IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 792 documents. Displaying 25 entries per page.


Heat treatment of wood strands for OSB production: Effect on the mechanical properties, water absorption and dimensional stability
2002 - IRG/WP 02-40238
The effect of heat treatment on the mechanical and physical properties of commercial OSB strands was evaluated. Heat treatment was applied under inert atmospheric conditions to wood strands. The aim of this study was to examine the heat treatment parameters to achieve significant reduction of thickness swelling (upon exposure to moisture in service) without causing excessive reductions in stren...
G J Goroyias, M D C Hale


Investigation of some technical properties of heat-treated wood
2003 - IRG/WP 03-40266
The objective of this study was to investigate some technical properties of heat-treated wood. Wood heat-treated according to a process intended for wood in above-ground end-uses (European hazard class 3) was subject to the following: · A delamination test according to EN 391 with glulam beams made of heat-treated pine (Pinus sylvestris) and spruce (Picea abies) laminations, assembled with PR...
C Bengtsson, J Jermer, A Clang, B Ek-Olausson


Novel wood modification processes for window and cladding products
2004 - IRG/WP 04-40285
Because of the low natural durability and low dimensional stability of European wood species, the usage of wood for window frames has decreased dramatically during the last decade. In a joint project of several German research institutes and the window industry, following wood modification systems were compared. heat treatment (3 different materials from 2 companies) acetylation (pine sapwood an...
A Krause, C Hof, H Militz


Effects of heat treatment on water repellence and anti-swelling efficiency of beech wood
2002 - IRG/WP 02-40223
The heating of solid wood to higher temperatures is the simplest and the cheapest means for stabilizing its dimensions. For the investigation of the effect of thermal treatment on water repellency effectiveness and anti-swelling efficiency of beech wood (Fagus orientalis Lipsky), air-seasoned samples of beech wood were heated in presence of air at temperatures of 130 C, 150 C, 180 C and 200 C for ...
S Yildiz


Study of the degradation of retified wood through ultrasonic and gravimetric techniques
1994 - IRG/WP 94-40030
One of the non-polluting processes that increase the natural durability of wood is a thermal treatment in an atmosphere poor in oxygen, producing what is normally denominated "retified wood". In this study the validity of a non-destructive technique (ultrasound) in order to determine the biodegradation suffered by wood across time has been studied. For this reason, the behavior of a wood species (...
D T De Troya, A M Navarrete


Thermal modification of non-durable wood species 1. The PLATO technology: thermal modification of wood
1998 - IRG/WP 98-40123
The PLATO technology is an innovative upgrading technology with low environmental impact, which can be applied to fast grown and non-durable wood species. This technology is based on a thermal modification of solid wood without the addition of chemicals (e.g. preservatives), consisting of a hydrothermal treatment, followed by drying and curing. The PLATO technology results in a substantial improve...
M J Boonstra, B F Tjeerdsma, H A C Groeneveld


Behaviour of some selective Indian species towards treatment with solvent based water repellent preservative
1984 - IRG/WP 3309
This paper discusses a solvent based preservative using PCP and a water repellent for preserving three species of timber commonly used in India for the manufacture of doors and windows. It examines the method of treatment to achieve desired levels of penetration and retention of the preservative-cum-water repellent, and tests made on these timbers to examine the success of the processing methods a...
V R Sonti, B Chatterjee


Lethal temperature for some wood-destroying fungi with respect to eradication by heat treatment
1984 - IRG/WP 1229
The lethal heat dosis as a function of temperature and time of exposure has been tested for mycelium and for wood infested by three strains of Serpula lacrymans and by Coniophora puteana, Poria monticola, Paxillus panuoides, Gloeophyllum trabeum and Gloeophyllum sepiarium. Even for Serpula lacrymans, which is well known for its sensivity to heat treatment, 30 min at 55°C were necessary to kill th...
M Miric, H Willeitner


