The influence of fungi causing blue – stain on absorptiveness of Scotch pine wood
2005 - IRG/WP 05-10565
The blue-stain fungi cause discoloration of the wood. In the course of their development in wood may have an effect on wood structures and properties influenced on its use value. Investigation has been undertaken to clear the influence of blue-stain fungi on wood absorptiveness as indicators for the wood ability to impregnation with water diluted wood preservatives. The wet sapwood samples of fres...
A Fojutowski


Laboratory and Pilot Evaluation of Chlorothalonil Formulations for Mold and Stain Control on some Wood Species
2003 - IRG/WP 03-30317
Laboratory and pilot test of the efficacy of several fungicides such as chlorothalonil and carbendazim for control of mold and sap- stain on bamboo and slash pine and rubberwood were conducted in this paper. The result indicates that: -- Clorothalonil/carbendazim are more effective for controlling mold and stain than that of carbendazim alone in laboratory test. --Higher concentration at 0.1-0.2...
Mingliang Jiang, Zhaobang Li


Mold and stain fungi associated with Radiata pine logs imported from New Zealand
2000 - IRG/WP 00-10346
The Korean sawmills have recently realized the importance of prevention of fungal discoloration due to increased losses in revenue. Before establishing integrated control strategies of fungal discoloration, more complete knowledge about causal organisms is needed. As a first step, we initiated a through survey of mold and stain fungi colonized commercially important softwood species (Pinus densifl...
Jae-Jin Kim, Gyu-Hyeok Kim


Blue stain in timber in service. Results of further IRG collaborative tests to compare different artificial weathering systems
1981 - IRG/WP 2146
The previous work described in Document No IRG/WP/286 examined 3 preservatives (1% phenyl mercury succinate - PMS, 5% pentachlorophenol - PCP and 1.5% Preventol A4 - PA4) subjected to 5 different artificial weathering systems (BAM Xenotest, Cuprinol Marr, EMPA Xenotest, Gori Atlas and PRL Marr) and after natural weathering at 5 sites (BAM, Cuprinol, EMPA, Gori and PRL). Results showed good correla...
A F Bravery, D J Dickinson


Susceptibility of painted wood to discolouring fungi - influence of binder, solvent and surfactant
1992 - IRG/WP 92-3714
Previous studies have shown that the basic composition of paints, without fungicide addition, can significantly contribute to the varying microbial susceptibility of painted wood. Previously, non-weathered water-borne acrylic paints applied to wood without a primer were shown to be more susceptible to mould attack than solvent-borne alkyd paints. The present study was initiated to reveal if this d...
J Bjurman, C Herder


The selected properties of Scots pine wood blue-stained by fungus Cladosporium herbarum
2003 - IRG/WP 03-10484
The fungi causing primary blue-stain of wood may change wood properties especially when acting in mixture of few fungi species. There were been undertaken investigation to clear the influence of pure culture of one fungus species on selected physical and mechanical properties of Scots pine wood. The twin samples of fresh cut Scots pine sapwood (Pinus sylvestris L.) were exposed into pure culture o...
A Fojutowski


Comparison between two laboratory test methods for determining the effectiveness on wood preservatives against blue stain in fresh wood
1987 - IRG/WP 2289
Most of the work done on determination of the effectiveness of new formulae for treating fresh wood against blue stain have been focussed on their use in the manufacture of saw timber. This work explains two laboratory methods, one which simulates the working and climatological conditions of factories making packages for fruit and vegetables in the Spanish Levante, showing that contamination of wo...
A M Navarrete, M T De Troya


Effect of climate, species, preservative concentration and water repellent on leaching from CCA-treated lumber exposed above ground
2001 - IRG/WP 01-50178
Few studies have examined leaching of chromated copper arsenate (CCA) from treated wood in above ground exposures due to the assumption that leaching is less severe compared to wood in continuous contact with soil or water. However, a significant portion of CCA treated wood is used for above ground applications, exposing considerable volumes of the preservative to precipitation and potential leach...
J L Taylor, P A Cooper


