Your search resulted in 439 documents. Displaying 25 entries per page.
Eco-Friendly Composites from Bagasse and Soy-based Resin
2009 - IRG/WP 09-40462
In this study, bagasse and soy-based resin were used for producing composite materials. The objective of this study was evaluation of some physical and mechanical properties of boards made of various ratios (100:0, 60:40, 40:60 and 0:100) of bagasse to wood fiber mixtures (wt: wt) with addition of Soy/PF resin at three levels (4, 8 and 10%) and 1.5% wax. All properties were tested according to AST...
G Rassam, B Jamnani
Biological Performance of Boron-based Chemicals Treated Wood Composites
2009 - IRG/WP 09-40464
In this study, the biological performance of wood-based composites panels treated with boron containing chemicals against to a fungus was determined. Boric acid, borax, zinc borate and agricultural borate (Tarım-bor™), developed and patented by National Boron Research Institute, were mixed with wood chips or fibers and then particleboard, medium strand board and middle density fiberboar...
Ü C Yıldız, H Kalaycıoğlu, S Yıldız, A Temiz, E Tomak Dizman, A Çavdar Dönmez
Extensive review of fire-retardant wood composites researches
2009 - IRG/WP 09-40471
The increased demand for public safety has led to greater interest in fire retardant materials in the recently years. Legislation relating to safety in the home, in work locations, on transport facilities and in public places continues to produce new regulation. There is average 524 thousand structure fires occurred every year in US, 3757 civilian in death, about 20 thousand civilian in juries, di...
Zhilin Chen, Zhiyong Cai, Feng Fu
Progress in Fire-Retardant Research on Wood and Wood-Based Composites: a China Perspective
2009 - IRG/WP 09-40476
The fire retardant research on wood and wood-based composites, which was carried out in China in the past two decades, was reviewed with 55 references. While many kinds of fire retardants for wood and wood-based composites have been studied, the mainstream is still the compound or the mixture containing phosphorus, nitrogen and boron elements, which can be used in the form of water solution in th...
Wang Qingwen, Wang Fengqiang, Hu Yunchu, Li Jian
Physical and Mechanical Properties of Bamboo Oriented Strand Board Treated with Copper-based Preservatives
2009 - IRG/WP 09-40482
Oriented strand board (OSB) has been gradually accepted, used and developed in China. Bamboo is a renewable and potential non-wood fibre resource for making OSB. But the nature of bamboo makes its products including bamboo OSB (BOSB) more prone to decay and mold. Protection BOSB from biodegradation is the key both to efficiently using bamboo resource and to improving the durability of the final pr...
Juwan Jin, Daochun Qin
Assessment of the marine borer resistance and abrasion resistance of lesser known hardwood timber species for use in marine construction
2010 - IRG/WP 10-10711
Naturally durable species of timber are used as an alternative to preservative treated timber for marine structures, but many species have not been evaluated for their potential for use in this environment. EN 275 specifies a 5-year test period - too long a period for screening tests to be economically viable. In this study, candidate timber species were selected for testing both in the laboratory...
J R Williams, G S Sawyer, G Malyon, S M Cragg, J D Icely, J Simm, M Meaden
Assessment of antagonism between lignicolous microorganisms: Research on possible use to preserve wood poles
2010 - IRG/WP 10-10718
Biological environments contain a certain number of microbial populations which, within a given ecological niche, display various relations ranging from symbiosis to parasitism. Researchers have been interested in these types of relations for around fifty years, especially in one very particular type of relationship: the antagonism exerted between individuals of the same microbial population. Toda...
J-F Labrecque, A Zaremski, L Gastonguay, Y Prin
Methods for Studying Penetration Depth of Wood Protection Products
2010 - IRG/WP 10-20432
EN 152 is an accepted standard in Europe for measuring how deep a wood protection product penetrates into the surface of treated pine wood. The method has provided consumers with a wide assortment of products that meet the specifications outlined in the standard. Because the test takes 8 or more months to carry out, artificial ageing procedures have evolved in order to standardize and speed up the...
