Your search resulted in 3797 documents. Displaying 25 entries per page.
Comparative Laboratory Leaching Test Methods to Study Post-Treatment Storage Period Impacts on CCA Leachability and Fixation in Treated Kempas (Koompassia malaccensis) Heartwood
2007 - IRG/WP 07-20376
Three laboratory leaching test methods were compared to determine the effects of different post-treatment storage fixation periods on leachability/fixation of CCA components from treated kempas (Koompassia malaccensis) permeable heartwood. End-sealed test wood blocks of permeable were treated with CCA to target retention of 5.6 kg/m3, immediately stored to fix at ambient conditions for 0 and 48 ho...
A H H Wong, H C Lai
Performance of softwood preservative treated stakes after 4 years exposure in-ground to decay fungi and termites in tropical Australia
2008 - IRG/WP 08-10643
This field study was based on the 1993 IUFRO method and designed as a graveyard (in-ground) test in the tropical region of the Northern Territory to examine the efficacy of novel preservative formulations developed as alternative protection for softwood timber against decay fungi and termites for Hazard Class 3 and 4. This study was supported by the Forest and Wood Products
Research and Develop...
B M Ahmed (Shiday), J R J French, S R Przewloka, P Vinden, J A Hann, P Blackwell
Relationship between coating properties and their performance on treated wooden decks
2008 - IRG/WP 08-30454
Preservative treated wood benefits from the application of a surface coating to protect it from weathering (UV and rain). Different preservative formulations may affect surface properties of treated wood differently; therefore compatibility of coatings with different preservative treated wood types should be considered. This paper examines coatings characteristics and their weathering performance ...
M Ahmadinejad, P A Cooper
Field Trial of Copper Treated Moso Bamboo in Southern China
2008 - IRG/WP 08-30455
The field trial of moso bamboo treated by 9 copper preservatives for 5 years in Guangzhou was conducted in the paper. The result shown that: two ammonia based copper azole formulations F17/F18 and 1 amine copper formulation with boron F10, as well as 2 ammonia based ACQ, at the copper retention of 3.2 kg/m3 or above, have good resistant for decay and fine resistant for termites after 5 year field ...
Mingliang Jiang
Influence of Polyvinyl acetate emulsion (PVA) on boron leaching and fungicidal properties
2008 - IRG/WP 08-30451
Boron compounds are very effective fungicides, but unfortunately they leach from wood. In order to improve boron fixation, boric acid, borax were combined with polyvinyl acetate emulsion (PVA). For comparison copper salts were included into this research as well. Selected preservative solutions were chosen for impregnation of Norway spruce wood specimens (Picea abies). Wood blocks were exposed to ...
M Humar, B Lesar, P Kralj
Preliminary evaluation of efficacy of copper in combination with boron and NHA (N'-N-(1, 8-naphthalyl) hydroxylamine) against wood decay
2008 - IRG/WP 08-30452
In this study, efficacy of various combinations of copper sulfate with either boric acid or calcium precipitating agent, NHA-Na (N'-N-(1, 8-naphthalyl) hydroxylamine) was evaluated. Wood specimens were treated with either 1%, 0.5%, or 0.1% concentrations of copper sulfate, boric acid, NHA-Na, copper sulfate + boric acid, or copper sulfate + NHA-Na mixtures. Treated specimens were subjecte...
E Terzi, C Köse, S N Kartal
Above and Below-Ground Copper-Azole and Copper, Chrome Arsenate Depletion from Pinus radiata and Fagus sylvatica at Thirteen New Zealand & Australian Sites
2008 - IRG/WP 08-30460
The objective was to determine the significance of site on preservative depletion from Pinus radiata D. Don and Fagus sylvatica L. 20 x 20 x 500 mm field test stakes treated with a ground contact retention of copper amine plus tebuconazole (CuAz) and copper chrome arsenate (CCA) after approximately 5 years exposure to widely different soil and climate conditions. Site, wood species and their inter...
R Wakeling
The role of chromium in wood preservatives under BPD - a review and the current situation in Europe
2008 - IRG/WP 08-30468
Already during the IRG-meeting in Trømso a paper was presented to give an overview regarding the situation on chromium (JÜNGEL et al. 2006). Already in that year there was an increased attempt to achieve a science-based correct and harmonised solution in Europe regarding the chromium-question by the European Commission. Nevertheless the competent authorities (CAs) and the industry were similarly...