Evaluation of chlorothalonil for stain and mould control on lumber
1992 - IRG/WP 92-3713
Chlorothalonil is a commercially important fungicide with many industrial and agricultural applications. It has a very low mammalian toxicity and is considered to be an environmentally benign material. This paper describes the laboratory evaluation of chlorothalonil as a wood antisapstain treatment. Chlorothalonil was tested as three formulation types - an emulsifiable concentrate (EC), a water-ba...
P E Laks, T L Woods, D L Richter


Blue stain in service on wood surface coatings. Part 1: The nutritional requirements of Aureobasidium pullulans
1992 - IRG/WP 92-1556
The nutritional requirements of Aureobasidium pullulans was examined with regard to nutrient sources that are potentially available in fresh and weathered wood. The study was designed to determine how far wood cell wall components need to be broken down during weathering before they provide a useful nutrient source for Aureobasidium pullulans. Various carbon sources were tested, with eight differe...
P R Sharpe, D J Dickinson


Laboratory studies on control of sapstain and mold on unseasoned wood by bacteria
1991 - IRG/WP 1493
A malt-agar and nonagar laboratory test was used to evaluate the efficacy of bacterial preparations as biological control agents against several sapwood-inhabiting fungi. Both nonsterilized and filter sterilized bacteria preparations prevented attack by the sapwood-inhabiting fungi. Streptomyces rimosus was the most effective bacteria, giving good protection, with a 1-hr soak in a filter-sterilize...
T L Highley, R Benko, S C Croan


Effectiveness of some microbiocides against the development of molds and sapstain in Pinus elliottii
1981 - IRG/WP 3169
Eleven commercial biocidal formulations were tested in the field to determine their effectiveness in protecting logs and lumber of Pinus elliottii sapwood from sap stain and molds. Among these formulations 2-(thiocyanomethylthio) benzothiazole showed the best performance in controlling both types of fungi. Potassium N-hydroxymethyl-N-methyl dithiocarbamate and the mixture potassium N-methyl dithio...
S Milano


Observations on the destruction of fishing craft in India by marine wood-borers with special reference to the West Coast
1981 - IRG/WP 468
The paper highlights the economic importance of the destruction of fishing craft in India by marine wood-destroying agencies. The annual loss involved is to the extent of over 94 million rupees. Thirty-nine spectes and one variety of woodborer have so far been recorded from India, of which Bankia campanellata, Bankia carinata, Bankia rochi, Dicyathifer manni, Lyrodus pedicellatus, Teredo clappi, T...
L N Santhakumaran, J C Jain


Sapstain development on Jack pine logs in Eastern Canada
2000 - IRG/WP 00-10358
During 1998-99, a study was initiated to investigate the influence of seasons, log types and storage time on the sapstain development on jack pine logs at two sites in Eastern Canada. Jack pine trees (Pinus banksiana) were harvested into whole-tree and cut-to-length logs in spring and in autumn. Sapstain development was examined in these logs at 2 to 4 week intervals after felling. The mean stain ...
Dian-Qing Yang, R Beauregard


Performance of Tuff Brite C™ and other formulations against blue-stain, mold and brown-stain in freshly-sawn rubberwood (Hevea brasiliensis) in the humid tropics of Peninsular Malaysia
1997 - IRG/WP 97-30163
The relative anti-sapstain and anti-mold efficacies, including brown-stain development in freshly-sawn rubberwood (Hevea brasiliensis) in the Malaysian tropics, between selected water-based product concentrations of formulations Tuff Brite CTM without/with added Borax (at 1.5/0, 1/1.5, 1.5/1.5 and 2%/1.5%), PQ8TM without/with added Borax (at 2.5/0, 1.5/1.5, 2/1.5 and 2.5%/1.5%) and NeXgenTM/NeX-Br...
A H H Wong, T L Woods


A field test with anti-stain chemicals on sawn pine timber in Brazil
1989 - IRG/WP 3513
Field tests were carried out in São Paulo State - Brazil, to evaluate pre-treatment formulations of O-Phenyl-Phenol (OPP) based products. The Sodium Pentachlorophenate solution was used as a reference formulation. The treated test blocks were stacked in a covered shed, and in an uncovered place for air drying. The evaluation was done by measuring the percentage of stained surface on each test blo...
M B B Monteiro, S Brazolin


