Restrictions on the use of chlorosilanes as potential wood preservatives
1985 - IRG/WP 3345
The biological protection of wood by chemical modification with different types of chlorosilanes has been investigated. The impregnation of wood has been carried out by means of liquid phase and vapor phase treatments using pure silane and silane-solvent systems. The biological efficacy against wood rotting fungi, molds and staining fungi was determined in a number of screening trials, subsequentl...
M Stevens


A comparison of the diffusion of boron from two types of solid preservative rods into the heartwood of 3 Eucalypt pole species
2000 - IRG/WP 00-30227
The ability of boron to diffuse from polyborate and boron/fluoride rods through the heartwood of three eucalypt pole species (blackbutt, red ironbark and spotted gum) was examined. The aim was simply to determine the effects of rod type, wood species and time on the longitudinal diffusion of boron in eucalypt heartwood. Rapid diffusion of boron from polyborate or boron/fluoride preservative rods o...
P J Beutel, P D Evans


Modification of solid wood: research and practical potential
1997 - IRG/WP 97-40098
The polymeric structure of the wooden cellwall mainly consists cellulose, hemicellulose and lignin. The most reactive sites on these components are the hydroxyl groups. The cellwall polymers (and its reactive hydroxyl groups) are responsible for most physical and chemical properties of wood. By changing the basic chemistry of the cellwall polymers, it is possible to change different undesirable at...
H Militz, E P J Beckers, W J Homan


Multiple-Phase Pressure (MPP) Process: One-stage CCA treatment and accelerated fixation process. 4. MPP compared with other processes for achieving acceptable treatment of radiata pine heartwood
1998 - IRG/WP 98-40115
Although radiata pine sapwood is very amenable to preservative treatment, it is often difficult to achieve the required standard for heartwood treatment. A preliminary investigation showed that to achieve the NZ Timber Preservation Council minimum penetration requirements for radiata pine heartwood using the Multiple-Phase Pressure (MPP) Process, a hydraulic pressure of at least 1250 kPa for 20 m...
K Nasheri, J A Drysdale, G Durbin, M E Hedley


Multiple-Phase Pressure (MPP) Process: One-stage CCA treatment and accelerated fixation process. 3. Effect of process variables on sapwood treatment and CCA fixation.
1998 - IRG/WP 98-40114
The Multiple-Phase Pressure (MPP) Process achieves treatment and fixation as combined process using hot CCA, within a 2-3 hour time-frame. Timber is treated to saturation with hot CCA using an empty cell process. During the pneumatic pressure phase, hot solution is held in the wood in an otherwise liquid-free treatment vessel until fixation is >95% complete. This report details a factorial des...
H Pearson, K Nasheri, J A Drysdale, G Durbin, M E Hedley


Chemical reactions involved in furfurylation of solid wood - An investigation by ATR-IR spectroscopy
2006 - IRG/WP 06-40347
Wood modification with furfuryl alcohol (FA) has gained renewed interest during the last five to ten years because of advances in process technology and because of increased focus on the environmental hazards of traditional wood impregnation. The reaction mechanisms involved in the furfurylation process are not yet understood in detail. In the work presented here, the chemical reactions and their ...
T Mark Venås, L Garbrecht Thygesen, S Barsberg


Development of preservative treatment method using sub and super critical carbon dioxide
2007 - IRG/WP 07-40385
Significant efforts have been devoted for developing biocide impregnation method into wood materials using supercritical fluid. Developing better understandings of fluid phase and its effect on treatment results would facilitate a more rational development of supercritical fluid (SCF) impregnation. In this project, the preservative treatabilities under super- and sub-critical fluid conditions we...
Myeung-Won Cho, Sung-Mo Kang, Gyu-Hyeok Kim


Evaluation of natural durability of solid wood and mixed heartwood-sapwood Cypress (Cupressus sempervirens L.) plywood against Basidiomycete fungi
2008 - IRG/WP 08-10645
The aim of this research was to study the response of mixed plywoods composed of durable heartwood and non-durable sapwood to fungal attack. For this purpose, the species of Cupressus sempervirens (cypress) was chosen for its well-known durable heartwood. The evaluation of durability of plywood panels against fungi was done according to ENV 12038 and the fungi used were Coriolus versicolor (CV) an...
F Faraji, M F Thévenon, N Lemenager, B Thibaut