P Jüngel, S Hellkamp
Accelerated fixation of ACQ-D treated Chinese fir with different post-treatments
2008 - IRG/WP 08-40400
With the enhanced focus on the environmental impact of the preservative-treated wood in recent years, it is necessary to perform some post treatments to prevent contamination of soil and ground water and reduce copper losses from ACQ treated wood in service. In this study, the potential of hot air, hot water, steaming and microwave post treatments to accelerate the fixation of copper in ACQ-D trea...
Lili Yu, Jinzhen Cao, P A Cooper
Termite resistance of DMDHEU-treated wood
2008 - IRG/WP 08-40401
Chemical wood modification with dimethyloldihydroxy-ethyleneurea (DMDHEU) or its derivatives are applicable to both solid lumber and wood-based composites. Advantages of DMDHEU-based modification are an increase of dimensional stability and high durability against white, brown and soft rot fungi. At higher chemical loadings, the hardness of the wood is considerably increased. Due to the durabil...
H Militz, S Schaffert, B C Peters, C J Fitzgerald
Effects of Murgul Copper Process flue gases (SO2) on compression strength parallel to the grain of Beech (Fagus orientalis Lipsky.) wood
2008 - IRG/WP 08-40404
In this study was investigated the effect on the compression strength parallel to the grain as mechanical properties of Fagus orientalis Lipsky. wood exposed to SO2 gas and non-exposed.
In the experiments the two of four (total) were obtained from Artvin-Ortaköy region and the other two from Artvin-Murgul region. The compression strength parallel to the grain was calculated at the compare of ...
N Ay, E Topaloglu, A Uncu
Effects of planning and sanding on penetration and retention properties of some softwood species treated with copper azole
2008 - IRG/WP 08-40410
This work investigates the effect of some woodworking treatments on penetration and retention properties of four different (scotch pine—SP, Siberian scotch pine—SSP, Siberian larch—SL, and oriental spruce—OS) heartwood species with the waterborne preservative copper azole (CBA-A). A 2.4% active ingredient solution of CBA-A was applied for use in vacuum/pressure treatment of the heartwood s...
Ü C Yildiz, S Yildiz
Measurement of wood decay by dynamic MOE in an accelerated soil contact test
2008 - IRG/WP 08-20390
Current laboratory and field testing of preservatives involves various techniques to determine the extent of fungal attack, including visual inspection, mass loss, and static bending and compression strength measurements. The objective of this study was to compare decay measurement by conventional compression strength versus dynamic MOE, employing small wood stakes in an accelerated laboratory so...
Gan Li, D D Nicholas, T P Schultz
Effectiveness of MOQ® OX 50 (CCB-Oxide) wood preservative – Part 2: Field tests
2008 - IRG/WP 08-30483
MOQ® OX 50 is a chromated copper borate preservative known around the world as CCB. In Brazil, this product is the only CCB-oxide type preservative with fungicide and insecticide properties registered at the Brazilian Institute for the Environment and Renewable Resources (IBAMA) that complies with the requirements of the Brazilian and European markets for preserved wood. For over five decades, s...
A Gandolfi Jr, C Salvela, D R Macedo, J M Vidal
Polymeric Betaine as a Wood Preservative
2008 - IRG/WP 08-30487
Didecyl polyoxyethyl ammonium borate (DPAB), also known as Polymeric Betaine, was developed as a co-biocide for chromium-free copper based wood preservatives in Europe in the 1980’s. This paper summarizes the properties of DPAB as a wood preservative. Unique properties related to the betaine nature of DPAB are discussed in terms of the structure-property relationship. Physical properties of D...
H Härtner, S Schmitt, Futong Cui, H M Barnes
Performance of dip and pressure treated wood in termite ground proximity exposures in Hilo, HI, and Colombia
2008 - IRG/WP 08-30491
A number of preservative systems were evaluated for their ability to control termite attack when applied as both dip and pressure treatments. With dip treatments, better performance was observed with southern pine than spruce-pine-fir using the same solution strength treatment, probably as a result of the about 50% greater uptake with southern pine and associated deeper preservative penetration. B...
