Your search resulted in 160 documents. Displaying 25 entries per page.


Effects of artificial UV weathering and soft rot decay on heat treated wood
2005 - IRG/WP 05-40302
Oil and inert gas oven heat treated pine wood strips 100 µm thick were mildly heat treated (200°C, 30 mins linseed oil, 120 mins oven). Following treatment, specimens were exposed to UV weathering (300 hours) and decay by the soft rot fungus, Chaetomium globosum. The effects of each treatment were assessed by zero span tensile testing, microscopy and by FTIR. Tensile testing of heat treated s...
M D C Hale, S C Ghosh, M J Spear


Decay types observed in small stakes of pine and Alstonia scholaris inserted in different types of unsterile soil
1990 - IRG/WP 1443
The attack of various wood-degrading microorganisms occurring in mini-stakes of pine and Alstonia scholaris buried in various types of unsterile soil was studied. Attacks by white rot, brown rot, soft rot, erosion bacteria, tunnelling bacteria and actinomycetes were found. Soft rot occurred in all soils, whereas attack by white rot and especially brown rot and erosion bacteria was rare. The type o...
T Nilsson, G F Daniel


Comparisons of differences in electrical conductivity and corrosivity between CCA-oxide and CCA-salt treated wood
1981 - IRG/WP 3178
CCA preservatives have served well in many applications throughout the world. In developed areas it is the preservative in demand for clean dry paintable surfaces with long durability. In developing areas it is widely used for economic and logistical reasons. With the current emphasis on energy resources, the CCA preservatives are gaining greater acceptance as a substitute for hydrocarbon-related ...
J A Taylor


Studies on the fungicidal effectiveness of a petrol derived product as a creosote alternative
1986 - IRG/WP 3384
This work, appears first because of the necessity to find out a profitable use for a residual product of the petrol pyrolisis, and second, because the lack of high natural durability wood used until now-a-days to build posts and sleepers in creosote lacking countries. Our main objective was pointed to the characterization of this new product and to find out the effectiveness against the wood-destr...
A M Navarrete, M T De Troya.


Preservative effectiveness of medium temperature creosote oil
1990 - IRG/WP 3597
Medium temperature creosote oil (MTC) was prepared by removing light naphthalene oil and heavy anthracene oil from the coal tar by means of fractional distillation. We conducted the effectiveness test of MTC in accordance with the JWPA method for testing effectiveness of surface coatings with preservatives against decay fungi. The soil treatment test against Serpula lacrymans was also carried out ...
S Doi, A Yamada, Y Suda


Fungus cellar and field tests with tall oil derivatives. Final report after 11 years' testing
1993 - IRG/WP 93-30007
Two derivatives of tall oil were tested as wood preservatives in a fungus cellar and in ground contact (field test). Stakes of Pinus sylvestris sapwood were used in the tests. For the field test the size of the stakes was 20 x 50 x 500 mm³ and for the fungus cellar test 20 x 20 x 250 mm³. The stakes were vacuum-pressure treated with the two products and exposed in 1981. The field test site used ...
J Jermer, Ö Bergman, T Nilsson


Properties of hot oil treated wood and the possible chemical reactions between wood and soybean oil during heat treatment
2005 - IRG/WP 05-40304
Thermal treatment with hot oil as the heating media based on the original idea from oil-heat treatment in Germany was investigated. The treatment was mainly carried out at 200ºC and 220ºC for 2 hours and 4 hours, and the wood species were mainly spruce and fir. This paper focuses on the difference between soybean oil and palm oil and the possible chemical reactions between wood and soybean oil. ...
Jieying Wang, P A Cooper


Diffuse cavity formation in soft rot of pine
1992 - IRG/WP 92-1541
A new type of soft rot of southern pine longitudinal tracheids is described. In this type, soft rot cavities form by diffuse degradation of the S2 cell wall layer by hyphae growing within the cell wall. Erosion is diffuse and irregular as opposed to the restricted, periodic erosion typical of type 1 soft rot cavity formation. Proboscis hyphae remain small (diameter 0.6 to 0.8 µm) and rapidly auto...
S E Anagnost, J J Worrall, C J K Wang


