Your search resulted in 115 documents. Displaying 25 entries per page.


Determination of corrosive effect of liquid wood preservatives to metals – First experiences with a National Standard which is in revision
2006 - IRG/WP 06-20321
The development of standards is an essential tool to characterise different kind of materials and products. An important aspect during the development of a new product is to check the corrosion behaviour with other materials. Corrosion can cause several problems like pitting corrosion. Consequently the knowledge concerning the corrosive effect of liquid wood preservatives is important due to the s...
E Melcher


Some fundamental thoughts on the prediction of field performance from lab-testing based on comparison of lab and field test results of some copper-free materials
2003 - IRG/WP 03-20269
In the paper results from lab testing (ENV 807 and EN 113) are compared with field results (EN 252) of differently treated wood. Depending on the type of the organic biocide containing material and depending on type of soil and type of decay differences were found in suitability of the lab methods to predict field performance. The attempt is made to interpret the found differences. Furthermore it ...
A O Rapp, U Augusta


Wood durability in the light of recent trends and research on the durability of building materials and components
2000 - IRG/WP 00-20195
Building-related research of today demonstrates a clear shift in focus from the design and production phases to usage and to the entire life time. A consequence is that the performance criteria of materials, components and of the entire building must be regarded over the life time rather than at the time of production or delivery. As one example can be mentioned the Building Construction Directive...
K Ödeen


Information from the COIPM Wood Group
1988 - IRG/WP 4146
Abstract from the COIPM minutes: Wood in marine environment: Mrs Gambetta stated that the main item discussed by the Group was the collaborative work to test the durability of heat shrinkable polyolephin sheating materials for the protection of wood against marine organisms. The work began last year when wood samples were sent out to the participants. Three samples of Pinus sylvestris wrapped in ...
A Gambetta


A field test on susceptibility of wood-based board materials to moulds
1989 - IRG/WP 3545
A field test on susceptibility of wood-based board materials to mould growth was carried out under practical, but severe, service-conditions. A total of 19 commercially available composite boards were investigated. It was found that all board materials tested were not completely immune to mould attack. Test results revealed that among the three main categories of wood-based boards involved, partic...
Qiao Wang, B Henningsson


Information from the COIPM wood group. (With Appendix: Préserver les matériaux en milieu marin sauvegarder l'environment marin telles sont la vocation et la mission du C.O.I.P.M.)
1989 - IRG/WP 4156
During the last COIPM Meeting, up to date information on cooperative work to test the resistance of plastic wrapping for pilings were submitted and discussed. In 1986 untreated wood samples wrapped with shrinkable polyolefin sleeves were submerged in 9 stations, situated in temperate and tropical waters. After 1 or 2 years of immersion the samples showed no sign of penetration by marine borers and...
A Gambetta


Serpula lacrymans the dry rot fungus. Revue on previous papers
1989 - IRG/WP 1393
It is found that the Dry rot fungus Serpula lacrymans grows in houses only because of its need for basic materials to neutralize the oxalic acid production or heavy metals which celate the oxalic acid. The average distance from the mycelium to the basic materials is found in average to be 14.2 cm with a variation from 0-100 cm. In contrast to Serpula lacrymans the Coniophora puteana and the Rigido...
J Bech-Andersen


Compatibility of deltamethrin with wood-finishing and construction materials
1993 - IRG/WP 93-30010
Under normal use conditions, treated wood comes to close contact with the structural components of a buiLding, and/or receives finishing, forming a new interface, which can affect the performance of a new product such as deltamethrin. To study this possibility, block-tests of Parana-Pine (Araucaria angustifolia), measuring 12 x 24 x 0.5 cm³ (with the largest dimension parallel to the wood-grain),...
E S Lepage


Aquatic toxicity research of structural materials
1998 - IRG/WP 98-50114
Continuing from preliminary results reported on the aquatic toxicity of some tropical hardwoods under high hazard conditions, a more comprehensive research study is set-up in order to assess the environmental toxicology of various structural materials in water applications. Hazard class 4 preservative treated wood is tested for its toxic response on a battery of aquatic test organisms, next to con...
G M F Van Eetvelde, S De Geyter, P Marchal, M Stevens