P Walcheski, A Zahora
High Temperature Treated Wood
2008 - IRG/WP 08-40429
High temperature can modify internal structure and physic-chemical properties of wood by a controlled pyrolysis process. Such treatment, among other changes in properties, modifies the wood color in a way that resembles exotic species, increasing its market value. The main objective of this work is to determine the changes in wood properties caused by the effect of temperature and time, in order t...
C C Borges, A L Barbosa, R Faber de Campos, S T Targas
Field Stake Performance of Parallel Strand Lumber Treated with Waterborne Copper Naphthenate
2008 - IRG/WP 08-40435
Wood and wood products have been considered a premium building material for residential and industrial structures for many centuries. More recently, structural composite lumber (SCL) products have played an increasing role in satisfying the needs of the building industry. However, both wood and wood composites are naturally biodegradable materials which require enhanced durability when used in ce...
G P Merrick, M H Freeman, J A Brient
Wood preservative obtained by recycling – preliminary selection of leaching inhibitor
2008 - IRG/WP 08-50252
Based on recycling of used household batteries, a process was developed to enable the recovery of major manufacturing components, leading to a solution of zinc (32 g.l-1) and manganese (15 g.l-1) salts, free of heavy metals. The potential use of the above solution as wood preservative was demonstrated by means of assays both of fungicidal activity -using white and brown rot fungi- and of insectici...
C Ibáñez, C Mantero, G Cecchetto, M Rabinovich, M Cerdeiras
Evaluation of Water Repellency of Treated Wood Using Several Alternative Methods
2009 - IRG/WP 09-20419
In this study, the results of water repellency testing using a digital swellometer method for water-borne organic-preservative systems with water repellent additives are reported. The findings suggest that the traditional method of using matched untreated controls as a reference developed from historic solvent-based treatments for determination anti-swelling efficacy (ASE) may underestimate the a...
L Jin, A F Preston
Effectiveness of sol-gel treatments coupled with copper and boron against subterranean termites
2009 - IRG/WP 09-30493
Wood modification by sol-gel treatments shows many positive features, like antimicrobial properties. Wood was also successfully modified with alkoxysilanes enhancing its resistance against soil micro-organisms. Silver, copper, zinc compounds, boric acid or organic biocides such as alkylammonium compounds may be added to the sol-gel to enhance its biocidal properties. Nevertheless, if some of these...
E Feci, L Nunes, S Palanti, S Duarte, G Predieri, F Vignali
A theoretical-industrial correlation and perspective on copper-based wood preservatives - a review of thermodynamic and kinetic aspects on copper-wood fixation mechanism
2009 - IRG/WP 09-30499
Copper was and it will continue to remain one of the key active component in wood protection industry. Over the past decades, a significant effort from R&D teams in industry, academia and research institutes was directed toward understanding the copper-wood fixation mechanism, optimising the copper retentions in the wood and reduce leaching in order to maximized performance, prolong the lifetime o...
R Craciun, M Maier, J Habicht
Leaching performance, decay and termite resistance of wood treated with boron compounds incorporated with phenol-formaldehyde resin
2009 - IRG/WP 09-30503
A resol-type phenol-formaldehyde (PF) resin was synthesized and designed to penetrate wood incorporated with boron compounds in order to immobilize boron in wood. The leaching performance, decay and termite resistance of treated wood was investigated. Three kinds of boron compounds, that is, boric acid (BA), borax (BX) and disodium octaborate tetrahydrate (DOT), were selected to mix with PF and tw...
Liping Yu, Jinzhen Cao
Resistance to decay fungi of ammonium borate oleate treated wood
2009 - IRG/WP 09-30505
Ammonium borate oleate molecule (ABO) produced from reaction between boric acid, ammonia and oleic acid was tested as wood preservative treatment against brown and white rot fungi according to European standards. This compound was prepared according to a previous study which has proved existence of synthesis reaction and effectiveness against termites (Lyon et al. 2007b). Four solutions of ABO in ...
F Lyon, M-F Thevenon, A Pizzi, J Gril
Thermal behavior of zinc borate-treated wood
2009 - IRG/WP 09-30511
The objective of this study was to investigate the thermal behavior of zinc borate (ZnB)-treated solid wood by thermal analysis (TA). Thermogravimetry (TG) and differential thermogravimetry (DTG) curves obtained from TA showed that ZnB-treated wood specimens had higher char yields and lower maximum thermal decomposition temperature than untreated wood specimens. Reducing thermal decomposition temp...
E Terzi, H Sutcu, S N Kartal