K Hansen, L Sites, D D Nicholas
Toward an assessment of copper bioavailability in treated wood
2010 - IRG/WP 10-20445
Many modern wood preservative systems rely on copper (Cu). Some oxalate-producing fungi detoxify Cu by immobilizing it in crystals, and this may decrease its physiological availability (bioavailability). Cu bioavailability may also decrease during wood treatment. Cu retention in wood, however, is typically measured as a weight-to-volume concentration without an estimate of its bioavailability and ...
J S Schilling, J J Inda
Onset of mould growth – the effect of climate variability and different geographic locations
2010 - IRG/WP 10-20446
This paper presents a study on how climate conditions at numerous locations in Sweden affect the risk of onset of mould on wood sheltered outdoors. The results indicate that the risk is clearly higher in the south compared to the north of Sweden. These differences are mainly explained by colder and dryer winter periods in the north which is unfavorable for development of mould. The results also sh...
M Häglund, T Isaksson, S Thelandersson
DNA-based tools for rapidly detecting, quantifying and monitoring ophiostomatoid fungi on beetles, in trees and wood products
2010 - IRG/WP 10-20450
Approximately half of the trees harvested for commercial purposes are lost because of native or introduced insects or insect-vectored microorganisms. Ophiostomatoid fungi, which are well adapted to dissemination by insects, include ~140 species of saprobes and pathogens. They are present worldwide, have high economical impact and many are subject to quarantine regulation. Thus, it is necessary to ...
L Khadempour, Young Woon Lim, S Massoumi Alamouti, C Breuil
Mould growth on wood-based materials – a comparative study
2010 - IRG/WP 10-20455
Ten different wood-based materials - preservative-treated wood, fire retardant-treated wood, modified wood, WPCs and untreated references of pine sapwood and spruce - were tested for mould growth according to SP method 2899 during 42 days at 90% RH and 22°C.
Even though the results must be interpreted carefully, they indicate significant differences in mould resistance between the materials tes...
P Johansson, J Jermer
Assessment of Boracol 200RH (FrameSaver) as a remedial treatment to control decay in pre-decayed model timber frame units
2010 - IRG/WP 10-30529
Model timber frame units constructed from untreated radiata pine were pre-wetted to approximately 40% moisture content and inoculated with Coniophora puteana and Oligoporus placenta. Units were transferred to a controlled environment room maintained at 25°C and 95% RH for 7 and 10 weeks to allow two levels of decay to become established in units. Following pre-decay, units were disassembled, clea...
Mick Hedley, Dave Page, Jackie van der Waals
Degradation of Carbon-Based Preservatives by Black-stain Fungi
2010 - IRG/WP 10-30533
Some black-stain fungi are known to exhibit resistance to carbon-based preservatives. However, the cause of this resistance is unclear. The fungi may have mechanisms to tolerate these chemicals, or they may be able to degrade and detoxify them. Fungi capable of degrading carbon-based preservatives are of interest for possible bioremediation of carbon-based preservative-treated wood at the end of i...
R Stirling, P I Morris
A Comparison of the Performance of Related Copper Based Preservatives against Soft Rot
2010 - IRG/WP 10-30540
The performance of pine and beech wood treated with either a soluble copper + quat (ACQ type D) preservative system or a particulate copper + quat system was evaluated in unsterile soil using the European standard ENV 807 soft rot decay test procedure.
In addition, to compare soft rot performance of soluble and particulate copper directly without the influence of co-biocides, beech and pine test...
M Ray, D Dickinson, K Archer
Studies on Effect of pH on Copper Availability in Copper-Based Preservatives
2010 - IRG/WP 10-30549
Laboratory methods have been employed to investigate the pH effect on the copper solubility of basic copper carbonate. The pH was controlled using two different approaches. One was with the adjustment of pH of the solutions by acid or base using sulfuric acid or sodium hydroxide until the solution equilibriums were obtained for each defined pH. A second approach was to control pH with buffer sol...
L Jin, P Walcheski, A F Preston
Evaluation of formulation type on the efficacy of bifenthrin as a glueline termiticide for veneer based wood products
2010 - IRG/WP 10-40486
Field trials were carried out in Australia on Coptotermes acinaciformis to evaluate the efficacy of various bifenthrin formulations. One trial tested plywood made by Zelam at their research facility in New Zealand and compared three emulsifiable concentrate formulations (EC), a suspension concentrate (SC) and an encapsulated formulation (CS). A second trial compared laminated veneer lumber (LVL)...