Termite resistance of pure and mixed heartwood-sapwood Cypress (Cupressus sempervirens L.) plywoods
2009 - IRG/WP 09-10693
The main objective of this research was to evaluate the ability of different plywoods made of durable heartwood and/or non-durable sapwood to resist termite damage. The well-known durable cypress (Cupressus sempervirens) was chosen for this study. The natural durability of cypress solid wood, divided into sapwood and heartwood, as well as the durability of 17 different laboratory manufactured plyw...
F Faraji, M-F Thévenon, B Thibaut


Performance of Fasteners in Treated Wood: A Comparative Study
2009 - IRG/WP 09-40465
Fastener performance is an important property for treated wood. Published data on screw and nail performance for different preservative systems currently on the market are, however, limited. In this study, screw and nail withdrawal strength for southern pine wood treated with ACQ (above ground and ground contact), MCQ (above ground and ground contact), borate (disodium octaborate tetrahydrate – ...
Q Wu, T Shupe, J Curole, K Ragon, M Voitier, M Freeman, D Ring


Effect of heating on aldehydes emissions from solid wood
2011 - IRG/WP 10-50277
We have found that acetaldehyde, a probable human carcinogen, is produced from wood through reaction with ethanol. Alcohols are increasingly being used in houses and buildings for cleaning purposes. Acetaldehyde emission from solid wood has been attributed to ethanol acidification by enzymes such as ethanol dehydrogenase. Heating could inactivate these enzymes. In this study, the effects of heatin...
A Ishikawa, K Miyamoto, S Tohmura, A Inoue


Decay initiation in plywood, OSB and solid wood under marginal moisture conditions
2011 - IRG/WP 11-20469
Hygrothermal models are increasingly used as research tools by building scientists and and design tools by designers to simulate heat, air, vapour, and water movements within and through building envelope and even to predict the consequences in terms of mould/decay growth and metal corrosion. This work was designed to generate data on decay initiation under marginal moisture conditions to support...
Jieying Wang, P Morris


Effects of nano-silver on brittleness of heat-treated solid woods
2011 - IRG/WP 11-40572
The present study is aimed at the effect of heat-treatment of normal as well as nano-silver-impregnated Populus nigra, Populus deltoides, and Fagus orientalis on brittleness. Specimens were impregnated with 200 ppm water-based solution of nano-silver particles under 3 bars in a pressure vessel using empty-cell process. For heat treatment, both nano-silver-impregnated and normal specimens were kept...
H Reza Taghiyari, B Moradi Malek, A Karimi


Determination of the natural durability of solid wood against wood-destroying fungi - a European round-robin test
2013 - IRG/WP 13-20511
In Europe the durability of wood against wood-destroying basidiomycetes is tested according to CEN/TS 15083-1 (2005). Hitherto existing experience with this standard is quite heterogeneous and results from previous round-robin tests have stayed unreported or have been reported incompletely. In particular the need for natural pre-weathering of the test specimens to allow potential detoxification of...
C Brischke, C R Welzbacher, A Gellerich, S Bollmus, M Humar, K Plaschkies, W Scheiding, G Alfredsen, J Van Acker, I De Windt


Ammoniacal zinc borate as solid wood preservative
2014 - IRG/WP 14-30659
Zinc borate, well-known for its fungicidal, insecticidal and flame resistant properties, is widely used in manufacture of lignocellulose particle board. This form of borate is the least water soluble form available providing advantages as well as disadvantages for use as a wood preservative. This form does not leach from wood under conditions of high humidity, but it is also very difficult to appl...
C Ibáñez, C Mantero, A Ibarra, M Rabinovich


Influence of the moon phase on durability against wood decay fungi of Larix kaempferi and Pseudotsuga menziesii wood species
2015 - IRG/WP 15-10836
The analysis of the natural durability of wood is essential when establishing the level of protection required, depending on the designated end use of timber. On the other hand, there is a popular belief based on the influence of the moon phase in felling timber, recommending the waning moon as the optimum for felling trees. In fact, some companies now offer among their products, sawn timber felle...
M T Troya, M Conde, M J Barriola, F Llinares, V Dorronsoro


Building solid foundations to support market growth of preserved wood in the UK – treatment quality, product approval and the largest national field trial of preservative treated wood in 50 years
2015 - IRG/WP 15-30662
The Wood Protection Association (WPA) has just commissioned Britain’s largest ever durability trial of home grown timber, having contracted Building Research Establishment (BRE) to conduct a long term controlled field trial of sawn and pressure treated British Softwood posts at two sites with differing soil conditions. This large scale Field Trial is the last of an innovative and substantial thr...
E Suttie, G Ewbank