Construction of dhows in Kuwait
1981 - IRG/WP 465
To most people Kuwait means oil and the opulence associated with it, but to the seafarer, Kuwait means Dhows. There are as early references to the Kuwaiti Dhows as the 17th century. The Danish explorer Nebuhr in 1756 described Kuwait as having a work power of 10,000 people and 800 wooden boats involved in fishing, pearl diving, and trade. Dhows might well have been the original carriers of "The Pe...
A S Zainal, M A Ghannoum


Performance of preservative-treated timber against biodeterioration in Indian waters
1984 - IRG/WP 4106
Results on the investigation on the durability of panels of 32 timber species, pressure-treated with various preservatives and exposed along the Indian coast for varying periods upto a maximum of 15 years, are summarised. Panels of even non-durable timber gave excellent results against biodeterioration after treatment. Their life was comparable to that of treated durable timber. The preservative t...
L N Santhakumaran, J C Jain, M C Tewari


Decay resistance of densified ammonia-plasticized stems of oil palm (Elaeis guineensis)
1991 - IRG/WP 3673
When wafers of oil palm stems (Elaeis guineensis) were plasticized with 28% aqueous ammonia and immediately compressed mechanically, the treated material, gained 73% in basic density (average basic density, 0.695 g/cm³), and was highly resistant to decay by wood rot basidiomycetes. Compared with the control specimens (density, 0.403 g/cm³), resistance to decay of the densified specimens by Corio...
A H H Wong, M P Koh


Biological resistance of wood treated with waterbased resins and drying oils in a mini-block test
1998 - IRG/WP 98-40107
In recent years it was found that the resistance of wood against fungal degradation could be increased by impregnation with an etherificated melamine formaldehyde resin. Using this resin as a reference, a waterbased fatty acid modificated alkyd-resin and two drying-oils were assessed for their biological performance in a mini-block laboratory test. Although drying-oils, like linseed-oil, are often...
M Sailer, A O Rapp, R-D Peek


Screening of the efficacy of tall oils against wood decaying fungi
2004 - IRG/WP 04-30354
Tall oil is a by-product in pulping of resinous wood by the sulphate process. Tall oil contains a complex mixture of wood extractives. Some of these extractives act as natural protection against wood decaying fungi while other serve as nutrition for the fungi. This report describes a screening of the efficacy of four refined tall oils with different chemical composition on wood decaying fungi. ...
G Alfredsen, P O Flæte, A Temiz, M Eikenes, H Militz


Interim balance after 20 months of lap-joint exposure
1999 - IRG/WP 99-20164
The application of natural resins and integrated resin systems to improve the performance of Pinus sylvestris was assessed in a lap-joint test according to DIN V ENV 12037 (1996). Lap-joints of Pinus sapwood were exposed at the test field in Hamburg (Germany) in May 1997. The treated lap-joints were assessed with regard to the performance of the resin treatments out of ground. The exposure of lap-...
M Sailer, A O Rapp, R-D Peek, A J Nurmi, E P J Beckers


Evaluation of outdoor weathering performance of modified wood
2004 - IRG/WP 04-20296
Interlace treated, oil treated, silicon treated as well as untreated Scots pine samples have been exposed outdoors. For evaluating the samples on their long term performance an internal standard had been developed. Parameters to be determined were the uptake of liquid water (submersion test), weight variation during exposure, crack performance, surface roughness and colour change. This paper disc...
Y Schulte, S Donath, A Krause, H Militz


Observations on the destruction of fishing craft in India by marine wood-borers with special reference to the West Coast
1981 - IRG/WP 468
The paper highlights the economic importance of the destruction of fishing craft in India by marine wood-destroying agencies. The annual loss involved is to the extent of over 94 million rupees. Thirty-nine spectes and one variety of woodborer have so far been recorded from India, of which Bankia campanellata, Bankia carinata, Bankia rochi, Dicyathifer manni, Lyrodus pedicellatus, Teredo clappi, T...
L N Santhakumaran, J C Jain


World list of wood preservative names
1980 - IRG/WP 387
The list contains names that have been collected by the author over many years and includes besides traditional wood preservatives, exterior wood finishes and preservative stains, and some preservative coatings. Generally, however, primers and paints have been deliberately excluded. The list includes also products that have been claimed as wood preservatives, as well as a few fire-retardant coatin...
R Cockcroft