Resistance of board materials against fungal decay: A comparative experiment on Kolle flask tests method and direct test method
1985 - IRG/WP 2243
Two sets of plywood (Aucoumea klaineana Pierre) 7 and 11 ply, treated by two preservatives, and untreated, were tested by two methods: 1. Kolle flask test method on malt-agar substrate according to the French standard NF B 51.295; 2. A direct test method in non sterile conditions according to DocNo: IRG/WP/2214. The exposure time far both methods was 12 weeks. After exposure, the degree of attack ...
G R Y Déon, L N Trong


Preservation of basidiomycete hyphae in ancient waterlogged wood materials
1992 - IRG/WP 92-1536
Studies on waterlogged archaeological wood show that basidiomycete hyphae may persist as long as 800 years. In two pine wood samples with Phellinus pini heartrot, one from the foremast of the ship Vasa and the other from a bulwark constructed in the first part of the 12th century, numerous resin covered hyphae were observed. Hyphae with clamp connections that were associated with brown and white r...
T Nilsson, G F Daniel


Control of Moisture Content in Wood Materials for Mold Growth
2007 - IRG/WP 07-10630
Mold growth on wood materials is a major concern for house owners, as it can cause health and aesthetic problems. Mold fungi, present everywhere, usually appear as black or gray patches on wood surfaces in humid environments, and are common in houses. Like any living organism, molds need food, water, oxygen, and a specific temperature range in order to grow. To avoid mold growth on wood materia...
Dian-Qing Yang


Do insects infest wood packing material with bark following heat-treatment?
2007 - IRG/WP 07-10633
As a result of international trade, many bark- and wood-infesting insects are inadvertently transported in wood packing materials (WPM) such as crating, dunnage, and pallets. WPM is suspected as the likely pathway for most of these borers, although the exact mode of entry into the USA is unknown for all 25 borers. The top 10 countries of origin were, in decreasing order, Italy, Germany, China, Spa...
R A Haack, T R Petrice, P Nzokou, D P Kamdem


Difficulties applying Heat Treatment according to ISPM No. 15, when fast growth species are used
2007 - IRG/WP 07-40386
In 2002, the Interim Commission on Phytosanitary Measures (ICPM) adopted the International Standard for Phytosanitary Measures (ISPM) No. 15 (Guidelines for regulating wood packaging material in international trade). Two treatments are recognized: Heat Treatment (HT), in which wood must be heated to a core temperature of 56°C for 30 minutes, and fumigation with methyl bromide. As the last treatme...
O Encinas, J. I Briceño


Brief introduction of a research project on the wood materials from an ancient Byzantine port unearthed during drilling for underground rail tunnel in Istanbul
2008 - IRG/WP 08-10641
A research project has been recently started to evaluate some properties of wooden materials from the biggest port of ancient times called Port of Theodosius I in Istanbul, Turkey. The ruins of the ancient Byzantine port during the excavations were recently uncovered in the Yenikapi site where an underground rail tunnel construction has been in progress in Istanbul. The wooden objects unearthed fr...
A D Dogu, C Köse, S N Kartal, N Erdin


Water Absorption of Various Building Materials and Mold Growth
2008 - IRG/WP 08-10657
Mold growth is a major problem for house owners, as it often occurs on the surface of building materials in damp houses. The principal method to control mold growth on building materials is to prevent water penetration into the materials. A study was recently conducted to determine water absorption rates of different wood species and panel materials used as building materials, when water intrusi...
Dian-Qing Yang


Eco-Friendly Composites from Bagasse and Soy-based Resin
2009 - IRG/WP 09-40462
In this study, bagasse and soy-based resin were used for producing composite materials. The objective of this study was evaluation of some physical and mechanical properties of boards made of various ratios (100:0, 60:40, 40:60 and 0:100) of bagasse to wood fiber mixtures (wt: wt) with addition of Soy/PF resin at three levels (4, 8 and 10%) and 1.5% wax. All properties were tested according to AST...
G Rassam, B Jamnani