Durability to decay organisms of Pinus nigra subsp. laricio var. corsicana. Influence of the moon phase
2016 - IRG/WP 16-10869
Actually the use of wood has an added value since it is a renewable, biodegradable and recyclable material. For this reason, the evaluation of it natural durability is essential when establishing the level of protection required, being depending on the designated end use of timber. On the other hand, there is a popular belief based on the influence of the moon phase in felling timber, recommending...
M T Troya, M Conde, M J Barriola, F Llinares, V Dorronsoro


Fabrication and characterization of MicroPCMs filled wood-plastic composites: Effects of polyethylene glycol on melamine–formaldehyde shell material
2016 - IRG/WP 16-40728
Microencapsulated phase change materials (MicroPCMs) containing dodecanol were fabricated using melamine-formaldehyde (MF) or polyethylene glycol 200 modified melamine-formaldehyde (PMF) resin as the shell materials by in situ polymerization. Wood flour/high-density polyethylene (WF/HDPE) composites with MF shell MicroPCMs (MF-MicroPCMs) or PMF shell MicroPCMs (PMF-MicroPCMs) were prepared, respec...
Xi Guo, Jinzhen Cao


Influence of pressure phase impregnation time on the uptake and distribution of wood preservatives in Scots pine material of diverse treatability
2016 - IRG/WP 16-40752
In spite of the general opinion that Scots pine sapwood is easy to impregnate considerable variations in treatability are reported. In order to study impregnation results of diverse Scots pine sapwood treated with increasing process times, Scots pine sapwood from two different predefined treatability groups was impregnated. A copper solution was used as impregnation agent in ten different vacuum p...
K Zimmer, B Kerfriden


Effects of heat treatment on sound absorption coefficients in nanosilver-impregnated and normal solid woods
2017 - IRG/WP 17-40770
Effects of impregnation with silver nano-suspension as well as heat-treatment on sound absorption coefficients (AC) were studied in tangential direction of five different solid woods based on their importance. AC was measured at two frequencies of 250 and 500 Hz. A 400 ppm nanosuspension was used for the impregnation; silver nanoparticles had a size range of 30-80 nm. Based on the obtained results...
A Esmailpour, J Norton, H R Taghiyari, H Zolfaghari, S Asadi


Effects of Nano-Wollastonite Impregnation on Fire Properties of Some Thermally-Treated Solid Wood Species
2017 - IRG/WP 17-40771
The effects of nano-wollastonite (NW) suspension impregnation on the fire-retarding properties of heat-treated solid wood of three species (beech, poplar, fir) were studied. Heat treatment was performed at two temperatures of 180 °C and 200 °C. Impregnation was carried out at a pressure of 3 bars for 30 min. The fire properties included ignition time, glowing time, back-darkening, back-splitting...
H R Taghiyari, R Hossinpourpia, S Adamopoulos, A Jahangiri, D Rabie


Solid Timber Bridges – Latest Developments
2017 - IRG/WP 17-40788
The technology of gluing in wood construction has evolved considerably in recent years. This has been shown especially in timber bridges that Glulam is now the main building material. A further development is the so-called block gluing, which provides a good basis for supporting structures. Numerous bridges, especially in central Europe, appeal by unique design and monolithic and solid construction. These structures base on two main developments: block lamination of glulam and the composite of timber and concrete to one structural system.
F Miebach


Long service life or cascading? The environmental impact of maintenance of wood-based materials for building envelope and their recycling options
2018 - IRG/WP 18-50336
A major restraint in choosing bio-based materials (i.e. wood-based) for external use, is the lack of confidence that architects, designers and customers have toward these materials. In particular, the limit state of bio-based materials, which defines the frequency of maintenance operations, might be reached earlier for wood than for other materials (i.e. concrete). On the other hand, resource and ...
M Petrillo, J Sandak, P Grossi, A Kutnar, A


Terrestrial laser scanning (TLS) – a potential tool for improved utilisation of the natural durability of Scots pine for solid wood products
2019 - IRG/WP 19-50358
The natural durability of sapwood of most species is generally low, while heartwood can be more resistant to biodeterioration. For the sawmill industry various lumber products require certain diameters and lengths of the logs in addition to requirements for wood properties. When utilising the heartwood, it is therefore important to acquire information already in the forest about which trees that c...
P-O Flaete