P Lobb, A Siraa
Extruded wood plastic composites based on ACQ and MCQ-treated wood materials
2010 - IRG/WP 10-40495
This paper deals with wood plastic composites manufactured using ACQ and MCQ-treated wood fibers recovered from a wood treatment plant. The goal was to investigate the effect of coupling treatments on the properties of manufactured wood plastic composites (WPCs) through injection molding and to manufacture co-extruded WPC with treated wood fibers. The result demonstrated sound mechanical propertie...
Qinglin Wu, Fei Yao, K Ragon, J Curole, M Voitier, T Shupe
Silicon compounds as additives improving alkyd-based wood coatings performance
2010 - IRG/WP 10-40531
The reactivity of cellulose with solvent-born alkyd-based wood coatings supplemented with organosilanes was analyzed. Structural analysis of cellulose subjected to the reaction with organosilanes and following extraction with water was performed using Fourier-transform infrared spectroscopy (FTIR). The analyzed IR spectra comprise bands 1250 cm-1 typical for the SiC group and 800 cm-1 typical for ...
B Mazela, I Ratajczak, K Wichłacz-Szentner, P Hochmańska
Effects of intumescent formulation of vinyl acetate-based coating on flame-retardancy of thin painted red lauan (Parashorea spp.) plywood
2011 - IRG/WP 10-40537
Using intumescent coatings on wood-based materials is an effective method for fire safety. The intumescent coatings consist of four major components: (1) binder resin (BR), (2) carbonizing substance (CS), (3) foam producing substance (FPS) and (4) dehydrating agent (DA). Previous studies have demonstrated that the formulation of the four components strongly influences the performance of coatings. ...
Chih-Shen Chuang, Kuang-Chung Tsai, Te-Hsin Yang, Ming-Kuang Wang, Chun-Han Ko
Increased sustainability for wood construction by recycling
2011 - IRG/WP 10-50275
Wood is the only renewable and certified industrially available construction material that has also unique opportunities as carbon storing, energy-independent and generally approved resource. However, if burning into energy is not counted, there are only few viable and competitive solutions for re-use or recycling of various wood products. The biggest challenge related to recycling of wood product...
H Heräjärvi, I Pirhonen, T Räty, P Saukkola
Influence of wood swelling agents on penetration and copper leaching of copper-ethanolamine based wood preservatives
2011 - IRG/WP 11-30556
Copper ethanolamine based preservatives are currently the most important solutions for impregnation of wood in ground contact in Europe. One of the issues related to those and similar water based solutions is insufficient penetration to refractory wood species like Norway spruce. In order to elucidate this issue, commercial copper ethanolamine based solution was supplemented with five different wo...
M Humar, N Thaler, B Lesar
Novel Approaches to the Development and Testing of Anti After-glow Additives for CCA-based Treatments of Poles
2011 - IRG/WP 11-30561
In this paper, a field fire stake testing screen method is described. This method uses stake samples from matched wood sources allowing replicates from different boards to be included. The method is easy to control and can provide quick comparative fire resistance test results. The parameters measured from the tests are percentage weight loss, minimum residual circumference and residual thicknes...
L Jin, P Walcheski, A Preston
Effectiveness of Water Based Bentonite-Borate Slurry for In-situ Remedial Protection of Historic Wooden Piles: The Eurobor Protocol, Part 2
2011 - IRG/WP 11-30574
The study of the biocide product Eurobor®, water mixture of boric acid, borax and sodium bentonite, aimed to verify previous findings regarding borates penetration from a clay-water mixture of foundation timber. The product was applied on samples from 100 year old timber foundation from the city of Göteborg. Although in ground for this long the timber was in acceptable god condition due to groun...
M. Theorin, K. Fimmerstad, K-M. Bandh
The potential of silicone-based formulations to enhance wood properties through industrial treatment for outdoor use
2011 - IRG/WP 11-30578
High hygroscopicity is one of the main weaknesses of wood as far as its susceptibility to biodegradation, and specifically to fungal decay. New wood preservation technologies are constantly entering the wood protection market, competing with traditional, biocide-based preservation. Silicones are commercially used as hydrophobic agents on stones and concrete. They belong to the restricted number of...
F Simon, F Marchal, F Pochon, M Kutnik, I Le Bayon