Kiln drying of poles as a means of solving the problems of pre-treatment decay in poles
1985 - IRG/WP 1263
The concept that pre-treatment decay can cause wide variation in the treatability of wood and especially wood poles has caused much discussion and debate in wood preservation circles. Yet it seem only logical that if decay has effected the strength characteristics of the wood and caused a differential moisture content in the wood the treatment of the end product will be highly variable and the lon...
J A Taylor


Durability of heat-treated wood
1999 - IRG/WP 99-40145
Heat-treated wood from the French process were laboratory tested against decay using agar block test and a modified soil block test. Water absorption, bending strength, lignin content and acid number were also determined to evaluate the effect of heat treatment. Heat treated samples exhibit a higher lignin content and a lower acid number compared to untreated control indicating the degradation of ...
D P Kamdem, A Pizzi, R Guyonnet, A Jermannaud


Interim balance after 20 months of lap-joint exposure
1999 - IRG/WP 99-20164
The application of natural resins and integrated resin systems to improve the performance of Pinus sylvestris was assessed in a lap-joint test according to DIN V ENV 12037 (1996). Lap-joints of Pinus sapwood were exposed at the test field in Hamburg (Germany) in May 1997. The treated lap-joints were assessed with regard to the performance of the resin treatments out of ground. The exposure of lap-...
M Sailer, A O Rapp, R-D Peek, A J Nurmi, E P J Beckers


Evaluation of outdoor weathering performance of modified wood
2004 - IRG/WP 04-20296
Interlace treated, oil treated, silicon treated as well as untreated Scots pine samples have been exposed outdoors. For evaluating the samples on their long term performance an internal standard had been developed. Parameters to be determined were the uptake of liquid water (submersion test), weight variation during exposure, crack performance, surface roughness and colour change. This paper disc...
Y Schulte, S Donath, A Krause, H Militz


Investigation of the suitability of silver fir (Abies alba Mill.) for thermal modification
2004 - IRG/WP 04-40275
In this study the suitability of silver fir (Abies alba Mill.) was examined for thermal modification. Comparative experimental investigations were performed with silver fir and Norway spruce (Picea abies Karst.) after thermal treatments. Besides properties, which characterize the quality of heat treatments, like dimensional stability and resistance against fungal attack, strength properties of the...
C Brischke, A O Rapp


Durability aspects of (hydro)thermal treated wood
2000 - IRG/WP 00-40160
Samples of several wood species were treated in a two steps process, subsequently hydrothermal and dry heat-treated, by the so-called PLATO-process and analysed for their resistance against fungal attack. Both PLATO-treated and dry heat-treated specimen were prepared and analysed, in order to study the influence of moisture during hydrothermal treatment of wood. The resistance against all of the s...
B F Tjeerdsma, M Stevens, H Militz


Thermal modification of non-durable wood species 2. Improved wood properties of thermal treated wood
1998 - IRG/WP 98-40124
Properties of wood treated in a new heat-treatment process called the PLATO-process have been studied. Several wood species have been treated using this new thermal modification process using a range of process conditions (mainly time and temperature). In this study the characteristics of the treated wood were determined using samples from whole planks treated on pilot plant scale. The modified ch...
B F Tjeerdsma, M J Boonstra, H Militz


Effects of heat treatment on modulus of elasticity of beech wood
2002 - IRG/WP 02-40222
Heat treatment is the oldest, simplest and cheapest method for reducing hygroscopicity of wood. The heat treatment protects wood against to biological organisms as well as giving wood dimensional stabilization without damaging environment. The effects of heat treatment on modulus of elasticity (MOE) of beech wood (Fagus orientalis Lipsky) naturally grown and intensively used in forest products in...
S Yildiz, G Çolakoglu, Ü C Yildiz, E D Gezer, A Temiz


Basidiospore structure and germination of Serpula lacrymans and Coniophora puteana
1988 - IRG/WP 1340
Using a nuclear staining technique and fluorescence microscopy, the basidiospores of Serpula lacrymans were shown to be uninucleate whereas those of Coniophora puteana were binucleate. The germination rate of the Serpula lacrymans spores, which was considerably lower than that of Coniophora puteana, decreased further after storage or heat treatment. Transmission electron micrographs indicate that ...
B M Hegarty, U Schmitt