Reduction of kiln brown stain in radiata pine lumber after log fumigation with methyl bromide
1997 - IRG/WP 97-30129
Methyl bromide fumigation of freshly felled radiata pine log sections effectively killed living cells in parenchyma to at least 75mm into sapwood. Lumber cut from logs (fumigated and control) stored 1 month outdoors (dry) showed slightly reduced brown stain when kiln dried at conventional temperatures. A more dramatic reduction and elimination of brown stain was noted in lumber cut from fumigated ...
E Schmidt, M E Hedley, D R Page, D Cross


Artificial weathering as an aid to assessing the effectiveness of chemicals for preventing blue stain in service - a co-operative study
1984 - IRG/WP 2215
The paper reports co-operative studies carried out within Working Group II of the International Research Group on Wood Preservation to assess the effects of different artificial weathering systems on the performance of fungicides to control blue-stain in service. It has been shown that Atlas, Xenotest and Marr equipments operated according to particular standard schedules can give essentially the ...
A F Bravery, D J Dickinson


Screening of modified linseed oils on their applicability in wood protection
2004 - IRG/WP 04-30346
In this study modified linseed oils, rape oil and three waxes were screened on their efficacy as wood protecting agents. By testing all products when impregnated with high retentions in Scots Pine sapwood on water repellence qualities, additionally an accelerated weathering test, drying quality, accelerated brown rot and blue stain test, an indication is formed of the capability of these products ...
A Treu, J Lückers, H Militz


Marine wood-borer test with preservatives on the coasts of Turkey
1995 - IRG/WP 95-10091
Marine wood-borer tests were carried out on the coasts of Turkey (Marmara, Mediterranean Sea and Black Sea). Sapwood blocks of 8 x 15 x 30 cm³ in size from Scots pine, Bornmüller's fir oriental beech and sessile oak were used. The test blocks were treated with CCB-salts by full cell process and coal tar creosote by empty cell process. The test blocks were installed on exposure sites bef...
A Bobat


Evaluation of the effectiveness of defence anti-stain in the control of sapstain in laboratory and field tests
1990 - IRG/WP 3593
The anti-sapstain product Defence Anti-stain (DAS) has been evaluated internationally in laboratory and field tests during the years 1988 and 1989. Results of tests carried out by institutes and by own companies in countries like Indonesia, Ivory Coast, Japan, Portugal, Belgium, The Netherlands and Spain will be presented. In the several tests Defence Anti-stain showed a high fungicidal activity t...
G Rustenburg, C J Klaver


The relationship between blue-stain and bark beetles
1971 - IRG/WP 19
The attack of bark beetles on standing or in newly-felled stems provides special growth conditions to wood-inhabiting fungi. In the wood attacked by bark beetles, a specific and rich fungus flora is found, and from these fungi the economically important group of blueing fungi has been more thoroughly investigated. These fungi live on nutritive substances present in the cells, especially in the med...
A Käärik


Molecular phylogeny of Ophiostoma spp. related to blue-stain in pine
2002 - IRG/WP 02-10432
Blue-stain in coniferous woods is an economically important disease in many temperate countries, caused specially by genus Ophiostoma. Classical taxonomy of genus Ophiostoma is limited for the correct identification of many species, because of the similar macroscopic and microscopic characters, as well as the existence of some species complex. Molecular identification is a good complement to eluci...
M Villarreal, F Arenal, J Sánchez-Ballesteros, M T De Troya, F Llinares, V Rubio, A Navarrete


Suitability of propiconazole (R 49362) as a new-generation fungicide
1989 - IRG/WP 3529
Propiconazole (R 49362), an anti-fungal triazole-compound of Janssen Pharmaceutica, has been extensively tested to determine its potential use as a wood preserving fungicide. Various tests in both private laboratories and official institutes indicate a good activity against Basidiomycetes (brown and white rot) and Ascomycetes (blue stain-in-service). The active ingredient seems very resistant to w...
A R Valcke


The susceptibility of acetylated Pinus radiata to mould and stain fungi
1992 - IRG/WP 92-1548
The aim of this investigation was to determine the effect of 5, 10, 15 and 20 percent acetylation weight gains on the susceptibility of Pinus radiata sapwood to mould and stain fungi, and to establish if an acrylic paint, an oil-based stain and a water repellant gave superior protection from fungal growth on wood treated to 20% acetylation weight gain, compared to untreated wood. One treatment set...