Drying Rates and Mold Growth on Various Building Materials under Different Environmental Conditions
2010 - IRG/WP 10-20454
Mold growth on building materials is a major problem for homeowners. The most suitable method to control mold growth on building materials is to utilize design features, construction tools and practices that prevent moisture accumulation, and keep the wood as dry as possible. In order to achieve this, engineers and homebuilders have to know the effects of various temperature and moisture conditi...
Dian-Qing Yang


Mould growth on wood-based materials – a comparative study
2010 - IRG/WP 10-20455
Ten different wood-based materials - preservative-treated wood, fire retardant-treated wood, modified wood, WPCs and untreated references of pine sapwood and spruce - were tested for mould growth according to SP method 2899 during 42 days at 90% RH and 22°C. Even though the results must be interpreted carefully, they indicate significant differences in mould resistance between the materials tes...
P Johansson, J Jermer


Extruded wood plastic composites based on ACQ and MCQ-treated wood materials
2010 - IRG/WP 10-40495
This paper deals with wood plastic composites manufactured using ACQ and MCQ-treated wood fibers recovered from a wood treatment plant. The goal was to investigate the effect of coupling treatments on the properties of manufactured wood plastic composites (WPCs) through injection molding and to manufacture co-extruded WPC with treated wood fibers. The result demonstrated sound mechanical propertie...
Qinglin Wu, Fei Yao, K Ragon, J Curole, M Voitier, T Shupe


Determination of Equilibrium Moisture Content (EMC) of wood in the neighboring Countries of Iran
2011 - IRG/WP 10-40540
The mean value of annual temperature and relative humidity of 33 cities in Azerbaijan, Armenia, Turkmenistan, Afghanistan, Pakistan, Oman, United Arab Emirates, Bahrain, Qatar, Kuwait, Iraq and Turkey were determined using climatic data of the past 11 years. The EMC values were calculated using the Hailwood-Horrobin sorption model and its annual fluctuation, together with Temperature and relati...
A A Enayati, H Z Hosseinabadi


Classification of wood materials using Fourier Transform Near Infrared Spectroscopy and multivariate analysis
2011 - IRG/WP 11-20471
A distinction between preservative-treated wood and non-treated wood can be demonstrated by the combination of Fourier Transform-Near Infrared Spectroscopy (FT-NIRS) and Multivariate Analysis (MVA). This technique is non-destructive, quick, easy to use and can be portable. The calibration models for different heavy metals are set up using principal component analysis (PCA) to classify species of t...
M A Bouslamti, M A Irle, C Belloncle, V Salvador, S Hulot, B Caron, E M Qannan


Life Cycle Assessment Comparison of Treated Wood to Alternate Materials – Overview, Results and Lessons
2011 - IRG/WP 11-50282
Life Cycle Assessment (LCA) has proven useful in documenting the “green” benefits of various treated products compared to the commonly used alternates. To date, six LCA comparisons have been done or are nearing completion using ISO14040 and 14044 principles and data from US EPA databases. In almost all cases, the impact indicators for treated wood products show considerably smaller adverse e...
T Stephen, P E Smith, C R McIntyre


Mould growth on wood-based materials – a simulated in-service study
2012 - IRG/WP 12-20503
Ten different wood-based materials including preservative-treated wood, fire retardant-treated wood, modified wood, WPCs and untreated references of pine sapwood and spruce were placed in three different environments (an attic and two crawl spaces) for a period of 26 months. Mould growth was analysed at five to seven month intervals in an effort to map the growth development. The relative humidit...
G Bok, P Johansson, J Jermer


Communities of mold fungi on flooded building materials
2013 - IRG/WP 13-10799
A small building built to residential code was flooded using farmland pond water to a depth of two feet at Tuskegee University. The building was drained and left enclosed for an additional three weeks. A total of 168 material samples were removed either immediately after opening (wet) or seven months after flooding (dry). Wall materials sampled included fiberglass batt insulation, gypsum wallboard...
F Skrobot III, H Aglan, S V Diehl


Previous Page | Next Page