Heat inactivation of mould fungi on wood
1993 - IRG/WP 93-40012
Heat treatments have been successfully used for eradication of dry rot. The effect of heat treatments at 40, 50 and 60°C for various time intervals on the inactivation of Penicillium brevicompactum was determined. The effect of heat on ungerminated spores and spores "pregerminated" for 24 hours was evaluated by plating on malt-extract agar. Although most ungerminated spores were inactivated after...
J Bjurman


New experiences with Dry Rot in Danish buildings, heat treatment and viability tests
1989 - IRG/WP 1423
An increasing number of concealed dry rot attacks, especially in older multi-storey houses under renovation, have been detected during the last few years. A necessary consequence is a demand for cheaper methods of repair, compared to the standard method used in Denmark for many years otherwise severely attacked houses will by pulled down. A heat-treatment has been developed and tested in practice....
A P Koch, C Kjerulf-Jensen, B Madsen


Biological resistance of steam-compressed wood pretreated with boric compounds
1999 - IRG/WP 99-30190
Wood compression under heating is aimed to enhance dimensional stability and surface hardness. Preservative treatment with an appropriate chemical is additionally required for the protection of wood against biological agents under hazardous service conditions. Boron pretreatment of compressed wood was targeted to a mutual benefit of increasing biological resistance of compressed wood as boron was ...
M K Yalinkilic, W Dwianto, Y Imamura, K Tsunoda, M Takahashi


Comparison of thermally modified wood originating from four industrial scale processes – durability
2002 - IRG/WP 02-40229
This study examined the differences in biological wood properties of heat treated wood originating from four different European industrial heat treatment plants. The manufacturers of heat treated material were: PLATO Hout B.V./Netherlands, Thermo Wood/Finland, New Option Wood/France and Menz Holz/Germany where Oil-Heat treated Wood (OHT) is produced. The results of miniblock tests with basidiomyc...
C R Welzbacher, A O Rapp


The effect of heat treatment on the properties of spruce
1994 - IRG/WP 94-40032
The effect of high temperature treatment (above 150°C) on the wood quality is studied at the VTT. Improved dimensional stability, lower equilibrium moisture content and increased durability against biodeterioration is achieved, depending on the environmental factors. The biodeterioration resistance of spruce is improved due to changes in chemical composition and lower equilibrium moisture content...
H Viitanen, S Jämsä, L Paajanen, A J Nurmi, P Viitaniemi


Chemical treatment of chips for outdoor storage. Evaluation of sodium N-methyldithiocarbamate + sodium 2,4-dinitrophenol treatment
1980 - IRG/WP 2134
Fresh slash pine chips were treated by spraying them with a dilute aqueous solution of sodium N-methyldithiocarbamate and sodium 2,4-dinitrophenol. The were then formed into an experimental chip file 10 feet high, and the pile was maintained for seven months. The treatment effectively slowed heat release and retarded losses in wood substances, tall oil, pulp yield, and pulp strenght. Under certain...
E L Springer, M Benjamin, W C Feist, L L Zoch, G J Hajny


Dimensational stabilisation of wood
1981 - IRG/WP 3171
A review is given of the studies on the dimensional stabilisation of wood which have been carried out in the laboratory 5.14 "Wood Technology" since 1967. All stabilisation methods known have first been compiled from the available literature. Practical studies were then started. Wood was treated with monomers (styrene, methyl metacrylate, isocyanate), formaldehyde, tannin and sugar. Despite a sati...
A Burmester


Effects of steaming heat treatment of wood on the stimulation of termite feeding
1997 - IRG/WP 97-10212
At the 26th IRG conference, we reported that steamed Japanese larch heartwood samples were suffered a serious attack by subterranean termite, Coptotermes formosanus both in choice and no-choice feeding tests. This is possibly caused by the yield of termites stimulants in the wood samples resulting from the steaming process. Since the steaming heat treatment has often been applied to other several ...
S Doi, Y Kurimoto, M Takahashi, T Yoshimura


Previous Page | Next Page