The evaluation of the effectiveness of wood preservatives by means of IUFRO's method for field tests with wooden stakes
1985 - IRG/WP 3348
Pinus elliottii and Eucalyptus saligna stakes treated with CCA-A, CCA-C, CCB, Cashew Nut Shell Oil and Benzotar solutions were exposed in seven test sites in Sao Paulo State, Brazil. After five years of exposure, between oil-borne preservatives Benzotar show better performance than CNSL (cashew nut shell liquid), and within waterborne preservatives the performance of CCB is not so good as that of ...
G A C Lopez, A M F Oliveira, E S Lepage


Evaluation of copperised Cashew nut shell liquid and Neem oil as wood preservatives
2005 - IRG/WP 05-30368
An effort has been made to develop eco-friendly wood preservatives using naturally available plant by-products with less toxicity. Copper was incorporated into Cashew nut shell liquid (CNSL) and Neem seed oil. Rubber wood samples were treated with these solutions employing dipping and pressure techniques in 3 different levels. These samples have been evaluated to find out the effectiveness as wood...
D Venmalar, H C Nagaveni


Screening of modified linseed oils on their applicability in wood protection
2004 - IRG/WP 04-30346
In this study modified linseed oils, rape oil and three waxes were screened on their efficacy as wood protecting agents. By testing all products when impregnated with high retentions in Scots Pine sapwood on water repellence qualities, additionally an accelerated weathering test, drying quality, accelerated brown rot and blue stain test, an indication is formed of the capability of these products ...
A Treu, J Lückers, H Militz


Fungicidal properties of wood tar being a side product of pyrolysis of previously treated wood with preservatives
2004 - IRG/WP 04-30340
The objective of the paper was to estimate the limit of the fungicidal value of wood tar being a product of pyrolysis of wood previously treated with creosote oil or salt preservative of the CCB type. The effectiveness of wood tar in wood protection against fungi causing brown rot and soft rot was compared to the effectiveness of creosote oil (type WEI-B). Wood was impregnated with alcohol solutio...
B Mazela, M Kielczewski, W Grzeskowiak


Fixation of CCA preservatives in cocos-, oil- and rattan-palm
1986 - IRG/WP 3371
In previous tests with jubaea-palm almost no fixation of a CCA-preservative Type B could be achieved, consequently, further leaching tests were carried out with samples of 1 cocos-, 1 oil- and 2 rattan-palms from Malaysia. A good fixation of chromium and copper took place in cocos-palm after 4 weeks storage at 28°C. Nevertheless the fixation was slower than in pine-wood and demanded an elevated t...
H Willeitner, K Brandt


Effectiveness of wood preservatives by IUFRO's method
1984 - IRG/WP 3305
Pinus elliottii and Eucalyptus saligna stakes treated with 4.9; 6.9; 9.6 and 13.5 kg/m³ of CCA-A, CCA-C and CCB and with 30-50; 60-80; 90-110 and 120-140 kg/m³ of Benzotar and CNSL (cashew-nut shell liquid) were exposed in seven test sites in Sao Paulo State, Brazil. After 4 years it was concluded that the mean useful life of untreated Pinus elliottii stakes was 8 months and of untreated Eucalyp...
G A C Lopez, E S Lepage, O B Neto


Effect of crude tall oil, linseed oil and rapeseed oil on the growth of the decay fungi
2002 - IRG/WP 02-30299
The influence of crude tall oil, linseed oil and rapeseed oil on the growth of Coniophora puteana, Poria placenta and Coriolus versicolor was studied. The selected test oils were observed to have different effects on the the fungal growth. Crude tall oil inhibited the radial growth of all fungi. Rapeseed oil either accelerated or inhibited the growth of fungi depending on the type of fungus involv...
L Paajanen, A-C Ritschkoff


Service Life Prediction of Wood Claddings by in-situ Measurement of Wood Moisture Content
2004 - IRG/WP 04-20304
The Danish Technological Institute is in co-operation with industry partners running a project aiming at predicting the service life of different wood protecting systems. The project focuses on examining the moisture reducing effect of different wood claddings and the ability to maintain the appearance of the surfaces, when the wood is used in service class 3. A façade construction is exposed t...