jong Bum Ra, P I Morris


Mould growth on spruce claddings and the effect of selected influencing factors after 4 years of outdoor testing
2015 - IRG/WP 15-30671
Norway spruce (Picea abies) is the most frequently chosen wood species as claddings in façades in Norway, and is used both coated and uncoated. The visual changes that occur during weathering can be colour changes, abrasion or wear, blistering, flaking, and even cracks in the wood or coating, but more often growth of mould and blue stain fungi is the main challenge. A field test with synchronous monitoring of relative humidity, air temperature, material temperature and wood moisture content in Norway spruce claddings has been performed in southern Norway as part of the ClimateLife project. Visual evaluation of blue stain and mould growth according to EN 927-3 was performed, and evaluation data after 46 months exposure is presented. The objectives were to study the effect of 1) environment, 2) cardinal direction and 3) colour of the coated surface on growth of blue stain and mould fungi and to study the variation in relative humidity, air temperature, wood moisture content and material temperature. After 46 months exposure, the red coating system had generally the lowest mould ratings and the uncoated claddings had the highest. Of the white coloured claddings the ones facing south had lower mould ratings than those facing north, but the opposite were found for red coloured claddings. The relative humidity was higher in front of claddings exposed northwards and in a shaded environment compared to an open environment against south. In an open environment red coloured claddings had the lowest wood moisture content and highest material temperature, and red coloured claddings against south had the highest maximum material temperature.
L Ross Gobakken, G I Vestøl


Fire protection of wooden facades in Norway
2015 - IRG/WP 15-40710
Wood products are experiencing a renaissance as construction material in Europe due to their environmental benefits. In Norwegian building design however, timber has always played an important role but has had its limitations in urban architecture. One of the reasons is a high demand to fire safety in dense house building and multi-story buildings. Though novel construction methods and fire safety...
U Hundhausen, K-C Mahnert


Susceptibility of wood substrates to Aurebasidium pullulans at different temperatures
2016 - IRG/WP 16-10863
There is an increasing awareness of how the aesthetical performance of wood exposed outdoors changes over time and especially in the first few years after installation. Mould and blue stain fungi are biological agents that contribute to the weather grey colour on a wooden façade, and the blue stain fungi Aureobasidium pullulans is commonly identified as colonizer on coated and uncoated wood expos...
L Ross Gobakken, G Alfredsen


Engineering for Rural and Civil Development. Uni Performance of wood exterior structures above ground contact in Spain built with softwood species. The situation of cases in northern Spain
2016 - IRG/WP 16-20597
Across Europe is very common to find exterior structures build in sawn and glue-laminated wood. Most of these exterior structures used softwood wood species such as fir, spruce, larch and pine. In Spain wood exterior structures, as for example bridges, became more and more popular since eighties, when sawn and glue-laminated wood were utilized for building exterior wooden structures in overall Spa...
D Lorenzo, J Fernández-Golfín, M Touza


Hygrothermal performance of ventilated wooden cladding
2016 - IRG/WP 16-40733
The risk for an attack of wooden claddings by decay and discolouring fungi strongly depends on the moisture and temperature conditions in the building envelope. The design of the cladding has a major influence on its hygrothermal performance. In the present study, different wooden ventilated cladding designs were investigated at a test house in Mid-Norway for four years. The objective was to incre...
K Nore, U Hundhausen


Fungal resistance and accelerated weathering of Wood-Plastic composites reinforced with Maritime pine wood flour
2016 - IRG/WP 16-40750
This study evaluates the durability of wood-polymer composites (WPCs) elaborated for use in cladding application from recycled polypropylene (rPP) and wood flour. Local Maritime pine wood flour derived from regional sawmills was used in the study to reduce the environmental impact associated with transport. Different wood-plastic ratios with and without UV stabilizers and biocide were tested. One ...
M Jebrane, T Fournier, N-E El Bounia, F Charrier-El Bouhtoury


Previous Page | Next Page